ASME SA213 TP304H Stainless Steel Tube
What is ASME SA213 TP304H Stainless Steel Tube
ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP304H under that Code Book text is the high-temperature 18-8 austenitic listed as UNS S30409, with a controlled carbon range of 0.04–0.10%, chromium 18.0–20.0%, nickel 8.0–11.0%, and a mandatory grain-size requirement of ASTM No. 7 or coarser after solution treatment. When a Code-stamped boiler or superheater datasheet calls for SA-213 TP304H, the purchase order and mill test certificate should carry the ASME H-grade designation, the carbon floor, and the grain-size result — not a tensile-only “304” nickname stamped as if it were H grade.
SHH STEEL can supply ASME SA213 TP304H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry, the tensile plus hardness acceptance set, and the ASTM E112 grain-size result for the heat-treatment lot. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.
Commercially the same tube is still called 304H, S30409 boiler tube, or SA213 304H superheater tube; none of those phrases replace the ASME H-grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP304, SA213 TP304L, SA213 TP321H, SA213 TP347H, and SA213 TP316H. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP304H.
Chemical Composition of SA213 TP304H
Two chemistry layers matter for TP304H under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements path (commonly ASTM A1016/A1016M as referenced by the ordered SA-213 edition). Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise tighter catalogue chemistry windows that the Code Book text does not publish.
The tables below reproduce the heat analysis for TP304H / UNS S30409, the product-analysis limits from A480 Table A1.1 tolerances, and a short carbon-band comparison across the 304 family. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; grain-size clause/table number wording across editions (public heat-treatment table shows grain-size column “7”) — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.
Melting analysis (heat / ladle analysis)
Source: public SA-213 / A213 grade-table summaries for TP304H / UNS S30409. Confirm the ordered ASME edition on the purchase order.
| Element | TP304H (UNS S30409) melting analysis |
|---|---|
| Carbon (C) | 0.04 – 0.10 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 18.0 – 20.0 |
| Nickel (Ni) | 8.0 – 11.0 |
| Molybdenum (Mo) | … (no requirement) |
| Nitrogen (N) | … (no requirement) |
Product analysis — A480/A480M Table A1.1 tolerances applied
| Element | Melting | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | 0.04 – 0.10 | 0.01 under / over | 0.03 – 0.11 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 18.0 – 20.0 | 0.20 under / over | 17.80 – 20.20 |
| Nickel (Ni) | 8.0 – 11.0 | 0.10 under / 0.15 over | 7.90 – 11.15 |
304-family carbon comparison (melt)
| Element | TP304L (S30403) | TP304 (S30400) | TP304H (S30409) |
|---|---|---|---|
| C | ≤ 0.035 | ≤ 0.08 | 0.04 – 0.10 |
| Mn | ≤ 2.00 | ≤ 2.00 | ≤ 2.00 |
| Cr | 18.0 – 20.0 | 18.0 – 20.0 | 18.0 – 20.0 |
| Ni | 8.0 – 12.0 | 8.0 – 11.0 | 8.0 – 11.0 |
The carbon floor at 0.04% is what separates TP304H from ordinary TP304 on paper and in creep-range service: low-carbon heats that clear TP304 tensile numbers do not automatically clear the H-grade carbon range or the coarse-grain requirement. Chromium 18–20% and nickel 8–11% keep the familiar 18-8 balance after the 1900 °F [1040 °C] solution treatment. Heats that also meet TP304 carbon and tensile rules can sometimes be dual-certified TP304/TP304H when grain size also clears — ask for that marking on the PO rather than assuming it from a PMI gun reading of “304.”
When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 17.80–20.20%, and Ni 7.90–11.15%. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project carbon floor or sulfur ceiling on the purchase order before the heat is selected.
Mechanical Properties of SA213 TP304H
ASME SA-213 sets the room-temperature tensile acceptance floor for TP304H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same tensile pair as standard TP304. The same mechanical table also lists a hardness maximum of 192 HBW / 200 HV or 90 HRB, and hardness tests are part of the lot acceptance scheme. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112.
Source: public SA-213 / A213 mechanical-table summaries for TP304H / UNS S30409 (commonly Table 4) and H-grade grain-size language. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.
| Property | TP304H requirement |
|---|---|
| Tensile strength, min | 75 ksi [515 MPa] |
| Yield strength (0.2% offset), min | 30 ksi [205 MPa] |
| Elongation in 2 in. or 50 mm, min | 35% |
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Grain size | ASTM No. 7 or coarser (per heat-treatment lot) |
Flattening and flaring tests are also required on a lot basis for finished tube. Room-temperature tensile equality with TP304 is why dual 304/304H stock is attractive; elevated-temperature allowables in the design code, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size is incomplete for TP304H — ask for the E112 result on the certificate before releasing the heat to fabrication. For creep-range service that needs stabilization chemistry rather than plain 18-8 H-grade, open SA213 TP321H or SA213 TP347H.
Dimensions and Tolerances
Dimensional supply for ASME SA213 TP304H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication — especially important on superheater and reheater tubes where remaining wall after oxidation or fireside attack is a design input.
Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.
| Item | Typical SA213 TP304H dimensional practice |
|---|---|
| Product form | Seamless only (cold-finished or hot-finished) |
| Usual size band | ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so) |
| Wall basis | Minimum wall (default commercial practice) or average wall when specified |
| OD / wall tolerances | Per general requirements for the finish route and size; cold-finished average wall often ±10% |
| Length | Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement |
| Secondary size note | ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout |
Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.
Equivalent Grades
Equivalence language around TP304H tube is often looser than a Code boiler purchase order can afford. ASME SA-213 Grade TP304H / UNS S30409 is the governing designation for this article; EN 1.4948 and JIS SUS304H are approximate wrought names that point to similar high-temperature 18-8 families but are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 304H,” confirm which product standard, carbon range, grain-size clause, and heat-treatment row the mill will actually certify.
| Designation | Notes |
|---|---|
| ASME SA-213 / SA-213M Grade TP304H | Governing ASME Code Book seamless boiler / HX tube product standard for this article |
| UNS S30409 | Unified number listed with the H-grade chemistry |
| ASTM A213 TP304H | Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP304H |
| EN 1.4948 (X6CrNi18-10) | Approximate wrought high-temperature designation; order EN tube forms under the relevant EN tube specs |
| JIS SUS304H | Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product |
| Related plate | A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards |
ASTM A213 TP304H is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare standard SA213 TP304, low-carbon SA213 TP304L, and stabilized H grades on their own ASME pages before swapping grades in a superheater bundle.
Heat Treatment and Delivery Condition
TP304H under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. The H-grade path also requires that grain size after heat treatment meet ASTM No. 7 or coarser for the heat-treatment lot. That combination — solution treatment plus coarse-grain control — is what separates TP304H paperwork from a tensile-only TP304 certificate. Both cold-finished and hot-finished seamless tube follow the heat-treatment requirement.
Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP304H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and grain-size result stated on the EN 10204 3.1 certificate. Straightening after anneal is controlled so cold work does not undermine the coarse-grain objective at the ends.
Stabilizing heat treatments used on titanium- or niobium-bearing grades are not the TP304H route; if the process needs stabilization chemistry, open SA213 TP321H or SA213 TP347H instead of stretching 304H beyond its design intent. When Supplementary Requirement language for intergranular-corrosion capability is ordered, the corrosion test report travels with the heat-treatment and grain-size record.
Corrosion Resistance
TP304H’s chromium-rich passive film handles the same broad band of oxidizing process fluids and steam-side duties as standard TP304 in many services, but the controlled carbon floor that serves creep strength also means sensitization risk after welding or after holding in the carbide-precipitation range must be managed deliberately. In chloride-bearing waters and many brine-leaning heat-exchanger services, pitting and crevice attack become limiting the same way they do for TP304, and buyers usually step up to SA213 TP316H or the non-H molybdenum sisters. Intergranular corrosion risk after tube-to-tubesheet welding is controlled by solution treating after fabrication when the sequence allows, by invoking the contractual corrosion test on the tube PO, or by choosing a stabilized H grade when the process demands it.
ASME SA-213 itself does not publish a corrosion-rate table for TP304H; selection for creep-range boiler service is driven by design-code allowables and grain-size control as much as by aqueous corrosion ranking. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed. SHH STEEL will not treat TP304H as interchangeable with TP304L for as-welded IGC duty — the carbon stories run in opposite directions.
Applications of SA213 TP304H Tube
Because TP304H exists for elevated-temperature boiler and superheater framing under the Code Book text, it shows up across power-plant steam systems, industrial boilers, and process heaters where design metal temperature and creep-rupture allowables drive the H-grade callout. The table below pairs typical application areas with a selection note so the grade is chosen for temperature and grain-size control — not only for the familiar “304H” name on the BOM.
| Application area | Typical use of TP304H tube | Selection note |
|---|---|---|
| Boiler / superheater | Seamless generating, screen, and superheater tubing ordered to SA-213 H-grade | Confirm design metal temperature and Code allowables for S30409 |
| Reheater / high-temp steam | Seamless tube where creep-rupture framing needs C floor + coarse grain | Grain-size result mandatory on MTC — reject tensile-only certs |
| Process heaters | Furnace and convection-section tube in oxidizing process heaters | Compare TP321H/TP347H if stabilization chemistry is specified |
| Heat exchangers (elevated T) | HX tubes where H-grade is written even if aqueous corrosion is mild | State min vs average wall and bend radius on the enquiry |
| General Code steam duty | Seamless tube where SA-213 H-grade documentation is preferred | Do not substitute standard TP304 paperwork for TP304H acceptance |
| Dual 304/304H programs | Stock that must clear both standard and H-grade rows | Ask for dual marking on the PO; grain size still required |
For as-welded low-carbon IGC service open SA213 TP304L; for stabilized high-temperature chemistry open SA213 TP321H / SA213 TP347H on the same SA213/SA213M hub.
Weldability
TP304H tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER308H / ER308 (or equivalent covered electrodes) under a qualified WPS when the H-grade carbon story must be preserved in the weld metal; many shops avoid defaulting to ER308L for H-grade base metal because the low-carbon deposit can undermine the high-temperature intent of the joint. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.
Because SA213 TP304H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, grain-size documentation on the base metal, and any contractual corrosion test. For tube that will enter service as-welded in a sensitizing aqueous environment, many owners change the base metal to SA213 TP304L rather than relying on a perfect weld procedure alone to protect H-grade carbon. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.
Surface Finishes
Standard mill delivery for ASME SA213 TP304H is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and superheater tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route — and must still deliver the ASTM No. 7 or coarser grain-size result. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.
When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and (on request) grain-size identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.
Inspection and Testing
Base ASME SA-213 testing for TP304H includes heat analysis (with carbon reported in the 0.04–0.10% band), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, grain-size determination to ASTM No. 7 or coarser per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.
Supplementary Requirements commonly added on TP304H tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, IGC testing, or dual 304/304H marking from a verbal “full certs” note.
| Option | Purpose |
|---|---|
| Product analysis | Confirms chemistry on finished tube (via general requirements / PO language) |
| Intergranular corrosion | A262 Practice E (or agreed practice) as a contractual Supplementary Requirement |
| Minimum vs average wall | States which wall basis the size callout uses |
| Fixed hydro or NDE method | Removes manufacturer’s option when the end user mandates one route |
| Third-party inspection / EN 10204 3.2 | Witnessed testing and certificate when the project requires it |
Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity and the E112 grain-size result clearly on the certificate. An MTC that omits grain size is incomplete for TP304H — reject it before the heat leaves the mill.
Packaging and Shipping
TP304H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.
Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.
Why Choose SHH STEEL
SHH STEEL treats ASME SA213 TP304H as a Code Book H-grade product standard with enforceable carbon range, tensile, hardness, heat-treatment, grain-size, and marking rules — not as a catalogue nickname for “any 304 tube with a high-temp story.” The MTC reports the full ladle chemistry, the 75/30 ksi tensile plus hardness acceptance set, and the ASTM E112 grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.
We keep the 304-family conversation honest for boiler and superheater duty. If standard carbon without grain-size control is enough, we open SA213 TP304. If as-welded IGC resistance is the driver, we open SA213 TP304L. If stabilization chemistry is required, we open SA213 TP321H / SA213 TP347H. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.
Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME H-grade callout the engineer wrote, with paperwork a third-party inspector can read without translation.
Supply Capability
SHH STEEL can supply ASME SA213 TP304H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and superheater duty.
| Item | SHH STEEL capability for TP304H |
|---|---|
| Standard | ASME SA213 / SA213M (dual A213 marking on request) |
| Grade | TP304H / UNS S30409 |
| Product form | Seamless only — cold-finished and hot-finished |
| Size | Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement |
| Wall / gauge | Minimum wall or average wall; BWG / gauge callouts accepted on enquiry |
| Length | Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry |
| Finish | Annealed and pickled; bright annealed or light polish by agreement |
| Testing | Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size ASTM No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order |
| Documents | EN 10204 3.1 with full ladle chemistry and grain-size result; third-party inspection / 3.2 on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes
SHH STEEL quotes TP304H tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.
| Item | Typical stock / enquiry range for TP304H |
|---|---|
| Outside diameter | 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other boiler/HX ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band) |
| Wall / BWG | BWG 10–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement |
| Common OD × wall examples | 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm; 50.8 × 3.38 mm — illustrative boiler/HX sizes, confirm min vs average wall |
| Length | Cut lengths for boiler / superheater / exchanger bundles; U-bends and straight random lengths on enquiry |
| Special | Non-standard OD/wall, bright anneal, dual SA-213/A213 marking, and dual TP304/TP304H — confirm on enquiry before the heat is reserved |
When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), grain-size reporting, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.
Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the 0.04–0.10% carbon band), tensile, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP304, SA213 TP347H, and SA213 UNS S30432 sit on the same hub when the datasheet steps beyond TP304H.
FAQ
-
Is ASME SA-213 the same as ASTM A213 for TP304H?
- No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
-
Does ASME SA213 TP304H include welded or HCW tube?
- No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP304H under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
-
Minimum wall vs average wall — which should I order for SA213 TP304H?
- Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from the general requirements.
-
Hydrostatic test vs NDE — which do I get on SA213 TP304H tube?
- ASME SA-213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
-
Does SA-213 require grain size for TP304H?
- Yes. Beyond the 75/30 ksi tensile floor and 192 HBW / 90 HRB hardness maximum, TP304H requires grain size ASTM No. 7 or coarser per heat-treatment lot, typically determined under ASTM E112. A tensile-only certificate that omits grain size is incomplete for the H grade. Ask the mill to report the E112 result on the EN 10204 3.1 certificate before releasing the heat to fabrication.
-
What is the UNS number and chemistry of ASME SA213 TP304H?
- TP304H is UNS S30409. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 18.0–20.0%, and nickel 8.0–11.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
-
TP304 vs TP304H — when do I need the H grade under SA213?
- Order TP304H when the boiler or superheater datasheet needs the H-grade carbon range (0.04–0.10%), grain-size controls (ASTM No. 7 or coarser), and creep-rupture framing that the H designation carries under SA-213. Standard TP304 remains appropriate for many moderate-temperature HX and general corrosive tube duties. Do not treat "304H" as a synonym stamp for ordinary TP304 on the MTC.
-
TP304H vs TP304L — are they interchangeable under SA213?
- No. TP304H raises carbon into a controlled floor for high-temperature strength and requires coarse grain; TP304L lowers carbon for as-welded intergranular resistance and uses a lower 70/25 ksi tensile floor. The carbon stories run in opposite directions. Dual TP304/TP304H is sometimes possible on qualifying heats; dual TP304H/TP304L is not a meaningful commercial path.
-
What heat treatment does ASME SA-213 require for TP304H?
- TP304H is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation, and grain size after heat treatment must meet ASTM No. 7 or coarser for the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that path. Ask the mill to state anneal temperature, quench method, and grain-size result on the EN 10204 3.1 certificate.
-
TP304H vs TP321H / TP347H — which H grade should I order?
- Order TP304H when plain 18-8 H-grade chemistry with carbon floor and coarse grain is what the datasheet specifies. Order TP321H or TP347H when the process needs titanium or niobium stabilization chemistry in addition to H-grade high-temperature framing. They are sister H grades under SA-213, not interchangeable stamps — follow the grade the engineer wrote.
-
Can you dual-certify ASME SA-213 and ASTM A213 TP304H, or TP304/TP304H?
- Yes on both axes when the heat and testing support it. Dual SA-213/A213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Dual TP304/TP304H is available when ladle chemistry meets the H-grade carbon range, tensile plus hardness clear both rows, and grain size meets ASTM No. 7 or coarser. Spell the required marking on the enquiry so the heat is selected correctly.
Conclusion
ASME SA213 TP304H / UNS S30409 is the H-grade 18-8 seamless stainless steel tube under the Code Book text when a boiler or superheater project needs the 0.04–0.10% carbon range, ASTM No. 7 or coarser grain size, and the creep-range framing that ordinary TP304 does not carry. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the tensile and hardness acceptance floors with grain size reported, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.
Contact: admin@steelspecs.com