ASME SA213 UNS S30432 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 UNS S30432 Stainless Steel Tube

ASME SA213 UNS S30432 (commercially Super304H / 18Cr-9Ni-3Cu-Nb-N) seamless boiler and superheater tube with C 0.07–0.13%, Cu 2.5–3.5%, Nb 0.30–0.60%, N 0.05–0.12%, a 2000 °F [1100 °C] solution anneal, and tensile floors of 86/34 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting Cu, Nb, N, Al, and B.
Grade
UNS S30432 (no TP letter — Cu–Nb–N austenitic)
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 UNS S30432 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. UNS S30432 under that Code Book text is the copper–niobium–nitrogen austenitic listed without a TP letter grade — commercially known as Super304H or 18Cr-9Ni-3Cu-Nb-N — with melting limits of carbon 0.07–0.13%, chromium 17.0–19.0%, nickel 7.5–10.5%, copper 2.5–3.5%, niobium 0.30–0.60%, nitrogen 0.05–0.12%, plus controlled aluminum and boron microalloying. When a Code-stamped USC or advanced boiler datasheet calls for SA-213 UNS S30432, the purchase order and mill test certificate should carry the ASME designation and the full Cu–Nb–N chemistry set — not a TP304H heat with a trade-name sticker, and not a catalogue “Super304H” claim that omits the UNS number on the stencil.

SHH STEEL can supply ASME SA213 UNS S30432 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and superheater OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including Cu, Nb, N, Al, and B — plus the 86/34 ksi tensile and hardness acceptance set after the 2000 °F [1100 °C] solution treatment. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called Super304H, S30432 boiler tube, 18Cr-9Ni-3Cu-Nb-N HX tube, or SA213 S30432 superheater tube; none of those phrases replace the ASME UNS designation on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP304H, SA213 TP321H, SA213 TP347H, SA213 TP347HFG, and SA213 TP310H. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 UNS S30432.

Chemical Composition of SA213 UNS S30432

Two chemistry layers matter for UNS S30432 under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Copper, niobium, nitrogen, aluminum, and boron are first-class elements for this grade — an MTC that reports only Cr–Ni–C is incomplete for S30432. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for UNS S30432 and the product-analysis limits that result from applying A480 Table A1.1 tolerances where published. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; A480 product-tolerance digits for Al and B microalloy bands if product analysis is contractual (edition-dependent practice) — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for UNS S30432. Confirm the ordered ASME edition on the purchase order.

Element UNS S30432 melting analysis
Carbon (C) 0.07 – 0.13
Manganese (Mn) ≤ 1.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.010
Silicon (Si) ≤ 0.30
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 7.5 – 10.5
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.05 – 0.12
Niobium (Nb) 0.30 – 0.60
Copper (Cu) 2.5 – 3.5
Aluminum (Al) 0.003 – 0.030
Boron (B) 0.001 – 0.010

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.07 – 0.13 0.01 under / over 0.06 – 0.14
Manganese (Mn) ≤ 1.00 0.03 over ≤ 1.03
Phosphorus (P) ≤ 0.040 0.010 over ≤ 0.050
Sulfur (S) ≤ 0.010 0.005 over ≤ 0.015
Silicon (Si) ≤ 0.30 0.05 over ≤ 0.35
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 7.5 – 10.5 0.10 under / 0.15 over 7.40 – 10.65
Nitrogen (N) 0.05 – 0.12 0.01 under / 0.02 over 0.04 – 0.14
Niobium (Nb) 0.30 – 0.60 0.05 under / over 0.25 – 0.65
Copper (Cu) 2.5 – 3.5 0.10 under / over 2.40 – 3.60
Aluminum (Al) 0.003 – 0.030 0.005 under / over (practice) 0.000 – 0.035 (confirm A480 edition)
Boron (B) 0.001 – 0.010 edition-dependent microalloy tolerance confirm A480 edition if contractual

Copper 2.5–3.5% and niobium 0.30–0.60% are the commercial point of S30432 relative to plain SA213 TP304H: Cu–Nb precipitation and nitrogen support the elevated 86/34 ksi tensile floor and the creep-oriented framing that advanced boiler programs specify. Carbon 0.07–0.13% is intentional for high-temperature strength — this is not a low-carbon LN story. Tight Mn ≤1.00%, Si ≤0.30%, and S ≤0.010% ceilings further distinguish the melt from ordinary 18-8 H-grade heats. When the datasheet only needs H-grade carbon and grain size without copper, open TP304H rather than stretching a Super304H trade name onto the wrong chemistry.

When product analysis is ordered, finished tube may read C 0.06–0.14%, Mn ≤1.03%, P ≤0.050%, S ≤0.015%, Si ≤0.35%, Cr 16.80–19.20%, Ni 7.40–10.65%, N 0.04–0.14%, Nb 0.25–0.65%, and Cu 2.40–3.60%, with Al and B product limits confirmed against the A480 edition named on the PO. Put any tighter project copper floor, niobium band, or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of SA213 UNS S30432

ASME SA-213 sets the tensile acceptance floor for UNS S30432 at 86 ksi [590 MPa] tensile strength and 34 ksi [235 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Hardness is capped at 219 HBW / 230 HV or 95 HRB — notably higher than the 192 HBW / 90 HRB ceiling used for TP304H. That elevated strength-and-hardness pair is the mechanical signature of the Cu–Nb–N chemistry and should appear on the MTC; a heat that only clears 75/30 ksi is not S30432 acceptance. Every lot sampled under the edition’s specimen rules must meet those numbers after the final 2000 °F solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for UNS S30432 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property UNS S30432 requirement
Tensile strength, min 86 ksi [590 MPa]
Yield strength (0.2% offset), min 34 ksi [235 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 219 HBW / 230 HV or 95 HRB

Flattening and flaring tests sit beside tension and hardness on a lot basis. Design calculations should use the 86/34 ksi pair unless the purchase order states higher guaranteed values the mill has accepted in writing. Public SA-213 / A213 grade text for S30432 does not mirror the H-grade ASTM No. 7 or coarser grain-size column used for TP304H — do not invent a grain-size requirement from a Super304H brochure. When the datasheet needs plain H-grade carbon and grain size without Cu–Nb, open SA213 TP304H; when fine-grain 347H framing is required, open SA213 TP347HFG.

Dimensions and Tolerances

Dimensional supply for ASME SA213 UNS S30432 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because remaining wall after steam-side oxidation is a design input on advanced superheater and reheater circuits.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 UNS S30432 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / reheater bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, bend form, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Cu–Nb–N austenitics work-harden and need careful bend-radius planning; discuss any post-bend heat treatment early. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around UNS S30432 tube is often looser than a Code or advanced-boiler purchase order can afford. ASME SA-213 UNS S30432 is the governing designation for this article; proprietary Super304H trade names and approximate wrought designations point to the same chemistry family but are not automatic substitutes for the UNS number on an SA-213 mill test certificate. When a datasheet says “equivalent to Super304H,” confirm which product standard, Cu–Nb–N bands, tensile floor, and heat-treatment temperature the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M UNS S30432 Governing ASME Code Book seamless boiler / superheater tube product standard for this article
UNS S30432 Unique identifier — no TP letter in the SA-213 grade table
ASTM A213 UNS S30432 Separate ASTM International product specification — dual-mark only when the PO asks; see A213 UNS S30432
Super304H (commercial) Trade name commonly used for this chemistry family — does not replace UNS S30432 on the stencil or MTC
Related H-grade 18-8 SA213 TP304H when Cu–Nb is not required
Related plate A240 / SA240 flat product may not list this tube-oriented UNS the same way — order plate and tube under their own product standards

ASTM A213 UNS S30432 is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare stabilized and fine-grain H grades such as SA213 TP347H and SA213 TP347HFG on their own ASME pages before swapping grades in a USC tube circuit.

Heat Treatment and Delivery Condition

UNS S30432 under ASME SA-213 is furnished solution treated at a minimum of 2000 °F [1100 °C] — notably hotter than the 1900 °F [1040 °C] row used for TP304 / TP304H — then water quenched or rapidly cooled. That higher solution temperature is intentional for dissolving Cu–Nb-related phases before quench. Skipping or under-cooling the anneal can leave a structure that fails both hardness and creep-oriented expectations even when ladle chemistry looked correct on paper.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL S30432 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for corrosion or special microstructural checks is ordered, those reports travel with the heat-treatment record. Do not borrow TP304H grain-size language onto an S30432 certificate unless the ordered edition and purchase order actually require it — and do not treat a 1900 °F anneal as interchangeable with the 2000 °F row this grade carries.

Corrosion Resistance

S30432 is framed for high-temperature steam oxidation and creep-oriented boiler service, not as a chloride-pitting upgrade over TP316. Copper and niobium serve strength and microstructural stability in steam service; they are not molybdenum. In wet chloride-bearing exchangers, do not select S30432 as a substitute for SA213 TP316L or higher-Mo grades. Intergranular corrosion after fabrication is a different conversation from steam oxidation: carbon 0.07–0.13% is intentional for creep strength, so as-welded wet-service IGC resistance is not the grade’s selling point.

ASME SA-213 itself does not publish a corrosion-rate or PREN table for S30432; selection remains engineering judgment against steam temperature, fireside environment, and the design code allowables. When a project specification adds a named corrosion or oxidation test, write that Supplementary Requirement onto the purchase order so the test is contractual. SHH STEEL will not rank Super304H-class tube as a chloride HX grade — that claim is not supported by the product standard.

Applications of SA213 UNS S30432 Tube

UNS S30432 is ordered for advanced boiler and superheater tubing — especially USC and high-efficiency fossil units — where Cu–Nb–N austenitic creep strength and steam oxidation resistance justify the chemistry premium over TP304H. It is not the default grade for general corrosive HX duty. The table below pairs typical application areas with a selection note so the grade is chosen for design metal temperature and Code allowables — not only for the Super304H trade name on the BOM.

Application area Typical use of S30432 tube Selection note
USC / advanced boiler superheaters Seamless tube where Super304H-class creep and oxidation framing is specified Confirm design metal temperature and Code allowables
Reheater / final superheater sections High steam-side metal temperature service Compare with TP347H / TP347HFG when Nb-stabilized fine-grain framing is preferred
High-efficiency fossil retrofit circuits Tube replacements where S30432 is named on the datasheet Do not substitute TP304H without engineering approval
Programs specifying 86/34 ksi austenitic tube When the mechanical table floor itself is a purchase driver Require Cu, Nb, N, Al, B on the MTC — not Cr–Ni alone
General corrosive HX duty Usually not the preferred selection Open TP304L / TP316L family instead
Chloride-rich cooling water Not a molybdenum substitute Open SA213 TP316L or higher

For plain H-grade 18-8 without copper open SA213 TP304H; for stabilized H grades browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

UNS S30432 tube welding for tube-to-tubesheet joints, attachment welds, and fabrication joins should follow a WPS qualified for the Cu–Nb–N chemistry and the applicable boiler Code — matching filler selection is not the same conversation as for plain TP304H. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility; SA-213 governs the seamless tube product, not the field or shop weld procedure. Because carbon sits in the 0.07–0.13% band, as-welded wet-service IGC resistance is not the grade’s primary claim — discuss post-weld heat treatment when the fabrication sequence and service environment require it.

Because SA213 UNS S30432 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual microstructural or corrosion checks on the base metal. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned, and confirm filler brand/AWS classification on the enquiry when the project locks a matching Super304H-class consumable.

Surface Finishes

Standard mill delivery for ASME SA213 UNS S30432 is solution annealed and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface and must be called out because it changes the heat-treatment route at the elevated 2000 °F solution temperature. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a project specification quotes an Ra maximum or a special OD grind for tube expanding, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for UNS S30432 includes heat analysis (with Cu, Nb, N, Al, and B reported), tension tests to the 86/34 ksi floor, hardness tests to the 219 HBW / 95 HRB maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, UNS number, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on S30432 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or special microstructural checks from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube including Cu–Nb–N microalloy bands
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Minimum vs average wall States which wall basis the size callout uses
Special microstructural / oxidation checks Project-specific Supplementary Requirements for USC programs
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate. An MTC that omits copper, niobium, or nitrogen, or that reports a 1900 °F anneal instead of the 2000 °F row, is incomplete for S30432 — reject it before the heat leaves the mill.

Packaging and Shipping

UNS S30432 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 UNS designation, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. Superheater and reheater cut lengths often need extra cradle or case protection so ends and bend forms are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 UNS S30432 as a Code Book product standard with enforceable Cu–Nb–N chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any Super304H tube.” The MTC reports the full ladle chemistry including Cu, Nb, N, Al, and B, the 86/34 ksi tensile plus hardness acceptance set, and the 2000 °F solution treatment; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the advanced-boiler conversation honest. If the datasheet only needs H-grade carbon and grain size without copper, we open SA213 TP304H. If Nb-stabilized or fine-grain framing is preferred, we open SA213 TP347H / SA213 TP347HFG. If chlorides dominate a wet exchanger, we open SA213 TP316L rather than stretching S30432 into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 UNS S30432 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for advanced boiler and superheater duty.

Item SHH STEEL capability for UNS S30432
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade UNS S30432 (no TP letter)
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / reheater bundles; mill random by agreement
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (86/34 ksi), hardness (max 219 HBW / 95 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry including Cu–Nb–N–Al–B on MTC; product analysis on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes UNS S30432 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for advanced boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for UNS S30432
Outside diameter 31.8, 38.1, 42.4, 44.5, 50.8, 57.0, 63.5, 76.2 mm (and other superheater/reheater ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–16 class walls and metric min-wall equivalents typical for superheater duty; lighter and heavier walls by agreement
Common OD × wall examples 38.1 × 3.40 mm; 42.4 × 3.40 mm; 44.5 × 3.60 mm; 50.8 × 3.60 mm; 50.8 × 4.00 mm; 63.5 × 4.00 mm — illustrative boiler/superheater sizes, confirm min vs average wall
Length Cut lengths for superheater / reheater circuits; straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual SA-213/A213 marking, and project Supplementary Requirements — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including Cu, Nb, N, Al, and B), tensile, hardness, and the 2000 °F solution treatment against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP304H, SA213 TP347H, and SA213 TP347HFG sit on the same hub when the datasheet steps beyond S30432.

FAQ

Is ASME SA-213 the same as ASTM A213 for UNS S30432?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 UNS S30432 have a TP grade letter?
No. S30432 is listed by UNS number in the SA-213 austenitic chemistry table without a TP letter such as TP304H. Purchase orders, stencils, and MTCs should carry UNS S30432 (and the ASME SA-213 designation), not a made-up "TP30432" nickname. Commercial Super304H trade names are useful for conversation but do not replace the UNS number on Code documentation.
Is Super304H the same as ASME SA213 UNS S30432?
Super304H is a commercial trade name commonly used for the Cu–Nb–N chemistry family that SA-213 lists as UNS S30432. They point to the same grade family when the mill actually certifies SA-213 UNS S30432 with the full chemistry and 86/34 ksi mechanical row. Do not accept a trade-name-only certificate that omits the ASME designation and UNS number when the datasheet calls for SA-213.
S30432 vs TP304H — when do I need the Cu–Nb–N grade under SA213?
Order UNS S30432 when the advanced boiler or USC datasheet needs the Cu–Nb–N chemistry, the 86/34 ksi tensile floor, the 219 HBW / 95 HRB hardness ceiling, and the 2000 °F solution treatment. Order TP304H when H-grade carbon 0.04–0.10%, ASTM No. 7 or coarser grain size, and the 75/30 ksi floor are enough without copper. They are not interchangeable stamps — confirm design metal temperature and Code allowables before swapping.
What heat treatment does ASME SA-213 require for UNS S30432?
UNS S30432 is solution treated at a minimum of 2000 °F [1100 °C] and then water quenched or rapidly cooled. That temperature is hotter than the 1900 °F [1040 °C] row used for TP304H and is intentional for the Cu–Nb chemistry. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate — a 1900 °F record is not acceptance for this grade.
What are the tensile and hardness numbers for SA213 UNS S30432?
The mechanical table sets tensile strength at 86 ksi [590 MPa] minimum, yield strength at 34 ksi [235 MPa] minimum (0.2% offset), elongation at 35% minimum in 2 in. or 50 mm, and hardness at a maximum of 219 HBW / 230 HV or 95 HRB. Those floors are higher than the TP304H 75/30 ksi and 192 HBW / 90 HRB pair. Design calculations should use the Code Book numbers unless the mill has accepted higher guaranteed values in writing.
Does SA-213 require a grain-size number for UNS S30432?
Public SA-213 / A213 grade text for S30432 does not mirror the H-grade ASTM No. 7 or coarser grain-size column used for TP304H. Do not invent a grain-size requirement from a Super304H brochure. If a project specification adds a grain-size Supplementary Requirement, write it onto the purchase order with the ASTM E112 method and acceptance number so the test is contractual.
Does ASME SA213 UNS S30432 include welded tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard. The process choice for S30432 under SA-213 is cold-finished versus hot-finished seamless tube, plus the 2000 °F heat-treatment and testing clauses of the ordered edition. Welded stainless pipe belongs to a different product standard family.
Minimum wall vs average wall — which should I order for SA213 S30432?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance — common on superheater and reheater circuits where remaining wall after oxidation is a design input. Order average wall only when the purchase order explicitly allows it and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling and tolerance tables.
Can S30432 replace TP316L in chloride service under SA213?
No as a general rule. S30432 is framed for high-temperature steam oxidation and creep-oriented boiler service; copper and niobium are not molybdenum. In wet chloride-bearing exchangers, open TP316L or higher-Mo grades on the SA213 hub rather than stretching Super304H-class tube into chloride HX duty. ASME SA-213 does not publish a chloride ranking that supports that substitution.
Can you dual-certify ASME SA-213 and ASTM A213 UNS S30432?
Yes when the heat and testing support both independent standards. Dual SA-213/A213 marking is available when the purchase order requests both names on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly — a Super304H trade-name-only certificate is not dual certification.

Conclusion

ASME SA213 UNS S30432 is the Cu–Nb–N austenitic seamless stainless steel tube grade for advanced boiler, superheater, and reheater service when Super304H-class chemistry, the 86/34 ksi tensile floor, and the 2000 °F solution treatment are required on the Code documentation. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the tensile and hardness acceptance floors, and documented on EN 10204 3.1 certificates that report Cu, Nb, N, Al, and B — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X