ASME SA213 TP321H Stainless Steel Tube

ASME SA213 TP321H / UNS S32109 seamless boiler, superheater and heat-exchanger tube with carbon 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–12.0%, titanium ≥4×(C+N) ≤0.70%, Table 4 floor 75/30 ksi, hardness max 192 HBW / 90 HRB, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report carbon band, titanium formula, finish-route anneal temperature, and E112 grain size.
Grade
TP321H / UNS S32109
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP321H Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. On Code-stamped boilers and superheaters that invoke the ASME adoption by name, SA-213 is the governing product standard for this titanium-stabilized H-grade tube — written as its own Code Book line, not as a dual synonym of ASTM A213. Start from SA213/SA213M when the enquiry is Code-led.

Grade TP321H / UNS S32109 is the high-temperature titanium-stabilized austenitic row built for creep-oriented boiler / superheater duty inside that SA-213 family. Carbon is a true 0.04–0.10% band with both floor and ceiling, chromium 17.0–19.0%, nickel 9.0–12.0%, and titanium ≥4 × (C + N) with a 0.70% ceiling — deliberately a lower multiplier than the 5 × rule on non-H TP321. ASTM grain size No. 7 or coarser is part of the heat-treatment lot acceptance, and solution temperatures split by finish route (cold-worked 2000 °F [1090 °C], hot-rolled 1925 °F [1050 °C]). A plain 321 heat cannot be remarked as 321H without those levers.

SHH STEEL can supply ASME SA213 TP321H as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report the carbon band, titanium formula, finish-route anneal temperature, E112 grain-size result, and the 75/30 ksi tensile set with hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP321H.

Shop names include “321H,” “S32109,” and “Ti-stabilized H-grade 18-8 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP321H / UNS S32109, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements (S2 when needed). Sister SA213 pages include SA213 TP321, SA213 TP304H, and SA213 TP347H. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP321H

Two chemistry layers matter for TP321H under ASME SA-213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. Two lines define the grade for a reviewer: the carbon band 0.04–0.10%, and titanium ≥4 × (C + N) with a 0.70% ceiling. That Ti multiplier is deliberately lower than the 5 × (C + N) rule on non-H SA213 TP321, so do not copy a TP321 titanium check onto a TP321H heat without reopening the formula.

The tables below reproduce the heat analysis for TP321H / UNS S32109, the product-analysis limits from A480 Table A1.1 practice, and a short carbon / titanium snapshot against TP321, TP304H, and TP347H. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP321H (UNS S32109) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 12.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement; analysis method by agreement when reported for the Ti formula)
Niobium (Nb) … (no requirement)
Titanium (Ti) ≥ 4 × (C + N), ≤ 0.70

Source: public SA-213 / A213 stainless chemistry table for Grade TP321H / UNS S32109 (same grade text family). Confirm the ordered edition. UNCERTAIN: exact edition year and stainless chem table number; N analysis method (Footnote B) when used for the Ti formula.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 12.0 0.10 under / 0.15 over 8.90 – 12.15
Titanium (Ti) ≥ 4 × (C+N), ≤ 0.70 0.05 over on max (Ti to 1.00 band practice) max ≤ 0.75 product; min tied to heat C+N

UNCERTAIN: A480 Ti product tolerance on the formula max from sister practice — confirm against the ordered A480 edition when product analysis is invoked. Footnote H / S2 full negotiated wording — confirm ordered edition.

Snapshot versus TP321, TP304H, and TP347H

Element TP321 (S32100) TP321H (S32109) TP304H (S30409) TP347H (S34709)
C ≤ 0.08 0.04 – 0.10 0.04 – 0.10 0.04 – 0.10
Cr 17.0 – 19.0 17.0 – 19.0 18.0 – 20.0 17.0 – 19.0
Ni 9.0 – 12.0 9.0 – 12.0 8.0 – 11.0 9.0 – 13.0
Stabilizer Ti ≥ 5 × (C+N), ≤ 0.70 Ti ≥ 4 × (C+N), ≤ 0.70 none Nb ≥ 8 × C, ≤ 1.10

H-grade carbon floor plus coarser grain and finish-route anneal temperatures — not titanium alone — separate TP321H from non-H 321. Compare SA213 TP304H and SA213 TP347H when the stabilizer choice is still open.

Mechanical Properties of SA213 TP321H

ASME SA-213 Table 4 sets the room-temperature tensile acceptance floor for TP321H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP321 and TP304H. Hardness maximum is 192 HBW / 200 HV or 90 HRB. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112, sitting beside the titanium stabilization chemistry.

Property TP321H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: public SA-213 / A213 Table 4 for TP321H / UNS S32109 and H-grade grain-size language (heat-treatment table showing grain-size column “7” for TP321H). UNCERTAIN: exact grain-size table/clause number in the ordered edition. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits grain size or titanium is incomplete for TP321H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP321H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Creep-range boiler and superheater datasheets that pick H-grade titanium-stabilized tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Finish route (cold-finished vs hot-finished) also selects which solution-temperature floor applies — it is not only a dimensional choice.

Item Typical SA213 TP321H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for boiler / superheater datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace carbon floor, titanium formula, or grain-size checks.

Equivalent Grades

Equivalence language around TP321H tube is often looser than a creep-range boiler purchase order can afford. ASME SA-213 Grade TP321H / UNS S32109 is the governing designation for this article; EN 1.4941 / X8CrNiTi18-10 family names and JIS SUS321H / SUS321HTB are approximate wrought names that point to similar titanium-stabilized high-temperature 18-8 families but are not automatic substitutes on an SA-213 mill test certificate.

Designation Notes
ASME SA-213 / SA-213M Grade TP321H Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S32109 Unified number listed in the stainless chemistry table
ASTM A213 TP321H Separate ASTM product specification — twin page A213 TP321H; dual-mark only when the PO asks
EN 1.4941 family (approx.) Approximate wrought Ti-stabilized H-grade designation; order EN tube forms under the relevant EN tube specs
Related non-H SA213 TP321 — C ≤0.08, Ti ≥5×(C+N), no mandatory grain size
Related H-grades SA213 TP304H, SA213 TP347H, SA213 TP347HFG
Related plate A240 / SA240 flat product in the same UNS family

Dual SA-213/A213 marking is a purchase-order option. Compare TP321, TP304H, and the niobium H grades on their own ASME SA213 pages before swapping grades on a familiar “321” PMI reading alone.

Heat Treatment and Delivery Condition

TP321H under ASME SA-213 is furnished solution treated, then quenched in water or cooled rapidly by other means. The public heat-treatment table sets separate minimum solution temperatures by finish route: cold-worked tube at 2000 °F [1090 °C], and hot-rolled tube at 1925 °F [1050 °C], with Footnote H on the hot-rolled path. Grain size after heat treatment must meet ASTM No. 7 or coarser for the heat-treatment lot. That combination — finish-route solution temperature, titanium chemistry, and coarse-grain control — is what separates TP321H paperwork from a tensile-only TP321 certificate.

Footnote H warns that a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure in the indicated grades, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. Supplementary Requirement S2 lists TP321H among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. S2 is not automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route that also selects which solution-temperature floor applies; it is not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP321H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, titanium result, and grain-size result stated on the EN 10204 3.1 certificate. For non-H titanium stabilization open SA213 TP321; for niobium H-grade open SA213 TP347H. UNCERTAIN: Footnote H / S2 full negotiated wording in the ordered edition.

Corrosion Resistance

ASME SA213 TP321H is selected for elevated-temperature boiler and superheater duty where titanium stabilization, a controlled carbon floor, and coarse grain support creep-oriented Code allowables — not as a drop-in upgrade for wet chloride heat-exchanger lists. The Ti ≥4 × (C + N) rule still ties up carbon for sensitizing-range framing after the higher H-grade solution anneal, subject to Footnote H caution on temperatures above 1950 °F.

It is not a molybdenum grade and is often a poor default for wet corrosive cooling-water service; many of those lists prefer L-carbon Mo-bearing or superaustenitic rows. For non-H Ti stabilization without grain-size / carbon-floor controls, open SA213 TP321.

SHH STEEL reports carbon band, titanium formula, anneal temperature, and E112 grain size on the 3.1 certificate so inspectors can verify the H-grade levers rather than accepting a tensile-only 321 heat stamped as 321H.

Applications of SA213 TP321H Tube

Typical ASME SA213 TP321H uses include Code-stamped boiler and superheater tubes in creep-range service that name TP321H, reheater and superheater sections where titanium H-grade chemistry is preferred over plain 304H, and replacement bundles that must match original S32109 MTCs on carbon floor, Ti formula, and grain size. It is also quoted when a project wants Ti stabilization with H-grade heat-treatment temperatures.

  • Boiler / superheater / reheater tubes naming SA-213 TP321H
  • Creep-range Code service needing Ti H-grade + grain size No. 7
  • Replacement tube matching original S32109 certificates
  • Projects choosing Ti stabilizer over Nb H-grade (TP347H)

For non-H Ti stabilization, compare SA213 TP321. For Nb H-grade, compare SA213 TP347H. For fine-grain Nb H-grade, compare SA213 TP347HFG.

Weldability

TP321H welds with matching titanium-stabilized austenitic filler practices appropriate for H-grade service — commonly ER321 / ER321H family wires selected to the project WPS, not a plain ER308H filler that omits titanium when the design relies on Ti stabilization in the weld metal. Carbon floor and grain-size controls on the base metal do not remove heat-input, interpass, and purge discipline on thin boiler tube.

When S2 stabilization heat treatment is required after the higher H-grade solution anneal, put it on the purchase order — it is not automatic with the grade stamp. Field welding of installed boiler tubes follows the project WPS; mill delivery remains solution annealed with grain size reported on the 3.1 certificate.

Do not dual-stamp a TP321 or TP304H weld procedure as TP321H without reopening carbon band, Ti multiplier, grain size, and finish-route anneal acceptance on the WPS / PQR.

Surface Finishes

Standard mill delivery for ASME SA213 TP321H is solution annealed and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace carbon floor, titanium formula, finish-route anneal temperature, or grain-size checks. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP321H includes heat analysis (C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–12.0%, Ti ≥4 × (C + N) ≤0.70%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, ASTM E112 grain size No. 7 or coarser for the heat-treatment lot, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm carbon floor, titanium formula, finish-route anneal temperature, and grain size together rather than trusting a tensile-only 321 MTC stamped as 321H. Product analysis, when ordered, applies A480 tolerances including the Ti max window noted as UNCERTAIN digit confirmation above. S2 applies only when named on the PO.

EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP321H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP321H, UNS S32109, heat number, size, and wall basis so receivers can match the 3.1 certificate — including carbon band, titanium formula, and grain size — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP321H only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP321H as a Code Book titanium-stabilized H-grade product with enforceable C 0.04–0.10%, Ti ≥4 × (C + N) ≤0.70%, finish-route solution temperatures, ASTM grain size No. 7 or coarser, 75/30 ksi tensile, hardness, and marking rules — not as “321 with a little more carbon” checked only by a tensile pair. Enquiry review verifies carbon floor, Ti formula, and grain size together before release.

That stops silent substitution with TP321 or TP304H heats on datasheets that actually require S32109. We keep SA-213 and A213 independent, dual-mark only on request, and put C + Ti + anneal temperature + E112 on the 3.1 certificate so inspectors can verify all H-grade levers.

Cross-links: SA213 TP321, SA213 TP304H, SA213 TP347H, SA213 TP347HFG, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP321H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for titanium-stabilized H-grade boiler and superheater tube.

Item SHH STEEL capability for TP321H
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP321H / UNS S32109
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with C band + Ti formula + finish-route anneal + E112 grain size; S2 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP321H against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for titanium-stabilized H-grade boiler and superheater tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small boiler / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common superheater / HX band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route (CF / HR), and whether dual A213 marking or S2 is required. We reply with available mill / stock options for ASME SA213 TP321H and the matching document set.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP321H?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–12.0%, and Ti ≥4 × (C + N) ≤0.70% — tensile 75/30 ksi, hardness, finish-route heat treatment, and grain size No. 7 align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP321H include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
How does TP321H differ from TP321 under ASME SA213?
TP321H requires carbon 0.04–0.10% (floor and ceiling), titanium ≥4 × (C + N) ≤0.70% (not the 5 × rule on non-H TP321), finish-route solution temperatures (cold-worked 2000 °F / hot-rolled 1925 °F), and ASTM grain size No. 7 or coarser. Non-H TP321 keeps C ≤0.08%, Ti ≥5 × (C + N), 1900 °F solution anneal, and no mandatory grain-size. Room-temperature tensile is the same 75/30 ksi pair on both grades.
What is the UNS number and chemistry of ASME SA213 TP321H?
UNS S32109. Check C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–12.0%, and titanium ≥4 × (C + N) with a 0.70% ceiling. Molybdenum and niobium have no requirement on this row. When nitrogen is reported for the Ti formula, the analysis method is by agreement (Footnote B). Do not copy a TP321 5 × titanium check onto a TP321H heat without reopening the formula.
Does SA-213 Table 4 set a hardness limit for TP321H?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Grade distinction versus non-H TP321 is carbon floor, Ti multiplier, finish-route heat treatment, and grain size No. 7 — not a harder room-temperature product. A tensile-only MTC that omits grain size is incomplete for TP321H.
Why does ASME SA-213 control grain size on TP321H?
H-grade austenitics for creep-range boiler / superheater duty carry ASTM grain size No. 7 or coarser per heat-treatment lot (E112) so elevated-temperature allowables and microstructure expectations stay aligned with the Code design basis. Non-H TP321 does not print that mandatory grain-size column. Skipping the grain-size check is why a tensile-only 321 certificate cannot be remarked as 321H.
What heat treatment does ASME SA-213 require for TP321H?
Solution treatment then rapid cool, with finish-route minimums: cold-worked tube 2000 °F [1090 °C], hot-rolled tube 1925 °F [1050 °C], plus Footnote H caution on temperatures above 1950 °F. Grain size after heat treatment must meet ASTM No. 7 or coarser. S2 stabilization at a lower temperature after the initial solution anneal applies only when the purchaser specifies S2.
What is Supplementary Requirement S2 for TP321H under SA213?
S2 lists TP321H among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. It is not automatic with the grade stamp. Footnote H separately addresses purchaser-specified lower-temperature stabilization or resolution anneal after a higher solution anneal; confirm full wording in the ordered edition.
TP321H vs TP347H — titanium or niobium for H-grade tube under SA213?
TP321H uses titanium ≥4 × (C + N) ≤0.70%; TP347H uses niobium ≥8 × C ≤1.10% (confirm ordered edition Nb formula). Both carry H-grade carbon bands and grain-size control, but stabilizer chemistry, filler selection, and some elevated-temperature habits differ. Compare SA213 TP347H (and TP347HFG for fine-grain Nb) before swapping on a familiar “H-grade 18-8” nickname alone.
Can TP321H tube be dual certified TP321/TP321H under SA213?
Only when the heat clears both chemistry rows and both heat-treatment / grain-size paths — including carbon inside 0.04–0.10% (which already satisfies TP321’s ≤0.08% max when ≤0.08%), Ti satisfying the stricter applicable formula check for each stamp, finish-route anneal temperatures for H, and grain size No. 7. Casual dual stamping of a non-H 321 heat as 321H is not valid. Dual SA-213/A213 marking for the same H grade is a separate PO option.
Minimum wall vs average wall — which should I order for SA213 TP321H?
Most boiler and superheater datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over ASME B36.19 pipe schedules as the primary size story, and state finish route because it selects the solution-temperature floor.
Is TP321H a good choice for wet corrosive heat-exchanger service under SA213?
Often no as a default. TP321H is framed for elevated-temperature boiler / superheater duty with Ti stabilization, carbon floor, and coarse grain — not as a molybdenum upgrade for wet chloride cooling water. Many wet HX lists prefer L-carbon Mo-bearing or superaustenitic grades. Evaluate the corrosion environment with the project engineer before defaulting to 321H on a familiar Ti PMI reading alone.

Conclusion

ASME SA213 TP321H / UNS S32109 is the titanium-stabilized H-grade seamless stainless steel tube for Code boiler, superheater, and heat-exchanger service when C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–12.0%, Ti ≥4 × (C + N) ≤0.70%, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, finish-route solution temperatures (CF 2000 °F / HR 1925 °F), and ASTM grain size No. 7 or coarser are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report carbon band, titanium formula, anneal temperature, and E112 grain size. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X