ASME SA213 TP317LMN Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP317LMN Stainless Steel Tube

ASME SA213 TP317LMN / UNS S31726 nitrogen-bearing Mo 4–5% seamless boiler, superheater and heat-exchanger tube — C ≤0.03%, Cr 17.0–20.0%, Ni 13.5–17.5%, Mo 4.0–5.0%, N 0.10–0.20%, Cu ≤0.75%, working Table 4 floor 80/35 ksi with elongation 35% min and hardness max 192 HBW / 90 HRB (UNCERTAIN — A213–13 Table 4 OCR omits S31726; confirm ordered edition), 1900 °F solution anneal (HT row also UNCERTAIN in local excerpt). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the mandatory nitrogen range with Mo and Cu.
Grade
TP317LMN / UNS S31726
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP317LMN Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. On Code-stamped exchangers that invoke the ASME adoption by name, SA-213 is the governing product standard for this nitrogen-bearing Mo 4–5% tube — an independent Code Book line, not a dual title with ASTM A213. Use SA213/SA213M as the series entry point.

Grade TP317LMN / UNS S31726 is the mandatory-nitrogen partner to TP317LM inside that family. Carbon stays ≤0.03%, molybdenum stays 4.0–5.0%, nickel stays 13.5–17.5%, and copper stays ≤0.75%, while chromium widens to 17.0–20.0% and nitrogen becomes a true 0.10–0.20% range rather than a ≤0.20% maximum. The working Table 4 tensile floor used for this pack is 80 ksi [550 MPa] / 35 ksi [240 MPa] with elongation 35% minimum and hardness max 192 HBW / 90 HRB — labeled UNCERTAIN because the local A213–13 Table 4 OCR omits the S31726 row; confirm the ordered edition before locking receiving checklists.

SHH STEEL can supply ASME SA213 TP317LMN as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report nitrogen inside 0.10–0.20% together with Mo 4–5%, Ni, Cu, and the tensile / hardness set named on the ordered edition. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP317LMN.

Shop names include “317LMN,” “S31726,” and “N-bearing Mo 4–5 317 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP317LMN / UNS S31726, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements. Sister SA213 pages include SA213 TP317LM, SA213 TP317L, and SA213 TP316N. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP317LMN

Two chemistry layers matter for TP317LMN under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The letter N on this grade is not cosmetic: nitrogen must land inside 0.10–0.20%, chromium is printed as 17.0–20.0% (wider than the 18–20 window on TP317LM), and molybdenum / nickel / copper stay aligned with the Mo 4–5% LM family.

The tables below reproduce the melt limits for TP317LMN / UNS S31726, the product-analysis limits from A480 Table A1.1 practice, and a short snapshot against TP317L and TP317LM including the working tensile digit. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP317LMN (UNS S31726) melting analysis
Carbon (C) ≤ 0.03
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 20.0
Nickel (Ni) 13.5 – 17.5
Molybdenum (Mo) 4.0 – 5.0
Nitrogen (N) 0.10 – 0.20
Copper (Cu) ≤ 0.75

Source: public SA-213 / A213 stainless chemistry table for Grade TP317LMN / UNS S31726 (same grade text family). Confirm the ordered edition. Nitrogen analysis method is a matter of agreement (Footnote B) when the element is reported. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.03 0.005 over ≤ 0.035
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 20.0 0.20 under / over 16.80 – 20.20
Nickel (Ni) 13.5 – 17.5 0.15 under / 0.20 over 13.35 – 17.70
Molybdenum (Mo) 4.0 – 5.0 0.10 under / over 3.90 – 5.10
Nitrogen (N) 0.10 – 0.20 0.01 under / 0.02 over 0.09 – 0.22
Copper (Cu) ≤ 0.75 0.03 over ≤ 0.78

UNCERTAIN: A480 N 0.10–0.20 tolerances (0.01 under / 0.02 over) and Ni / Mo / Cu product digits are taken from sister A480 LN / Mo practice — confirm against the ordered A480 edition when product analysis is invoked.

Snapshot versus TP317L and TP317LM

Element TP317L (S31703) TP317LM (S31725) TP317LMN (S31726)
C ≤ 0.035 ≤ 0.03 ≤ 0.03
Cr 18.0 – 20.0 18.0 – 20.0 17.0 – 20.0
Ni 11.0 – 15.0 13.5 – 17.5 13.5 – 17.5
Mo 3.0 – 4.0 4.0 – 5.0 4.0 – 5.0
N … ≤ 0.20 0.10 – 0.20
Working Table 4 tensile 75/30 ksi 75/30 ksi 80/35 ksi (UNCERTAIN)

The N floor blocks casual dual marking with SA213 TP317LM. A heat below 0.10% N is not TP317LMN even when Mo clears 4.0%.

Mechanical Properties of SA213 TP317LMN

Working acceptance values used for this ASME SA213 TP317LMN pack are 80 ksi [550 MPa] tensile strength and 35 ksi [240 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB. Those digits follow sister N-bearing A213 practice (TP304N / TP316N) plus A240 S31726 tensile/yield cross-check — UNCERTAIN because the local A213–13 Table 4 OCR omits the S31726 row between S31725 and S32050. Do not copy A240 plate elongation 40% or 96 HRB blindly onto tube. Confirm the ordered SA-213 / A213 edition’s Table 4 row before locking MTC acceptance.

Property TP317LMN working requirement (UNCERTAIN)
Tensile strength, min 80 ksi [550 MPa] (UNCERTAIN)
Yield strength (0.2% offset), min 35 ksi [240 MPa] (UNCERTAIN)
Elongation in 2 in. or 50 mm, min 35% (UNCERTAIN)
Hardness, max 192 HBW / 200 HV or 90 HRB (UNCERTAIN)

Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits the nitrogen range or molybdenum is incomplete for TP317LMN. When the datasheet only needs Mo 4–5% with N as a maximum, open SA213 TP317LM instead.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP317LMN is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Nitrogen-bearing Mo 4–5% exchanger lists usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The mandatory N range does not rewrite dimensional tolerance tables; it rewrites which heat clears the grade stamp and which tensile floor the ordered edition prints.

Item Typical SA213 TP317LMN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the 0.10–0.20% nitrogen range.

Equivalent Grades

Equivalence language around 317LMN tube often collapses it with TP317LM or with plain N-bearing 316N. ASME SA-213 Grade TP317LMN / UNS S31726 is the governing designation for this article; EN and mill nicknames that point to similar Mo 4–5% + N chemistry families are not automatic substitutes on an SA-213 MTC.

Designation Notes
ASME SA-213 / SA-213M Grade TP317LMN Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31726 Unified number in the stainless chemistry table
ASTM A213 TP317LMN Separate ASTM product specification — twin page A213 TP317LMN; dual-mark only when the PO asks
Related Mo 4–5% max-N SA213 TP317LM — N ≤0.20, working tensile 75/30
Related Mo 3–4% L SA213 TP317L — Mo 3–4%, N ellipsis
Related N-bearing 316 SA213 TP316N — Mo 2–3%, different chemistry row
Related superaustenitic SA213 UNS S31254 — Mo ~6%, separate UNS row
Related plate A240 / SA240 flat product — do not copy plate elong./HRB blindly onto tube

Dual SA-213/A213 marking is a purchase-order option. Compare TP317LM and S31254 on their own ASME SA213 pages before swapping grades on a familiar Mo PMI reading alone.

Heat Treatment and Delivery Condition

Working heat-treatment practice used for this ASME SA213 TP317LMN pack is solution treatment at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. UNCERTAIN: the local A213–13 heat-treatment table OCR also omits the S31726 row — working temperature is taken from the S31725 sister; confirm the ordered edition’s HT table before writing WPS or MTC templates. Public excerpts used here do not print a mandatory ASTM grain-size number for UNS S31726.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP317LMN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, Mo, Ni, N-range, and Cu results on the EN 10204 3.1 certificate.

If a project datasheet asks for ASTM A262 Practice E, put that Supplementary Requirement on the purchase order. For Mo 4–5% without a mandatory nitrogen range, open SA213 TP317LM instead of stretching an off-range N heat into an LMN stamp.

Corrosion Resistance

ASME SA213 TP317LMN is selected when chloride-leaning or reducing acid heat-exchanger duty needs Mo 4–5% together with a controlled nitrogen range that supports strength and PREN framing beyond a ≤0.20% N maximum. Low carbon (≤0.03%) supports as-welded intergranular resistance; copper remains a ≤0.75% maximum rather than a copper-bearing specialty alloy claim.

It is still not a 6% Mo superaustenitic. Lists that need higher crevice or seawater-leaning performance should open SA213 UNS S31254 rather than stretching LMN chemistry. Localized attack still depends on temperature, chloride, deposit, and weld practice — Mo + N alone does not guarantee immunity.

SHH STEEL reports the nitrogen range with Mo, Ni, and Cu on the 3.1 certificate so inspectors can verify the LMN row rather than accepting a max-N LM heat stamped as LMN.

Applications of SA213 TP317LMN Tube

Typical ASME SA213 TP317LMN uses include Code-stamped heat-exchanger tubes where the datasheet names S31726 or “317LMN,” process coolers that combine Mo 4–5% with a mandatory nitrogen band, and replacement bundles that must match original LMN MTCs on N-range and tensile floor. It is also quoted when a project wants the higher working tensile pair that travels with N-bearing 317 chemistry.

  • Chemical / petrochemical HX tubes naming S31726 or 317LMN
  • Process coolers needing Mo 4–5% plus N 0.10–0.20%
  • Replacement tube matching original LMN certificates
  • Code boiler / HX service when SA-213 TP317LMN is the named grade

For Mo 4–5% without mandatory N, compare SA213 TP317LM. For Mo ~6%, compare SA213 UNS S31254.

Weldability

TP317LMN welds with matching or overalloyed austenitic filler practices appropriate for Mo 4–5% + nitrogen chemistry — filler selection follows the project WPS, not a plain 316N wire that under-matches molybdenum. Low carbon supports as-welded intergranular framing; nitrogen in the base metal still requires heat-input and purge discipline on thin HX tube.

Autogenous orbital welds need cleanliness and purge control; the N range does not remove those controls. Post-weld solution anneal is uncommon on installed bundles — when A262 demonstration is required, put it on the purchase order for mill tube.

Do not dual-stamp a TP317LM or TP316N weld procedure as TP317LMN without reopening Mo, N-range, and tensile acceptance on the WPS / PQR.

Surface Finishes

Standard mill delivery for ASME SA213 TP317LMN is solution annealed and pickled, leaving a clean matte finish suitable for heat-exchanger and process-tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the mandatory nitrogen range or Mo 4–5% chemistry. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP317LMN includes heat analysis (C ≤0.03%, Mo 4.0–5.0%, Cr 17.0–20.0%, Ni 13.5–17.5%, N 0.10–0.20%, Cu ≤0.75%), tension and hardness tests to the ordered edition’s Table 4 row (working 80/35 ksi / 35% / 192 HBW labeled UNCERTAIN here), and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm nitrogen inside 0.10–0.20% and molybdenum inside 4.0–5.0% rather than trusting a max-N LM heat or a 316N PMI story. Product analysis, when ordered, applies A480 tolerances including the N-range window noted as UNCERTAIN digit confirmation above.

Supplementary Requirements, A262 practices by agreement, and third-party witness are available on request. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP317LMN tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP317LMN, UNS S31726, heat number, size, and wall basis so receivers can match the 3.1 certificate — including the nitrogen range with Mo and Cu — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP317LMN only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP317LMN as a Code Book nitrogen-bearing Mo 4–5% product with enforceable C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N 0.10–0.20%, Cu ≤0.75%, and the ordered edition’s tensile / hardness set — not as “317LM with a little nitrogen” checked only by a Mo PMI peak. Enquiry review verifies the N range with Mo before release.

That stops silent substitution with TP317LM or TP316N heats on datasheets that actually require S31726. We keep SA-213 and A213 independent, dual-mark only on request, label UNCERTAIN tensile digits honestly until the ordered Table 4 row is confirmed, and put N-range + Mo + Cu on the 3.1 certificate.

Cross-links: SA213 TP317LM, SA213 TP317L, SA213 TP316N, SA213 UNS S31254, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP317LMN stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for N-bearing Mo 4–5% heat-exchanger tube.

Item SHH STEEL capability for TP317LMN
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP317LMN / UNS S31726
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / process bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with N 0.10–0.20% + Mo 4–5% + Cu; A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP317LMN against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for nitrogen-bearing Mo 4–5% heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common process exchanger band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route, and whether dual A213 marking or A262 is required. We reply with available mill / stock options for ASME SA213 TP317LMN and the matching document set — including confirmation of the ordered edition’s Table 4 tensile row.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP317LMN?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N 0.10–0.20%, and Cu ≤0.75% — aligns in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP317LMN include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
What is the UNS number and chemistry focus of ASME SA213 TP317LMN?
UNS S31726. Check C ≤0.03%, Cr 17.0–20.0%, Ni 13.5–17.5%, Mo 4.0–5.0%, N 0.10–0.20%, and Cu ≤0.75% together. Nitrogen is a mandatory range on this row, not a ≤0.20% maximum. A heat below 0.10% N is not TP317LMN even when molybdenum clears 4.0%.
TP317LMN vs TP317LM — what does the N letter change under SA213?
TP317LMN requires nitrogen inside 0.10–0.20%, widens chromium to 17.0–20.0%, and typically travels with a higher working tensile floor (80/35 ksi — UNCERTAIN until the ordered Table 4 row is confirmed). TP317LM keeps N as a ≤0.20% maximum and stays at 75/30 ksi. Do not dual-stamp LM and LMN unless both chemistries and tensile floors clear the named editions.
Why are tensile digits labeled UNCERTAIN on this TP317LMN page?
The local A213–13 Table 4 OCR omits the S31726 row between S31725 and S32050. Working 80/35 ksi tensile/yield, 35% elongation, and 192 HBW / 90 HRB follow sister N-bearing A213 practice plus A240 S31726 tensile/yield cross-check — A240 plate 40% elong. / 96 HRB must not be copied blindly onto tube. Confirm the ordered SA-213 / A213 edition’s Table 4 row before locking receiving checklists.
Does SA-213 set a hardness limit for TP317LMN?
Working practice used here caps hardness at 192 HBW / 200 HV or 90 HRB alongside the 80/35 ksi tensile pair — labeled UNCERTAIN with the Table 4 omission note above. Grade distinction versus TP317LM is the mandatory N range and the higher working tensile floor, not a claim that LMN is a harder product family in every edition.
What heat treatment does ASME SA-213 require for TP317LMN?
Working practice is solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool — also UNCERTAIN because the local HT table OCR omits S31726; temperature is taken from the S31725 sister. Confirm the ordered edition. Public excerpts used here do not mandate an ASTM grain-size number for TP317LMN.
Minimum wall vs average wall — which should I order for SA213 TP317LMN?
Most heat-exchanger datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over ASME B36.19 pipe schedules as the primary size story on tube RFQs.
Can I dual-certify TP317LMN with TP317LM on the same heat?
Only when the heat clears both chemistry rows — including N inside 0.10–0.20% for LMN (which already satisfies LM’s ≤0.20% max when inside range) — and both named editions’ tensile / hardness rules. A heat at 0.08% N can be LM chemistry but not LMN. Dual SA-213/A213 marking for the same LMN grade is a separate PO option.
When should I step from TP317LMN to UNS S31254 under SA213?
Step to the ~6% Mo superaustenitic row when PREN, crevice, or seawater-leaning duty exceeds what Mo 4–5% + N 0.10–0.20% can support. S31254 is a separate UNS chemistry and tensile story — not a dual stamp of TP317LMN. Compare SA213 UNS S31254 before stretching an LMN heat into a 6Mo claim on PMI alone.
Does SA-213 require copper reporting on TP317LMN?
Copper is part of the melting analysis for UNS S31726 with a ≤0.75% maximum, so a complete heat analysis reports Cu. Product analysis applies the A480 over-tolerance when product analysis is ordered. SHH STEEL includes Cu with Mo, Ni, and the nitrogen range on the EN 10204 3.1 certificate for TP317LMN.
TP317LMN vs TP316N — are the nitrogen grades interchangeable under SA213?
No. TP316N carries Mo 2.00–3.00% with a different Cr/Ni window; TP317LMN carries Mo 4.0–5.0%, Ni 13.5–17.5%, and Cu ≤0.75%. Shared nitrogen strengthening does not make the grades interchangeable on a familiar N PMI reading. Compare SA213 TP316N and SA213 TP317LMN on their own pages before swapping tube in an exchanger list.

Conclusion

ASME SA213 TP317LMN / UNS S31726 is the nitrogen-bearing Mo 4–5% seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N 0.10–0.20%, Cu ≤0.75%, and the ordered edition’s tensile / hardness set (working 80/35 ksi with 35% elongation and 192 HBW / 90 HRB — UNCERTAIN until Table 4 is confirmed) are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the N range with Mo and Cu. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X