ASME SA213 TP347LN Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP347LN Stainless Steel Tube

ASME SA213 TP347LN / UNS S34751 ultra-low-carbon niobium-stabilized nitrogen-bearing seamless boiler, superheater and heat-exchanger tube — C 0.005–0.020%, N 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb 0.20–0.50% and ≥15×C, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnote F). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the C / N / Nb package.
Grade
TP347LN / UNS S34751
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP347LN Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped exchangers or registered systems invoke that adoption by name for ultra-low-carbon niobium-stabilized service, SA-213 is the governing product standard for this LN tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP347LN / UNS S34751 combines an ultra-low carbon band 0.005–0.020%, intentional nitrogen 0.06–0.10%, and niobium held both in a fixed 0.20–0.50% band and at ≥15 × C per Footnote F. Chromium sits at 17.0–19.0% and nickel at 9.0–13.0%. Table 4 keeps the 75/30 ksi tensile pair with 35% elongation and hardness max 192 HBW / 90 HRB — nitrogen recovers strength that a bare ultra-low-C melt would otherwise lose. This is not a dual stamp of TP347, TP304LN, or TP347H.

SHH STEEL can supply ASME SA213 TP347LN as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report carbon inside 0.005–0.020%, nitrogen inside 0.06–0.10%, niobium inside 0.20–0.50% and clearing ≥15 × C, and the 75/30 ksi tensile set. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP347LN.

Shop names include “347LN,” “S34751,” and “low-carbon Nb 347 with nitrogen.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP347LN / UNS S34751, wall basis, OD × wall or BWG, finish route, nitrogen analysis method when contractual (Footnote B), and any Supplementary Requirements. Sister SA213 pages include SA213 TP347, SA213 TP347H, SA213 TP304LN, and SA213 TP347HFG. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP347LN

Two chemistry layers matter for TP347LN under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. Three lines define the grade for a reviewer: carbon locked inside 0.005–0.020% (tighter than any L-grade ceiling alone), nitrogen 0.06–0.10%, and niobium held both in a fixed 0.20–0.50% band and at ≥15 × C per Footnote F. A heat with 0.015% carbon needs at least 0.225% Nb from the formula and still must land inside 0.20–0.50%; a heat at the carbon ceiling of 0.020% needs at least 0.30% Nb. Chromium 17.0–19.0% is narrower than TP347’s 17.0–20.0% window.

The tables below reproduce the melt limits for TP347LN / UNS S34751, the product-analysis limits from A480 Table A1.1 practice, and a short C/N/Nb snapshot against TP347, TP304LN, and TP347H. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. Nitrogen analysis method is a matter of agreement (Footnote B) — write the method on the PO when N is contractual.

Melting analysis (heat / ladle analysis)

Element TP347LN (UNS S34751) melting analysis
Carbon (C) 0.005 – 0.020
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.06 – 0.10
Niobium (Nb / Cb) 0.20 – 0.50 and ≥ 15 × C (Footnote F)
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for Grade TP347LN / UNS S34751 (same grade text family). Confirm the ordered edition. UNCERTAIN: exact edition year; stainless chem table number; Footnote B nitrogen analysis method wording when N is contractual.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.005 – 0.020 0.005 under / over (tight low-C band practice) 0.000 – 0.025 (confirm A480 edition)
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Nitrogen (N) 0.06 – 0.10 0.01 under / 0.02 over (sister LN practice) 0.05 – 0.12
Niobium (Nb) 0.20 – 0.50 and ≥ 15 × C 0.05 under / over on band (Nb range practice) 0.15 – 0.55 product band; formula min still tied to heat C

UNCERTAIN: A480 product-tolerance digits for the ultra-low C band and the fixed Nb 0.20–0.50 band — confirm against the ordered A480 edition when product analysis is invoked.

C / N / Nb snapshot — TP347 / TP347LN / TP304LN / TP347H

Element TP347 (S34700) TP347LN (S34751) TP304LN (S30453) TP347H (S34709)
C ≤ 0.08 0.005 – 0.020 ≤ 0.035 0.04 – 0.10
N … (no req.) 0.06 – 0.10 0.10 – 0.16 … (no req.)
Cr 17.0 – 20.0 17.0 – 19.0 18.0 – 20.0 17.0 – 19.0
Ni 9.0 – 13.0 9.0 – 13.0 8.0 – 11.0 9.0 – 13.0
Nb / stabilizer ≥ 10 × C, ≤ 1.10 0.20 – 0.50 and ≥ 15 × C none (N strengthens) ≥ 8 × C, ≤ 1.10

Do not treat TP347LN as a dual stamp of SA213 TP347 or SA213 TP304LN. TP347 allows higher carbon with a 10 × C Nb formula and no mandatory nitrogen band; TP304LN strengthens with nitrogen but carries no niobium. Dual TP347LN/TP347H is blocked by carbon bands that do not overlap.

Mechanical Properties of SA213 TP347LN

ASME SA-213 Table 4 sets the tensile acceptance floor for TP347LN / UNS S34751 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB — the same room-temperature pair as TP347 and TP304 despite the ultra-low carbon, because intentional nitrogen recovers strength that a bare low-C melt would otherwise lose. The public heat-treatment table does not print a mandatory ASTM grain-size number for TP347LN (unlike TP347H’s “7” and TP347HFG’s “7–10”), so a tensile-and-hardness MTC without grain size can still be complete unless the purchase order adds a grain-size Supplementary Requirement.

Property TP347LN requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM number in the public Table 3 row (confirm ordered edition)

Source: public SA-213 / A213 Table 4 for UNS S34751 / TP347LN. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits carbon, nitrogen, or niobium is incomplete for TP347LN. For H-grade grain-size and carbon-floor framing open SA213 TP347H; for standard Nb framing open SA213 TP347.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP347LN is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Heat-exchanger datasheets that pick ultra-low-C Nb-stabilized tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The C / N / Nb package does not change the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 TP347LN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX / boiler datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the C / N / Nb package check.

Equivalent Grades

Equivalence language around 347LN tube often collapses it with non-H 347 or with nitrogen-only LN grades. ASME SA-213 Grade TP347LN / UNS S34751 is the governing designation for this article; European or Japanese wrought names that mention “347LN” or low-carbon Nb-stabilized 18-8 point to related families but are not automatic substitutes on an SA-213 mill test certificate.

Designation Notes
ASME SA-213 / SA-213M Grade TP347LN Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S34751 Unified number in the stainless chemistry table
ASTM A213 TP347LN Separate ASTM product specification — twin page A213 TP347LN; dual-mark only when the PO asks
Related Nb grades SA213 TP347 / S34700 and SA213 TP347H / S34709 — different C/Nb formulas
Related LN (no Nb) SA213 TP304LN / S30453 — nitrogen-strengthened without niobium
Related fine-grain HFG SA213 TP347HFG — different carbon floor, grain band, and tensile
Related plate A240 / SA240 flat product in related UNS families

Dual SA-213/A213 marking is a purchase-order option. Compare TP347 and TP304LN before swapping grades on a familiar “347” or “LN” PMI reading alone.

Heat Treatment and Delivery Condition

TP347LN under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table marks this row with Footnote F. Footnote F ties quench capability to A262 Practice E demonstrability when that test is ordered (Supplementary Requirement S4). Unlike TP347 and TP348, the public Table 3 row for TP347LN does not carry Footnote H beside the solution temperature. The public table also does not print a mandatory ASTM grain-size number for TP347LN.

Supplementary Requirement S2 in the public A213–13 excerpt lists TP347, TP347H, TP348, and TP348H among grades that shall receive a stabilization heat treatment when specified — TP347LN is not on that printed list. Supplementary Requirement S1 lists TP304L, TP316L, TP321, TP347, and TP348 for stress-relieved annealed delivery — again without TP347LN. Do not assume S1 or S2 from a verbal “stabilize like 347” note; write negotiated stabilization language on the purchase order if the project needs it for this UNS. UNCERTAIN: S1/S2 negotiated wording if a buyer insists despite absence from the printed lists.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP347LN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and the C / N / Nb results on the EN 10204 3.1 certificate. For standard Nb framing open SA213 TP347; for H-grade carbon and grain-size controls open SA213 TP347H.

Corrosion Resistance

ASME SA213 TP347LN is selected when ultra-low carbon plus niobium stabilization (and intentional nitrogen for strength recovery) are preferred for sensitizing-range intergranular framing while keeping a standard 18-8 austenitic alloy without molybdenum. The 0.005–0.020% carbon band plus Nb 0.20–0.50% and ≥15 × C is a different lever from either L-carbon alone or the non-H TP347 10 × C formula at higher carbon.

It is not a molybdenum grade and is not automatically better than TP304L or TP304LN in every chloride wet service. Versus SA213 TP304LN, TP347LN adds niobium; versus SA213 TP347, it locks carbon much lower and adds a mandatory nitrogen band. It does not replace H-grade carbon floor and grain-size control for creep-range boiler duty — that path is SA213 TP347H.

SHH STEEL reports the C / N / Nb package on the 3.1 certificate so inspectors can verify the full LN+Nb chemistry rather than accepting a plain 347 or 304LN heat stamped as 347LN.

Applications of SA213 TP347LN Tube

Typical ASME SA213 TP347LN uses include Code-stamped heat-exchanger and condenser tubes where ultra-low-carbon niobium stabilization with nitrogen is specified, process heaters that need both low C and Nb rather than H-grade carbon, and replacement tube matching original S34751 MTCs.

  • Heat-exchanger / condenser tubes naming TP347LN / S34751
  • Process heaters needing ultra-low C + Nb + N rather than H-grade carbon
  • Services that reject both plain TP347 and nitrogen-only TP304LN certificates
  • Replacement bundles matching original S34751 certificates

For standard Nb framing, compare SA213 TP347. For nitrogen-only LN without Nb, compare SA213 TP304LN. For H-grade creep-range Nb, compare SA213 TP347H.

Weldability

TP347LN welds with matching niobium-stabilized austenitic filler practices — commonly ER347 family wires selected to the project WPS, with attention to the ultra-low carbon and nitrogen package in the base metal. Still follow qualified procedures for heat input, interpass, and purge on thin HX tube.

Do not assume S1 or S2 from a verbal “stabilize like 347” note — those Supplementary Requirements are not on the printed TP347LN lists in the public A213–13 excerpt. Write negotiated stabilization language on the purchase order if the project needs it.

Do not dual-stamp a TP347 or TP304LN weld procedure as TP347LN without reopening the C 0.005–0.020% band, N 0.06–0.10%, Nb 0.20–0.50% and ≥15 × C formula, and filler selection on the WPS / PQR.

Surface Finishes

Standard mill delivery for ASME SA213 TP347LN is solution annealed and pickled, leaving a clean matte finish suitable for heat-exchanger and boiler tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the C / N / Nb package check. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP347LN includes heat analysis (C 0.005–0.020%, N 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb 0.20–0.50% and ≥15 × C), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order. When nitrogen is contractual, name the analysis method (Footnote B) on the PO.

Certificate reviewers should confirm the full C / N / Nb package rather than trusting a “347 family” or “LN family” PMI without those three checks. Stabilization / A262 practices apply only when named on the PO — S1/S2 are not automatic for this UNS.

EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP347LN tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP347LN, UNS S34751, heat number, size, and wall basis so receivers can match the 3.1 certificate — including carbon, nitrogen, and niobium — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP347LN only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP347LN as a Code Book ultra-low-carbon niobium-stabilized nitrogen-bearing product with enforceable C 0.005–0.020%, N 0.06–0.10%, Cr 17–19%, Ni 9–13%, Nb 0.20–0.50% and ≥15 × C, 75/30 ksi tensile, 35% elongation, hardness, and marking rules — not as “347 with LN stamped on” or “304LN with a niobium trace” checked only by a PMI peak. Enquiry review verifies the full C / N / Nb package before release.

That stops silent substitution with TP347 or TP304LN heats on datasheets that actually require S34751. We keep SA-213 and A213 independent, dual-mark only on request, and put C / N / Nb on the 3.1 certificate so inspectors can verify the LN+Nb chemistry.

Cross-links: SA213 TP347, SA213 TP347H, SA213 TP304LN, SA213 TP347HFG, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP347LN stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for ultra-low-carbon niobium-stabilized heat-exchanger and boiler tube.

Item SHH STEEL capability for TP347LN
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP347LN / UNS S34751
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with C / N / Nb package; N method / A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347LN against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for ultra-low-C Nb-stabilized heat-exchanger and boiler tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common HX / boiler band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX / boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route, nitrogen analysis method if contractual, and whether dual A213 marking or negotiated stabilization is required. We reply with available mill / stock options for ASME SA213 TP347LN and the matching document set.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP347LN?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C 0.005–0.020%, N 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, and Nb 0.20–0.50% with ≥15 × C — tensile 75/30 ksi, elongation 35%, and hardness floors align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP347LN include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
What are the C / N / Nb limits for ASME SA213 TP347LN?
Carbon 0.005–0.020%, nitrogen 0.06–0.10%, and niobium both 0.20–0.50% and ≥15 × C (Footnote F). Chromium is 17.0–19.0% and nickel 9.0–13.0%. A heat that clears standard TP347 chemistry without landing inside these tighter C / N / Nb windows is not TP347LN. When nitrogen is contractual, name the analysis method (Footnote B) on the purchase order.
TP347LN vs TP347 — when do I need the LN package under SA213?
Order TP347LN when the datasheet needs ultra-low carbon 0.005–0.020%, intentional nitrogen 0.06–0.10%, and Nb 0.20–0.50% with ≥15 × C rather than the non-H TP347 package (C ≤0.08%, Nb ≥10 × C ≤1.10%, no mandatory N). They are different chemistry rows — not dual stamps. Dual TP347LN/TP347H is blocked by non-overlapping carbon bands.
TP347LN vs TP304LN — why choose Nb + LN over nitrogen-only under SA213?
TP304LN strengthens with nitrogen (typically 0.10–0.16%) without niobium and uses a different Cr/Ni window. TP347LN adds niobium 0.20–0.50% and ≥15 × C beside a tighter carbon band and a different nitrogen window (0.06–0.10%). Order the package the datasheet names — they are not interchangeable on a familiar “LN” PMI reading alone. Compare SA213 TP304LN before swapping.
What does Footnote F mean for TP347LN chemistry and heat treatment under SA213?
For chemistry, Footnote F ties the niobium requirement to both the fixed 0.20–0.50% band and the ≥15 × C formula. For heat treatment, Footnote F on the solution-anneal row ties quench capability to A262 Practice E demonstrability when that test is ordered (S4). Unlike TP347, the public Table 3 row for TP347LN does not carry Footnote H beside the solution temperature. Confirm full Footnote F wording in the ordered edition.
Are S1 and S2 listed for TP347LN under SA213?
In the public A213–13 excerpt used for this pack, S2 lists TP347, TP347H, TP348, and TP348H — not TP347LN. S1 lists TP304L, TP316L, TP321, TP347, and TP348 — again without TP347LN. Do not assume S1 or S2 from a verbal “stabilize like 347” note. UNCERTAIN: negotiated wording if a buyer insists despite absence from the printed lists — write it explicitly on the PO.
Does SA-213 set a hardness limit for TP347LN?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation — the same room-temperature pair as TP347 despite ultra-low carbon, because intentional nitrogen recovers strength. Grade distinction is the C / N / Nb package, not a different tensile floor. A tensile-only MTC that omits C, N, or Nb is incomplete.
Minimum wall vs average wall — which should I order for SA213 TP347LN?
Most heat-exchanger and boiler datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in. State wall basis, OD × wall or BWG, finish route, and nitrogen analysis method if contractual on the RFQ.
Can you dual-certify TP347LN with TP347 under SA213?
Honest dual marking requires the heat to clear both named rows. TP347LN’s carbon ceiling (0.020%) sits well below TP347’s ≤0.08% ceiling, but TP347’s Nb formula is ≥10 × C ≤1.10% without a fixed 0.20–0.50% band or mandatory nitrogen. Do not assume dual TP347LN/TP347 from a PMI gun — write both grades on the PO only when the mill confirms both chemistry packages and tensile/hardness paths clear.
Is TP347LN a good choice for chloride-rich cooling water under SA213?
Not automatically. Ultra-low carbon plus niobium addresses sensitizing-range intergranular framing; it does not add molybdenum for chloride pitting/crevice performance. Many wet cooling-water lists prefer Mo-bearing grades. Keep TP347LN where the datasheet names the C / N / Nb package, and compare Mo grades when chloride is the driver.
What solution temperature applies to TP347LN under SA213?
Public heat-treatment language furnishes TP347LN solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means, with Footnote F on quench capability. Unlike TP347, the public Table 3 row does not carry Footnote H beside the solution temperature. Cold-finished versus hot-finished selects process route, not a substitute for the anneal.

Conclusion

ASME SA213 TP347LN / UNS S34751 is the ultra-low-carbon niobium-stabilized nitrogen-bearing seamless stainless steel tube for Code boiler, superheater, and heat-exchanger service when C 0.005–0.020%, N 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb 0.20–0.50% and ≥15 × C, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the C / N / Nb package. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X