ASME SA213 TP309LMoN Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP309LMoN Stainless Steel Tube

ASME SA213 TP309LMoN / UNS S30925 seamless boiler, superheater and heat-exchanger tube — low-carbon high-Cr austenitic with C ≤0.025%, Cr 23.0–26.0%, Ni 13.0–16.0%, Mo 0.5–1.2%, N 0.25–0.40%, a 93/38 ksi tensile floor, hardness max 256 HBW / 100 HRB, 1920 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Mo, N, and grain size.
Grade
TP309LMoN / UNS S30925
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP309LMoN Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP309LMoN under that Code Book text is the low-carbon, molybdenum- and nitrogen-bearing higher chromium–nickel austenitic listed as UNS S30925, with melting limits of carbon ≤0.025%, chromium 23.0–26.0%, nickel 13.0–16.0%, molybdenum 0.5–1.2%, and nitrogen 0.25–0.40%, plus ASTM grain size No. 7 or coarser on the heat-treatment lot. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP309LMoN, the purchase order and mill test certificate should carry the ASME designation and the Mo+N lines — not a shop nickname such as “309LMoN HX tube,” and not an assumed swap from TP309S simply because both sit in the 309 family.

SHH STEEL can supply ASME SA213 TP309LMoN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including measured Mo and N — the tensile plus hardness acceptance set at the higher 93/38 ksi floor, and the grain-size result. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 309LMoN, S30925 boiler tube, high-N 309 Mo tube, or L+Mo+N 309 tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP309S, SA213 TP316LN, SA213 XM-19, SA213 TP310S, and SA213 TP304LN. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP309LMoN.

Chemical Composition of SA213 TP309LMoN

Two chemistry layers matter for TP309LMoN under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Four lines drive selection before anything else: carbon ≤0.025% (a true L-grade ceiling, tighter than classic 309S), chromium 23.0–26.0%, molybdenum 0.5–1.2%, and nitrogen 0.25–0.40%. SHH STEEL reports the actual ladle values — including Mo and N — and the product values when ordered, and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP309LMoN / UNS S30925 and the product-analysis limits that result from applying A480 Table A1.1 tolerances, plus a snapshot versus TP309S and TP316LN. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; A480 tolerances for C ≤0.025 / Mo 0.5–1.2 / N 0.25–0.40 / Cr 23–26 — applied from sister A480 practice; nitrogen analysis method Footnote B; grain-size clause number — confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP309LMoN / UNS S30925. Confirm the ordered ASME edition on the purchase order.

Element TP309LMoN (UNS S30925) melting analysis
Carbon (C) ≤ 0.025
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 0.70
Chromium (Cr) 23.0 – 26.0
Nickel (Ni) 13.0 – 16.0
Molybdenum (Mo) 0.5 – 1.2
Nitrogen (N) 0.25 – 0.40
Niobium (Nb / Cb) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.025 0.005 over ≤ 0.030
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.040 0.010 over ≤ 0.050
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 0.70 0.05 over ≤ 0.75
Chromium (Cr) 23.0 – 26.0 0.25 under / over 22.75 – 26.25
Nickel (Ni) 13.0 – 16.0 0.15 under / over 12.85 – 16.15
Molybdenum (Mo) 0.5 – 1.2 0.05 under / over 0.45 – 1.25
Nitrogen (N) 0.25 – 0.40 0.02 under / 0.04 over 0.23 – 0.44

Snapshot — TP309S vs TP309LMoN vs TP316LN

Element TP309S (S30908) TP309LMoN (S30925) TP316LN (S31653)
C ≤ 0.08 ≤ 0.025 ≤ 0.035
Cr 22.0 – 24.0 23.0 – 26.0 16.0 – 18.0
Ni 12.0 – 15.0 13.0 – 16.0 10.0 – 14.0
Mo … 0.5 – 1.2 2.00 – 3.00
N … 0.25 – 0.40 0.10 – 0.16

TP309LMoN is not a renamed TP309S with a verbal Mo add. Carbon is capped at 0.025%, phosphorus at 0.040%, and silicon at 0.70% — tighter residual windows than classic 309S — while chromium steps up to 23–26% and nitrogen sits in a high 0.25–0.40% band that underpins the 93/38 ksi tensile floor. Molybdenum at 0.5–1.2% is real but modest compared with the 2–3% Mo of SA213 TP316LN; do not treat LMoN as a seawater-leaning 316 substitute. When ordinary 22–24% Cr oxidation resistance without Mo/N is enough, open SA213 TP309S.

When product analysis is ordered, finished tube may read up to C 0.030%, Mn 2.04%, P 0.050%, S 0.035%, and Si 0.75%, with Cr 22.75–26.25%, Ni 12.85–16.15%, Mo 0.45–1.25%, and N 0.23–0.44%. Put any tighter project carbon, molybdenum, or nitrogen window on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP309LMoN

ASME SA-213 sets the tensile acceptance floor for TP309LMoN at 93 ksi [640 MPa] tensile strength and 38 ksi [260 MPa] yield strength (0.2% offset), with elongation of 30% minimum in 2 in. or 50 mm — a distinctly higher strength pair than the 75/30 ksi / 35% elongation story of TP309S. Hardness maximum is 256 HBW / 270 HV or 100 HRB. Public heat-treatment language also assigns ASTM grain size No. 7 or coarser for the heat-treatment lot. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment, and the grain-size result must be reported.

Source: public SA-213 / A213 mechanical-table and heat-treatment summaries for TP309LMoN / UNS S30925. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP309LMoN requirement
Tensile strength, min 93 ksi [640 MPa]
Yield strength (0.2% offset), min 38 ksi [260 MPa]
Elongation in 2 in. or 50 mm, min 30%
Hardness, max 256 HBW / 270 HV or 100 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Flattening and flaring tests sit beside tension and hardness on a lot basis. Design calculations should use the 93/38 ksi pair unless the purchase order states higher guaranteed values the mill has accepted in writing. When the datasheet only needs classic 309 oxidation resistance at 75/30 ksi, open SA213 TP309S; when higher molybdenum (2–3%) with a lower Cr–Ni balance and a lower nitrogen band is the driver, open SA213 TP316LN; when a different high-nitrogen austenitic chemistry is specified, open SA213 XM-19.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP309LMoN is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because the higher design allowable implied by the 93/38 ksi floor still depends on remaining wall after tolerance and service thinning.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP309LMoN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler / high-temperature bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP309LMoN tube is sparse in shop nicknames — the UNS number S30925 is often the cleanest cross-reference. ASME SA-213 Grade TP309LMoN / UNS S30925 is the governing designation for this article; do not treat it as automatic dual-cert stock with TP309S, TP316LN, or XM-19. When a datasheet says “equivalent to 309LMoN,” confirm which product standard, tensile/hardness table, Mo+N lines, grain-size clause, and heat-treatment temperature the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP309LMoN Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30925 Unified number listed with the grade chemistry
ASTM A213 TP309LMoN Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP309LMoN
Related classic 309 SA213 TP309S — lower strength, no Mo/N mandate
Related LN Mo grade SA213 TP316LN — higher Mo 2–3%, lower Cr–Ni, lower N band
Related high-N austenitic SA213 XM-19 — different high-N chemistry family
Related plate A240 / SA240 flat product in related high-Cr families — order plate and tube under their own product standards

ASTM A213 TP309LMoN is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare SA213 TP309S and SA213 TP316LN on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP309LMoN under ASME SA-213 is furnished solution treated at a minimum of 1920 °F [1050 °C], then quenched in water or cooled rapidly by other means — note the 20 °F [about 10 °C] higher minimum versus the 1900 °F [1040 °C] row used for TP309S / TP309H / TP309Cb. That heat-treatment row also carries ASTM grain size No. 7 or coarser for the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that path.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size result. Delivery condition for SHH STEEL TP309LMoN is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature, quench method, measured Mo and N, and grain size stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability is ordered, the corrosion test report travels with the heat-treatment record. The higher anneal minimum and grain-size clause do not rewrite classic 309S acceptance — use SA213 TP309S when the datasheet only needs the 1900 °F / 75/30 ksi path without Mo+N.

Corrosion Resistance

TP309LMoN is selected for a combination of high-temperature oxidation resistance from its 23–26% chromium / 13–16% nickel balance, modest molybdenum at 0.5–1.2%, and nitrogen-driven strength at 0.25–0.40% N under a true L-grade carbon ceiling. In oxidizing furnace atmospheres and elevated-temperature process circuits that also want a higher design allowable than classic 309S, the grade fills a niche that neither plain TP309S nor TP316LN covers alone. In seawater-leaning or heavy-chloride cooling waters, buyers usually still step to higher-Mo grades such as SA213 TP316 / SA213 TP316L / SA213 TP316LN rather than treating 0.5–1.2% Mo as equivalent to 2–3% Mo.

ASME SA-213 itself does not publish a corrosion-rate, PREN ranking, or oxidation-life table for TP309LMoN; selection remains engineering judgment against temperature, atmosphere, chloride level, velocity, and inspection philosophy. Intergranular corrosion risk after welding is moderated by the ≤0.025% carbon ceiling, by solution treating after fabrication when the sequence allows, or by invoking a contractual A262 Practice E Supplementary Requirement on the tube PO. SHH STEEL will not rank TP309LMoN as a seawater substitute for 316LN — the Mo band is intentionally lower while Cr–Ni and nitrogen sit higher.

Applications of SA213 TP309LMoN Tube

Because TP309LMoN brings low carbon, modest molybdenum, high nitrogen, and a 93/38 ksi tensile floor under SA-213 on a 23–26% Cr / 13–16% Ni balance, it shows up in high-temperature oxidation-prone boiler and process circuits that also need higher strength than classic 309S, and in HX duty where L+Mo+N chemistry is written into the datasheet. The table below pairs typical application areas with a selection note so the grade is chosen for atmosphere, strength, and Mo/N need — not only for the familiar “309LMoN” name on the BOM.

Application area Typical use of TP309LMoN tube Selection note
High-temp oxidation + higher strength Seamless tube where 23–26 Cr scale resistance and 93/38 ksi floors are specified together Confirm design metal temperature, atmosphere, and tensile callout
Boiler / process steam (strength-limited) Seamless generating or process tubing ordered to SA-213 with Mo+N reported Prefer TP309S if 75/30 ksi and no Mo/N are enough
Furnace / hot-gas heat exchangers Straight and U-bend tubes needing L+Mo+N on a high-Cr balance Prefer TP310S if even higher Ni oxidation resistance without Mo/N is specified
Modest-chloride oxidizing service Tube where 0.5–1.2% Mo helps but full 2–3% Mo is not required Prefer TP316LN if chlorides dominate and Mo 2–3% is mandatory
Heavy chloride / seawater-leaning Usually not the preferred selection at Mo ≤1.2% Open higher-Mo grades on the hub
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For classic 309 without Mo/N open SA213 TP309S; for higher Mo LN chemistry open SA213 TP316LN; for alternate high-N austenitics open SA213 XM-19; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP309LMoN tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses low-carbon austenitic fillers under a qualified WPS; many fabricators prefer ER309L-class or project-specified Mo-bearing deposits when the base tube already carries Mo 0.5–1.2% and high nitrogen. Heat input control, interpass limits, and nitrogen retention in the weld metal remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP309LMoN is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, grain-size and Mo/N reporting on the MTC, and any contractual corrosion test on the base metal. The ≤0.025% carbon ceiling reduces sensitization risk, but high nitrogen and modest Mo still need a qualified WPS; discuss whether a post-weld solution treatment better protects the joint when service temperatures sit in the sensitizing range. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP309LMoN is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route and must still clear the 1920 °F minimum and grain-size requirement. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, Mo+N identity, and grain-size reporting as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP309LMoN includes heat analysis (with Mo and N reported), tension tests to the 93/38 ksi floor, hardness tests to the 256 HBW / 100 HRB maximum, grain-size determination to ASTM No. 7 or coarser on the heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP309LMoN tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry — including Mo and N — on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity and grain-size result clearly on the certificate so hardness, tension, and grain-size specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP309LMoN tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes that call out Mo, N, and grain-size reporting.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP309LMoN as a Code Book product standard with enforceable chemistry — including C ≤0.025%, Mo 0.5–1.2%, and N 0.25–0.40% — tensile at the 93/38 ksi floor, hardness, grain-size, heat-treatment at 1920 °F minimum, and marking rules, not as a catalogue nickname for “any high-N 309 tube.” The MTC reports the full ladle chemistry with measured Mo and N, the tensile/hardness acceptance set, and the grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 309-family conversation honest for high-temperature and higher-strength HX duty. If classic 22–24% Cr oxidation resistance at 75/30 ksi without Mo/N is enough, we open SA213 TP309S. If higher molybdenum (2–3%) with a lower Cr–Ni balance is the driver, we open SA213 TP316LN. If a different high-nitrogen austenitic is specified, we open SA213 XM-19. If chlorides dominate a wet exchanger beyond what 0.5–1.2% Mo can support, we open SA213 TP316 / SA213 TP316L rather than stretching LMoN into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP309LMoN stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for low-carbon Mo+N high-Cr boiler and heat-exchanger duty.

Item SHH STEEL capability for TP309LMoN
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP309LMoN / UNS S30925
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (93/38 ksi), hardness (max 256 HBW / 100 HRB), grain size No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry including Mo and N on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry, Mo, N, and grain size; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309LMoN tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for L+Mo+N high-Cr boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP309LMoN
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative high-temp HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Mo/N and grain-size reporting callouts, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), Mo/N and grain-size reporting expectation, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry including Mo and N, tensile at the 93/38 ksi floor, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP309S, SA213 TP316LN, and SA213 XM-19 sit on the same hub when the datasheet steps beyond TP309LMoN.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP309LMoN?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP309LMoN include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP309LMoN under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP309LMoN?
TP309LMoN is UNS S30925. Melting limits include carbon ≤0.025%, manganese ≤2.00%, phosphorus ≤0.040%, sulfur ≤0.030%, silicon ≤0.70%, chromium 23.0–26.0%, nickel 13.0–16.0%, molybdenum 0.5–1.2%, and nitrogen 0.25–0.40%, with niobium as a no-requirement ellipsis. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP309LMoN vs TP309S — why is the strength higher under SA213?
TP309LMoN carries a 93 ksi / 38 ksi tensile floor versus 75/30 ksi for TP309S, driven largely by the high nitrogen band of 0.25–0.40% together with the higher chromium window and modest molybdenum. TP309S remains the right call when classic 22–24% Cr oxidation resistance without Mo/N and without the higher strength pair is what the datasheet actually needs. Do not treat the two grades as interchangeable on a Code MTC.
TP309LMoN vs TP316LN — which Mo+N grade should I order under SA213?
Order TP309LMoN when the datasheet wants a high-Cr (23–26%) / high-N (0.25–0.40%) balance with modest Mo 0.5–1.2% and the 93/38 ksi floor. Order TP316LN when molybdenum 2.00–3.00% on an 16–18% Cr / 10–14% Ni LN chemistry is the driver and the nitrogen band sits lower at 0.10–0.16%. Mo level and Cr–Ni balance differ enough that one is not an automatic substitute for the other.
Does TP309LMoN require grain size under SA213?
Yes. Public heat-treatment language assigns ASTM grain size No. 7 or coarser for the heat-treatment lot of TP309LMoN, alongside the 1920 °F [1050 °C] minimum solution treatment. Ask the mill to report the grain-size result on the EN 10204 3.1 certificate for every heat-treatment lot — grain size is part of acceptance, not an optional catalogue claim.
What heat treatment does ASME SA-213 require for TP309LMoN?
TP309LMoN is solution treated at a minimum of 1920 °F [1050 °C] — about 20 °F higher than the 1900 °F row used for TP309S / TP309H / TP309Cb — and then water quenched or rapidly cooled, with ASTM grain size No. 7 or coarser required on the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that path. Ask the mill to state anneal temperature, quench method, measured Mo and N, and grain size on the certificate.
Does SA-213 set a hardness limit for TP309LMoN?
Yes. The mechanical table for TP309LMoN lists tensile strength, yield strength, elongation, and a hardness maximum of 256 HBW / 270 HV or 100 HRB — higher than the 192 HBW / 90 HRB ceiling used on classic 309S. Hardness tests are part of lot acceptance under SA-213. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
Minimum wall vs average wall — which should I order for SA213 TP309LMoN?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance — especially important when the higher 93/38 ksi allowable still depends on remaining wall after service thinning. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling.
Is TP309LMoN enough molybdenum for seawater-leaning exchangers under SA213?
Usually no for heavy chloride or seawater-leaning duty. Molybdenum at 0.5–1.2% is real but modest compared with the 2–3% Mo of TP316 / TP316L / TP316LN. TP309LMoN is framed for high-Cr oxidation resistance plus nitrogen-driven strength with only modest Mo help. Open higher-Mo grades on the SA213 hub when chlorides dominate the selection.
Can you dual-certify ASME SA-213 and ASTM A213 TP309LMoN?
Yes when the heat and testing support both independent standards, including Mo, N, and grain-size reporting. Dual SA-213/A213 marking is available when the purchase order requests both names on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly — a "309LMoN" nickname alone is not dual certification.

Conclusion

ASME SA213 TP309LMoN / UNS S30925 is the low-carbon Mo+N 23–26% Cr / 13–16% Ni seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.025%, Mo 0.5–1.2%, N 0.25–0.40%, the 93/38 ksi tensile floor, 1920 °F solution treatment, and ASTM grain size No. 7 or coarser are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to those acceptance floors, with Mo, N, and grain size reported on EN 10204 3.1 certificates — and dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Mo/N reporting expectation, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X