ASME SA213 TP347HFG Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP347HFG Stainless Steel Tube

ASME SA213 TP347HFG / UNS S34710 fine-grain niobium-stabilized H-grade seamless boiler, superheater and heat-exchanger tube — C 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb ≥8×C ≤1.10%, Table 4 80/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, ASTM grain size No. 7 to 10, cold-finished only after Footnote I softening. SHH STEEL supplies cold-finished seamless tube with EN 10204 3.1 MTCs that report Nb, carbon floor, softening/solution temperatures, and grain size inside 7–10.
Grade
TP347HFG / UNS S34710
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished only — SA-213 / A213 6.1)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP347HFG Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers or superheaters invoke that adoption by name for fine-grain niobium H-grade service, SA-213 is the governing product standard for this HFG tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP347HFG / UNS S34710 is the fine-grain H-grade niobium-stabilized austenitic row. Melting carbon is locked inside 0.06–0.10% (a higher floor than TP347H’s 0.04%), chromium 17.0–19.0%, nickel 9.0–13.0%, and niobium ≥8 × C ≤1.10% — the same Nb formula as TP347H, not the non-H 10 × C rule. Table 4 raises tensile to 80 ksi [550 MPa] / 30 ksi [205 MPa] with 35% elongation and hardness max 192 HBW / 90 HRB, and grain size must fall in ASTM No. 7 to 10. Manufacture is cold-finished only (clause 6.1), after a Footnote I softening heat treatment before cold work. This is not a dual stamp of TP347H or TP347.

SHH STEEL can supply ASME SA213 TP347HFG as seamless cold-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report carbon inside 0.06–0.10%, the 8 × C niobium result, softening and solution temperatures, grain size inside 7–10, and the 80/30 ksi tensile set. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP347HFG.

Shop names include “347HFG,” “S34710,” “fine-grain 347H,” and “FG 347H tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP347HFG / UNS S34710, wall basis, OD × wall or BWG, and any Supplementary Requirements. Hot-finished delivery is not an option for this UNS row. Sister SA213 pages include SA213 TP347H, SA213 TP347, SA213 TP321H, and SA213 TP347LN. Seamless cold-finished only — no Manufacturing Types (SML / WLD / HCW) H2 and no hot-finished capability claim on this product page.

Chemical Composition of SA213 TP347HFG

Two chemistry layers matter for TP347HFG under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. Three chemistry lines define the grade for a reviewer beside the process rules: carbon 0.06–0.10% (higher floor than TP347H), niobium ≥8 × C ≤1.10% (same formula as TP347H, not the non-H 10 × C rule), and chromium/nickel 17.0–19.0% / 9.0–13.0%. The fine-grain and cold-finished rules live in manufacture and heat-treatment clauses, not in a unique Nb formula.

The tables below reproduce the melt limits for TP347HFG / UNS S34710, the product-analysis limits from A480 Table A1.1 practice, and a short carbon / grain / tensile snapshot against TP347 and TP347H. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. Creep-rupture allowables that buyers associate with “fine-grain 347H” are design-code language — SA-213 itself publishes the chemistry, grain band, and tensile floors, not a creep curve on the product page.

Melting analysis (heat / ladle analysis)

Element TP347HFG (UNS S34710) melting analysis
Carbon (C) 0.06 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) ≥ 8 × C, ≤ 1.10
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for Grade TP347HFG / UNS S34710 (same grade text family). Confirm the ordered edition. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.06 – 0.10 0.01 under / over 0.05 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Niobium (Nb) ≥ 8 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C

UNCERTAIN: A480 Nb product-tolerance digits — applied from sister-pack Nb practice; confirm A480 edition if product analysis is contractual.

Carbon, grain, and tensile snapshot — TP347 / TP347H / TP347HFG

Item TP347 (S34700) TP347H (S34709) TP347HFG (S34710)
C ≤ 0.08 0.04 – 0.10 0.06 – 0.10
Nb ≥ 10 × C, ≤ 1.10 ≥ 8 × C, ≤ 1.10 ≥ 8 × C, ≤ 1.10
Grain size (Table 3) no mandatory number No. 7 or coarser No. 7 – 10
Table 4 tensile, min 75 ksi [515 MPa] 75 ksi [515 MPa] 80 ksi [550 MPa]
Manufacture CF or HF CF or HF Cold-finished only

Dual TP347H/TP347HFG is not a casual chemistry path: the carbon floors differ (0.04 vs 0.06), the grain rules differ (“7 or coarser” vs “7–10”), the tensile floors differ (75 vs 80 ksi), and hot-finished TP347H cannot meet the HFG cold-finished-only manufacture rule. Dual TP347/TP347HFG is likewise blocked by carbon floor and grain/tensile/manufacture differences. Versus SA213 TP321H, TP347HFG carries niobium rather than titanium and adds the fine-grain / Footnote I package.

Mechanical Properties of SA213 TP347HFG

ASME SA-213 Table 4 sets the tensile acceptance floor for TP347HFG / UNS S34710 at 80 ksi [550 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. That tensile floor is 5 ksi higher than TP347 and TP347H (both 75 ksi). Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance. Grain size must fall in ASTM No. 7 to 10 — a band with both a coarse bound (7) and a fine bound (10) — determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112. UNCERTAIN: how design-code creep-rupture allowables for fine-grain S34710 are framed relative to coarse-grain S34709 on a given Code edition — SA-213 publishes the grain band and tensile floors, not the allowables table.

Property TP347HFG requirement (Table 4)
Tensile strength, min 80 ksi [550 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 to 10 (per heat-treatment lot)

Source: public SA-213 / A213 Table 4 for UNS S34710 / TP347HFG and Table 3 grain-size column “7–10”. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits grain size inside the 7–10 band, or that reports 75 ksi as if the heat were TP347H, is incomplete for TP347HFG. Do not accept a coarse-grain “7 or coarser” reading that sits outside the fine bound of 10 as HFG acceptance.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP347HFG is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and superheater datasheets that pick fine-grain HFG tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Manufacture is cold-finished only; do not request hot-finished delivery for this UNS row.

Item Typical SA213 TP347HFG dimensional practice
Product form Seamless cold-finished only (clause 6.1)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for boiler / superheater datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for cold-finished tube
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the carbon floor, Nb formula, Footnote I path, or 7–10 grain-size check.

Equivalent Grades

Equivalence language around 347HFG tube often collapses it with coarse-grain 347H or with non-H 347. ASME SA-213 Grade TP347HFG / UNS S34710 is the governing designation for this article; wrought names that mention “fine-grain 347H” point to related families but are not automatic substitutes on an SA-213 mill test certificate.

Designation Notes
ASME SA-213 / SA-213M Grade TP347HFG Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S34710 Unified number in the stainless chemistry table
ASTM A213 TP347HFG Separate ASTM product specification — twin page A213 TP347HFG; dual-mark only when the PO asks
Related coarse-grain H SA213 TP347H — C 0.04–0.10, grain 7 or coarser, 75 ksi, CF or HF
Related non-H Nb SA213 TP347 — C ≤0.08, Nb ≥10×C, no mandatory grain number
Related Ti H-grade SA213 TP321H — titanium, not niobium; no HFG fine-grain package
Related plate A240 / SA240 flat product in related UNS families

Dual SA-213/A213 marking is a purchase-order option. Do not substitute coarse-grain TP347H paperwork for fine-grain TP347HFG without reopening carbon, grain, tensile, and manufacture rules.

Heat Treatment and Delivery Condition

TP347HFG under ASME SA-213 is furnished solution treated at 2150 °F [1175 °C] (public Table 3), then quenched in water or cooled rapidly by other means, with Footnote F on the quench capability. Grain size after heat treatment must fall in ASTM No. 7 to 10 for the heat-treatment lot. Footnote I on the TP347HFG heat-treatment row requires that solution treatment be preceded by a softening heat treatment prior to cold working: the softening temperature shall be at least 90 °F [50 °C] higher than the solution heat treatment temperature, which Footnote I states shall be at 2150 °F [1180 °C] minimum. UNCERTAIN: the SI conversion difference between the Table 3 bracket [1175 °C] and the Footnote I body [1180 °C] — confirm the ordered edition wording and mill practice before treating either digit as the sole contractual temperature.

Clause 6.1 states that Grade TP347HFG shall be cold finished — so the Footnote I softening-before-cold-work sequence is not optional process folklore; it is part of how the grade is made. Hot-finished delivery is not an SA-213 option for this UNS row. The public SA-213 / A213–13 Supplementary Requirement S2 list includes TP347 and TP347H but does not list TP347HFG in the excerpt used here — UNCERTAIN whether a later edition adds HFG to S2; do not assume S2 from the TP347H listing alone. Write any stabilization or IGC Supplementary Requirement explicitly on the purchase order.

Delivery condition for SHH STEEL TP347HFG is cold-finished, solution annealed (after the Footnote I softening sequence) and pickled (or bright annealed by agreement), with softening temperature, solution temperature, quench method, niobium result, and grain-size result inside 7–10 stated on the EN 10204 3.1 certificate. For coarse-grain H-grade Nb without the HFG package open SA213 TP347H; for non-H Nb open SA213 TP347.

Corrosion Resistance

ASME SA213 TP347HFG is selected when fine-grain niobium H-grade packaging — carbon 0.06–0.10%, Nb ≥8 × C, grain size No. 7–10, 80 ksi tensile, cold-finished manufacture after Footnote I softening — is named for creep-range boiler and superheater service. Niobium stabilization addresses sensitizing-range intergranular framing; the fine-grain band and higher tensile floor are what separate HFG from coarse-grain SA213 TP347H.

It is not a molybdenum grade and is not automatically better than TP304L in every chloride wet service. Creep-rupture allowables that buyers associate with fine-grain S34710 are design-code language — confirm the Code edition allowables table rather than assuming SA-213 publishes them on the product page. UNCERTAIN: exact creep-allowable framing relative to S34709 on a given Code edition.

SHH STEEL reports carbon, niobium, softening/solution temperatures, and grain size inside 7–10 on the 3.1 certificate so inspectors can verify the full HFG package rather than accepting a coarse-grain 347H heat stamped as HFG.

Applications of SA213 TP347HFG Tube

Typical ASME SA213 TP347HFG uses include Code-stamped boiler and superheater tubes where fine-grain 347H / S34710 is named, high-temperature creep-range services that reject coarse-grain-only TP347H certificates, and replacement tube matching original HFG MTCs with grain size inside 7–10 and 80 ksi tensile.

  • Boiler / superheater tube naming SA-213 TP347HFG or fine-grain 347H
  • Creep-range Code services that require grain size No. 7–10 and 80 ksi tensile
  • Cold-finished-only Nb H-grade bundles after Footnote I softening
  • Replacement bundles matching original S34710 certificates

For coarse-grain H-grade Nb without the HFG package, compare SA213 TP347H. For non-H Nb, compare SA213 TP347. For titanium H-grade, compare SA213 TP321H.

Weldability

TP347HFG welds with matching niobium-stabilized austenitic filler practices — commonly ER347 / ER347H family wires selected to the project WPS. Niobium in the base metal supports as-welded intergranular framing; still follow qualified procedures for heat input, interpass, and purge on thin boiler / HX tube.

Do not assume S2 stabilization from the TP347H listing — write any stabilization or IGC Supplementary Requirement explicitly on the purchase order for this UNS. Do not dual-stamp a TP347H weld procedure as TP347HFG without reopening carbon floor (0.06%), grain-size band 7–10, 80 ksi tensile, cold-finished-only manufacture, and Footnote I path on the WPS / PQR.

Fine-grain and Footnote I controls do not remove purge discipline on thin-wall orbital welds; they add certificate checks the fabricator must verify before release.

Surface Finishes

Standard mill delivery for ASME SA213 TP347HFG is cold-finished, solution annealed (after Footnote I softening) and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the carbon floor, Nb formula, Footnote I path, or 7–10 grain-size check. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP347HFG includes heat analysis (C 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb ≥8 × C ≤1.10%), tension tests to the 80/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, grain size inside No. 7–10 per heat-treatment lot, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm carbon floor, niobium formula, softening/solution temperatures, and E112 grain-size result inside 7–10 rather than trusting a “347H family” PMI without those HFG checks. Do not accept a 75 ksi tensile reading as HFG acceptance. Stabilization / A262 practices apply only when named on the PO.

EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP347HFG tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP347HFG, UNS S34710, heat number, size, and wall basis so receivers can match the 3.1 certificate — including carbon, niobium, softening/solution temperatures, and grain size inside 7–10 — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP347HFG only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP347HFG as a Code Book fine-grain niobium H-grade product with enforceable C 0.06–0.10%, Cr 17–19%, Ni 9–13%, Nb ≥8 × C ≤1.10%, grain size No. 7–10, 80/30 ksi tensile, cold-finished-only manufacture after Footnote I softening, and marking rules — not as “347H with FG stamped on” checked only by a PMI peak. Enquiry review verifies the full HFG package before release.

That stops silent substitution with coarse-grain TP347H or non-H TP347 heats on datasheets that actually require S34710. We keep SA-213 and A213 independent, dual-mark only on request, and put softening/solution temperatures and grain size inside 7–10 on the 3.1 certificate.

Cross-links: SA213 TP347H, SA213 TP347, SA213 TP321H, SA213 TP347LN, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP347HFG stainless steel tube against the edition named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for fine-grain cold-finished niobium H-grade boiler and superheater tube.

Item SHH STEEL capability for TP347HFG
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP347HFG / UNS S34710
Product form Seamless cold-finished only (no hot-finished option)
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with C, Nb, softening/solution temps, and grain size 7–10; witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347HFG against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for fine-grain cold-finished boiler and superheater tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small superheater / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common boiler / superheater band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, and whether dual A213 marking or additional Supplementary Requirements are required. We reply with available mill / stock options for ASME SA213 TP347HFG and the matching document set — cold-finished only.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP347HFG?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, and Nb ≥8 × C ≤1.10% — tensile 80/30 ksi, elongation 35%, hardness, grain size No. 7–10, and cold-finished-only manufacture align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP347HFG allow hot-finished or welded tube?
No. Clause 6.1 requires Grade TP347HFG to be cold finished, and this SA213 product page covers seamless tube only. Hot-finished delivery is not an SA-213 option for UNS S34710. Welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
TP347HFG vs TP347H — why are they not interchangeable under SA213?
Carbon floors differ (0.06–0.10% vs 0.04–0.10%), grain rules differ (No. 7–10 band vs “7 or coarser”), tensile floors differ (80 ksi vs 75 ksi), manufacture differs (cold-finished only vs CF or HF), and HFG adds the Footnote I softening-before-cold-work path. Do not treat coarse-grain TP347H paperwork as HFG acceptance. Compare SA213 TP347H on its own page before substituting.
What is the UNS number and chemistry focus of ASME SA213 TP347HFG?
UNS S34710. Check C 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, and niobium ≥8 × C with a 1.10% ceiling — the same Nb formula as TP347H, not the non-H 10 × C rule. Grain size No. 7–10, 80 ksi tensile, and cold-finished-only manufacture after Footnote I softening complete the HFG package beside chemistry.
Why is the Table 4 tensile floor 80 ksi for TP347HFG?
Public SA-213 / A213 Table 4 sets TP347HFG at 80 ksi [550 MPa] tensile and 30 ksi [205 MPa] yield with 35% elongation — 5 ksi higher tensile than TP347 and TP347H (both 75 ksi). Hardness still caps at 192 HBW / 90 HRB. A certificate that reports 75 ksi as if the heat were TP347H is incomplete for TP347HFG. Ask for the 80 ksi floor and the E112 result inside 7–10 together.
What does Footnote I require for TP347HFG under SA213?
Footnote I requires a softening heat treatment prior to cold working, with softening temperature at least 90 °F [50 °C] higher than the solution heat treatment temperature, which Footnote I states shall be at 2150 °F [1180 °C] minimum. Public Table 3 lists solution treatment at 2150 °F [1175 °C]. UNCERTAIN: the SI conversion difference between [1175 °C] and [1180 °C] — confirm the ordered edition wording and mill practice before treating either digit as the sole contractual temperature.
Is Supplementary Requirement S2 listed for TP347HFG under SA213?
The public SA-213 / A213–13 Supplementary Requirement S2 list includes TP347 and TP347H but does not list TP347HFG in the excerpt used for this pack. UNCERTAIN whether a later edition adds HFG to S2. Do not assume S2 from the TP347H listing alone — write any stabilization or IGC Supplementary Requirement explicitly on the purchase order for this UNS.
Can I substitute TP347H stock for a TP347HFG datasheet under SA213?
Not without reopening carbon floor, grain-size band 7–10, 80 ksi tensile, cold-finished-only manufacture, and Footnote I path. Hot-finished TP347H cannot meet the HFG cold-finished-only rule, and a “7 or coarser” grain reading outside the fine bound of 10 fails HFG acceptance. Order TP347HFG by name when the datasheet requires the fine-grain package.
Minimum wall vs average wall — which should I order for SA213 TP347HFG?
Most boiler and superheater datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in. State wall basis, OD × wall or BWG on the RFQ — manufacture is cold-finished only for this grade.
Is TP347HFG a good choice for chloride-rich cooling water under SA213?
Not automatically. Fine-grain Nb H-grade packaging addresses creep-range and sensitizing-range framing; it does not add molybdenum for chloride pitting/crevice performance. Many wet cooling-water lists prefer L-carbon or Mo-bearing grades. Keep TP347HFG where the datasheet names fine-grain 347H boiler / superheater service.
Can you dual-certify ASME SA-213 and ASTM A213 TP347HFG?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including C 0.06–0.10%, Cr 17–19%, Ni 9–13%, Nb ≥8 × C ≤1.10%, grain size No. 7–10, 80/30 ksi, cold-finished manufacture, and Footnote I path. Dual marking does not merge the standards into one document. See also the twin page A213 TP347HFG.
What hydrostatic or NDE path applies to SA213 TP347HFG?
Hydrostatic testing or nondestructive examination follows the path selected on the purchase order under the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Neither hydro nor NDE replaces the chemistry, 80 ksi tensile, grain-size 7–10, or Footnote I certificate checks that define this fine-grain H-grade row. Name the preferred test path on the RFQ.

Conclusion

ASME SA213 TP347HFG / UNS S34710 is the fine-grain niobium-stabilized H-grade seamless stainless steel tube for Code boiler and superheater service when C 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb ≥8 × C ≤1.10%, ASTM grain size No. 7 to 10, an 80/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and cold-finished manufacture after Footnote I softening are required together. SHH STEEL supplies cold-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report carbon, niobium, softening/solution temperatures, and grain size inside 7–10. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X