ASME SA213 TP317LM / UNS S31725 low-carbon Mo 4–5% seamless boiler, superheater and heat-exchanger tube — C ≤0.03%, Cr 18.0–20.0%, Ni 13.5–17.5%, Mo 4.0–5.0%, N ≤0.20%, Cu ≤0.75%, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the Mo 4–5% band, nickel, nitrogen, and copper.
Grade
TP317LM / UNS S31725
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP317LM Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped exchangers or registered systems invoke that adoption by name, SA-213 is the governing product standard for this Mo 4–5% tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Start from SA213/SA213M when the enquiry is Code-led.

Grade TP317LM / UNS S31725 sits one molybdenum step above the TP317L row inside that stainless family. Melting carbon is capped at 0.03%, chromium stays 18.0–20.0%, nickel rises to 13.5–17.5%, and molybdenum moves into the 4.0–5.0% band. Nitrogen and copper appear as maxima (N ≤0.20%, Cu ≤0.75%) rather than as a mandatory nitrogen range. Table 4 keeps the 75 ksi [515 MPa] / 30 ksi [205 MPa] tensile pair with elongation 35% minimum and hardness max 192 HBW / 90 HRB — the same room-temperature floor as TP317L, not the 80/35 ksi pair used on the mandatory-N sister. A heat that only clears Mo 3.5% and Ni 12% is still a 317L-family story, not TP317LM.

SHH STEEL can supply ASME SA213 TP317LM as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report molybdenum inside 4.0–5.0%, nickel inside 13.5–17.5%, nitrogen and copper at or below their maxima, and the 75/30 ksi tensile set with 35% elongation and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP317LM.

Shop names include “317LM,” “S31725,” and “Mo 4–5 low-carbon 317 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP317LM / UNS S31725, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements. Sister SA213 pages include SA213 TP317L, SA213 TP317LMN, SA213 TP317, and SA213 TP316L. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP317LM

Two chemistry layers matter for TP317LM under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. Four lines separate this row from TP317L: carbon drops to ≤0.03%; nickel rises to 13.5–17.5%; molybdenum steps into 4.0–5.0%; and nitrogen plus copper appear as explicit maxima instead of ellipses. Chromium remains 18.0–20.0%.

The tables below reproduce the melt limits for TP317LM / UNS S31725, the product-analysis limits from A480 Table A1.1 practice, and a short Mo / Ni / N snapshot against TP317L and TP317LMN. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP317LM (UNS S31725) melting analysis
Carbon (C) ≤ 0.03
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 13.5 – 17.5
Molybdenum (Mo) 4.0 – 5.0
Nitrogen (N) ≤ 0.20
Copper (Cu) ≤ 0.75

Source: public SA-213 / A213 stainless chemistry table for Grade TP317LM / UNS S31725 (same grade text family). Confirm the ordered edition. Nitrogen analysis method is a matter of agreement (Footnote B) when the element is reported. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.03 0.005 over ≤ 0.035
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 13.5 – 17.5 0.15 under / 0.20 over 13.35 – 17.70
Molybdenum (Mo) 4.0 – 5.0 0.10 under / over 3.90 – 5.10
Nitrogen (N) ≤ 0.20 0.01 over ≤ 0.21
Copper (Cu) ≤ 0.75 0.03 over ≤ 0.78

UNCERTAIN: A480 Ni 13.5–17.5 / Mo 4–5 / Cu ≤0.75 product-tolerance digits are taken from sister A480 practice for this chemistry family — confirm against the ordered A480 edition when product analysis is invoked. Footnote F quench / A262 capability wording near the S31725 row — confirm ordered edition.

Snapshot versus TP317L and TP317LMN

Element TP317L (S31703) TP317LM (S31725) TP317LMN (S31726)
C ≤ 0.035 ≤ 0.03 ≤ 0.03
Cr 18.0 – 20.0 18.0 – 20.0 17.0 – 20.0
Ni 11.0 – 15.0 13.5 – 17.5 13.5 – 17.5
Mo 3.0 – 4.0 4.0 – 5.0 4.0 – 5.0
N … ≤ 0.20 0.10 – 0.20
Cu … ≤ 0.75 ≤ 0.75

Mo bands do not dual with TP317L. A mandatory nitrogen range belongs on SA213 TP317LMN, not on a ≤0.20% N maximum heat stamped as LM.

Mechanical Properties of SA213 TP317LM

ASME SA-213 Table 4 sets the tensile acceptance floor for TP317LM / UNS S31725 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB. That is the same room-temperature pair as TP317L — nitrogen here is a maximum, not a strengthening range, so Table 4 does not step up to the 80/35 ksi floor used on mandatory-N sisters. Receiving checklists must not import an 80 ksi expectation from a 317LMN or plate row onto an SA-213 TP317LM tube heat.

Property TP317LM requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

Source: public SA-213 / A213 Table 4 for UNS S31725 / TP317LM. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits molybdenum, nickel, or nitrogen is incomplete for TP317LM. When the datasheet also wants a mandatory nitrogen range and the higher tensile floor that often travels with it, open SA213 TP317LMN.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP317LM is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Heat-exchanger datasheets that pick Mo 4–5% tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Mo 4–5% chemistry does not change the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 TP317LM dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace Mo 4–5% or the Ni 13.5–17.5% band.

Equivalent Grades

Equivalence language around 317LM tube often treats it as “317L with a little more Mo” or collapses it with nitrogen-bearing 317LMN. ASME SA-213 Grade TP317LM / UNS S31725 is the governing designation for this article; EN and mill nicknames that point to similar Mo 4–5% chemistry families are not automatic substitutes on an SA-213 MTC.

Designation Notes
ASME SA-213 / SA-213M Grade TP317LM Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31725 Unified number in the stainless chemistry table
ASTM A213 TP317LM Separate ASTM product specification — twin page A213 TP317LM; dual-mark only when the PO asks
Related Mo 3–4% L SA213 TP317L — Mo 3–4%, Ni 11–15, N ellipsis
Related N-range sister SA213 TP317LMN — Mo 4–5%, N 0.10–0.20, Cr 17–20
Related superaustenitic SA213 UNS S31254 — Mo ~6%, separate UNS row
Related plate A240 / SA240 flat product in the 317LM family — order plate and tube under their own standards

Dual SA-213/A213 marking is a purchase-order option. Compare TP317L and TP317LMN on their own ASME SA213 pages before swapping Mo 4–5% tube inside an exchanger list.

Heat Treatment and Delivery Condition

TP317LM under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table does not print a mandatory ASTM grain-size number for UNS S31725. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Elevated molybdenum and low carbon improve corrosion framing, but they do not replace the solution anneal.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP317LM is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, Mo, Ni, N, and Cu results on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

If a project datasheet asks for ASTM A262 Practice E, put that Supplementary Requirement on the purchase order rather than assuming base SA-213 includes it. For mandatory nitrogen-range lists with the higher tensile floor that often accompanies them, open SA213 TP317LMN instead of stretching a ≤0.20% N heat. UNCERTAIN: Footnote F / Practice E full negotiated wording when ordered — confirm the edition named on the PO.

Corrosion Resistance

ASME SA213 TP317LM is selected when chloride-leaning or reducing acid heat-exchanger duty needs more molybdenum than the 3–4% Mo window on TP317L, while keeping carbon at ≤0.03% for as-welded intergranular framing. The Mo 4.0–5.0% band and the elevated nickel floor (13.5%) are the primary levers versus standard 316L / 317L families; nitrogen at ≤0.20% is a maximum, not a PREN-boosting range that redesigns the grade into LMN.

It is not a 6% Mo superaustenitic and is not interchangeable with SA213 UNS S31254 on a familiar Mo PMI peak alone. Wet cooling-water lists that need higher PREN or crevice performance should open the superaustenitic row rather than stretching LM chemistry. Localized attack still depends on temperature, chloride, deposit, and weld practice — Mo alone does not guarantee immunity.

SHH STEEL reports Mo, Ni, N, and Cu on the 3.1 certificate so inspectors can verify the Mo 4–5% band rather than accepting a “317L family” heat that only clears 3.5% Mo.

Applications of SA213 TP317LM Tube

Typical ASME SA213 TP317LM uses include Code-stamped heat-exchanger and condenser tubes in chemical and pulp-and-paper service where Mo 4–5% is specified, process coolers handling chloride-leaning media above the 317L window, and selected boiler / HX bundles that name S31725 explicitly. The grade is also quoted for replacement tube when original 317LM MTCs must be matched on Mo and Ni.

  • Chemical and petrochemical heat-exchanger / condenser tubes (Mo 4–5% lists)
  • Pulp-and-paper and bleach-plant coolers naming S31725
  • Process HX bundles stepping up from TP317L on molybdenum
  • Code boiler / superheater / HX tube when the datasheet names SA-213 TP317LM

For mandatory nitrogen-range and higher tensile floors, compare SA213 TP317LMN. For Mo ~6% superaustenitic duty, compare SA213 UNS S31254.

Weldability

TP317LM welds with matching or overalloyed austenitic filler practices appropriate for Mo 4–5% chemistry — commonly ER317L / ER317LMo family wires selected to the project WPS, not a plain 316L filler that under-matches molybdenum. Low carbon (≤0.03%) supports as-welded intergranular framing; still follow qualified procedures for heat input, interpass, and purge on thin HX tube.

Autogenous orbital welds on thin-wall exchanger tube need cleanliness and purge discipline; Mo 4–5% does not remove those controls. Post-weld solution anneal is uncommon on installed HX bundles — when A262 demonstration is required, put it on the purchase order for mill tube or specify field PWHT separately.

Do not dual-stamp a TP317L weld procedure as TP317LM without reopening Mo and Ni acceptance on the WPS / PQR.

Surface Finishes

Standard mill delivery for ASME SA213 TP317LM is solution annealed and pickled, leaving a clean matte finish suitable for heat-exchanger and process-tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace Mo 4–5% chemistry or the Ni 13.5–17.5% band. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP317LM includes heat analysis (C ≤0.03%, Mo 4.0–5.0%, Cr 18.0–20.0%, Ni 13.5–17.5%, N ≤0.20%, Cu ≤0.75%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm molybdenum inside 4.0–5.0% and nickel inside 13.5–17.5% rather than trusting a “317L family” PMI Mo peak below 4.0%. Product analysis, when ordered, applies A480 tolerances including the Mo/Ni/Cu windows noted as UNCERTAIN digit confirmation above.

Supplementary Requirements, A262 practices by agreement, and third-party witness are available on request. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP317LM tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP317LM, UNS S31725, heat number, size, and wall basis so receivers can match the 3.1 certificate — including Mo, Ni, N, and Cu — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP317LM only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP317LM as a Code Book Mo 4–5% product with enforceable C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N ≤0.20%, Cu ≤0.75%, 75/30 ksi tensile, 35% elongation, hardness, and marking rules — not as “317L with a little more molybdenum” checked only by a Mo PMI peak below 4.0%. Enquiry review verifies Mo and Ni together before release.

That stops silent substitution with TP317L heats on datasheets that actually require S31725. We keep SA-213 and A213 independent, dual-mark only on request, and put Mo + Ni + N + Cu on the 3.1 certificate so inspectors can verify all four levers.

Cross-links: SA213 TP317L, SA213 TP317LMN, SA213 TP317, SA213 UNS S31254, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP317LM stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for Mo 4–5% heat-exchanger and process tube.

Item SHH STEEL capability for TP317LM
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP317LM / UNS S31725
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / process bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Mo 4–5% + Ni + N + Cu; A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP317LM against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for Mo 4–5% heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common process exchanger band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route, and whether dual A213 marking or A262 is required. We reply with available mill / stock options for ASME SA213 TP317LM and the matching document set.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP317LM?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N ≤0.20%, and Cu ≤0.75% — tensile 75/30 ksi, elongation 35%, and hardness floors align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP317LM include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
What is the UNS number and chemistry focus of ASME SA213 TP317LM?
UNS S31725. Check C ≤0.03%, Cr 18.0–20.0%, Ni 13.5–17.5%, Mo 4.0–5.0%, N ≤0.20%, and Cu ≤0.75% together. Nitrogen is a maximum on this row, not a 0.10–0.20% strengthening range. Mo bands do not dual with TP317L — a heat that only clears Mo 3.5% and Ni 12% remains a 317L-family story.
TP317LM vs TP317L — why step to Mo 4–5% under SA213?
Order TP317LM when the datasheet needs molybdenum in the 4.0–5.0% band with nickel at 13.5–17.5% and carbon ≤0.03%. Order TP317L when Mo 3.0–4.0% and Ni 11–15% are enough. Same 75/30 ksi tensile floor and 35% elongation on both rows — the step is chemistry, not a higher room-temperature tensile number. Compare SA213 TP317L before stretching a 317L heat into an LM stamp.
TP317LM vs TP317LMN — what does the N letter change?
TP317LMN adds a mandatory nitrogen range of 0.10–0.20%, widens chromium to 17.0–20.0%, and typically travels with a higher working tensile floor (80/35 ksi — labeled UNCERTAIN on that page). TP317LM keeps N as a ≤0.20% maximum and stays at 75/30 ksi. Do not dual-stamp LM and LMN on the same heat unless both chemistries and tensile floors clear the ordered editions.
Does SA-213 set a hardness limit for TP317LM?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Grade distinction versus TP317L is Mo 4–5% and elevated Ni, not a harder product; versus TP317LMN the room-temperature tensile floor stays at 75/30 because nitrogen is a maximum, not a range.
What heat treatment does ASME SA-213 require for TP317LM?
Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool. Public excerpts used here do not mandate an ASTM grain-size number for TP317LM. Name A262 Practice E on the PO when demonstration of intergranular corrosion resistance is required; it is not automatic with the grade stamp.
Minimum wall vs average wall — which should I order for SA213 TP317LM?
Most heat-exchanger datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over ASME B36.19 pipe schedules as the primary size story on tube RFQs.
Can I dual-certify TP317LM with TP317L on the same heat?
Only when the heat clears both chemistry rows — including Mo 4.0–5.0% and Ni 13.5–17.5% for LM, which already exceed TP317L’s Mo 3–4% / Ni 11–15 windows — and both named editions’ tensile / hardness rules. Casual dual stamping of a Mo 3.5% heat as both grades is not valid. Dual SA-213/A213 marking for the same LM grade is a separate PO option.
Why is tensile still 75/30 ksi on TP317LM instead of 80/35?
Nitrogen on TP317LM is a ≤0.20% maximum, not a mandatory strengthening range. Table 4 therefore keeps the same 75/30 ksi floor used on TP317L. The 80/35 ksi working floor belongs with mandatory-N sisters such as TP317LMN (labeled UNCERTAIN on that pack until the ordered edition’s Table 4 row is confirmed). Do not import 80 ksi onto an LM receiving checklist.
When should I step from TP317LM to UNS S31254 under SA213?
Step to the ~6% Mo superaustenitic row when PREN, crevice, or seawater-leaning duty exceeds what Mo 4–5% LM chemistry can support. S31254 is a separate UNS chemistry and tensile story — not a dual stamp of TP317LM. Compare SA213 UNS S31254 before stretching an LM heat into a 6Mo claim on PMI alone.
Does SA-213 require copper reporting on TP317LM?
Copper is part of the melting analysis for UNS S31725 with a ≤0.75% maximum, so a complete heat analysis reports Cu. Product analysis applies the A480 over-tolerance when product analysis is ordered. SHH STEEL includes Cu with Mo, Ni, and N on the EN 10204 3.1 certificate for TP317LM so inspectors can verify the full row.

Conclusion

ASME SA213 TP317LM / UNS S31725 is the low-carbon Mo 4–5% seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N ≤0.20%, Cu ≤0.75%, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report Mo, Ni, N, and Cu. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X