ASME SA213 TP317L Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP317L Stainless Steel Tube

ASME SA213 TP317L / UNS S31703 low-carbon higher-molybdenum seamless boiler, superheater and heat-exchanger tube — C ≤0.035% (no Footnote D 0.040% path in public table), Cr 18.0–20.0%, Ni 11.0–15.0%, Mo 3.0–4.0%, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP317L / UNS S31703
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP317L Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped exchangers, boilers, or registered systems invoke that adoption by name, SA-213 is the governing product standard — an independent Code Book line, not a merged title with ASTM A213. Use SA213/SA213M as the series entry point.

Grade TP317L / UNS S31703 is the low-carbon partner to SA213 TP317 inside that stainless family. Melting carbon is capped at 0.035%, chromium stays at 18.0–20.0%, nickel at 11.0–15.0%, and molybdenum remains in the 3.0–4.0% band that sits a full percentage point above the 316-family Mo window. Table 4 sets tensile at 75 ksi [515 MPa] / 30 ksi [205 MPa] with elongation 35% minimum — one point above the 34% printed for standard TP317 — and hardness max 192 HBW / 90 HRB. Buyers who write “317L HX tube” on a bill of materials still need to name SA-213 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the L-grade carbon check together with the elevated Mo floor.

SHH STEEL can supply ASME SA213 TP317L as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report carbon at or below 0.035% and molybdenum inside 3.0–4.0% together with the 75/30 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP317L.

Shop names include “317L,” “S31703,” and “low-carbon higher-Mo 317 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP317L / UNS S31703, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements. Sister SA213 pages include SA213 TP317, SA213 TP316L, SA213 TP317LM, and SA213 TP317LMN when Mo 4–5% paths are required. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2.

Chemical Composition of SA213 TP317L

Two chemistry layers matter for TP317L under ASME SA-213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M). Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. Reviewers should verify C ≤0.035%, Mo 3.0–4.0%, Cr 18.0–20.0%, and Ni 11.0–15.0% together — a heat that clears TP316L Mo 2–3% fails this row, and Mo bands do not dual-stamp between 316L and 317L families.

UNCERTAIN: exact SA-213 / A213 edition year; stainless chemistry table number; A480 Mo 3–4 / Ni 11–15 product-tolerance digits (0.10 under/over on Mo and 0.15 under/over on Ni from sister practice); Footnote F quench / A262 wording when Practice E is ordered — confirm on the ordered edition. Public table for TP317L does not print Footnote D beside C ≤0.035 — do not import the 316L 0.040% thin-wall path.

Melting analysis

Element TP317L (UNS S31703) melting analysis
Carbon (C) ≤ 0.035
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 11.0 – 15.0
Molybdenum (Mo) 3.0 – 4.0
Nitrogen (N) … (no requirement; analysis method by agreement when reported)

That melt table is the acceptance chemistry for every heat of SA213 TP317L. Carbon must clear the L ceiling at 0.035%; molybdenum must sit inside 3.0–4.0%. Unlike TP316L, the public table excerpt used here does not attach Footnote D’s 0.040% thin-wall path to TP317L — do not invent that allowance on the certificate. Nitrogen has no mandatory requirement on this row.

Product analysis (when required)

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.035 0.01 over ≤ 0.045
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 11.0 – 15.0 0.15 under / over 10.85 – 15.15
Molybdenum (Mo) 3.0 – 4.0 0.10 under / over 2.90 – 4.10

When product analysis is invoked, A480 tolerances apply as shown. Molybdenum’s product window uses the 0.10-under / 0.10-over practice associated with Mo 3–4 bands, and nickel uses 0.15 under/over — both treated as UNCERTAIN digit confirmation on the ordered A480 path. Carbon’s product limit of ≤0.045% is the ordinary 0.01-over practice on the 0.035% melt max.

Snapshot vs sister grades

Element TP316L (S31603) TP317 (S31700) TP317L (S31703) TP317LM (S31725)
C ≤ 0.035 ≤ 0.08 ≤ 0.035 ≤ 0.03
Cr 16.0 – 18.0 18.0 – 20.0 18.0 – 20.0 18.0 – 20.0
Ni 10.0 – 14.0 11.0 – 15.0 11.0 – 15.0 13.5 – 17.5
Mo 2.00 – 3.00 3.0 – 4.0 3.0 – 4.0 4.0 – 5.0
Table 4 elong. min 35% 34% 35% 35%

Against SA213 TP316L, Mo rises a full point and Cr/Ni windows move up while tensile stays at 75/30 ksi rather than dropping to 70/25. Against SA213 TP317, carbon drops to the L path and elongation rises to 35%. Against Mo 4–5% sisters, see SA213 TP317LM / SA213 TP317LMN.

Mechanical Properties of SA213 TP317L

ASME SA-213 sets the tensile acceptance floor for TP317L at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness capped at 192 HBW / 200 HV or 90 HRB. That 75/30 / 35% set matches ordinary TP316 mechanical numbers while keeping Mo 3–4% — and it sits above TP316L’s 70/25 ksi floor even though both are L-grades. Versus TP317, elongation rises one point from 34% to 35%.

Property TP317L requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number in the public heat-treatment table for TP317L

Public heat-treatment excerpts used for this pack do not print a mandatory ASTM grain-size number for TP317L the way H-grades do. Do not invent a No. 7 clause on the MTC unless the ordered edition or purchase order requires one. Hardness and tensile review still use the 192 HBW / 75/30 ksi caps with the 35% elongation floor.

Flattening, flaring, and reverse-bend tests follow SA-213 / general-requirements practice. Hydrostatic testing or NDE is selected per specification and PO. Dual-marked jobs still clear SA-213 mechanical text — see A213 TP317L.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP317L is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Heat-exchanger datasheets that pick low-carbon higher-Mo tube usually assume minimum wall — state wall basis on the purchase order. Do not assume Footnote D’s 0.040% carbon path from TP316L applies here; the public TP317L row used for this pack does not print that footnote. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M).

Item Typical SA213 TP317L dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace L-carbon or Mo 3–4% chemistry.

Equivalent Grades

Equivalence talk around TP317L must keep the Mo 3–4% band, L-carbon ceiling, and elevated Cr/Ni windows intact. ASME SA-213 Grade TP317L / UNS S31703 is the governing designation for this article; “317L or 316L” on a drawing is not automatic interchange when the datasheet actually needs Mo above the 316L ceiling.

Designation Notes
ASME SA-213 / SA-213M Grade TP317L Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31703 Unified number in the stainless chemistry table
ASTM A213 TP317L Separate ASTM product specification — dual-mark only when the PO asks
Related standard-C SA213 TP317 — same Mo 3–4%, C ≤0.08, elong. 34%
Related Mo 2–3% L SA213 TP316L — Mo 2–3%, Cr 16–18 / Ni 10–14, 70/25 ksi
Related Mo 4–5% SA213 TP317LM / SA213 TP317LMN — separate Mo / Ni / N rows
Related plate A240 / SA240 flat product in the 317L family — order plate and tube under their own standards

If a datasheet says “317L or equivalent,” confirm C ≤0.035, Mo 3.0–4.0, Cr 18–20, Ni 11–15, and SA-213 naming. Plate under A240 / SA240 does not automatically qualify as SA-213 tube. Non-Code ASTM purchase: A213 TP317L.

Heat Treatment and Delivery Condition

TP317L under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table does not print a mandatory ASTM grain-size number for this grade. That heat-treatment row applies to both cold-finished and hot-finished seamless tube.

Low carbon plus elevated molybdenum reduce sensitization and pitting risk, but they do not replace the solution anneal — under-cooling can still leave a structure that fails a contractual A262 check even when ladle chemistry looked acceptable on paper. Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal.

Delivery condition for SHH STEEL TP317L is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, carbon, and molybdenum on the EN 10204 3.1 certificate. Unlike H grades such as SA213 TP316H, TP317L has no carbon floor and no grain-size mandate. If a project datasheet asks for ASTM A262 Practice E, put that Supplementary Requirement on the purchase order rather than assuming base SA-213 includes it. UNCERTAIN: exact Footnote F / Practice E edition cross-reference when ordered — confirm on the ordered text.

Corrosion Resistance

TP317L’s defining corrosion claim pairs two levers: molybdenum 3.0–4.0% for pitting and crevice resistance relative to the 316L Mo band, and carbon ≤0.035% for as-welded intergranular resistance relative to standard TP317. That pairing makes TP317L the default higher-Mo seamless tube grade when tube-to-tubesheet joints remain as-welded and chloride-leaning aqueous service sits above ordinary 316L PREN.

It is still not a duplex or super-austenitic alloy, and it is still not a Mo 4–5% grade — those belong on SA213 TP317LM / SA213 TP317LMN. SA-213 itself does not publish a corrosion-rate table for TP317L; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy.

When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual. SHH STEEL will not claim TP317L equals Mo 4–5% families or superaustenitics in severe brine — those are separate grade rows with their own chemistries. For Mo 2–3% L duty see SA213 TP316L; for standard-carbon higher Mo see SA213 TP317.

Applications of SA213 TP317L Tube

TP317L is ordered for Code and near-Code heat-exchanger, condenser, and process-tube circuits that specify low-carbon higher-molybdenum austenitic seamless tube — typically where tube-to-tubesheet joints remain as-welded, chloride-leaning aqueous duty needs Mo 3–4%, and the designer will not accept ordinary 316L PREN. Boiler / superheater use appears when the datasheet names the grade; H-grade creep duty points elsewhere.

Enquiry patterns ask for seamless cold-finished HX OD × minimum-wall tube, sometimes with ID polish or U-bends for bundle replacement. Hot-finished seamless remains available when size favors it. MTC review should always show C at or below 0.035% and Mo inside 3.0–4.0% together with the 75/30 ksi tensile set and 35% elongation.

Sister steering: standard-C higher Mo → SA213 TP317; Mo 2–3% L → SA213 TP316L; Mo 4–5% → SA213 TP317LM / SA213 TP317LMN.

Weldability

TP317L tube welds with matching or near-matching higher-Mo low-carbon austenitic filler selected for the project WPS (fabricators often call ER317L or project-approved Mo grades above ordinary 316L fillers). Low carbon in the base metal is the primary sensitization lever; elevated molybdenum improves localized-corrosion resistance without rewriting the need for clean practice and controlled heat input.

Tube-to-tubesheet procedures should name TP317L / S31703. Do not assume a TP316L WPS covers Mo 3–4% without review, and do not treat TP317L as an automatic TP317LM substitute when the datasheet actually needs Mo 4–5%.

Dual SA-213/A213 marking does not change filler selection. If A262 Practice E after fabrication or on mill product is required, state that Supplementary Requirement on the purchase order so the test is contractual rather than assumed.

Surface Finishes

Standard mill delivery for ASME SA213 TP317L is solution annealed and pickled, leaving a clean matte finish suitable for heat-exchanger and process-tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace L-carbon or Mo 3–4% chemistry. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP317L includes heat analysis (C ≤0.035%, Mo 3.0–4.0%, Cr 18.0–20.0%, Ni 11.0–15.0%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm carbon at the L ceiling and molybdenum inside 3.0–4.0% rather than trusting a “316L family” PMI Mo peak below 3.0%. Product analysis, when ordered, applies A480 tolerances including the Mo/Ni windows noted as UNCERTAIN digit confirmation above.

Supplementary Requirements, A262 practices by agreement, and third-party witness are available on request. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP317L tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP317L, UNS S31703, heat number, size, and wall basis so receivers can match the 3.1 certificate — including C and Mo — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP317L only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP317L as a Code Book low-carbon higher-Mo product with enforceable C ≤0.035%, Mo 3–4%, Cr 18–20%, Ni 11–15%, 75/30 ksi tensile, 35% elongation, hardness, and marking rules — not as “316L with a little more molybdenum” checked only by a Mo PMI peak below 3.0%. Enquiry review verifies C and Mo together before release.

That stops silent substitution with TP316L or TP317 heats on datasheets that actually require S31703. We keep SA-213 and A213 independent, dual-mark only on request, and put C + Mo on the 3.1 certificate so inspectors can verify both levers.

Cross-links: SA213 TP317, SA213 TP316L, SA213 TP317LM, SA213 TP317LMN, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP317L stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for low-carbon higher-Mo heat-exchanger and process tube.

Item SHH STEEL capability for TP317L
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP317L / UNS S31703
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / process bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with C + Mo 3–4%; A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP317L against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for as-welded higher-Mo heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common process exchanger band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, finish route, any A262 Practice E requirement, and whether dual A213 marking is required. SHH STEEL returns capability against ASME SA213 TP317L / UNS S31703 — not a TP316L or TP317 substitute.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP317L?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.035% and Mo 3.0–4.0% — tensile 75/30 ksi, elongation 35%, and hardness floors align closely for a given referenced edition, but they remain independent standards. Dual-mark only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP317L include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing-type labels from pipe standards are not used as product-form options on this pack. If your datasheet actually needs welded stainless pipe, order it under the matching pipe specification.
What is the UNS number and chemistry focus of ASME SA213 TP317L?
UNS S31703. Check C ≤0.035%, Cr 18.0–20.0%, Ni 11.0–15.0%, and Mo 3.0–4.0% together. Nitrogen has no mandatory requirement on this row. Public table does not print Footnote D’s 0.040% path for TP317L — do not invent it. Product analysis, when ordered, applies A480 A1.1 tolerances.
TP317L vs TP317 — when do I need low carbon under SA213?
Order TP317L when as-welded intergranular resistance needs C ≤0.035% together with Mo 3–4% (elongation 35%). Order TP317 when the project accepts C ≤0.08% and the datasheet names standard-carbon 317 (elongation 34%). Same Mo identity; different carbon paths and elongation digits.
TP317L vs TP316L — why choose the higher molybdenum L-grade?
TP317L raises Mo from 2.00–3.00% to 3.0–4.0% and moves Cr/Ni to 18–20 / 11–15, while keeping C ≤0.035%. Tensile stays at 75/30 ksi rather than dropping to TP316L’s 70/25 ksi floor. Order TP317L when chloride-leaning duty needs Mo above the 316L ceiling and as-welded IGC resistance still matters.
Does Footnote D raise TP317L carbon to 0.040% on small-OD tube?
Not on the public table excerpt used for this pack. Unlike TP316L / TP316LNM, the TP317L row does not print Footnote D beside C ≤0.035%. Do not import the 0.040% thin-wall path from 316L habit. If an ordered edition adds such wording, confirm it explicitly — until then treat C ≤0.035% as the melt ceiling.
Why does TP317L keep 75/30 ksi while TP316L drops to 70/25?
Table 4 prints 75/30 ksi for TP317L and 70/25 ksi for TP316L even though both are L-grades. The higher-Mo 317L row keeps the standard austenitic tensile floor; plain 316L accepts the lower pair. Do not assume every L-grade shares the same tensile numbers.
Does SA-213 set a hardness limit for TP317L?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Grade distinction versus TP316L is Mo 3–4% and elevated Cr/Ni, not a harder product; versus TP317 the elongation digit rises from 34% to 35%.
What heat treatment does ASME SA-213 require for TP317L?
Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool. Public excerpts used here do not mandate an ASTM grain-size number for TP317L. Name A262 Practice E on the PO when demonstration testing is contractual.
Minimum wall vs average wall — which should I order for SA213 TP317L?
Most heat-exchanger datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over B36.19 pipe schedules.
Can you dual-certify ASME SA-213 and ASTM A213 TP317L?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including C ≤0.035%, Mo 3–4%, Cr 18–20%, Ni 11–15%, 75/30 ksi, and 35% elongation. Dual marking is stencil and documentation practice, not proof the names are synonyms. Otherwise SA-213 stands alone for Code Book jobs.
When should I step from TP317L to TP317LM or TP317LMN under SA213?
Step up when the datasheet needs Mo 4.0–5.0% (and the matching Ni / N rows on those grades) rather than Mo 3–4%. TP317LM and TP317LMN are separate chemistry rows — not dual stamps of TP317L. Compare their SA213 pages before substituting inside a boiler or exchanger list.

Conclusion

ASME SA213 TP317L / UNS S31703 is the low-carbon higher-molybdenum seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.035%, Mo 3.0–4.0%, Cr 18.0–20.0%, Ni 11.0–15.0%, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report C and Mo. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X