ASME SA213 TP309Cb Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP309Cb Stainless Steel Tube

ASME SA213 TP309Cb / UNS S30940 seamless boiler, superheater and heat-exchanger tube — niobium-stabilized 22–24% Cr austenitic with Ni 12.0–16.0%, C ≤0.08%, Nb 10×C–1.10%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. Chosen when 309-family oxidation resistance needs Cb stabilization rather than H-grade carbon and grain-size alone. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb.
Grade
TP309Cb / UNS S30940
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP309Cb Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP309Cb under that Code Book text is the niobium-stabilized higher chromium–nickel austenitic listed as UNS S30940, with melting limits of carbon ≤0.08%, chromium 22.0–24.0%, nickel 12.0–16.0%, and niobium (columbium) held between ten times the carbon content and 1.10%. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP309Cb, the purchase order and mill test certificate should carry the ASME designation and the Nb line — not a shop nickname such as “309Cb HX tube,” and not an assumed swap from TP309S simply because both clear a 75/30 ksi tensile floor.

SHH STEEL can supply ASME SA213 TP309Cb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including the measured Nb — and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 309Cb, 309Nb, S30940 boiler tube, or niobium-stabilized 309 tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP309S, SA213 TP309H, SA213 TP309HCb, SA213 TP347, and SA213 TP310S. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP309Cb.

Chemical Composition of SA213 TP309Cb

Two chemistry layers matter for TP309Cb under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Read the niobium line first: Nb must be at least ten times the carbon content and not more than 1.10%. SHH STEEL reports the actual ladle values — including Nb — and the product values when ordered, and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP309Cb / UNS S30940 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; A480 Cr/Ni/Nb tolerance digits for the 22–24% Cr / 12–16% Ni band and the formula-minimum Nb path — applied from sister high-Cr / Nb practice; confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP309Cb / UNS S30940. Confirm the ordered ASME edition on the purchase order.

Element TP309Cb (UNS S30940) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 16.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) 10×C – 1.10

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 22.0 – 24.0 0.25 under / over 21.75 – 24.25
Nickel (Ni) 12.0 – 16.0 0.15 under / over 11.85 – 16.15
Niobium (Nb) 10×C – 1.10 0.05 under / over on max; min remains formula-tied max ≤ 1.15; min still ≥10×C on melt basis — confirm A480 path if contractual

Two points separate TP309Cb from ordinary SA213 TP309S. First, nickel is allowed up to 16.0% rather than the 15.0% ceiling used on TP309S and TP309H, giving the melt a slightly wider austenite window while chromium stays at 22.0–24.0%. Second, niobium is mandatory: the 10×C minimum ties Nb to the actual carbon of the heat so carbides are preferentially niobium carbides rather than chromium carbides after welding or elevated-temperature exposure. Carbon itself is still capped at 0.08% — this is not an H-grade carbon story. When creep-range boiler service needs both controlled carbon 0.04–0.10% and ASTM No. 7 or coarser grain size on top of the same Nb stabilization, open SA213 TP309HCb rather than stretching standard TP309Cb.

When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 21.75–24.25% and Ni 11.85–16.15%. The Nb maximum may move to 1.15% under the usual A480 0.05 over path, while the formula minimum remains melt-tied — confirm the contractual A480 reading if product Nb is acceptance-critical. Put any tighter project carbon, sulfur, or niobium window on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP309Cb

ASME SA-213 sets the tensile acceptance floor for TP309Cb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Hardness is capped at 192 HBW / 200 HV or 90 HRB. That room-temperature pair matches TP309S and TP309H; the commercial reason to pay for 309Cb is niobium stabilization chemistry plus the wider nickel window, not a higher tensile floor. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP309Cb / UNS S30940 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP309Cb requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM number in public heat-treatment excerpt (unlike H grades)

Flattening and flaring tests sit beside tension and hardness on a lot basis. Design calculations should use the 75/30 ksi pair unless the purchase order states higher guaranteed values the mill has accepted in writing. Public heat-treatment language does not assign a mandatory ASTM grain-size number to TP309Cb — that clause belongs to the H grades. When the datasheet needs H-grade carbon 0.04–0.10%, Nb 10×C–1.10%, and ASTM No. 7 or coarser grain size together, open SA213 TP309HCb; when Nb is not required and ordinary 22–24% Cr oxidation resistance is enough, open SA213 TP309S.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP309Cb is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because remaining wall after high-temperature oxidation is often a design input on the circuits where niobium-stabilized 309 is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP309Cb dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler / high-temperature bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP309Cb tube is often looser than a Code or heat-exchanger purchase order can afford. ASME SA-213 Grade TP309Cb / UNS S30940 is the governing designation for this article; EN and JIS wrought names that point to similar Nb-stabilized high-Cr–Ni families are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 309Cb,” confirm which product standard, tensile/hardness table, Nb line, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP309Cb Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30940 Unified number listed with the grade chemistry
ASTM A213 TP309Cb Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP309Cb
Related S-grade SA213 TP309S — same Cr band, Ni 12–15, no Nb
Related H+Cb SA213 TP309HCb — H-grade carbon + Nb + grain size
Related 18-8 stabilized SA213 TP347 — Nb-stabilized at lower Cr–Ni
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP309Cb is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare H-grade SA213 TP309H and combined H+Cb SA213 TP309HCb on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP309Cb under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. High chromium–nickel austenitics with mandatory niobium still need a thorough solution treatment so unwanted phases do not leave the tube in a condition that undercuts oxidation or corrosion performance in service.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP309Cb is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature, quench method, and measured Nb stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment. Public heat-treatment language does not assign a mandatory ASTM grain-size number to TP309Cb — grain-size rules belong to the H grades.

When Supplementary Requirement language for intergranular-corrosion capability is ordered, the corrosion test report travels with the heat-treatment record. H-grade grain-size rules do not rewrite the TP309Cb path — use SA213 TP309HCb when the datasheet calls for H-grade carbon, Nb stabilization, and grain-size controls together.

Corrosion Resistance

TP309Cb is selected primarily for high-temperature oxidation and scaling resistance from its 22–24% chromium and 12–16% nickel balance, with niobium stabilization added to prefer Nb carbides over chromium carbides after welding or elevated-temperature exposure. In oxidizing furnace atmospheres, hot-process gas circuits, and many elevated-temperature steam or air services, the higher Cr–Ni oxide scale outperforms ordinary 18-8 grades, and the Nb line helps keep chromium available for the scale rather than tied up as chromium carbide. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 309Cb as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP309Cb; selection remains engineering judgment against temperature, atmosphere, velocity, and inspection philosophy. Intergranular corrosion risk after welding is moderated by the mandatory Nb stabilization, by solution treating after fabrication when the sequence allows, or by invoking a contractual A262 Practice E Supplementary Requirement on the tube PO. SHH STEEL will not rank TP309Cb as equal to 316 in chlorides — niobium is not a molybdenum substitute.

Applications of SA213 TP309Cb Tube

Because TP309Cb brings a 22–24% Cr / 12–16% Ni balance under SA-213 with mandatory niobium and without adding molybdenum, it shows up in high-temperature oxidation-prone boiler and process circuits, furnace-related heat exchangers, and elevated-temperature HX duty where 18-8 scales too quickly and where Nb stabilization is preferred over a plain S-grade stamp. The table below pairs typical application areas with a selection note so the grade is chosen for atmosphere, metal temperature, and stabilization need — not only for the familiar “309Cb” name on the BOM.

Application area Typical use of TP309Cb tube Selection note
High-temperature oxidation + stabilization Seamless tube where 22Cr-12Ni scale resistance plus Nb carbides are specified Confirm design metal temperature, atmosphere, and Nb line on the PO
Boiler / process steam (oxidation-limited) Seamless generating or process tubing ordered to SA-213 with Nb reported For creep-critical H+Cb carbon/grain open TP309HCb
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits needing stabilization Prefer TP310S / TP310Cb if even higher Cr–Ni is specified
Welded or as-welded high-temp circuits Tube where Nb stabilization reduces chromium-carbide risk after joining Still qualify the WPS; Nb does not replace PWHT when Code requires it
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For plain S-grade without Nb open SA213 TP309S; for H-grade carbon and grain-size without Nb open SA213 TP309H; for combined H+Cb open SA213 TP309HCb; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP309Cb tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER309 / ER309L or niobium-bearing austenitic fillers under a qualified WPS; many fabricators prefer low-carbon deposits even when the base tube already carries Nb stabilization. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP309Cb is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. The mandatory Nb line on the tube chemistry reduces — but does not eliminate — sensitization risk in the heat-affected zone; discuss whether a post-weld solution treatment or a move to HCb better protects the joint when service temperatures sit in the sensitizing range. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP309Cb is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and Nb identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP309Cb includes heat analysis (with Nb reported), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP309Cb tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry — including Nb — on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP309Cb tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes that call out Nb reporting.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP309Cb as a Code Book product standard with enforceable chemistry — including the Nb 10×C–1.10% line — tensile, hardness, heat-treatment, and marking rules, not as a catalogue nickname for “any stabilized 309 tube.” The MTC reports the full ladle chemistry with measured Nb and the tensile/hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 309-family conversation honest for boiler and HX duty. If Nb is not required and ordinary 22–24% Cr oxidation resistance is enough, we open SA213 TP309S. If creep-range H-grade carbon and grain-size controls are required without Nb, we open SA213 TP309H. If both H-grade and Nb are specified together, we open SA213 TP309HCb. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 309Cb into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP309Cb stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for niobium-stabilized high-temperature boiler and heat-exchanger duty.

Item SHH STEEL capability for TP309Cb
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP309Cb / UNS S30940
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry including Nb on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry and Nb; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309Cb tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for niobium-stabilized high-temperature boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP309Cb
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative high-temp HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Nb reporting callouts, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), Nb reporting expectation, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry including Nb, tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP309S, SA213 TP309HCb, and SA213 TP347 sit on the same hub when the datasheet steps beyond TP309Cb.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP309Cb?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP309Cb include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP309Cb under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP309Cb?
TP309Cb is UNS S30940. Melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, nickel 12.0–16.0%, and niobium (Cb) 10×C–1.10%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the general-requirements path. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
What does Cb mean in TP309Cb under SA213?
Cb is the older commercial abbreviation for columbium, which is the same element as niobium (Nb). Under SA-213 the grade name keeps the historical Cb spelling while the chemistry table reports Nb (or Nb/Cb) as 10×C minimum up to 1.10% maximum. Ask the mill to report measured Nb on the EN 10204 3.1 certificate so receiving inspection can clear the heat without translating shop nicknames.
TP309Cb vs TP309S — when do I need niobium stabilization under SA213?
Order TP309Cb when the datasheet requires Nb 10×C–1.10% on the 22–24% Cr balance and accepts the wider Ni 12.0–16.0% window. Order TP309S when ordinary S-grade chemistry without niobium is enough for the oxidizing service. Both share a 75/30 ksi tensile floor, so tensile equality alone is not a reason to swap; confirm whether Nb is contractual before substituting either grade for the other.
TP309Cb vs TP309H — which SA213 grade should I order?
Order TP309Cb when niobium stabilization at C ≤0.08% is the requirement and no mandatory ASTM grain-size number is called out. Order TP309H when the boiler or superheater datasheet needs carbon 0.04–0.10% and ASTM No. 7 or coarser grain size without a niobium line. When both H-grade carbon/grain-size and Nb are required together, open TP309HCb rather than stretching either sister grade.
TP309Cb vs TP347 — which stabilized grade fits under SA213?
Both grades carry niobium stabilization, but TP309Cb sits on the 22–24% Cr / 12–16% Ni oxidation balance while TP347 is the classic 18-8 Nb-stabilized grade. Order TP309Cb when high-temperature oxidation resistance from the higher Cr–Ni balance is the driver; order TP347 when an 18-8 stabilized chemistry is what the datasheet and design metal temperature actually call for. Do not treat them as automatic dual-cert stock.
Does SA-213 set a hardness limit for TP309Cb?
Yes. The mechanical table for TP309Cb lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under SA-213, which differs from many SA312 / A312 pipe rows for related UNS numbers that omit a hardness cap. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What heat treatment does ASME SA-213 require for TP309Cb?
TP309Cb is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Public language does not assign a mandatory ASTM grain-size number to TP309Cb — that clause belongs to the H grades. Ask the mill to state anneal temperature, quench method, and measured Nb on the EN 10204 3.1 certificate.
Minimum wall vs average wall — which should I order for SA213 TP309Cb?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance — especially important when remaining wall after high-temperature oxidation is a design input. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling.
Is TP309Cb a good choice for chloride-rich cooling water under SA213?
Usually no. TP309Cb is framed for high-temperature oxidation resistance plus niobium stabilization, not for molybdenum-driven chloride pitting resistance. In seawater-leaning cooling water and wet brine exchangers, open TP316 / TP316L or higher-Mo grades on the SA213 hub. ASME SA-213 does not publish a chloride ranking that supports treating 309Cb as a 316 substitute.
Can you dual-certify ASME SA-213 and ASTM A213 TP309Cb?
Yes when the heat and testing support both independent standards. Dual SA-213/A213 marking is available when the purchase order requests both names on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly — a "309Cb" nickname alone is not dual certification.

Conclusion

ASME SA213 TP309Cb / UNS S30940 is the niobium-stabilized 22–24% Cr / 12–16% Ni seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when high-temperature oxidation resistance needs Cb stabilization rather than H-grade carbon and grain-size alone. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the 75/30 ksi tensile and hardness acceptance floors, with Nb reported on EN 10204 3.1 certificates — and dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Nb reporting expectation, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X