ASME SA213 TP201 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP201 Stainless Steel Tube

ASME SA213 TP201 / UNS S20100 seamless boiler, superheater and heat-exchanger tube — a manganese-nitrogen austenitic with Mn 5.5–7.5%, Ni 3.5–5.5%, Cr 16.0–18.0%, N ≤0.25% and C ≤0.15%. Under SA-213 the tensile floor is 95/38 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP201 / UNS S20100
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP201 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP201 under that Code Book text is the manganese-nitrogen austenitic listed as UNS S20100 — not a nickel-lean “304 substitute” stamp, but its own chemistry with manganese 5.5–7.5%, nickel 3.5–5.5%, chromium 16.0–18.0%, nitrogen ≤0.25%, and carbon ≤0.15%. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP201, the purchase order and mill test certificate should carry the ASME designation and the 95/38 ksi tensile floor that belongs to this grade, not a borrowed 304 mechanical row.

SHH STEEL can supply ASME SA213 TP201 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including manganese and nitrogen — and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 201, Mn-N austenitic, S20100 boiler tube, or SA213 201 HX tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP202, SA213 TP304, SA213 TP316, and SA213 TP XM-19. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP201.

Chemical Composition of SA213 TP201

Two chemistry layers matter for TP201 under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements path (commonly ASTM A1016/A1016M as referenced by the ordered SA-213 edition). Product-analysis tolerances are not reprinted as a standalone chemistry table inside SA-213 itself; when ordered, they typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle manganese inside 5.5–7.5% and nitrogen at or below 0.25%, and does not advertise tighter catalogue chemistry windows that the Code Book text does not publish.

The tables below reproduce the heat analysis for TP201 / UNS S20100 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text. Nitrogen analysis method is by agreement when the edition footnote applies; A480 product-tolerance digits for the high-Mn band should be confirmed against the A480 edition if product analysis is contractual.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP201 / UNS S20100. Confirm the ordered ASME edition on the purchase order.

Element TP201 (UNS S20100) melting analysis
Carbon (C) ≤ 0.15
Manganese (Mn) 5.5 – 7.5
Phosphorus (P) ≤ 0.060
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 3.5 – 5.5
Molybdenum (Mo) … (no requirement)
Nitrogen (N) ≤ 0.25

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.15 0.01 over ≤ 0.16
Manganese (Mn) 5.5 – 7.5 0.05 under / 0.06 over 5.45 – 7.56
Phosphorus (P) ≤ 0.060 0.010 over ≤ 0.070
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 3.5 – 5.5 0.07 under / 0.10 over 3.43 – 5.60
Nitrogen (N) ≤ 0.25 0.02 over ≤ 0.27

Manganese and nitrogen are what make TP201 a different alloy from TP304: Mn at 5.5–7.5% and N ≤0.25% strengthen the austenite while nickel sits only at 3.5–5.5%, and carbon is allowed up to 0.15% — well above the 0.08% TP304 ceiling. Phosphorus is capped at 0.060% (higher than the 0.045% common on 300-series rows). A PMI gun that only checks Cr and Ni can mis-identify this grade; the MTC must show Mn and N in the required bands.

When product analysis is ordered, finished tube may read up to C 0.16%, P 0.070%, S 0.035%, Si 1.05%, and N 0.27%, with Mn 5.45–7.56%, Cr 15.80–18.20%, and Ni 3.43–5.60%. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project nitrogen or manganese window on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP201

ASME SA-213 sets the tensile acceptance floor for TP201 at 95 ksi [655 MPa] tensile strength and 38 ksi [260 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. That 95 ksi tensile floor is noticeably higher than the 75 ksi floor SA-213 lists for TP304 — manganese and nitrogen strengthen the austenite, and the product standard captures that in the mechanical-table row rather than leaving it as a catalogue claim. Hardness maximum is 219 HBW / 230 HV or 95 HRB, and hardness tests are part of the lot acceptance scheme under SA-213.

Source: public SA-213 / A213 mechanical-table summaries for TP201 / UNS S20100 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP201 requirement
Tensile strength, min 95 ksi [655 MPa]
Yield strength (0.2% offset), min 38 ksi [260 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 219 HBW / 230 HV or 95 HRB

Flattening and flaring tests are also required on a lot basis for finished tube; they sit beside tension and hardness rather than replacing them. Do not import SA312 / A312 pipe tensile numbers onto an SA-213 tube enquiry for this grade — pipe product standards have historically carried different pairs for related 201 chemistry, and the tube product standard’s 95/38 ksi floor is what the MTC must clear. Actual mill certificates often clear the floor with margin, but design calculations should still use the Code Book floor unless the purchase order states higher guaranteed values that the mill has accepted in writing.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP201 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition — do not treat a catalogue one-liner as a substitute for the table.

Item Typical SA213 TP201 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled. Because TP201 work-hardens more aggressively than 304-family heats in some drawing sequences, state the finish route early so the mill can plan cold reductions against the hardness maximum.

Equivalent Grades

Equivalence language around TP201 tube is often looser than a Code or heat-exchanger purchase order can afford. ASME SA-213 Grade TP201 / UNS S20100 is the governing designation for this article; EN 1.4372 and JIS SUS201 are approximate wrought names that point to similar Mn-N chemistry families but are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 201” or “201 instead of 304,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify — the 95/38 ksi floor and Mn/N bands are not optional.

Designation Notes
ASME SA-213 / SA-213M Grade TP201 Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S20100 Unified number listed with the grade chemistry
ASTM A213 TP201 Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP201
EN 1.4372 (X12CrMnNiN17-7-5) Approximate wrought stainless designation; order EN tube forms under the relevant EN tube specs, not by EN number alone on an SA-213 MTC
JIS SUS201 Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP201 is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare SA213 TP202 and the 300-series sisters on their own pages before treating TP201 as a drop-in for TP304 in a Code tube bundle.

Heat Treatment and Delivery Condition

TP201 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave a structure that fails the hardness maximum or sensitizes in service even when ladle manganese and nitrogen looked acceptable on paper.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal: cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL TP201 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability (commonly tied to ASTM A262 Practice E) is ordered, the corrosion test report travels with the heat-treatment record. Do not import H-grade grain-size rules from TP304H onto TP201 — this grade’s mechanical and chemistry story is the Mn-N austenitic row, not an H-grade carbon floor.

Corrosion Resistance

TP201’s chromium-rich passive film handles a useful band of oxidizing and mild process fluids, but the grade is not a molybdenum alloy and should not be sold as equal to TP316 in chlorides. Nickel is lower than in the 300-series, and carbon is allowed higher, so intergranular and pitting behavior in aggressive media needs case-by-case engineering judgment rather than a catalogue claim that “201 replaces 304 everywhere.” In chloride-bearing waters and many brine-leaning heat-exchanger services, buyers usually step up to SA213 TP316 / SA213 TP316L.

ASME SA-213 itself does not publish a corrosion-rate table for TP201; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note. SHH STEEL will not rank TP201 as interchangeable with TP304 or TP316 on corrosion grounds alone — the product standard’s chemistry and 95/38 ksi floor are what the MTC clears.

Applications of SA213 TP201 Tube

TP201 seamless tube under SA-213 shows up where the datasheet specifically calls the Mn-N austenitic grade, or where the higher 95/38 ksi tensile floor and lower nickel content are intentional design choices — not as a silent substitute for TP304 on a Code boiler or exchanger that was written around 18-8 chemistry. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid, temperature, and fabrication route — not only for the familiar “201” name on the BOM.

Application area Typical use of TP201 tube Selection note
Heat exchangers / condensers Straight and U-bend HX tubes when SA-213 TP201 is the named grade State min vs average wall, BWG, and bend radius; do not assume 304 tensile floors
General corrosive tube duty Seamless tube where Mn-N austenitic and 95 ksi tensile are accepted Confirm fluid compatibility — not a Mo grade
Structural / high-strength austenitic tube Applications that use the higher tensile/yield floor of the TP201 mechanical row Hardness max 219 HBW / 95 HRB — plan cold work accordingly
Boiler and moderate-temperature steam Only when the Code datasheet names TP201 Do not substitute for TP304/TP304H without engineering review
Cost-sensitive austenitic HX Projects that deliberately specify S20100 chemistry Keep SA-213 documentation; do not swap to pipe paperwork
Sister Mn-N comparison Side-by-side with TP202 when higher Mn is considered Open SA213 TP202 for the higher-Mn sister

For conventional 18-8 Code tube open SA213 TP304; for chloride-leaning Mo service open TP316 / TP316L on the same SA213/SA213M hub. Treat TP201 as its own grade with its own MTC numbers.

Weldability

TP201 tube can be welded with austenitic fillers selected for the Mn-N base chemistry and the project’s corrosion expectations; many fabricators use 201-matched or 308-family fillers under a qualified WPS, but the filler choice is a welding-engineering decision — SA-213 does not prescribe a single electrode grade for TP201. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP201 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. Higher carbon allowance versus L-grades means as-welded IGC risk should be reviewed explicitly — do not assume L-grade behavior from a “201” nickname. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP201 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP201 includes heat analysis (with manganese and nitrogen reported in the required bands), tension tests to the 95/38 ksi mechanical-table floors, hardness tests to the 219 HBW / 95 HRB maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP201 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry — including Mn and N — on finished tube
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive. Receiving inspectors should verify the 95 ksi tensile floor and 219 HBW hardness maximum — not a borrowed 304 row.

Packaging and Shipping

TP201 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP201 as a Code Book product standard with enforceable Mn-N chemistry, a 95/38 ksi tensile floor, a 219 HBW / 95 HRB hardness maximum, heat-treatment, and marking rules — not as a catalogue nickname for “cheap 304 tube.” The MTC reports manganese inside 5.5–7.5% and nitrogen at or below 0.25%; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 200-series conversation honest for boiler and HX duty. If the datasheet needs conventional 18-8 chemistry and a 75/30 ksi floor, we open SA213 TP304 / SA213 TP304L. If chlorides dominate, we open SA213 TP316 / SA213 TP316L. If a higher-Mn sister is named, we open SA213 TP202. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP201 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.

Item SHH STEEL capability for TP201
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP201 / UNS S20100
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (95/38 ksi), hardness (max 219 HBW / 95 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry including Mn and N on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP201 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for Mn-N austenitic boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP201
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry — including manganese and nitrogen — tensile against the 95/38 ksi floor, hardness against the 219 HBW / 95 HRB maximum, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP202, SA213 TP XM-19, and SA213 TP304 sit on the same hub when the datasheet steps beyond TP201.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP201?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP201 include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP201 under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
Minimum wall vs average wall — which should I order for SA213 TP201?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from the general requirements.
Hydrostatic test vs NDE — which do I get on SA213 TP201 tube?
ASME SA-213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
Does SA-213 set a hardness limit for TP201?
Yes. The mechanical table for TP201 lists tensile strength, yield strength, elongation, and a hardness maximum of 219 HBW / 230 HV or 95 HRB — higher than the 192 HBW / 90 HRB cap on TP304. Hardness tests are part of lot acceptance under SA-213. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What is the UNS number and chemistry of ASME SA213 TP201?
TP201 is UNS S20100. Melting limits include carbon ≤0.15%, manganese 5.5–7.5%, phosphorus ≤0.060%, sulfur ≤0.030%, silicon ≤1.00%, chromium 16.0–18.0%, nickel 3.5–5.5%, and nitrogen ≤0.25%, with molybdenum as a no-requirement ellipsis. Product-analysis limits apply only when ordered. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP201 vs TP304 — can I substitute under SA213?
Not as a silent substitute. TP201 is a Mn-N austenitic with a 95/38 ksi tensile floor and hardness max 219 HBW / 95 HRB; TP304 is an 18-8 grade with a 75/30 ksi floor and 192 HBW / 90 HRB hardness maximum. Chemistry, nickel content, and corrosion framing differ. Order the grade the datasheet names, or obtain engineering approval before changing grades on a Code tube bundle.
TP201 vs TP202 — which SA213 Mn-N tube should I order?
Order TP201 when the datasheet names S20100 chemistry with Mn 5.5–7.5% and Ni 3.5–5.5%. Order TP202 when the higher manganese band and TP202 chemistry row are specified. Both are Mn-N austenitics under SA-213, but they are not interchangeable stamps. Open the TP202 page on the hub and compare the chemistry tables before swapping on the purchase order.
What tensile floor does ASME SA-213 set for TP201?
SA-213 sets 95 ksi [655 MPa] tensile strength and 38 ksi [260 MPa] yield strength (0.2% offset), with 35% elongation minimum and hardness max 219 HBW / 230 HV or 95 HRB. Do not import pipe-product tensile numbers or TP304’s 75/30 ksi pair onto a TP201 tube enquiry. Design and MTC acceptance should use the TP201 mechanical-table row for the ordered edition.
What heat treatment does ASME SA-213 require for TP201?
TP201 is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
Can you dual-certify ASME SA-213 and ASTM A213 TP201?
Yes when the heat and testing support it. Dual SA-213/A213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Chemistry must still clear the Mn 5.5–7.5% and N ≤0.25% bands, and tensile plus hardness must clear the 95/38 ksi and 219 HBW / 95 HRB rows. Spell the required marking on the enquiry so the heat is selected correctly.

Conclusion

ASME SA213 TP201 / UNS S20100 is the manganese-nitrogen austenitic seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when the datasheet names S20100 chemistry and the 95/38 ksi tensile floor — not a silent stand-in for TP304. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the TP201 tensile and hardness acceptance floors, and documented on EN 10204 3.1 certificates with manganese and nitrogen reported — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X