ASME SA213 TP316H Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP316H Stainless Steel Tube

ASME SA213 TP316H / UNS S31609 seamless boiler, superheater and heat-exchanger tube — H-grade Mo-bearing 16–18% Cr / 11–14% Ni with C 0.04–0.10%, Mo 2.00–3.00%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, a 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP316H / UNS S31609
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP316H Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. On Code-stamped boilers, superheaters, and heat exchangers that invoke the ASME adoption by name, SA-213 is the governing product standard for this H-grade Mo tube — written as its own Code Book line, not as a dual synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP316H / UNS S31609 is the high-carbon molybdenum austenitic row built for creep-oriented and elevated-temperature boiler / superheater duty inside that SA-213 family. Carbon is a true 0.04–0.10% band with both floor and ceiling — not “316 with a little more carbon” written as a single max — and nickel starts at 11.0% rather than the 10.0% floor used on TP316 / TP316L, while molybdenum stays 2.00–3.00%. ASTM grain size No. 7 or coarser is part of the heat-treatment lot acceptance, which is why a plain 316 heat cannot be remarked as 316H.

SHH STEEL can supply ASME SA213 TP316H as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report Mo inside 2.00–3.00%, carbon inside 0.04–0.10%, and E112 grain size No. 7 or coarser. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP316H.

Commercial maps say “316H,” “S31609,” or “H-grade 316 Mo tube.” Useful for RFQ triage; the purchase order should still carry ASME SA-213 Grade TP316H / UNS S31609, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements. Sister SA213 pages on the same spine include SA213 TP316, SA213 TP316L, SA213 TP316Ti, and SA213 TP304H when H-grade carbon is wanted without Mo. Seamless tube only — no Manufacturing Types (SML / WLD / HCW) H2.

Chemical Composition of SA213 TP316H

Two chemistry layers matter for TP316H under ASME SA-213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M). Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. The carbon band is the first line a reviewer should check: 0.04–0.10% with both floor and ceiling. The second line is molybdenum 2.00–3.00%. The third is nickel 11.0–14.0% — floor 11%, not 10%.

UNCERTAIN: exact SA-213 / A213 edition year; stainless chemistry table number (Table 1 vs Table 2 by edition); grain-size clause/table number; A480 Cr/Ni/Mo tolerance digits for the 16–18 / 11–14 / 2–3 bands applied from sister A480 practice — confirm ordered edition before treating catalogues as acceptance text. Nitrogen shows as no-requirement ellipsis (…) in the public stainless table used here; do not invent ≤0.10% unless the ordered edition lists it.

Melting analysis

Element TP316H (UNS S31609) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 11.0 – 14.0
Molybdenum (Mo) 2.00 – 3.00
Nitrogen (N) … (no requirement; analysis method by agreement when reported)

That melt table is the acceptance chemistry for every heat of SA213 TP316H. Carbon below 0.04% fails the H-grade floor even if Mo and Cr–Ni look perfect; carbon above 0.10% fails the ceiling. Nickel must clear 11.0% — a heat sitting at 10.5% Ni that would pass TP316 can fail TP316H. Molybdenum remains mandatory at 2.00–3.00%, the same Mo band as TP316 but now paired with H-grade carbon and grain size.

Product analysis (when required)

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 11.0 – 14.0 0.10 under / 0.15 over 10.90 – 14.15
Molybdenum (Mo) 2.00 – 3.00 0.05 under / 0.10 over 1.95 – 3.10

When product analysis is invoked, A480 A1.1 tolerances widen the melt windows as shown. Carbon product limits of 0.03–0.11% still have to protect the H-grade intent; Mo product 1.95–3.10% matches sister 316-family practice. Nitrogen remains without a melt requirement in the public table used here.

Snapshot vs sister grades

Element TP316L (S31603) TP316 (S31600) TP316H (S31609)
C ≤ 0.035 ≤ 0.08 0.04 – 0.10
Cr 16.0 – 18.0 16.0 – 18.0 16.0 – 18.0
Ni 10.0 – 14.0 10.0 – 14.0 11.0 – 14.0
Mo 2.00 – 3.00 2.00 – 3.00 2.00 – 3.00
Grain size not H-mandate not H-mandate ASTM No. 7 or coarser

Against SA213 TP316, the H grade raises the carbon floor, lifts the nickel floor to 11%, and adds the grain-size mandate. Against SA213 TP316L, carbon philosophy is opposite — L is capped low for as-welded IGC; H keeps carbon in band for creep strength. For Ti-stabilized Mo tube without H carbon, see SA213 TP316Ti.

Mechanical Properties of SA213 TP316H

ASME SA-213 sets the tensile acceptance floor for TP316H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness capped at 192 HBW / 200 HV or 90 HRB. Those tensile numbers match the standard 316-family floors; what separates H-grade acceptance is the chemistry band plus ASTM grain size No. 7 or coarser on the heat-treatment lot — not a higher Table 4 tensile row.

Property TP316H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Grain-size reporting is first-class on TP316H certificates. A heat that clears 75/30 ksi and 192 HBW but fails No. 7 or coarser is not acceptable H-grade tube under the heat-treatment row. Creep-oriented boiler and superheater datasheets rely on that controlled grain structure together with the 0.04–0.10% carbon band.

Flattening, flaring, and reverse-bend tests follow SA-213 / general-requirements practice for the ordered size. Hydrostatic testing or NDE is selected per specification and PO. Dual-marked jobs still clear SA-213 mechanical and grain-size text — see also A213 TP316H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP316H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and superheater datasheets that pick H-grade Mo tube almost always assume minimum wall because remaining wall after high-temperature oxidation and creep is a design input — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows.

Item Typical SA213 TP316H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for many boiler / superheater datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length for boiler and superheater circuits

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. Cut lengths for retube campaigns are commercial options on top of SA-213 dimensional rules — they do not replace minimum-wall or grain-size discipline.

Equivalent Grades

Equivalence language around TP316H must keep H-grade carbon, nickel floor, Mo, and grain size intact. ASME SA-213 Grade TP316H / UNS S31609 is the governing designation for this article; “316 or equivalent” on a creep datasheet is not automatic cover for S31609.

Designation Notes
ASME SA-213 / SA-213M Grade TP316H Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31609 Unified number in the stainless chemistry table
ASTM A213 TP316H Separate ASTM product specification — dual-mark only when the PO asks
Related standard 316 SA213 TP316 — C ≤0.08, Ni 10–14, no grain-size mandate
Related L-grade SA213 TP316L — C ≤0.035, lower tensile floors on some editions’ L rows, no H carbon floor
Related 304H SA213 TP304H — H-grade without Mo; different Cr–Ni
Related plate A240 / SA240 flat product in the 316 family — order plate and tube under their own standards

When a datasheet says “316H or equivalent,” confirm C 0.04–0.10, Ni ≥11%, Mo 2–3, grain No. 7 or coarser, and SA-213 (or dual A213) naming. Plate under A240 / SA240 does not automatically qualify as SA-213 tube. Non-Code ASTM purchase: A213 TP316H.

Heat Treatment and Delivery Condition

TP316H under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot. That heat-treatment row applies to both cold-finished and hot-finished seamless tube.

Skipping or under-cooling the solution treatment can leave a structure that fails the grain-size check or sensitizes in service even when ladle chemistry looked acceptable on paper. Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check.

Delivery condition for SHH STEEL TP316H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, molybdenum result, carbon band, and E112 grain-size result on the EN 10204 3.1 certificate. Public excerpts used for this pack do not place TP316H on the S2 stabilizing-hold list the way some Ti/Nb grades appear — if a project specification adds a stabilizing Supplementary Requirement, name it explicitly on the PO rather than assuming it is automatic.

Corrosion Resistance

TP316H keeps the molybdenum advantage of the 316 family — better resistance to chloride pitting and crevice attack than non-Mo 18-8 — while the H-grade carbon band and controlled grain size support elevated-temperature strength for boiler and superheater duty. It is not the first choice for as-welded intergranular-corrosion service; that path usually goes to SA213 TP316L or a stabilized grade.

In chloride-bearing cooling water and coastal condensers, Mo still helps, but H-grade carbon means fabrication welding needs procedures that manage sensitization risk if the equipment will see corrosive aqueous duty after welding. Creep-rupture and oxidation behavior at superheater temperatures are why datasheets pick H; aqueous IGC after welding is why they sometimes dual-specify L for cooler circuits.

Honest selection separates creep-oriented steam-side duty from aqueous process duty. For Ti-stabilized Mo tube aimed at sensitization resistance without L carbon, see SA213 TP316Ti. For non-Mo H-grade, see SA213 TP304H.

Applications of SA213 TP316H Tube

TP316H is ordered for Code boiler, superheater, and heat-exchanger circuits that need molybdenum austenitic tube with H-grade carbon and grain-size control — typically elevated-temperature steam-side or process exchangers where creep strength matters and Mo is required for the environment. It is less often the default for ambient chloride HX bundles, where TP316 or TP316L is more common.

Enquiry patterns ask for seamless cold-finished or hot-finished tube in boiler / superheater OD × minimum-wall sizes, cut-to-length for retube, with MTCs showing C band, Mo, and grain size. Hot-finished route remains available when wall and OD favor it.

Sister steering: standard Mo without H carbon → SA213 TP316; as-welded IGC / low carbon → SA213 TP316L; Ti-stabilized Mo → SA213 TP316Ti; H without Mo → SA213 TP304H.

Weldability

TP316H tube welds with matching or near-matching molybdenum austenitic filler (commonly ER316H / E316H family selections where the WPS calls H-grade carbon). Heat input and interpass control matter because the 0.04–0.10% carbon band raises sensitization risk relative to TP316L if the fabricated equipment will see corrosive aqueous service after welding.

For tube-to-tubesheet joints on superheater and boiler circuits, procedures should name TP316H / S31609 and address whether post-weld solution treatment or project-specific hold practices apply. Do not assume a TP316L WPS automatically covers H-grade carbon without requalification review.

When as-welded aqueous IGC resistance is the dominant requirement rather than creep-oriented H carbon, stewards usually change the base metal to TP316L (or TP316Ti) instead of trying to “weld around” H-grade carbon. Dual SA-213/A213 marking does not change filler selection.

Surface Finishes

Standard mill delivery for ASME SA213 TP316H is solution annealed and pickled, leaving a clean matte finish suitable for boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere is available by agreement.

ID/OD polish and special cleanliness are commercial options on top of SA-213 delivery condition — they do not replace carbon-band, Mo, grain-size, or anneal reporting. End caps and dry packaging matter more than paint on pickled stainless for export boiler tube.

SHH STEEL notes the ordered surface route on the packing list and keeps it consistent with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP316H includes heat analysis (carbon inside 0.04–0.10%, Mo inside 2.00–3.00%, Ni ≥11.0%), tension tests to 75/30 ksi floors, hardness to 192 HBW / 90 HRB, grain-size check to ASTM No. 7 or coarser per heat-treatment lot, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should verify grain-size results and the carbon band, not only tensile and Mo. A compliant 316 heat with C = 0.03% or Ni = 10.5% is not TP316H even if tensile looks fine.

Supplementary Requirements and third-party witness are available when named. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP316H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix. Bundle tags repeat ASME SA-213 Grade TP316H, UNS S31609, heat number, size, and wall basis so receivers can match the 3.1 certificate — including grain size — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP316H only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP316H as a Code Book H-grade Mo product with enforceable carbon band, nickel floor, molybdenum, grain-size, tensile, hardness, and marking rules — not as “316 that tested a bit high on carbon.” Enquiry review checks C 0.04–0.10, Ni ≥11%, Mo 2–3, and No. 7 or coarser grain size before release.

That discipline stops silent substitution with TP316 or TP316L heats on creep datasheets. We keep SA-213 and A213 independent, dual-mark only on request, and put Mo + carbon band + grain size on the 3.1 certificate.

Cross-links: SA213 TP316, SA213 TP316L, SA213 TP316Ti, SA213 TP304H, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP316H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for H-grade Mo boiler and superheater tube.

Item SHH STEEL capability for TP316H
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP316H / UNS S31609
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles
Documentation EN 10204 3.1 MTC with Mo + C band + grain size; A262 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP316H against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for boiler, superheater, and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common boiler / HX band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier superheater / HX wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, finish route, and whether dual A213 marking is required. SHH STEEL returns capability against ASME SA213 TP316H / UNS S31609 — not a dual stamp of TP316.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP316H?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry, tensile, hardness, and grain-size floors align closely for a given referenced edition, but they remain independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP316H include welded or HCW tube?
No. This page covers seamless boiler, superheater, and heat-exchanger tube only. WLD and HCW manufacturing-type labels from pipe standards are not product-form options on this pack. Welded stainless pipe belongs to a different product-standard family.
What is the UNS number and chemistry of ASME SA213 TP316H?
UNS S31609. Melting analysis centers on carbon 0.04–0.10%, chromium 16.0–18.0%, nickel 11.0–14.0%, and molybdenum 2.00–3.00%, with Mn ≤2.00, P ≤0.045, S ≤0.030, Si ≤1.00. Nitrogen is a no-requirement ellipsis in the public table used here. Product analysis, when ordered, applies A480 A1.1 tolerances.
TP316H vs TP316 — which SA213 tube should I order?
Order TP316H when the datasheet needs H-grade carbon 0.04–0.10%, nickel floor 11%, Mo 2–3%, and ASTM grain size No. 7 or coarser for creep-oriented boiler / superheater duty. Order TP316 when standard C ≤0.08%, Ni 10–14, Mo 2–3 without the H grain-size mandate is enough. A 316 heat is not a dual stamp of 316H.
TP316H vs TP304H — do I need molybdenum under SA213?
Yes when the environment or datasheet requires Mo 2–3%. TP304H is the H-grade path without molybdenum (different Cr–Ni). If chlorides or other pitting-active species drove the original Mo selection, staying on TP316H (or another Mo grade) matters; if the duty is non-Mo H-grade steam service, TP304H may be the named grade instead.
Why is the nickel floor 11% on SA213 TP316H?
The stainless chemistry table for TP316H / S31609 sets nickel at 11.0–14.0%, one percent higher on the floor than TP316 / TP316L (10.0–14.0%). A heat at 10.5% Ni can pass TP316 and still fail TP316H. Certificate review should check the Ni floor together with the carbon band and Mo window.
Does SA-213 require grain-size testing for TP316H?
Yes. ASTM grain size No. 7 or coarser is required per heat-treatment lot. The result belongs on the EN 10204 3.1 certificate with the 1900 °F solution anneal. That grain-size mandate is a primary reason TP316H is not interchangeable with TP316 by tensile numbers alone.
Does SA-213 set a hardness limit for TP316H?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Those mechanical floors match the standard 316 family; H-grade distinction sits in chemistry and grain size rather than a higher tensile row.
What heat treatment does ASME SA-213 require for TP316H?
Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool, plus ASTM grain size No. 7 or coarser per heat-treatment lot. Cold-finished versus hot-finished does not replace that anneal. Public excerpts used here do not auto-apply an S2 stabilizing hold to TP316H — name any extra hold on the PO if the project requires it.
Minimum wall vs average wall — which should I order for SA213 TP316H?
Boiler and superheater datasheets almost always assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over B36.19 pipe schedules.
Is TP316H a good as-welded choice for aqueous IGC under SA213?
Usually no. H-grade carbon 0.04–0.10% raises sensitization risk after welding compared with TP316L. For as-welded aqueous intergranular-corrosion duty, stewards typically order TP316L (or a stabilized grade such as TP316Ti) and reserve TP316H for creep-oriented elevated-temperature circuits where the carbon band and grain size are required.
Can you dual-certify ASME SA-213 and ASTM A213 TP316H?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including carbon band, Ni ≥11%, Mo, and grain size. Dual marking is documentation and stencil practice, not proof the names are synonyms. Otherwise SA-213 stands alone for Code Book jobs.

Conclusion

ASME SA213 TP316H / UNS S31609 is the H-grade molybdenum seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when creep-oriented duty needs C 0.04–0.10%, Ni 11.0–14.0%, Mo 2.00–3.00%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, a 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report Mo, the carbon band, and grain size. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X