ASME SA213 TP309H Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP309H Stainless Steel Tube

ASME SA213 TP309H / UNS S30909 seamless boiler, superheater and heat-exchanger tube — the H-grade 22–24% Cr / 12–15% Ni austenitic with controlled carbon 0.04–0.10%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting grain size.
Grade
TP309H / UNS S30909
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP309H Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP309H under that Code Book text is the high-temperature 22–24% chromium / 12–15% nickel austenitic listed as UNS S30909, with a controlled carbon range of 0.04–0.10% and a mandatory grain-size requirement of ASTM No. 7 or coarser after solution treatment. When a Code-stamped boiler or superheater datasheet calls for SA-213 TP309H, the purchase order and mill test certificate should carry the ASME H-grade designation, the carbon floor, and the grain-size result — not a tensile-only “309S” nickname stamped as if it were H grade.

SHH STEEL can supply ASME SA213 TP309H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry, the tensile plus hardness acceptance set, and the ASTM E112 grain-size result for the heat-treatment lot. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 309H, S30909 boiler tube, or SA213 309H superheater tube; none of those phrases replace the ASME H-grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP309S, SA213 TP310H, SA213 TP304H, SA213 TP321H, and SA213 TP347H. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP309H.

Chemical Composition of SA213 TP309H

Two chemistry layers matter for TP309H under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements path (commonly ASTM A1016/A1016M as referenced by the ordered SA-213 edition). Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise tighter catalogue chemistry windows that the Code Book text does not publish.

The tables below reproduce the heat analysis for TP309H / UNS S30909, the product-analysis limits from A480 Table A1.1 tolerances, and a short carbon-band comparison against TP309S. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; grain-size clause/table number wording across editions (public heat-treatment table shows grain-size column “7”) — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP309H / UNS S30909. Confirm the ordered ASME edition on the purchase order.

Element TP309H (UNS S30909) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 15.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 22.0 – 24.0 0.25 under / over 21.75 – 24.25
Nickel (Ni) 12.0 – 15.0 0.15 under / over 11.85 – 15.15

309-family carbon comparison (melt)

Element TP309S (S30908) TP309H (S30909)
C ≤ 0.08 0.04 – 0.10
Cr 22.0 – 24.0 22.0 – 24.0
Ni 12.0 – 15.0 12.0 – 15.0
Grain size not H-grade mandatory ASTM No. 7 or coarser

The carbon floor at 0.04% is what separates TP309H from ordinary TP309S on paper and in creep-range service: low-carbon or mid-carbon heats that clear TP309S tensile numbers do not automatically clear the H-grade carbon range or the coarse-grain requirement. Chromium 22–24% and nickel 12–15% keep the oxidation-resistant balance after the 1900 °F [1040 °C] solution treatment. Heats that also meet TP309S carbon and tensile rules can sometimes be dual-certified TP309S/TP309H when grain size also clears — ask for that marking on the PO rather than assuming it from a PMI gun reading of “309.”

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 21.75–24.25%, and Ni 11.85–15.15%. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project carbon floor or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP309H

ASME SA-213 sets the room-temperature tensile acceptance floor for TP309H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same tensile pair as standard TP309S. The same mechanical table also lists a hardness maximum of 192 HBW / 200 HV or 90 HRB, and hardness tests are part of the lot acceptance scheme. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112.

Source: public SA-213 / A213 mechanical-table summaries for TP309H / UNS S30909 (commonly Table 4) and H-grade grain-size language. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP309H requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Flattening and flaring tests are also required on a lot basis for finished tube. Room-temperature tensile equality with TP309S is why dual 309S/309H stock is attractive; elevated-temperature allowables in the design code, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size is incomplete for TP309H — ask for the E112 result on the certificate before releasing the heat to fabrication. For higher Cr–Ni H-grade oxidation framing, open SA213 TP310H; for 18-8 H-grade without the 22Cr step-up, open SA213 TP304H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP309H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication — especially important on superheater tubes where remaining wall after oxidation or fireside attack is a design input.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP309H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP309H tube is often looser than a Code or boiler purchase order can afford. ASME SA-213 Grade TP309H / UNS S30909 is the governing designation for this article; approximate wrought names that point to 22Cr-12Ni H-grade families are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 309H,” confirm which product standard, carbon band, grain-size clause, and heat-treatment temperature the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP309H Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30909 Unified number listed with the H-grade chemistry
ASTM A213 TP309H Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP309H
Related S sister SA213 TP309S for C ≤0.08% without H-grade grain-size mandatory language
Related higher-alloy H SA213 TP310H when even higher Cr–Ni H-grade framing is required
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP309H is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare 18-8 H-grade SA213 TP304H and stabilized H grades on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP309H under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row also carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot — the clause that separates H-grade acceptance from ordinary TP309S solution treatment at the same temperature. Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check.

Delivery condition for SHH STEEL TP309H is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature, quench method, and ASTM E112 grain-size result stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability is ordered, the corrosion test report travels with the heat-treatment and grain-size record. Do not treat a TP309S anneal certificate as automatic TP309H acceptance — without the carbon floor and the coarse-grain result, the H grade is not complete. For Cb-bearing 309H variants when the datasheet names them, open the matching sister page on the hub rather than assuming Nb is present in standard TP309H.

Corrosion Resistance

TP309H is selected for high-temperature oxidation and creep-oriented boiler service on a 22–24% Cr / 12–15% Ni balance, with the H-grade carbon and grain-size controls supporting elevated-temperature performance. It is not framed as a molybdenum chloride-pitting upgrade. In wet chloride-bearing exchangers, do not select TP309H as a substitute for SA213 TP316L or higher-Mo grades. Intergranular corrosion after fabrication is a different conversation from steam oxidation: carbon 0.04–0.10% is intentional for H-grade strength, so as-welded wet-service IGC resistance is not the grade’s selling point.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP309H; selection remains engineering judgment against design metal temperature, atmosphere, and Code allowables. When a project specification adds a named corrosion test, write that Supplementary Requirement onto the purchase order so the test is contractual. SHH STEEL will not rank TP309H as equal to 316 in chlorides — higher chromium plus H-grade carbon is not a molybdenum substitute.

Applications of SA213 TP309H Tube

Because TP309H combines 22–24% Cr / 12–15% Ni oxidation resistance with H-grade carbon and grain-size controls under SA-213, it shows up in creep-range boiler and superheater circuits, high-temperature process exchangers, and elevated-temperature steam service where ordinary TP309S lacks the carbon floor and coarse-grain documentation. The table below pairs typical application areas with a selection note so the grade is chosen for design metal temperature and Code allowables — not only for the familiar “309H” name on the BOM.

Application area Typical use of TP309H tube Selection note
Creep-range boiler / superheater Seamless tube where H-grade carbon and grain size are specified on 22Cr-12Ni chemistry Require E112 grain size on the MTC
High-temperature oxidation + creep Circuits needing both scale resistance and H-grade framing Compare with TP310H if higher Cr–Ni is named
Process steam / hot-gas HX Elevated metal temperature exchangers ordered to SA-213 Confirm atmosphere and remaining-wall basis
Programs dual-certifying 309S/309H When stock must clear both carbon paths and grain size Ask for dual marking on the PO — do not assume from PMI
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For standard-carbon 309S without H-grade grain-size mandatory language open SA213 TP309S; for higher Cr–Ni H-grade open SA213 TP310H; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP309H tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER309 / ER309H-oriented consumables under a qualified WPS aligned with the H-grade base metal carbon story; some fabricators still use ER309L when the WPS qualifies it, but the filler carbon path should be discussed against the service temperature and Code rules. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP309H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and the contractual grain-size result on the base metal certificate. Because carbon sits in the 0.04–0.10% H-grade band, as-welded wet-service IGC resistance is not the grade’s primary claim — discuss post-weld solution treatment when the fabrication sequence and service environment require it. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP309H is solution annealed and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface and must be called out because it changes the heat-treatment route while still needing to clear the grain-size requirement. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a project specification quotes an Ra maximum or a special OD grind for tube expanding, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and grain-size identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP309H includes heat analysis (with carbon in the 0.04–0.10% band), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, grain-size determination to ASTM No. 7 or coarser per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP309H tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Grain-size reporting detail Ensures ASTM E112 method and lot identity are explicit on the MTC
Intergranular corrosion A262 Practice E (or agreed practice) when contractually required
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness, tension, and grain-size specimens map cleanly to the bundle you receive. An MTC that omits grain size or that reports carbon outside 0.04–0.10% is incomplete for S30909 — reject it before the heat leaves the mill.

Packaging and Shipping

TP309H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. Superheater cut lengths and U-bent tubes need extra cradle or case protection so ends and bend radii are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP309H as a Code Book product standard with enforceable chemistry, tensile, hardness, grain-size, heat-treatment, and marking rules — not as a catalogue nickname for “any 309 tube with a high-temp sticker.” The MTC reports the full ladle chemistry including carbon in the 0.04–0.10% band, the 75/30 ksi tensile plus hardness acceptance set, and the ASTM E112 grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 309-family conversation honest for boiler and HX duty. If standard-carbon 309S without H-grade grain-size mandatory language is enough, we open SA213 TP309S. If even higher chromium–nickel H-grade oxidation framing is specified, we open SA213 TP310H. If 18-8 H-grade without the 22Cr step-up is enough, we open SA213 TP304H. If chlorides dominate a wet exchanger, we open SA213 TP316L rather than stretching 309H into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP309H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for creep-range boiler and superheater duty.

Item SHH STEEL capability for TP309H
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP309H / UNS S30909
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size ASTM No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry and grain size; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309H tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for H-grade high-temperature boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP309H
Outside diameter 25.4, 31.8, 38.1, 42.4, 44.5, 50.8, 57.0, 63.5, 76.2 mm (and other boiler/superheater ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–16 class walls and metric min-wall equivalents typical for superheater duty; lighter and heavier walls by agreement
Common OD × wall examples 31.8 × 2.77 mm; 38.1 × 3.40 mm; 42.4 × 3.40 mm; 44.5 × 3.60 mm; 50.8 × 3.60 mm; 50.8 × 4.00 mm; 63.5 × 4.00 mm — illustrative boiler/superheater sizes, confirm min vs average wall
Length Cut lengths for boiler / superheater circuits; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual SA-213/A213 or dual TP309S/TP309H marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the 0.04–0.10% carbon band), tensile, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP309S, SA213 TP310H, and SA213 TP304H sit on the same hub when the datasheet steps beyond TP309H.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP309H?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP309H include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP309H under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP309H?
TP309H is UNS S30909. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, and nickel 12.0–15.0%, with molybdenum, nitrogen, and niobium as no-requirement ellipses on the standard TP309H row. Product-analysis limits apply only when ordered. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP309H vs TP309S — which SA213 grade should I order?
Order TP309H when the boiler or superheater datasheet needs carbon 0.04–0.10% and ASTM No. 7 or coarser grain size on the 22–24% Cr / 12–15% Ni balance. Order TP309S when the specification calls for C ≤0.08% without H-grade carbon and grain-size controls. Room-temperature tensile floors match at 75/30 ksi, so tensile equality alone is not a reason to treat them as synonyms. Spell the required grade on the enquiry.
TP309H vs TP304H — when do I need the higher Cr–Ni H grade under SA213?
Order TP309H when high-temperature oxidation resistance from 22–24% Cr / 12–15% Ni is required together with H-grade carbon and grain-size controls. Order TP304H when 18-8 H-grade framing is enough without the chromium–nickel step-up. Both carry 75/30 ksi room-temperature floors and ASTM No. 7 or coarser grain size, but they are different chemistries on the MTC. Confirm design metal temperature and atmosphere before swapping.
Why does SA-213 require grain size for TP309H?
The H-grade heat-treatment path under SA-213 pairs the controlled carbon range with a coarse-grain requirement — ASTM No. 7 or coarser per heat-treatment lot, typically determined by ASTM E112. That combination supports elevated-temperature creep-oriented framing that ordinary TP309S solution treatment at the same 1900 °F temperature does not automatically provide. A tensile-only MTC that omits grain size is incomplete for TP309H.
Does SA-213 set a hardness limit for TP309H?
Yes. The mechanical table for TP309H lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB, alongside the grain-size requirement. Hardness tests are part of lot acceptance under SA-213. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What heat treatment does ASME SA-213 require for TP309H?
TP309H is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled, with ASTM grain size No. 7 or coarser required for the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that path. Ask the mill to state anneal temperature, quench method, and E112 grain-size result on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
Minimum wall vs average wall — which should I order for SA213 TP309H?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance — especially important on superheater circuits where remaining wall after oxidation is a design input. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling.
Is TP309H a good choice for chloride-rich cooling water under SA213?
Usually no. TP309H is framed for high-temperature oxidation and creep-oriented boiler service on a Cr–Ni H-grade balance, not for molybdenum-driven chloride pitting resistance. In seawater-leaning cooling water and wet brine exchangers, open TP316L or higher-Mo grades on the SA213 hub. ASME SA-213 does not publish a chloride ranking that supports treating 309H as a 316 substitute.
Can you dual-certify ASME SA213 TP309S and TP309H?
Yes when the heat clears both carbon paths and the H-grade grain-size requirement, and when tensile plus hardness clear both mechanical-table rows. Dual TP309S/TP309H marking is a purchase-order option, not something to assume from a PMI gun reading of "309." Spell the required dual marking on the enquiry so the heat is selected and tested correctly.
Can you dual-certify ASME SA-213 and ASTM A213 TP309H?
Yes when the heat and testing support both independent standards. Dual SA-213/A213 marking is available when the purchase order requests both names on the stencil and MTC, including grain-size documentation. Spell the required marking on the enquiry so Code and non-Code paperwork stay cleanly aligned.

Conclusion

ASME SA213 TP309H / UNS S30909 is the H-grade 22–24% Cr / 12–15% Ni seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when controlled carbon 0.04–0.10%, ASTM No. 7 or coarser grain size, and high-temperature oxidation framing are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the 75/30 ksi tensile and hardness acceptance floors with grain size reported, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X