ASME SA213 UNS S30615 high-silicon aluminium-bearing austenitic seamless boiler, superheater and heat-exchanger tube — C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17.0–19.5%, Ni 13.5–16.0%, Table 4 90/40 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal with Footnote F. No TP letter — order by UNS. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Si and Al together.
Grade
UNS S30615 (no TP letter — high-Si Al austenitic)
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 UNS S30615 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers, process heaters, or heat exchangers invoke that adoption by name, SA-213 is the governing product standard for this high-silicon, aluminium-bearing austenitic tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

UNS S30615 sits in the stainless chemistry table without a TP grade letter (Footnote C practice). Melting carbon is held in a 0.16–0.24% band, silicon in a deliberate 3.2–4.0% window, aluminium at 0.8–1.5%, chromium at 17.0–19.5%, and nickel at 13.5–16.0%, with phosphorus and sulfur each capped at ≤0.030%. Molybdenum, nitrogen, niobium, and titanium have no requirement on the public row. Table 4 sets tensile at 90 ksi [620 MPa] / 40 ksi [275 MPa] with elongation 35% minimum and hardness max 192 HBW / 90 HRB. Buyers who write “RA85H” or “high-Si Al HX tube” on a bill of materials still need to name SA-213 UNS S30615 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the Si/Al windows together. This is not a dual stamp of SA213 TP XM-15 (Si 1.50–2.50%, no Al) or of TP310S.

SHH STEEL can supply ASME SA213 UNS S30615 as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report the silicon and aluminium windows together with the 90/40 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 UNS S30615.

Shop names include “S30615,” “RA85H,” and “high-Si Al 18Cr.” Helpful for routing; the commercial nickname does not replace UNS S30615 on the MTC. The purchase order should still carry ASME SA-213 UNS S30615, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements when needed. Sister SA213 pages include SA213 TP304, SA213 TP310S, SA213 TP XM-15, and SA213 UNS S30815 when that pack is live. Seamless only — no Manufacturing Types (SML / WLD / HCW) product-form split on this page.

Chemical Composition of SA213 UNS S30615

Two chemistry layers matter for UNS S30615 under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The defining package for a reviewer is silicon 3.2–4.0% together with aluminium 0.8–1.5%, carbon 0.16–0.24%, chromium 17.0–19.5%, and nickel 13.5–16.0% — not a classic 18-8 window and not the XM-15 Si/Ni story. Phosphorus and sulfur are each capped at 0.030%. There is no mandatory Mo, N, Nb, or Ti band on the public row.

The tables below reproduce the melt limits for UNS S30615, the product-analysis limits from A480 Table A1.1 practice, and a short Si/Al snapshot against XM-15 and related high-temperature grades. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. UNCERTAIN: the public PDF OCR line for carbon reads “0.016–0.24”; mill / RA85H cross-checks and the intended high-carbon heat-resistant band support 0.16–0.24 — confirm the ordered Code Book digit before heat selection. Exact edition year and stainless chem table number are also UNCERTAIN until the PO names them.

Melting analysis (heat / ladle analysis)

Element UNS S30615 melting analysis
Carbon (C) 0.16 – 0.24 (UNCERTAIN vs OCR 0.016–0.24 — confirm edition)
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.030
Silicon (Si) 3.2 – 4.0
Chromium (Cr) 17.0 – 19.5
Nickel (Ni) 13.5 – 16.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb) … (no requirement)
Titanium (Ti) … (no requirement)
Aluminum (Al) 0.8 – 1.5

Source: public SA-213 / A213 stainless chemistry table for UNS S30615 (same grade text family; public A213/A213M − 13 excerpt). Every controlled element — especially Si and Al — must appear on the certificate; an MTC that omits aluminum is incomplete for S30615. Where ellipses appear, the ordered edition sets no requirement for that element.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.16 – 0.24 0.01 under / over 0.15 – 0.25
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.030 0.005 over ≤ 0.035
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) 3.2 – 4.0 0.10 under / over (high-Si practice) 3.10 – 4.10 (confirm A480 edition)
Chromium (Cr) 17.0 – 19.5 0.20 under / over 16.80 – 19.70
Nickel (Ni) 13.5 – 16.0 0.15 under / over 13.35 – 16.15
Aluminum (Al) 0.8 – 1.5 0.05 under / over (practice) 0.75 – 1.55 (UNCERTAIN — confirm A480)

Product analysis is not automatic — order it when the project needs finished-tube chemistry, especially the silicon and aluminium windows. UNCERTAIN: A480 product-tolerance digits for the high-Si band and for aluminium should be confirmed against the ordered A480 edition if the PO makes product analysis contractual.

Si / Al snapshot — XM-15 / S30615 / S30815

Element XM-15 (S38100) S30615 S30815
Si 1.50 – 2.50 3.2 – 4.0 1.40 – 2.00
Al none required 0.8 – 1.5 none required
Ce / N none required none required Ce 0.03–0.08 / N 0.14–0.20
Ni 17.5 – 18.5 13.5 – 16.0 10.0 – 12.0

Reading tip: a heat that clears XM-15 still fails S30615 if silicon sits near 2% or aluminium is absent. Do not accept a verbal “high-Si furnace tube” shop note as proof that the MTC prints S30615 with the Si and Al windows satisfied.

Mechanical Properties of SA213 UNS S30615

Table 4 of the public SA-213 / A213 grade text family sets UNS S30615 tensile strength at 90 ksi [620 MPa] minimum and yield (0.2% offset) at 40 ksi [275 MPa] minimum — above the 75/30 ksi floors used for TP304 and XM-15 under the same product standard. Elongation in 2 in. or 50 mm is 35% minimum, and hardness is capped at 192 HBW / 200 HV or 90 HRB. The higher tensile/yield pair reflects the Si–Al strengthening and the higher carbon band; hardness stays at the familiar commodity austenitic ceiling rather than stepping to a higher HBW row.

Property UNS S30615 requirement (Table 4)
Tensile strength, min 90 ksi [620 MPa]
Yield strength (0.2% offset), min 40 ksi [275 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number

S30615 has no mandatory ASTM grain-size number in the heat-treatment column. If a project datasheet asks for an E112 grain-size report, put that supplementary requirement on the purchase order rather than assuming base SA-213 includes it. Mechanical property requirements generally do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring follow the general requirements for the ordered size; hydrostatic or nondestructive examination follows the path selected on the PO. Do not accept an XM-15 or TP304H certificate as S30615 clearance — aluminium, the 3.2–4.0% silicon band, the carbon range, and the 90/40 ksi pair must all match.

Dimensions and Tolerances

Dimensional supply for ASME SA213 UNS S30615 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Furnace, boiler, and heat-exchanger datasheets that pick high-Si Al S30615 usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The Si/Al package does not change the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 UNS S30615 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for furnace / HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the silicon and aluminium window checks.

Equivalent Grades

Equivalence talk for S30615 should start from the Code Book product standard and the UNS, not from the commercial RA85H nickname. ASME SA-213 UNS S30615 is the governing designation on this page. ASTM A213 UNS S30615 is the separate ASTM twin used when dual marking or a non-Code purchase is agreed — it is not a substitute lead standard for an SA-213 order. Related high-Si or high-temperature grades (XM-15, S30815, TP310S) are sister options under the same hub family, not automatic dual stamps.

Designation Notes
ASME SA-213 / SA-213M UNS S30615 Governing Code Book seamless boiler / HX tube product standard for this article
UNS S30615 Unified number — no TP letter (Footnote C)
RA85H (commercial) Shop name for the high-Si Al chemistry family — does not replace S30615 on the MTC
ASTM A213 UNS S30615 Separate ASTM product specification — dual-mark only when the PO asks; twin page A213 UNS S30615
Related high-Si (no Al) SA213 TP XM-15 — Si 1.50–2.50%, Ni 17.5–18.5%; not interchangeable
Related Ce–N grade SA213 UNS S30815 — Ce–N package; separate chemistry story
Related plate A240 / SA240 flat product in related high-Si families — order plate and tube under their own standards

Hub entry point: SA213/SA213M. When a bill of materials only says “RA85H,” ask whether Si 3.2–4.0% and Al 0.8–1.5% are actually required before shipping S30615 or an XM-15 / TP310S alternative.

Heat Treatment and Delivery Condition

UNS S30615 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries Footnote F for this grade: quench rate must be sufficient to prevent carbide re-precipitation, as demonstrable by the capability of tubes — heat treated by separate solution annealing or by direct quenching — to pass Practices A262, Practice E. The manufacturer is not required to run the A262 test unless the purchase order specifies it (see Supplementary Requirement S4).

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. High-silicon, aluminium-bearing austenitics need a thorough solution treatment so Si and Al stay distributed rather than forming unwanted phases that cut toughness or oxidation performance. Delivery condition for SHH STEEL S30615 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature and quench method on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

S30615 has no mandatory ASTM grain-size number in the heat-treatment column. If a project datasheet asks for an E112 grain-size report, put that supplementary requirement on the purchase order rather than assuming base SA-213 includes it. Do not treat a verbal “annealed RA85H” note as proof that the mill ran the 1900 °F SA-213 path with Footnote F quench capability. UNCERTAIN: full Footnote F / S4 wording on the ordered edition — confirm against the Code Book text named on the PO.

Corrosion Resistance

S30615 under ASME SA-213 is selected primarily for high-temperature oxidation, scaling, and carburization resistance associated with elevated silicon plus aluminium — furnace and process-heater framing — not as a general wet-chloride upgrade over TP304 or TP316. The Si 3.2–4.0% band with Al 0.8–1.5% supports oxide-scale adherence and carburization resistance relative to low-silicon 18-8 in many dry or mildly oxidizing services, but the grade is not a duplex or molybdenum-bearing superaustenitic for aggressive aqueous chlorides.

Where a datasheet mixes “RA85H” with wet process condensates or chloride deposits, ask whether the service is actually looking for a molybdenum-bearing or duplex tube instead of a high-Si Al austenitic. SHH STEEL will not treat a silicon PMI peak alone as proof of aqueous corrosion suitability — chemistry, heat treatment, and the intended medium have to be read together. For Ce–N high-temperature framing without aluminium, open SA213 UNS S30815.

Applications of SA213 UNS S30615 Tube

Typical ASME SA213 UNS S30615 placements are Code-stamped boiler, superheater, process-heater, and heat-exchanger tubes where the material list names S30615 or explicitly requires Si 3.2–4.0% with Al 0.8–1.5% — not generic “304 family,” “XM-15,” or “310” replacements. Furnace coils and high-temperature HX bundles that already distinguish RA85H-class chemistry from TP304 or XM-15 are the natural fit.

When the enquiry only says “high-Si Al tube” without UNS language, confirm whether the buyer actually needs SA213 TP XM-15, SA213 TP310S, or the Ce–N grade before substituting. SHH STEEL quotes S30615 when the enquiry names the UNS or the Si/Al package explicitly.

Weldability

S30615 welds as a high-silicon, aluminium-bearing austenitic. Filler selection should respect the elevated silicon and aluminium rather than copying a plain ER308 procedure without review. Matching or near-matching austenitic fillers with adequate silicon are the usual starting point; confirm chemistry against the WPS when the project treats Si/Al as contractual on the weld metal as well as the tube.

Autogenous welds and thin-wall HX joints need heat-input control to protect the as-annealed condition near the HAZ. Post-weld heat treatment is not a default SA-213 requirement for this grade — if the vessel code or the buyer wants a separate resolution anneal after welding, write that as a negotiated step. SHH STEEL can coordinate weld coupons when the PO asks.

Surface Finishes

Standard mill delivery for ASME SA213 UNS S30615 is solution annealed and pickled, leaving a clean matte finish suitable for furnace, boiler, and heat-exchanger tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the silicon and aluminium window checks. End caps and dry export packaging matter more than paint on pickled stainless. SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for UNS S30615 includes heat analysis (C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17.0–19.5%, Ni 13.5–16.0%, P/S ≤0.030%), tension tests to the 90/40 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm the silicon and aluminium windows rather than trusting an “RA85H” shop nickname or a TP304-family PMI without Si ≥3.2% and Al present. Product analysis, when ordered, applies A480 tolerances with Si and Al digits noted as UNCERTAIN above if the ordered A480 edition differs. A262 Practice E applies only when S4 is named on the PO. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

S30615 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 UNS S30615, heat number, size, and wall basis so receivers can match the 3.1 certificate — including Si and Al — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 UNS S30615 only when dual ASTM marking was ordered. The commercial RA85H nickname may appear in packing notes for routing, but the stencil and MTC still carry UNS S30615.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 UNS S30615 as a Code Book high-silicon aluminium-bearing product with enforceable C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17–19.5%, Ni 13.5–16%, P/S ≤0.030%, 90/40 ksi tensile, 35% elongation, hardness, and marking rules — not as “XM-15 with more silicon” checked only by a Si PMI peak. Enquiry review verifies the silicon and aluminium windows before release.

That stops silent substitution with XM-15 or TP310S heats on datasheets that actually require S30615. We keep SA-213 and A213 independent, dual-mark only on request, and put Si and Al on the 3.1 certificate so inspectors can verify the grade. The commercial RA85H nickname is allowed for routing — it never replaces S30615 on the MTC.

Cross-links: SA213 TP XM-15, SA213 TP310S, SA213 UNS S30815, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 UNS S30615 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for high-Si Al furnace and heat-exchanger tube.

Item SHH STEEL capability for UNS S30615
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade UNS S30615 (no TP letter)
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for furnace / HX bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Si / Al windows; S4 A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S30615 against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for high-Si Al furnace and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common furnace / HX band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX / furnace wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, length mix, finish route, and any dual-mark or A262 needs with the RFQ so we can align mill capacity to the Si/Al package on the first reply.

FAQ

Is ASME SA-213 the same as ASTM A213 for UNS S30615?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17.0–19.5%, Ni 13.5–16.0%, and P/S ≤0.030% — tensile 90/40 ksi, elongation 35%, and hardness floors align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 UNS S30615 have a TP grade letter?
No. S30615 appears in the stainless chemistry table without a TP letter (Footnote C practice). Order and mark by UNS S30615 under ASME SA-213 / SA-213M. Do not invent a “TP30615” stencil or assume the grade dual-stamps as TP304, XM-15, or TP310S. The purchase order and MTC should carry the UNS designation explicitly so inspectors can match chemistry and tensile to the correct row.
Is RA85H the same as ASME SA213 UNS S30615?
RA85H is a commercial shop name for the high-Si Al chemistry family around S30615. It is useful for routing, but it does not replace ASME SA-213 UNS S30615 on the purchase order or the MTC. SHH STEEL will stencil and certify UNS S30615; packing notes may mention RA85H only as a buyer routing aid when requested. Always confirm Si 3.2–4.0% and Al 0.8–1.5% against the certificate.
How does S30615 differ from XM-15 under SA-213?
S30615 carries a much higher silicon band (3.2–4.0%) plus aluminium 0.8–1.5%, with nickel 13.5–16.0% and a 90/40 ksi tensile floor. XM-15 uses Si 1.50–2.50% and Ni 17.5–18.5% without mandatory aluminium, at 75/30 ksi. They are related high-Si concepts, not dual stamps. If the material list names aluminium or Si above 3%, review S30615 instead of assuming XM-15 covers it.
What hardness limit applies to ASME SA213 UNS S30615 tube?
Table 4 caps S30615 hardness at 192 HBW / 200 HV or 90 HRB — the same ceiling as many commodity austenitics, even though tensile sits at 90/40 ksi. Hardness is checked together with the tensile set and 35% elongation. A hardness result alone does not prove Si/Al compliance; certificate reviewers should still read the silicon and aluminium windows on the MTC.
What heat treatment applies to SA213 UNS S30615?
Solution treatment at a minimum of 1900 °F [1040 °C] followed by rapid cooling is the public path, with Footnote F quench-capability language tied to A262 Practice E demonstrability when that test is ordered. The manufacturer is not required to run A262 unless Supplementary Requirement S4 is on the purchase order. There is no mandatory ASTM grain-size number for this grade in the public heat-treatment column.
Should I order minimum wall or average wall for S30615?
Furnace, boiler, and heat-exchanger datasheets that pick S30615 usually assume minimum wall. Average wall is acceptable when the purchase order says so and the general requirements for the ordered finish are applied. State wall basis, OD × wall or BWG, and length mix on the RFQ so the mill does not default to a basis your inspector will reject at receiving.
Is S30615 suitable for wet chloride heat-exchanger service?
Not as a default upgrade. S30615 is framed for high-temperature oxidation, scaling, and carburization resistance with elevated silicon and aluminium. Aggressive aqueous chlorides usually need molybdenum-bearing, duplex, or other project-specified alloys instead of a high-Si Al austenitic. Ask for a corrosion review before substituting S30615 into a wet-chloride HX datasheet that never named the UNS.
Does ASME SA213 UNS S30615 cover welded or HCW tube?
No. ASME SA-213 for this stainless series is a seamless boiler, superheater, and heat-exchanger tube product standard. SHH STEEL supplies S30615 as seamless cold-finished or hot-finished tube only. Welded (WLD) or heavily cold-worked welded (HCW) manufacturing types are outside this page’s product form and are not offered as a Manufacturing Types split under the SA213 UNS S30615 listing.
Can SHH STEEL dual-certify SA-213 and A213 for S30615?
Yes, when the purchase order asks for dual marking and the heat meets both product standards’ grade text for UNS S30615. Dual marking is a documentation and stencil option — it does not merge the two standards into one title. For non-Code purchases that only want the ASTM twin, see A213 UNS S30615; for Code-led work, keep SA-213 as the lead standard on the PO.
Why is the carbon range for S30615 marked UNCERTAIN on this page?
The public PDF OCR excerpt for the stainless chemistry table reads “0.016–0.24,” while mill practice and RA85H-class cross-checks support the high-carbon heat-resistant band 0.16–0.24%. SHH STEEL labels that digit UNCERTAIN and asks buyers to confirm the ordered SA-213 / A213 edition before heat selection. Do not treat either OCR reading as final without the edition named on the purchase order.

Conclusion

ASME SA213 UNS S30615 is the high-silicon aluminium-bearing seamless stainless steel tube grade for Code boiler, superheater, furnace, and heat-exchanger service when C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17.0–19.5%, Ni 13.5–16.0%, P/S ≤0.030%, a 90/40 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal with Footnote F are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the Si and Al windows. The commercial RA85H nickname does not replace UNS S30615 on the certificate. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X