ASME SA213 TP347W / UNS S34705 tungsten-bearing niobium-stabilized seamless boiler, superheater and heat-exchanger tube — C ≤0.05%, Cr 17.0–20.0%, Ni 8.00–11.0%, N 0.10–0.25%, Nb 0.25–0.50%, V 0.20–0.50%, W 1.50–2.60%, Table 4 90/38 ksi with elongation 30% min, hardness max 219 HBW / 95 HRB, 2000 °F solution anneal, grain size ASTM No. 7–10. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report W, V, N, and Nb together.
Grade
TP347W / UNS S34705
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP347W Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers or superheaters invoke that adoption by name, SA-213 is the governing product standard for this tungsten-bearing niobium grade — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP347W / UNS S34705 sits inside that stainless family as a deliberately alloyed row: melting carbon is capped at 0.05%, chromium at 17.0–20.0%, nickel at 8.00–11.0%, nitrogen at 0.10–0.25%, niobium in a fixed 0.25–0.50% band (not a 10 × C formula), vanadium at 0.20–0.50%, and tungsten at 1.50–2.60%. Table 4 raises the tensile floor to 90 ksi [620 MPa] / 38 ksi [260 MPa] with elongation 30% minimum and hardness max 219 HBW / 95 HRB — a step above the 75/30 ksi / 35% set on plain TP347. Buyers who write “347W superheater tube” still need to name SA-213 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the W/V/N/Nb package together. This is not a dual stamp of TP347, TP347H, or TP347HFG.

SHH STEEL can supply ASME SA213 TP347W as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report tungsten, vanadium, nitrogen, and niobium together with the 90/38 ksi tensile set, 30% elongation, hardness, and the ASTM No. 7–10 grain-size window. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP347W.

Shop names include “347W,” “S34705,” and “W-bearing 347 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP347W / UNS S34705, wall basis, OD × wall or BWG, finish route, and any negotiated stabilization language — public Supplementary Requirements S1 and S2 do not list TP347W the way they list TP347 / TP348. Sister SA213 pages include SA213 TP347, SA213 TP347H, SA213 TP347HFG, and SA213 TP347LN. Seamless only — no Manufacturing Types (SML / WLD / HCW) product-form split on this page.

Chemical Composition of SA213 TP347W

Two chemistry layers matter for TP347W under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The defining package for a reviewer is the combination of C ≤0.05%, N 0.10–0.25%, Nb 0.25–0.50% as a fixed band, V 0.20–0.50%, and W 1.50–2.60% — not a plain Nb ≥10 × C check copied from TP347. Phosphorus is capped at 0.040% on this row (tighter than the 0.045% ceiling on many sister 18-8 grades). Nickel sits at 8.00–11.0%, a narrower and slightly leaner window than TP347’s 9–13% band.

The tables below reproduce the melt limits for TP347W / UNS S34705, the product-analysis limits from A480 Table A1.1 practice (with W and V tolerance digits labeled UNCERTAIN pending the ordered A480 edition), and a short W/V/N/Nb snapshot against TP347, TP347H, and TP347HFG. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. Nitrogen method is often Footnote B practice — write the method on the PO when N is contractual.

Melting analysis (heat / ladle analysis)

Element TP347W (UNS S34705) melting analysis
Carbon (C) ≤ 0.05
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 20.0
Nickel (Ni) 8.00 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.10 – 0.25
Niobium (Nb / Cb) 0.25 – 0.50
Vanadium (V) 0.20 – 0.50
Tungsten (W) 1.50 – 2.60
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for Grade TP347W / UNS S34705 (same grade text family). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text; Footnote B nitrogen-method wording if the edition prints it.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.05 0.01 over ≤ 0.06
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.040 0.010 over ≤ 0.050
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 20.0 0.20 under / over 16.80 – 20.20
Nickel (Ni) 8.00 – 11.0 0.15 under / 0.20 over 7.85 – 11.20
Nitrogen (N) 0.10 – 0.25 0.01 under / 0.02 over (sister N practice) 0.09 – 0.27
Niobium (Nb) 0.25 – 0.50 0.05 under / over (Nb range practice) 0.20 – 0.55
Vanadium (V) 0.20 – 0.50 0.05 under / over (UNCERTAIN — confirm A480) 0.15 – 0.55
Tungsten (W) 1.50 – 2.60 0.05 under / over (UNCERTAIN — confirm A480) 1.45 – 2.65

Product analysis is not automatic — order it when the project needs finished-tube chemistry. UNCERTAIN: A480 product-tolerance digits for W and V are applied from sister-pack practice pending the ordered A480 edition.

W / V / N / Nb snapshot — TP347 / TP347W / TP347H / TP347HFG

Element TP347 (S34700) TP347W (S34705) TP347H (S34709) TP347HFG (S34710)
C ≤ 0.08 ≤ 0.05 0.04 – 0.10 0.06 – 0.10
Ni 9.0 – 13.0 8.00 – 11.0 9.0 – 13.0 9.0 – 13.0
N … 0.10 – 0.25 … …
Nb ≥ 10 × C, ≤ 1.10 0.25 – 0.50 ≥ 8 × C, ≤ 1.10 ≥ 8 × C, ≤ 1.10
V / W none V 0.20–0.50; W 1.50–2.60 none none
Table 4 TS/YS 75 / 30 ksi 90 / 38 ksi 75 / 30 ksi 80 / 30 ksi

Reading tip: a heat that clears TP347’s Nb ≥10 × C formula still fails TP347W if tungsten, vanadium, or the fixed Nb band is missing. Do not accept a verbal “treat like 347H” note as chemistry equivalence under SA-213.

Mechanical Properties of SA213 TP347W

Table 4 of the public SA-213 / A213 grade text family sets TP347W tensile strength at 90 ksi [620 MPa] minimum and yield (0.2% offset) at 38 ksi [260 MPa] minimum — fifteen ksi above the classic 75/30 ksi floors on TP347 and TP347H. Elongation in 2 in. or 50 mm is 30% minimum (not 35%), and hardness is capped at 219 HBW / 230 HV or 95 HRB. The higher tensile floor tracks the W/V/N strengthening package; it is not a substitute for naming the correct UNS on the purchase order.

Property TP347W requirement
Tensile strength, min (Table 4) 90 ksi [620 MPa]
Yield strength (0.2% offset), min (Table 4) 38 ksi [260 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 30%
Hardness, max (Table 4) 219 HBW / 230 HV or 95 HRB
Grain size (Table 3) ASTM No. 7 – 10

Grain size ASTM No. 7–10 is a bounded window on the heat-treatment / grain-size table for this grade — not an open “No. 7 or coarser” H-grade note. Certificate reviewers should read tensile, hardness, and grain size together with the W/V/N/Nb chemistry rather than accepting a 75 ksi TP347 MTC as cover for a TP347W line item. Flattening and flaring follow the general requirements for the ordered size; hydrostatic or nondestructive examination follows the path selected on the PO.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP347W is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and superheater datasheets that pick tungsten-bearing TP347W usually assume minimum wall for remaining-life calculations — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The W/V package does not change the dimensional tolerance tables; it changes which heat clears the grade stamp and which tensile floor applies.

Item Typical SA213 TP347W dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for boiler / superheater datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. Heavier-wall superheater sizes are a common enquiry lean for this grade — they still sit inside the same SA-213 usual band unless the PO agrees otherwise.

Equivalent Grades

Equivalence talk for TP347W should start from the Code Book product standard and the UNS, not from a shop nickname. ASME SA-213 Grade TP347W / UNS S34705 is the governing designation on this page. ASTM A213 TP347W is the separate ASTM twin used when dual marking or a non-Code purchase is agreed — it is not a substitute lead standard for an SA-213 order. Related niobium grades without mandatory W/V bands (TP347, TP347H, TP347HFG, TP347LN) are sister options under the same hub, not automatic dual stamps.

Designation Notes
ASME SA-213 / SA-213M Grade TP347W Governing Code Book seamless boiler / HX tube product standard for this article
UNS S34705 Unified number listed in the stainless chemistry table
ASTM A213 TP347W Separate ASTM product specification — dual-mark only when the PO asks; twin page A213 TP347W
Related Nb grades TP347 / S34700, TP347H / S34709, TP347HFG / S34710, TP347LN / S34751 — no W/V mandatory bands
Related plate A240 / SA240 flat product in related UNS families — order plate and tube under their own product standards

Hub entry point: SA213/SA213M. When a bill of materials only says “347 stainless tube,” ask whether W/V/N chemistry and the 90/38 ksi floor are actually required before shipping TP347W or a plain TP347 alternative.

Heat Treatment and Delivery Condition

TP347W under ASME SA-213 is furnished solution treated at a minimum of 2000 °F [1100 °C], then quenched in water or cooled rapidly by other means. That solution minimum is 100 °F [about 55 °C] higher than the 1900 °F path on TP347 and TP347LN. The public heat-treatment table prints ASTM grain size 7–10 for this grade — a bounded window, not an open “7 or coarser” H-grade note. Footnotes F and H are not printed beside the TP347W solution-temperature cell in the public A213–13 excerpt the way they sit beside TP347 / TP348.

Supplementary Requirement S2 in the public A213–13 excerpt lists TP347, TP347H, TP348, and TP348H among grades that shall receive a stabilization heat treatment when specified — TP347W is not on that printed list. Supplementary Requirement S1 likewise omits TP347W. Do not assume S1 or S2 from a verbal “treat like 347H” note; write negotiated stabilization language on the purchase order if the project needs it for this UNS. Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size window.

Delivery condition for SHH STEEL TP347W is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment. UNCERTAIN: full negotiated S1/S2 wording if a buyer insists on stabilization language beyond the public list — confirm against the ordered edition and write it explicitly on the PO.

Corrosion Resistance

TP347W under ASME SA-213 is selected primarily for high-temperature boiler and superheater strength with a tungsten-vanadium-nitrogen package, not as a general wet-chloride upgrade over TP304. The fixed Nb band supports intergranular resistance in the sensitization window relative to unstabilized 18-8, but the grade is not a duplex or superaustenitic for aggressive aqueous chlorides. Oxidation and scaling resistance track the chromium window and the elevated solution anneal; they do not replace a project-specific corrosion review.

Where a datasheet mixes “347W” with wet process condensates or chloride deposits, ask whether the service is actually looking for a molybdenum-bearing or duplex tube instead of a W-bearing austenitic. SHH STEEL will not treat a W PMI peak alone as proof of aqueous corrosion suitability — chemistry, heat treatment, and the intended medium have to be read together.

Applications of SA213 TP347W Tube

Typical ASME SA213 TP347W placements are Code-stamped boiler and superheater tubes where the tungsten-bearing chemistry and the 90/38 ksi tensile floor are written into the material list — not generic “304 family” HX replacements. Refinery and power-plant enquiries that already name S34705, or that ask for W and V on the MTC together with a grain-size window, are the natural fit.

Heat-exchanger duty is possible when the PO accepts the higher tensile / lower elongation set and the 2000 °F anneal path, but many HX sheets that only say “347” are actually looking for SA213 TP347 or SA213 TP347H. Confirm before substituting. SHH STEEL quotes TP347W when the enquiry names the UNS or the W/V/N package explicitly.

Weldability

TP347W welds as a niobium-bearing austenitic, but filler and procedure selection should respect the tungsten and vanadium contents rather than copying a plain ER347 procedure without review. Matching or near-matching Nb-stabilized fillers are the usual starting point; confirm W and V pickup against the WPS when the project treats chemistry as contractual on the weld metal as well as the tube.

Autogenous welds and thin-wall boiler tube joints need heat-input control to protect the grain-size window and the as-annealed condition near the HAZ. Post-weld heat treatment is not a default SA-213 requirement for this grade — if the vessel code or the buyer wants stabilization after welding, write that as a separate negotiated step. SHH STEEL can coordinate weld coupons when the PO asks.

Surface Finishes

Standard mill delivery for ASME SA213 TP347W is solution annealed and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the W/V/N/Nb chemistry check or the grain-size window. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP347W includes heat analysis (C ≤0.05%, Cr 17.0–20.0%, Ni 8.00–11.0%, N 0.10–0.25%, Nb 0.25–0.50%, V 0.20–0.50%, W 1.50–2.60%), tension tests to the 90/38 ksi floors with 30% elongation, hardness to 219 HBW / 95 HRB, grain size ASTM No. 7–10, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm tungsten, vanadium, nitrogen, and the fixed Nb band rather than trusting a “347 family” PMI without W. Product analysis, when ordered, applies A480 tolerances with W/V digits labeled UNCERTAIN above. S1 / S2 are not on the public list for this grade — order negotiated language if needed. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP347W tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP347W, UNS S34705, heat number, size, and wall basis so receivers can match the 3.1 certificate — including W, V, N, and Nb — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP347W only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP347W as a Code Book tungsten-bearing product with enforceable C ≤0.05%, N 0.10–0.25%, Nb 0.25–0.50%, V 0.20–0.50%, W 1.50–2.60%, 90/38 ksi tensile, 30% elongation, hardness, grain size 7–10, and marking rules — not as “347 with a tungsten trace” checked only by a W PMI peak. Enquiry review verifies the full W/V/N/Nb package before release.

That stops silent substitution with TP347 or TP347H heats on datasheets that actually require S34705. We keep SA-213 and A213 independent, dual-mark only on request, and put W, V, N, and Nb on the 3.1 certificate so inspectors can verify the grade.

Cross-links: SA213 TP347, SA213 TP347H, SA213 TP347HFG, SA213 TP347LN, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP347W stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for tungsten-bearing boiler and superheater tube.

Item SHH STEEL capability for TP347W
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP347W / UNS S34705
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with W/V/N/Nb and grain size; negotiated stabilization / A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347W against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for tungsten-bearing boiler and superheater tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 14–10 / ~0.083–0.134 in. Small superheater / instrument sizes
1-1/4 – 2 BWG 12–8 / ~0.109–0.165 in. Common boiler / superheater band
2-1/2 – 3 0.150 – 0.280 in. min wall Heavier-wall leaning enquiry
3-1/2 – 5 0.200 – 0.320 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, length mix, finish route, and any dual-mark or grain-size witness needs with the RFQ so we can align mill capacity to the W/V/N/Nb package on the first reply.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP347W?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.05%, N 0.10–0.25%, Nb 0.25–0.50%, V 0.20–0.50%, and W 1.50–2.60% — tensile 90/38 ksi, elongation 30%, hardness, and grain size 7–10 align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does SA213 TP347W cover welded or HCW tube?
No. ASME SA-213 for this stainless series is a seamless boiler, superheater, and heat-exchanger tube product standard. SHH STEEL supplies TP347W as seamless cold-finished or hot-finished tube only. Welded (WLD) or heavily cold-worked welded (HCW) manufacturing types are outside this page’s product form and are not offered as a Manufacturing Types split under the SA213 TP347W listing.
What chemistry defines ASME SA213 TP347W versus TP347?
TP347W / UNS S34705 requires C ≤0.05%, Ni 8.00–11.0%, N 0.10–0.25%, Nb in a fixed 0.25–0.50% band, V 0.20–0.50%, and W 1.50–2.60%, with P ≤0.040%. Plain TP347 / S34700 uses C ≤0.08%, Ni 9–13%, and Nb ≥10 × C ≤1.10% with no mandatory W, V, or N bands. A heat that clears the TP347 niobium formula still fails TP347W if tungsten or vanadium is missing.
Why is the tensile floor 90/38 ksi on TP347W?
Table 4 of the public SA-213 / A213 grade text family sets TP347W at 90 ksi [620 MPa] tensile and 38 ksi [260 MPa] yield with 30% elongation and hardness max 219 HBW / 95 HRB. That higher floor tracks the tungsten-vanadium-nitrogen strengthening package. Do not accept a 75/30 ksi TP347 certificate as cover for a TP347W line item, and do not assume the higher tensile replaces naming UNS S34705 on the purchase order.
How does SA213 TP347W differ from SA213 TP347H?
TP347H is an H-grade with C 0.04–0.10%, Nb ≥8 × C ≤1.10%, no mandatory W/V/N bands, a finish-route solution anneal, and grain size No. 7 or coarser, with Table 4 still at 75/30 ksi. TP347W uses a fixed Nb band plus W and V, a 2000 °F solution minimum, grain size 7–10, and the 90/38 ksi tensile set. They are sister grades under SA213/SA213M, not interchangeable dual stamps.
Is TP347W the same as TP347HFG under SA-213?
No. TP347HFG / S34710 is a fine-grain H-leaning niobium grade without mandatory tungsten or vanadium, and its Table 4 tensile floor is 80/30 ksi — not the 90/38 ksi / W/V package on TP347W. If the material list names S34705 or requires W and V on the MTC, order TP347W; if it names fine-grain 347H chemistry, review SA213 TP347HFG instead.
What heat treatment and grain size apply to SA213 TP347W?
Solution treatment at a minimum of 2000 °F [1100 °C] followed by rapid cooling is the public path, with ASTM grain size No. 7–10 as a bounded window. Footnotes F and H are not printed beside this grade’s solution cell the way they sit beside TP347 / TP348 in the public excerpt. Cold-finished versus hot-finished is a process route, not a substitute for the anneal or the grain-size report on the certificate.
Are Supplementary Requirements S1 and S2 listed for TP347W?
In the public A213–13 excerpt used as the shared grade-text reference, S1 and S2 list TP347, TP347H, TP348, and TP348H among others — TP347W is not on those printed lists. Do not assume stabilization or stress-relief wording from a verbal “treat like 347” note. If the project needs stabilization after solution anneal, write negotiated language on the purchase order and confirm it against the ordered SA-213 edition.
What hardness limit applies to ASME SA213 TP347W tube?
Table 4 caps TP347W hardness at 219 HBW / 230 HV or 95 HRB — higher than the 192 HBW / 90 HRB ceiling on plain TP347. Hardness is checked together with the 90/38 ksi tensile set and the grain-size window. A soft TP347 hardness result on a certificate does not prove TP347W compliance, and a hard result alone does not replace the W/V/N chemistry check.
Should I order minimum wall or average wall for TP347W?
Boiler and superheater datasheets that pick TP347W usually assume minimum wall for remaining-life and design calculations. Average wall is acceptable when the purchase order says so and the general requirements for the ordered finish are applied. State wall basis, OD × wall or BWG, and length mix on the RFQ so the mill does not default to a basis your inspector will reject.
Can SHH STEEL dual-certify SA-213 and A213 for TP347W?
Yes, when the purchase order asks for dual marking and the heat meets both product standards’ grade text for TP347W / UNS S34705. Dual marking is a documentation and stencil option — it does not merge the two standards into one title. For non-Code purchases that only want the ASTM twin, see A213 TP347W; for Code-led work, keep SA-213 as the lead standard on the PO.
Is TP347W suitable for wet chloride heat-exchanger service?
Not as a default upgrade. TP347W is framed for high-temperature boiler and superheater strength with a W/V/N package. Aggressive aqueous chlorides usually need molybdenum-bearing, duplex, or other project-specified alloys instead of a tungsten-bearing 18-8. Ask for a corrosion review before substituting TP347W into a wet-chloride HX datasheet that never named S34705.

Conclusion

ASME SA213 TP347W / UNS S34705 is the tungsten-bearing niobium-stabilized seamless stainless steel tube grade for Code boiler and superheater service when C ≤0.05%, Cr 17.0–20.0%, Ni 8.00–11.0%, N 0.10–0.25%, Nb 0.25–0.50%, V 0.20–0.50%, W 1.50–2.60%, a 90/38 ksi tensile floor with 30% elongation, hardness max 219 HBW / 95 HRB, a 2000 °F solution anneal, and grain size ASTM No. 7–10 are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report W, V, N, and Nb. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X