ASME SA213/SA213M

Product Showcase

ASME SA213/SA213M Stainless Steel Products

ASME SA213 is the ASME code version of seamless ferritic and austenitic alloy-steel boiler, superheater and heat-exchanger tubes. It covers the same grade family as ASTM A213, including T11, T22, T91, TP304, TP316L, TP321 and TP347, and is intended for use under ASME Boiler and Pressure Vessel Code rules. SHH STEEL supplies ASME SA213 tubes with mill certification, competitive pricing and global delivery support.

ASME SA213 TP309S Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP309S Stainless Steel Tube

ASME SA213 TP309S / UNS S30908 seamless boiler, superheater and heat-exchanger tube — a 22–24% Cr / 12–15% Ni austenitic with C ≤0.08%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. Chosen for high-temperature oxidation resistance rather than molybdenum chloride service. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 UNS S30432 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 UNS S30432 Stainless Steel Tube

ASME SA213 UNS S30432 (commercially Super304H / 18Cr-9Ni-3Cu-Nb-N) seamless boiler and superheater tube with C 0.07–0.13%, Cu 2.5–3.5%, Nb 0.30–0.60%, N 0.05–0.12%, a 2000 °F [1100 °C] solution anneal, and tensile floors of 86/34 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting Cu, Nb, N, Al, and B.
View More
ASME SA213 TP304LN Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP304LN Stainless Steel Tube

ASME SA213 TP304LN / UNS S30453 seamless boiler, superheater and heat-exchanger tube — low-carbon nitrogen-strengthened 18-8 with C ≤0.035% (Footnote D to 0.040%), N 0.10–0.16%, Cr 18.0–20.0%, Ni 8.0–11.0%, and a 75/30 ksi tensile floor with hardness max 192 HBW / 90 HRB. Solution anneal 1900 °F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting C and N.
View More
ASME SA213 TP304N Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP304N Stainless Steel Tube

ASME SA213 TP304N / UNS S30451 seamless boiler, superheater and heat-exchanger tube — nitrogen-strengthened 18-8 with N 0.10–0.16%, Cr 18.0–20.0%, Ni 8.0–11.0%, C ≤0.08%, and an 80/35 ksi tensile floor with hardness max 192 HBW / 90 HRB. Solution anneal 1900 °F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting nitrogen.
View More
ASME SA213 TP304H Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP304H Stainless Steel Tube

ASME SA213 TP304H / UNS S30409 seamless boiler, superheater and heat-exchanger tube — the H-grade 18-8 with C 0.04–0.10%, Cr 18.0–20.0%, Ni 8.0–11.0%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and ASTM No. 7 or coarser grain size after the 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting grain size.
View More
ASME SA213 TP XM-19 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP XM-19 Stainless Steel Tube

ASME SA213 XM-19 / UNS S20910 (Nitronic 50) seamless boiler, superheater and heat-exchanger tube with Cr 20.5–23.5%, Ni 11.5–13.5%, Mo 1.50–3.00%, N 0.20–0.40%, Nb and V 0.10–0.30% each. Mechanical floor 100/55 ksi with hardness max 250 HBW / 25 HRC; solution anneal 1900 °F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 TP202 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP202 Stainless Steel Tube

ASME SA213 TP202 / UNS S20200 seamless boiler, superheater and heat-exchanger tube — the higher-manganese Mn–N austenitic with Mn 7.5–10.0%, Ni 4.0–6.0%, Cr 17.0–19.0%, N ≤0.25% and C ≤0.15%. Mechanical floor 90/45 ksi with hardness max 219 HBW / 95 HRB; solution anneal 1900 °F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 TP201 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP201 Stainless Steel Tube

ASME SA213 TP201 / UNS S20100 seamless boiler, superheater and heat-exchanger tube — a manganese-nitrogen austenitic with Mn 5.5–7.5%, Ni 3.5–5.5%, Cr 16.0–18.0%, N ≤0.25% and C ≤0.15%. Under SA-213 the tensile floor is 95/38 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 TP316L Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP316L Stainless Steel Tube

ASME SA213 TP316L / UNS S31603 seamless boiler, superheater and heat-exchanger tube with C ≤0.035% (Footnote D to 0.040% on small-OD / light-wall), Cr 16.0–18.0%, Ni 10.0–14.0%, Mo 2.00–3.00%, a 70/25 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 TP316 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP316 Stainless Steel Tube

ASME SA213 TP316 / UNS S31600 seamless boiler, superheater and heat-exchanger tube with Cr 16.0–18.0%, Ni 10.0–14.0%, Mo 2.00–3.00% and C ≤0.08%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 TP304L Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP304L Stainless Steel Tube

ASME SA213 TP304L / UNS S30403 seamless boiler, superheater and heat-exchanger tube with C ≤0.035% (Footnote D to 0.040% on small-OD / light-wall), Cr 18.0–20.0%, Ni 8.0–12.0%, a 70/25 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASME SA213 TP304 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP304 Stainless Steel Tube

ASME SA213 TP304 / UNS S30400 seamless boiler, superheater and heat-exchanger tube with Cr 18.0–20.0%, Ni 8.0–11.0% and C ≤0.08%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More

ASME SA213/SA213M Stainless Steel Products

ASME SA213 UNS S35045 Stainless Steel Tube ASME SA213 UNS S31277 Stainless Steel Tube ASME SA213 UNS S31272 Stainless Steel Tube ASME SA213 UNS S31254 Stainless Steel Tube
ASME SA213 UNS S31002 Stainless Steel Tube ASME SA213 UNS S30815 Stainless Steel Tube ASME SA213 UNS S30615 Stainless Steel Tube ASME SA213 TP XM-15 Stainless Steel Tube
ASME SA213 TP348H Stainless Steel Tube ASME SA213 TP348 Stainless Steel Tube ASME SA213 TP347W Stainless Steel Tube ASME SA213 TP347LN Stainless Steel Tube
ASME SA213 TP347HFG Stainless Steel Tube ASME SA213 TP347H Stainless Steel Tube ASME SA213 TP347 Stainless Steel Tube ASME SA213 TP321H Stainless Steel Tube
ASME SA213 TP321 Stainless Steel Tube ASME SA213 TP317LMN Stainless Steel Tube ASME SA213 TP317LM Stainless Steel Tube ASME SA213 TP317L Stainless Steel Tube
ASME SA213 TP317 Stainless Steel Tube ASME SA213 TP316LNM Stainless Steel Tube ASME SA213 TP316N Stainless Steel Tube ASME SA213 TP316Ti Stainless Steel Tube
ASME SA213 TP316H Stainless Steel Tube ASME SA213 TP310MoCbN Stainless Steel Tube ASME SA213 TP310MoLN Stainless Steel Tube ASME SA213 TP310HCbN Stainless Steel Tube
ASME SA213 TP310HCb Stainless Steel Tube ASME SA213 TP310Cb Stainless Steel Tube ASME SA213 TP310H Stainless Steel Tube ASME SA213 TP310S Stainless Steel Tube
ASME SA213 TP309LMoN Stainless Steel Tube ASME SA213 TP309HCb Stainless Steel Tube ASME SA213 TP309Cb Stainless Steel Tube ASME SA213 TP309H Stainless Steel Tube
ASME SA213 TP309S Stainless Steel Tube ASME SA213 UNS S30432 Stainless Steel Tube ASME SA213 TP304LN Stainless Steel Tube ASME SA213 TP304N Stainless Steel Tube
ASME SA213 TP304H Stainless Steel Tube ASME SA213 TP XM-19 Stainless Steel Tube ASME SA213 TP202 Stainless Steel Tube ASME SA213 TP201 Stainless Steel Tube
ASME SA213 TP316L Stainless Steel Tube ASME SA213 TP316 Stainless Steel Tube ASME SA213 TP304L Stainless Steel Tube ASME SA213 TP304 Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X