ASME SA213 TP310HCbN Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP310HCbN Stainless Steel Tube

ASME SA213 TP310HCbN / UNS S31042 seamless boiler, superheater and heat-exchanger tube — H-grade 24–26% Cr / 19–22% Ni with C 0.04–0.10%, Nb 0.20–0.60% (fixed band), N 0.15–0.35%, a 95/43 ksi tensile floor, hardness max 256 HBW / 100 HRB, a 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. Chosen for creep-oriented USC / high-temperature duty needing nitrogen-driven strength above classic 75/30 ksi 310 rows. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb, N, and grain size.
Grade
TP310HCbN / UNS S31042
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP310HCbN Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP310HCbN under that Code Book text is the nitrogen-strengthened H-grade niobium member of the 310 family, listed as UNS S31042, with melting carbon 0.04–0.10%, chromium 24.0–26.0%, nickel 19.0–22.0%, niobium 0.20–0.60% as a fixed band (not the 10×C formula used on TP310HCb), nitrogen 0.15–0.35%, and ASTM grain size No. 7 or coarser on the heat-treatment lot. That package exists for creep-oriented USC / high-temperature boiler and furnace tube that needs 25Cr–20Ni oxidation resistance, intentional carbon and coarse grain, Cb/Nb stabilization, and nitrogen-driven room-temperature strength above the classic 75/30 ksi 310 rows — not as a casual dual stamp of TP310HCb plus nitrogen.

SHH STEEL can supply ASME SA213 TP310HCbN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report ladle chemistry including niobium and nitrogen, the tensile plus hardness acceptance set, and the ASTM E112 grain-size result for the heat-treatment lot. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 310HCbN, HR3C-type 310, S31042, or H-grade Nb-N 25Cr-20Ni tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP310HCb, SA213 TP310H, SA213 TP310Cb, SA213 TP310S, and SA213 TP309HCb. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP310HCbN.

Chemical Composition of SA213 TP310HCbN

Two chemistry layers matter for TP310HCbN under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Reviewers should check four lines together before anything else: the 0.04–0.10% carbon band, the Nb 0.20–0.60% range (fixed band, not 10×C), the N 0.15–0.35% band, and the 24–26 / 19–22 Cr–Ni windows. Missing any one of those means the heat is not TP310HCbN. Nitrogen analysis method is a matter of agreement between purchaser and producer (Footnote B in public table text) — put the agreed method on the PO when N reporting must follow a named technique. SHH STEEL reports the actual ladle values — including Nb and N — and the product values when ordered.

The tables below reproduce the melt limits for TP310HCbN / UNS S31042 and the product-analysis limits that result from applying A480 Table A1.1 practice, plus an HCb vs HCbN snapshot. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; Footnote B nitrogen-analysis wording; Footnote F/H superscript placement near HCbN rows across editions; A480 N/Nb tolerance digits for these bands — applied from sister-pack A480 practice; S2 full temperature/time text — confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP310HCbN / UNS S31042. Confirm the ordered ASME edition on the purchase order.

Element TP310HCbN (UNS S31042) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.15 – 0.35
Niobium (Nb / Cb) 0.20 – 0.60

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20
Nitrogen (N) 0.15 – 0.35 0.02 under / 0.04 over 0.13 – 0.39
Niobium (Nb) 0.20 – 0.60 0.05 under / over 0.15 – 0.65

HCb vs HCbN snapshot

Element TP310HCb (S31041) TP310HCbN (S31042) TP310H (S31009)
C 0.04 – 0.10 0.04 – 0.10 0.04 – 0.10
Nb (Cb) 10×C – 1.10 0.20 – 0.60 …
N … 0.15 – 0.35 …
Tensile / yield 75 / 30 ksi 95 / 43 ksi 75 / 30 ksi
Grain size No. 7 or coarser No. 7 or coarser No. 7 or coarser

Do not confuse the niobium rule: SA213 TP310HCb uses the formula minimum 10×C up to 1.10%, while TP310HCbN uses a fixed 0.20–0.60% Nb band plus mandatory nitrogen. Molybdenum remains a no-requirement ellipsis on both — wet chloride framing still belongs with Mo grades such as SA213 TP316L or higher. When only H-grade carbon/grain-size without Nb or N is required, stay on SA213 TP310H.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 23.75–26.25%, Ni 18.85–22.20%, N 0.13–0.39%, and Nb 0.15–0.65% under the A480 practice applied above. Nitrogen and niobium product tolerances for these bands are taken from sister-pack A480 practice — confirm the A480 edition if product analysis is contractual. Put any tighter project floors on the purchase order before heat selection.

Mechanical Properties of SA213 TP310HCbN

ASME SA-213 sets a distinctly higher room-temperature tensile floor for TP310HCbN than for ordinary 310 H or HCb rows: 95 ksi [655 MPa] tensile strength and 43 ksi [295 MPa] yield strength (0.2% offset), with elongation of 30% minimum in 2 in. or 50 mm. Hardness maximum is 256 HBW or 100 HRB (public mechanical-table excerpts for S31042 print Brinell and Rockwell without a Vickers companion on this row). The nitrogen band is the primary reason those floors sit above the 75/30 ksi pair used on SA213 TP310H and SA213 TP310HCb. Grain size No. 7 or coarser remains mandatory on the heat-treatment lot.

Source: public SA-213 / A213 mechanical-table summaries for TP310HCbN / UNS S31042 (commonly Table 4) and H-grade grain-size language. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP310HCbN requirement
Tensile strength, min 95 ksi [655 MPa]
Yield strength (0.2% offset), min 43 ksi [295 MPa]
Elongation in 2 in. or 50 mm, min 30%
Hardness, max 256 HBW or 100 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

A complete TP310HCbN release package reports tensile, hardness, carbon band, niobium band, nitrogen band, and grain size together. A tensile-only MTC that omits N, Nb, or E112 grain size is not a complete HCbN acceptance package — ask for all of those results on the EN 10204 3.1 certificate before releasing the heat to fabrication. Flattening and flaring tests sit beside tension and hardness on a lot basis.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP310HCbN is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. Creep-range and USC boiler datasheets almost always assume minimum wall — state wall basis on the purchase order, because remaining wall after high-temperature oxidation and creep is often a design input on the circuits where HCbN is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP310HCbN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / superheater / furnace) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / furnace / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, design metal temperature, S2 stabilizing needs, nitrogen analysis method, Nb/N/grain-size reporting expectation, and end preparation on the enquiry. Minimum wall remains first-class for HCbN tube the same way it does for other SA-213 H grades.

Equivalent Grades

Equivalence language around TP310HCbN often collapses HR3C-type shop names, plate forms, and ordinary HCb into one nickname. ASME SA-213 Grade TP310HCbN / UNS S31042 is the governing designation for this article; near-chemistry plate or cast forms are not automatic SA-213 substitutes. When a datasheet says “equivalent to 310HCbN,” confirm which product standard, tensile floor, Nb band (fixed vs 10×C), nitrogen band, and grain-size clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP310HCbN Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31042 Unified number listed with the grade chemistry
ASTM A213 TP310HCbN Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP310HCbN
Related HCb SA213 TP310HCb — Nb formula 10×C–1.10, no N band, 75/30 ksi
Related H-grade SA213 TP310H — H carbon/grain-size without Nb or N
Related Cb SA213 TP310Cb — Nb formula without H package or N
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own product standards

ASTM A213 TP310HCbN is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP310HCb and TP310H on their own ASME SA213 pages before assuming a mixed nickname equals TP310HCbN on the MTC.

Heat Treatment and Delivery Condition

TP310HCbN under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries ASTM grain size No. 7 or coarser for the heat-treatment lot. Public PDF layout places Footnote F/H markers near the TP310HCb / TP310HCbN rows — confirm the ordered edition’s superscripts before freezing Footnote H language on the purchase order. Footnote H, where applicable, warns that a solution-treating temperature above 1950 °F [1065 °C] may impair resistance to intergranular corrosion after subsequent sensitizing exposure; when the purchaser specifies it, a lower-temperature stabilization or resolution anneal shall follow the higher-temperature solution anneal.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal, the grain-size check, or any ordered stabilizing hold. Delivery condition for SHH STEEL TP310HCbN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, niobium, nitrogen, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Supplementary Requirement S2 (stabilizing heat treatment) explicitly lists TP310HCbN among the grades that shall be given a stabilizing treatment after the solution anneal when the purchaser specifies S2. Write S2 onto the purchase order when the datasheet requires that post-solution stabilizing hold — do not assume base SA-213 includes it automatically for every HCbN shipment. Full temperature/time wording is edition text — confirm on the ordered edition. When only the classic 75/30 ksi HCb path without nitrogen is required, stay on SA213 TP310HCb.

Corrosion Resistance

TP310HCbN is built for high-temperature oxidation resistance from 24–26% Cr / 19–22% Ni, plus niobium stabilization against intergranular corrosion, plus H-grade carbon/grain-size controls, plus nitrogen for strength — not for molybdenum-driven chloride pitting resistance. In oxidizing furnace atmospheres, hot-process gas circuits, and creep-range USC steam services where ordinary 310 H or HCb tensile floors are not enough, the nitrogen-strengthened package is the commercial reason to pay for HCbN. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 310HCbN as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP310HCbN; selection remains engineering judgment against temperature, atmosphere, velocity, and inspection philosophy. Optional S2 and any ordered A262 Practice E exist because Nb-bearing H grades can lose IGC resistance if solution temperatures run too high without a subsequent stabilizing or resolution step. Put those Supplementary Requirements on the purchase order when the project requires demonstrated IGC performance rather than chemistry-and-grain-size assurance alone. Sulfidation and carburizing atmospheres still need process-specific review beyond a generic stainless catalogue claim. SHH STEEL will not rank TP310HCbN as equal to 316 in chlorides — higher chromium, nickel, niobium, and nitrogen are not a molybdenum substitute.

Applications of SA213 TP310HCbN Tube

Because TP310HCbN brings controlled carbon 0.04–0.10%, fixed Nb 0.20–0.60%, nitrogen 0.15–0.35%, ASTM No. 7 or coarser grain size, and a 95/43 ksi tensile floor on a 24–26% Cr / 19–22% Ni oxidation balance under SA-213, it shows up in creep-oriented USC / high-temperature boiler and superheater circuits, furnace-related heat exchangers, and elevated-temperature HX duty where classic 75/30 ksi 310 rows are not enough. The table below pairs typical application areas with a selection note so the grade is chosen for metal temperature, strength, and Code language — not only for an HR3C-type shop nickname on the BOM.

Application area Typical use of TP310HCbN tube Selection note
Creep-oriented USC / high-temp boiler Seamless generating or superheater tubing ordered to SA-213 with N, Nb, and grain-size reporting Confirm design metal temperature, tensile floor, and S2 needs
Severe high-temperature oxidation + strength Seamless tube where 25Cr-20Ni scale resistance and 95/43 ksi floors sit together Prefer TP310HCb if 75/30 ksi is enough
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits with elevated strength need Open TP310H if Nb/N are not required
Chemical process (oxidizing, low chloride) Tube-side circuits with hot oxidizing media Prefer TP316/TP316L if chlorides dominate
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General Code tube duty Seamless tube where SA-213 HCbN documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For classic 75/30 ksi H+Cb without nitrogen open SA213 TP310HCb; for H-grade without Nb or N open SA213 TP310H; for Nb without H package open SA213 TP310Cb; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP310HCbN tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER310 / Nb-bearing or nitrogen-aware deposits under a qualified WPS; fabricators often prefer controlled-composition fillers when the base tube relies on both niobium and nitrogen for post-weld properties on an H-grade carbon heat. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP310HCbN is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), niobium, nitrogen, and grain-size documentation on the base metal, tube-to-tubesheet joint quality, and any contractual corrosion test. For tube that will enter service as-welded in a sensitizing environment, discuss whether S2 stabilizing or a post-weld solution treatment better protects the joint. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP310HCbN is solution annealed and pickled, leaving a clean matte finish suitable for most boiler, furnace, and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route while still needing to clear the H-grade grain-size requirement and any ordered S2 stabilizing hold. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and grain-size identity as standard requirements and reports niobium and nitrogen on the MTC; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP310HCbN includes heat analysis (with niobium and nitrogen), tension tests to the 95/43 ksi floor, hardness tests to the 256 HBW / 100 HRB maximum, grain-size determination to ASTM No. 7 or coarser per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP310HCbN tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, S2 stabilizing, or intergranular-corrosion testing from a verbal “full certs” note. Grain size, niobium, and nitrogen are all part of the base HCbN acceptance — confirm all three results appear on the certificate before releasing the heat. Put the agreed nitrogen analysis method on the PO when Footnote B reporting must follow a named technique.

Option Purpose
Product analysis Confirms chemistry including Nb and N on finished tube (via general requirements / PO language)
S2 stabilizing heat treatment Post-solution stabilizing hold — explicitly listed for TP310HCbN when purchaser specifies S2
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement; related to Footnote H
Nitrogen analysis method Agreed method per Footnote B when N reporting must follow a named technique
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness, tension, grain-size, and chemistry specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP310HCbN tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes — including the Nb, N, and grain-size reporting expectations that distinguish HCbN release packages.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP310HCbN as a Code Book product standard with enforceable chemistry (including niobium and nitrogen), tensile, hardness, heat-treatment, grain-size, and marking rules — not as a catalogue nickname for “any HR3C-type 310 tube.” The MTC reports the full ladle chemistry with Nb and N, the 95/43 ksi tensile/hardness acceptance set, and the E112 grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 310-family conversation honest for creep-oriented USC and high-temperature boiler duty. If classic 75/30 ksi H+Cb without nitrogen is enough, we open SA213 TP310HCb. If only H-grade carbon/grain-size without Nb or N is required, we open SA213 TP310H. If only Nb stabilization without the H package is required, we open SA213 TP310Cb. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 310HCbN into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME HCbN callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP310HCbN stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this HCbN grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for creep-oriented USC / high-temperature boiler and furnace tube with nitrogen-strengthened tensile floors.

Item SHH STEEL capability for TP310HCbN
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP310HCbN / UNS S31042
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / furnace / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (95/43 ksi), hardness (max 256 HBW / 100 HRB), grain size ASTM No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry including Nb and N on MTC; product analysis / S2 / IGC on order
Documents EN 10204 3.1 with full ladle chemistry, Nb, N, and grain-size result; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310HCbN tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for creep-oriented high-temperature oxidation-resistant boiler and furnace tube with nitrogen-strengthened tensile floors; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP310HCbN
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/furnace/HX ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative HCbN boiler/furnace sizes, confirm min vs average wall
Length Cut lengths for boiler, superheater, and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Nb/N/grain-size reporting confirmation, nitrogen analysis method, S2 stabilizing, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), Nb/N/grain-size reporting expectation, nitrogen analysis method, S2 needs, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry including Nb and N, tensile, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP310HCb, SA213 TP310H, and SA213 TP310S sit on the same hub when the datasheet steps beyond TP310HCbN.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP310HCbN?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, niobium, nitrogen, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP310HCbN include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP310HCbN under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP310HCbN?
TP310HCbN is UNS S31042. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 24.0–26.0%, nickel 19.0–22.0%, nitrogen 0.15–0.35%, and niobium 0.20–0.60% as a fixed band (not the 10×C formula), with molybdenum as a no-requirement ellipsis. Product-analysis limits apply only when ordered. Confirm the ordered SA-213 edition and the agreed nitrogen analysis method before treating a secondary catalogue as acceptance text.
TP310HCbN vs TP310HCb — which SA213 grade should I order?
Order TP310HCbN when the datasheet needs the higher 95/43 ksi tensile floor, fixed Nb 0.20–0.60%, and nitrogen 0.15–0.35% on the same 24–26% Cr / 19–22% Ni H-grade path. Order TP310HCb when classic 75/30 ksi floors with Nb formula 10×C–1.10% (no nitrogen band) are enough. Do not treat "310HCbN" as a casual dual stamp of TP310HCb plus nitrogen on the MTC.
Why is the niobium rule different on TP310HCbN?
TP310HCb uses the formula minimum Nb ≥10×C up to 1.10%. TP310HCbN uses a fixed Nb band of 0.20–0.60% plus mandatory nitrogen 0.15–0.35%. Those are different chemistry acceptance stories on the same Cr–Ni H-grade carbon path. Confirm which Nb rule the datasheet actually calls for before ordering either grade — swapping them on the strength of a shop nickname is a common MTC rejection cause.
Why does SA-213 require grain size for TP310HCbN?
The H-grade heat-treatment row requires ASTM No. 7 or coarser grain size per heat-treatment lot because coarse grain is part of the elevated-temperature / creep-oriented acceptance package. A tensile-only certificate that omits the E112 result — or that reports N and Nb without grain size — is incomplete for TP310HCbN release. Ask for Nb, N, and grain size together on the EN 10204 3.1 mill test certificate.
What is S2 stabilizing heat treatment for TP310HCbN?
Supplementary Requirement S2 explicitly lists TP310HCbN among grades that shall be given a stabilizing treatment after the solution anneal when the purchaser specifies S2. Write S2 onto the purchase order when the datasheet requires that post-solution stabilizing hold — do not assume base SA-213 includes it automatically for every HCbN shipment. Full temperature/time wording is edition text; confirm on the ordered edition and relate it to Footnote H language about high solution temperatures.
Does SA-213 set a hardness limit for TP310HCbN?
Yes. Public mechanical-table summaries for TP310HCbN set a hardness maximum of 256 HBW or 100 HRB alongside the 95 ksi tensile and 43 ksi yield floors — higher than the 192 HBW / 90 HRB ceiling on ordinary 310 H and HCb rows. Hardness testing sits on a lot basis with tension, flattening, flaring, and grain-size determination. If a project quotes a tighter hardness window, put it on the purchase order as a contractual extra.
What heat treatment does ASME SA-213 require for TP310HCbN?
TP310HCbN is solution treated at a minimum of 1900 °F [1040 °C] and quenched in water or cooled rapidly by other means. The same heat-treatment row carries ASTM grain size No. 7 or coarser for the heat-treatment lot; confirm Footnote F/H superscripts on the ordered edition. Cold-finished versus hot-finished is a dimensional route, not a substitute for the anneal, the grain-size check, or any ordered S2 stabilizing hold. Delivery condition is typically solution annealed and pickled, with anneal temperature, quench method, Nb, N, and E112 result on the MTC.
Minimum wall vs average wall — which should I order for SA213 TP310HCbN?
Creep-range and USC boiler datasheets almost always assume minimum wall because remaining wall after high-temperature oxidation and creep is a design input. Average wall is acceptable when the purchase order says so and the general-requirements tolerances for that finish route are understood. State the wall basis explicitly on the enquiry so mill and stock lengths are rolled and accepted to the correct table — do not leave wall basis implied by a BWG number alone.
Is TP310HCbN a good choice for chloride-rich cooling water under SA213?
Usually no. TP310HCbN is built for high-temperature oxidation resistance, niobium stabilization, H-grade carbon/grain-size controls, and nitrogen-driven strength; molybdenum is a no-requirement ellipsis. For chloride-rich cooling water and wet brine-leaning exchangers, open molybdenum grades such as SA213 TP316 / TP316L or higher rather than treating 310HCbN as a chloride upgrade. Higher chromium, nickel, niobium, and nitrogen are not a molybdenum substitute.
Can you dual-certify ASME SA-213 and ASTM A213 TP310HCbN?
Yes, when the purchase order asks for both independent standards on the stencil and mill test certificate. ASME SA-213 and ASTM A213 remain separate documents even when chemistry and tensile floors align for a referenced edition. Dual-mark only when both names are required; do not assume an A213-only certificate substitutes for an SA-213 Code callout, or the reverse.

Conclusion

ASME SA213 TP310HCbN / UNS S31042 is the nitrogen-strengthened H-grade niobium 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for Code boiler, superheater, and furnace heat-exchanger service when creep-oriented USC / high-temperature duty needs fixed Nb 0.20–0.60%, nitrogen 0.15–0.35%, ASTM No. 7 or coarser grain size, and a 95/43 ksi tensile floor above classic 75/30 ksi 310 rows. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F with Footnote H / S2 awareness, tested to the 95/43 ksi tensile and hardness acceptance floors with Nb, N, and grain-size reporting, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Nb/N/grain-size reporting expectation, nitrogen analysis method, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X