ASME SA213 TP316N Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP316N Stainless Steel Tube

ASME SA213 TP316N / UNS S31651 nitrogen-strengthened Mo seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Cr 16.0–18.0%, Ni 10.0–13.0%, Mo 2.00–3.00%, N 0.10–0.16%, Table 4 80/35 ksi floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal with Footnote F quench capability. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP316N / UNS S31651
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP316N Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When a registered vessel, Code-stamped exchanger, or owner specification invokes that adoption by name, SA-213 is the governing product standard — an independent Code Book line, not a merged title with ASTM A213. Use SA213/SA213M as the series entry point for the stainless tube spine.

Grade TP316N / UNS S31651 is the nitrogen-strengthened molybdenum austenitic row inside that SA-213 family. Melting carbon stays ≤0.08%, chromium 16.0–18.0%, nickel sits in a narrower 10.0–13.0% window (not the 10–14% band used on TP316 / TP316L), molybdenum 2.00–3.00%, and nitrogen is locked into a mandatory 0.10–0.16% range. That nitrogen floor is why Table 4 lifts tensile acceptance to 80 ksi [550 MPa] / 35 ksi [240 MPa] — five ksi above ordinary SA213 TP316 on both tensile and yield — while molybdenum still carries the chloride-leaning corrosion work that a non-Mo N grade cannot claim.

SHH STEEL can supply ASME SA213 TP316N as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report nitrogen and molybdenum together with the 80/35 ksi tensile set and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP316N.

Shop names include “316N,” “S31651,” and “N-strengthened 316 Mo tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP316N / UNS S31651, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements (including S4 / A262 Practice E when Footnote F capability must be demonstrated). Sister SA213 pages include SA213 TP316, SA213 TP316LNM, SA213 TP316L, and SA213 TP304N when N strength is wanted without Mo. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2.

Chemical Composition of SA213 TP316N

Two chemistry layers matter for TP316N under ASME SA-213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M). Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. Reviewers should verify Mo 2.00–3.00%, N 0.10–0.16%, and the narrower Ni 10.0–13.0% band together — molybdenum alone does not make a heat S31651, and a heat that would pass TP316 can fail the N floor or the Ni ceiling.

UNCERTAIN: exact SA-213 / A213 edition year; stainless chemistry table number (Table 1 vs Table 2 by edition); A480 N product-tolerance digits (0.01 under / 0.02 over from sister LN practice applied here); full Footnote F / S4 Practice E wording — confirm on the ordered edition.

Melting analysis

Element TP316N (UNS S31651) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 10.0 – 13.0
Molybdenum (Mo) 2.00 – 3.00
Nitrogen (N) 0.10 – 0.16

That melt table is the acceptance chemistry for every heat of SA213 TP316N. Nitrogen must clear 0.10% and must not exceed 0.16%; nickel must stay inside 10.0–13.0% — a heat at 13.5% Ni that would pass ordinary TP316 fails this row. Molybdenum 2.00–3.00% remains mandatory and is what separates TP316N from SA213 TP304N on chloride-leaning duty.

Product analysis (when required)

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 10.0 – 13.0 0.10 under / 0.15 over 9.90 – 13.15
Molybdenum (Mo) 2.00 – 3.00 0.05 under / 0.10 over 1.95 – 3.10
Nitrogen (N) 0.10 – 0.16 0.01 under / 0.02 over 0.09 – 0.18

When product analysis is invoked, A480 tolerances apply as shown. Nitrogen’s product window uses the 0.01-under / 0.02-over practice associated with sister LN bands — treated as UNCERTAIN digit confirmation on the ordered A480 path. Nickel’s product ceiling lands at 13.15%, which still sits below the ordinary TP316 product ceiling.

Snapshot vs sister grades

Element TP316 (S31600) TP316N (S31651) TP316LNM (S31653)
C ≤ 0.08 ≤ 0.08 ≤ 0.035
Ni 10.0 – 14.0 10.0 – 13.0 10.0 – 13.0
Mo 2.00 – 3.00 2.00 – 3.00 2.00 – 3.00
N … 0.10 – 0.16 0.10 – 0.16
Table 4 tensile / yield 75 / 30 ksi 80 / 35 ksi 75 / 30 ksi

Against SA213 TP316, the N band and the 80/35 ksi floor are the commercial point; Ni also tightens to a 13% ceiling. Against SA213 TP316LNM, carbon stays at the standard 0.08% max rather than the L path, so tensile stays higher while as-welded IGC risk needs separate review. Against SA213 TP304N, molybdenum is the separator — same N-strength idea, different chloride ranking.

Mechanical Properties of SA213 TP316N

ASME SA-213 sets the tensile acceptance floor for TP316N at 80 ksi [550 MPa] tensile strength and 35 ksi [240 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness capped at 192 HBW / 200 HV or 90 HRB. That 80/35 pair is five ksi above the ordinary TP316 / TP316LNM mechanical row on both tensile and yield — the commercial reason buyers write “316N” when recoverable strength sits beside Mo corrosion duty.

Property TP316N requirement (Table 4)
Tensile strength, min 80 ksi [550 MPa]
Yield strength (0.2% offset), min 35 ksi [240 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number in the public heat-treatment table for TP316N

Hardness stays on the same 192 HBW / 90 HRB ceiling as ordinary TP316; the grade distinction is the higher tensile/yield pair driven by nitrogen, not a harder product. Public heat-treatment excerpts used for this pack do not print a mandatory ASTM grain-size number for TP316N the way H-grades do — do not invent a No. 7 clause on the MTC unless the ordered edition or purchase order requires one.

Flattening, flaring, and reverse-bend tests follow SA-213 / general-requirements practice. Hydrostatic testing or NDE is selected per specification and PO. Dual-marked jobs still clear SA-213 mechanical text — see A213 TP316N.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP316N is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Heat-exchanger and process datasheets that pick N-strengthened Mo tube usually assume minimum wall — state wall basis on the purchase order so the mill does not default to an average-wall path the designer did not intend. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows.

Item Typical SA213 TP316N dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options on top of SA-213 dimensional rules — they do not replace N-band chemistry or the 80/35 ksi floor.

Equivalent Grades

Equivalence talk around TP316N must keep the N band, Mo band, and narrower Ni window intact. ASME SA-213 Grade TP316N / UNS S31651 is the governing designation for this article; “316N or 316” on a drawing is not automatic interchange when the datasheet actually needs the 80/35 ksi floor.

Designation Notes
ASME SA-213 / SA-213M Grade TP316N Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31651 Unified number in the stainless chemistry table
ASTM A213 TP316N Separate ASTM product specification — dual-mark only when the PO asks
Related Mo grade SA213 TP316 — same Mo band, no N requirement, 75/30 ksi, Ni 10–14
Related L+N+Mo SA213 TP316LNM — same N band, C ≤0.035, 75/30 ksi
Related N grade SA213 TP304N — N-strengthened without Mo
Related plate A240 / SA240 flat product in the 316N family — order plate and tube under their own standards

If a datasheet says “316N or equivalent,” confirm N 0.10–0.16, Mo 2–3, Ni 10.0–13.0, and the 80/35 ksi floor under SA-213 naming. Plate under A240 / SA240 does not automatically qualify as SA-213 tube. Non-Code ASTM purchase: A213 TP316N.

Heat Treatment and Delivery Condition

TP316N under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries Footnote F for this grade: quench at a rate sufficient to prevent re-precipitation of carbides, as demonstrable by the capability of tubes to pass ASTM A262 Practice E when that test is specified on the purchase order. The manufacturer is not required to run A262 Practice E unless Supplementary Requirement S4 / the PO calls for it. That heat-treatment row applies to both cold-finished and hot-finished seamless tube.

UNCERTAIN: full Footnote F / S4 Practice E edition wording and any edition-specific cross-reference path — confirm on the ordered SA-213 / general-requirements text before treating secondary catalogues as acceptance language.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the solution anneal or the Footnote F quench capability. Delivery condition for SHH STEEL TP316N is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, nitrogen, and molybdenum on the EN 10204 3.1 certificate. Unlike H grades such as SA213 TP316H, TP316N has no mandatory ASTM grain-size number in the public heat-treatment table.

Corrosion Resistance

TP316N inherits molybdenum’s contribution to pitting and crevice resistance from the 316 family while using nitrogen to raise strength rather than to rewrite the fundamental chloride ranking of the alloy. The 2.00–3.00% Mo band is why buyers step up from SA213 TP304N when chloride-leaning or process-side aqueous corrosion sits beside a need for the 80/35 ksi floor.

It is still not an L-grade: carbon up to 0.08% means as-welded intergranular corrosion risk after tube-to-tubesheet welding needs separate review — many owners move to SA213 TP316LNM when low carbon and nitrogen must travel together. SA-213 itself does not publish a corrosion-rate table for TP316N; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy.

Footnote F’s A262 Practice E capability is a quench-quality demonstration path when ordered — write S4 / Practice E onto the purchase order so the test is contractual. SHH STEEL will not rank TP316N as equal to higher-Mo grades such as TP317 / TP317L in severe chlorides — that claim is not supported by the product standard.

Applications of SA213 TP316N Tube

TP316N is ordered for Code and near-Code heat-exchanger, condenser, and process-tube circuits that specify nitrogen-strengthened molybdenum austenitic seamless tube — often where recoverable tensile capacity must sit above the ordinary 316 floor while Mo still covers chloride-leaning aqueous duty. Boiler / superheater use appears when the datasheet names the grade; H-grade creep duty with carbon floor and grain-size mandates usually points to SA213 TP316H instead.

Enquiry patterns ask for seamless cold-finished HX OD × minimum-wall tube, sometimes with ID polish or U-bends for bundle replacement. Hot-finished seamless remains available when size favors it. MTC review should always show N inside 0.10–0.16% and Mo inside 2.00–3.00% together with the 80/35 ksi tensile set.

Sister steering: plain Mo → SA213 TP316; L+N+Mo → SA213 TP316LNM; N without Mo → SA213 TP304N; H-grade Mo → SA213 TP316H.

Weldability

TP316N tube welds with matching or near-matching Mo-bearing austenitic filler selected for the project WPS (fabricators often call ER316L / ER316LSi or project-approved Mo grades). Nitrogen in the base metal raises strength; it does not remove sensitization risk in the HAZ when carbon sits up to 0.08% and heat input is poorly controlled. Clean practice, controlled heat input, and appropriate filler for chloride or process duty remain mandatory.

Tube-to-tubesheet procedures should name TP316N / S31651. Do not assume a TP304N WPS covers Mo-bearing 316N without review, and do not treat TP316N as an automatic L-grade substitute on as-welded IGC-critical lists — many stewards simply order TP316LNM when low carbon is the dominant need.

Dual SA-213/A213 marking does not change filler selection. If A262 Practice E after fabrication or on mill product is required, state Supplementary Requirement S4 (or edition-equivalent) on the purchase order so Footnote F capability becomes contractual rather than assumed.

Surface Finishes

Standard mill delivery for ASME SA213 TP316N is solution annealed and pickled, leaving a clean matte finish suitable for heat-exchanger and process-tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace N-band chemistry, Mo, or the 80/35 ksi tensile floor. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP316N includes heat analysis (Mo 2.00–3.00%, N 0.10–0.16%, Ni 10.0–13.0%), tension tests to the 80/35 ksi floors, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm nitrogen inside the mandatory band and nickel under the 13% ceiling rather than trusting a “316 family” PMI Mo peak alone. Product analysis, when ordered, applies A480 tolerances including the N window noted as UNCERTAIN digit confirmation above.

Supplementary Requirements (including S4 / A262 Practice E when Footnote F capability must be demonstrated), and third-party witness are available on request. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP316N tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP316N, UNS S31651, heat number, size, and wall basis so receivers can match the 3.1 certificate — including N and Mo — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP316N only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP316N as a Code Book N-strengthened Mo product with enforceable Mo 2–3%, N 0.10–0.16%, Ni 10.0–13.0%, 80/35 ksi tensile, hardness, Footnote F quench capability, and marking rules — not as “316 with a little nitrogen” checked only by PMI Mo. Enquiry review verifies the N band and the narrower Ni window before release.

That stops silent substitution with TP316 or TP304N heats on datasheets that actually require S31651 and the 80/35 ksi floor. We keep SA-213 and A213 independent, dual-mark only on request, and put Mo + N on the 3.1 certificate so inspectors can verify both levers.

Cross-links: SA213 TP316, SA213 TP316LNM, SA213 TP304N, SA213 TP316H, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP316N stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for N-strengthened Mo heat-exchanger and process tube.

Item SHH STEEL capability for TP316N
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP316N / UNS S31651
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / process bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Mo + N; S4 / A262 Practice E / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP316N against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for boiler and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common process exchanger band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, finish route, any S4 / A262 Practice E requirement, and whether dual A213 marking is required. SHH STEEL returns capability against ASME SA213 TP316N / UNS S31651 — not a TP316 or TP304N substitute.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP316N?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including the N 0.10–0.16% band and Mo 2–3% — tensile 80/35 ksi, and hardness floors align closely for a given referenced edition, but they remain independent standards. Dual-mark only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP316N include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing-type labels from pipe standards are not used as product-form options on this pack. If your datasheet actually needs welded stainless pipe, that is a different product-standard family and should be ordered under the matching pipe specification.
What is the UNS number and chemistry focus of ASME SA213 TP316N?
UNS S31651. Check C ≤0.08%, Cr 16.0–18.0%, Ni 10.0–13.0%, Mo 2.00–3.00%, and N 0.10–0.16% together. The narrower nickel ceiling and the mandatory nitrogen band are what separate this row from ordinary TP316. Product analysis, when ordered, applies A480 A1.1 tolerances.
TP316N vs TP316 — what does the N add under SA213?
Nitrogen 0.10–0.16% raises Table 4 tensile acceptance from 75/30 ksi on TP316 to 80/35 ksi on TP316N, and nickel tightens from 10–14% to 10.0–13.0%. Molybdenum stays 2–3% on both. Order TP316N when the datasheet needs that strength floor; order TP316 when standard Mo chemistry without an N band is enough.
TP316N vs TP316LNM — when do I need low carbon?
Order TP316LNM when as-welded intergranular resistance needs C ≤0.035% together with the same N 0.10–0.16% and Mo 2–3% bands (tensile then sits at 75/30 ksi). Order TP316N when the project accepts C ≤0.08% and wants the higher 80/35 ksi floor. They share Mo and N identity but are not dual stamps.
Why is the nickel band 10.0–13.0% on SA213 TP316N instead of 10–14%?
The stainless chemistry table for TP316N / S31651 sets Ni 10.0–13.0%, tighter at the top than the 10.0–14.0% window on TP316 / TP316L. A heat at 13.5% Ni that would pass ordinary TP316 fails TP316N. Certificate review should check Ni together with Mo and the N band.
What does Footnote F mean for SA213 TP316N heat treatment?
Footnote F requires quench at a rate sufficient to prevent carbide re-precipitation, demonstrable by the capability of tubes to pass ASTM A262 Practice E when that test is specified. The mill is not required to run Practice E unless Supplementary Requirement S4 / the PO calls for it. Exact edition wording is UNCERTAIN — confirm on the ordered SA-213 text.
Does SA-213 set a hardness limit for TP316N?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 80 ksi tensile, 35 ksi yield, and 35% elongation. Hardness matches ordinary TP316; the grade distinction is the higher tensile/yield pair driven by nitrogen, not a harder product.
What heat treatment does ASME SA-213 require for TP316N?
Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool, under Footnote F quench-capability wording. Public excerpts used here do not mandate an ASTM grain-size number for TP316N. Name S4 / A262 Practice E on the PO when demonstration testing is contractual.
Minimum wall vs average wall — which should I order for SA213 TP316N?
Most heat-exchanger datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over B36.19 pipe schedules.
Is TP316N a good choice for as-welded IGC-critical tube-to-tubesheet joints?
Often not by itself. Carbon up to 0.08% leaves sensitization risk after welding that L-grades address with C ≤0.035%. Many owners move to SA213 TP316LNM when low carbon and nitrogen must travel together, or specify A262 Practice E on the PO when quench quality must be demonstrated on TP316N product.
Can you dual-certify ASME SA-213 and ASTM A213 TP316N?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including N 0.10–0.16%, Mo 2–3%, Ni 10.0–13.0%, and the 80/35 ksi floor. Dual marking is stencil and documentation practice, not proof the names are synonyms. Otherwise SA-213 stands alone for Code Book jobs.

Conclusion

ASME SA213 TP316N / UNS S31651 is the nitrogen-strengthened molybdenum seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when Mo 2.00–3.00%, N 0.10–0.16%, Ni 10.0–13.0%, an 80/35 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal with Footnote F quench capability are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report Mo and N. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X