ASME SA213 TP310H Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP310H Stainless Steel Tube

ASME SA213 TP310H / UNS S31009 seamless boiler, superheater and heat-exchanger tube — the H-grade 24–26% Cr / 19–22% Ni austenitic with controlled carbon 0.04–0.10%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, a 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. Chosen for creep-range oxidation duty above the 309H family. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
Grade
TP310H / UNS S31009
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP310H Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP310H under that Code Book text is the high-temperature carbon-controlled member of the 310 family, listed as UNS S31009, with melting carbon held in a 0.04–0.10% band, chromium 24.0–26.0%, nickel 19.0–22.0%, and a mandatory ASTM grain-size requirement of No. 7 or coarser after solution treatment. When a Code-stamped boiler, superheater, or furnace heat-exchanger datasheet calls for SA-213 TP310H, the purchase order and mill test certificate should carry the ASME H-grade designation, the carbon floor and ceiling, and the grain-size result — not a tensile-only “310S” nickname stamped as if it were the H grade.

SHH STEEL can supply ASME SA213 TP310H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry, the tensile plus hardness acceptance set, and the ASTM E112 grain-size result for the heat-treatment lot. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 310H, S31009 boiler tube, H-grade 25Cr-20Ni tube, or SA213 310H tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP310S, SA213 TP310Cb, SA213 TP310HCb, SA213 TP309H, and SA213 TP304H. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP310H.

Chemical Composition of SA213 TP310H

Two chemistry layers matter for TP310H under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. The carbon range is the first line a Code reviewer should check: TP310H is not “310S with a little more carbon” written as a max — it is a 0.04–0.10% band with both floor and ceiling, paired with the same 24–26 / 19–22 Cr–Ni windows as TP310S. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP310H / UNS S31009 and the product-analysis limits that result from applying A480 Table A1.1 tolerances, plus a carbon snapshot versus TP310S and TP310Cb. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; grain-size clause or heat-treatment table number across editions; A480 Cr/Ni tolerance digits for the 24–26% Cr / 19–22% Ni band — applied from sister 310 / high-Cr practice; confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP310H / UNS S31009. Confirm the ordered ASME edition on the purchase order.

Element TP310H (UNS S31009) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20

Carbon snapshot — TP310S / TP310H / TP310Cb

Element TP310S (S31008) TP310H (S31009) TP310Cb (S31040)
C ≤ 0.08 0.04 – 0.10 ≤ 0.08
Cr 24.0 – 26.0 24.0 – 26.0 24.0 – 26.0
Ni 19.0 – 22.0 19.0 – 22.0 19.0 – 22.0
Nb (Cb) … … 10×C – 1.10
Grain size no mandate No. 7 or coarser no mandate

The 24–26% chromium and 19–22% nickel balance is why TP310H sits above the 309H family for high-temperature oxidation resistance on an H-grade carbon path: more chromium builds a more durable oxide scale, and the higher nickel keeps the structure fully austenitic after the 1900 °F solution treatment. Carbon 0.04–0.10% is intentional for elevated-temperature strength and coarse-grain acceptance — not an L-grade mindset. Heats that also meet the TP310S carbon ceiling can be dual-certified TP310S/TP310H when tensile, hardness, and grain-size results clear both rows — ask for that dual marking on the PO rather than assuming it from a PMI reading. Dual TP310H/TP310Cb is not automatic: niobium is a no-requirement ellipsis on TP310H. When Nb stabilization plus H-grade carbon is required, open SA213 TP310HCb; when a step down in Cr–Ni is enough on an H path, open SA213 TP309H.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 23.75–26.25%, and Ni 18.85–22.20%. Note the asymmetric A480 Ni product tolerance on this band (0.15 under / 0.20 over). Put any tighter project carbon floor on the purchase order before the heat is selected — the H-grade carbon floor is intentional for elevated-temperature service.

Mechanical Properties of SA213 TP310H

ASME SA-213 sets the room-temperature tensile acceptance floor for TP310H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP310S. Hardness is capped at 192 HBW / 200 HV or 90 HRB. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP310H / UNS S31009 (commonly Table 4) and H-grade grain-size language. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP310H requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Flattening and flaring tests sit beside tension and hardness on a lot basis. Room-temperature tensile equality with TP310S is why dual 310S/310H stock is attractive; elevated-temperature allowables, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size is incomplete for TP310H — ask for the E112 result on the EN 10204 3.1 certificate before releasing the heat to fabrication. When the datasheet also needs niobium stabilization on the same H-grade carbon path, open SA213 TP310HCb; when a step down in Cr–Ni is enough, open SA213 TP309H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP310H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. Boiler and superheater datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order, because remaining wall after high-temperature oxidation and creep is often a design input on the circuits where 310H is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP310H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / furnace / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, design metal temperature context, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept for 310H the same way it is for other H-grade tube: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP310H tube often collapses plate, cast, and tube product forms into one nickname. ASME SA-213 Grade TP310H / UNS S31009 is the governing designation for this article; EN and JIS wrought names that point to similar high-Cr–Ni chemistry families are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 310H,” confirm which product standard, tensile/hardness table, grain-size clause, and heat-treatment row the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP310H Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31009 Unified number listed with the grade chemistry
ASTM A213 TP310H Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP310H
Related S-grade SA213 TP310S — same Cr–Ni, C ≤0.08, no grain-size mandate
Related H+Cb SA213 TP310HCb — H-grade carbon plus niobium stabilization
Related 309H SA213 TP309H — lower Cr–Ni oxidation step with the same H-grade carbon/grain-size pattern
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own product standards

ASTM A213 TP310H is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP310S, TP310Cb, and TP310HCb on their own ASME SA213 pages before swapping 310-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP310H under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That heat-treatment row also carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot — the clause that separates H-grade acceptance from ordinary TP310S solution treatment at the same temperature. Grain size is determined per ASTM E112 on the heat-treatment lot and reported on the mill test certificate.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP310H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Nb stabilization is also required on an H-grade carbon heat, do not assume TP310H covers it — specify SA213 TP310HCb, which adds the 10×C–1.10 niobium band and carries Footnote H / S2 stabilizing language when the purchaser invokes those options. When only the standard C ≤0.08% path without grain-size controls is needed, stay on SA213 TP310S.

Corrosion Resistance

TP310H is selected primarily for high-temperature oxidation and creep-oriented boiler or furnace service from its 24–26% chromium / 19–22% nickel balance and intentional H-grade carbon path, not for molybdenum-driven chloride pitting resistance. In oxidizing furnace atmospheres, hot-process gas circuits, and elevated-temperature steam services where 18-8 and even 309H scale too quickly, the higher Cr–Ni oxide scale is the commercial reason to pay for 310H. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 310H as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP310H; selection remains engineering judgment against temperature, atmosphere, velocity, and inspection philosophy. The 0.04–0.10% carbon band intentionally raises carbon relative to an L-grade mindset; sensitization risk in the weld heat-affected zone is managed by procedure, not by pretending TP310H is a low-carbon grade. When intergranular corrosion after thermal cycling is a datasheet driver alongside H-grade carbon, evaluate niobium-stabilized SA213 TP310HCb. Sulfidation and carburizing atmospheres still need process-specific review beyond catalogue oxidation claims. SHH STEEL will not rank TP310H as equal to 316 in chlorides — higher chromium and nickel are not a molybdenum substitute.

Applications of SA213 TP310H Tube

Because TP310H brings a controlled 0.04–0.10% carbon band, ASTM No. 7 or coarser grain size, and a 24–26% Cr / 19–22% Ni oxidation balance under SA-213, it shows up in creep-range boiler and superheater circuits, furnace-related heat exchangers, and elevated-temperature HX duty where ordinary 310S lacks the H-grade carbon and grain-size package. The table below pairs typical application areas with a selection note so the grade is chosen for metal temperature, atmosphere, and Code grain-size language — not only for the familiar “310H” name on the BOM.

Application area Typical use of TP310H tube Selection note
Creep-range boiler / superheater Seamless generating or superheater tubing ordered to SA-213 with grain-size reporting Confirm design metal temperature and carbon/grain callout
Severe high-temperature oxidation Seamless tube where 25Cr-20Ni scale resistance outperforms 18-8 and 309H Prefer TP309H if a step down in Cr–Ni is enough
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits Open TP310HCb if Nb stabilization is also required
Chemical process (oxidizing, low chloride) Tube-side circuits with hot oxidizing media Prefer TP316/TP316L if chlorides dominate
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General Code tube duty Seamless tube where SA-213 H-grade documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For standard C ≤0.08% without grain-size controls open SA213 TP310S; for Nb stabilization open SA213 TP310Cb or SA213 TP310HCb; for a step down in Cr–Ni open SA213 TP309H; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP310H tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER310 / ER310H-type deposits (or equivalent covered electrodes) under a qualified WPS; some fabricators still prefer controlled-carbon deposits when the base tube carbon sits near the top of the 0.04–0.10% band. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP310H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), grain-size documentation on the base metal, tube-to-tubesheet joint quality, and any contractual corrosion test. For tube that will enter service as-welded in a sensitizing environment, discuss whether a post-weld solution treatment or a move to TP310HCb better protects the joint. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP310H is solution annealed and pickled, leaving a clean matte finish suitable for most boiler, furnace, and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route while still needing to clear the H-grade grain-size requirement. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and grain-size identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP310H includes heat analysis, tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, grain-size determination to ASTM No. 7 or coarser per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP310H tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note. Grain size is part of the base H-grade heat-treatment acceptance — confirm the E112 result appears on the certificate before releasing the heat.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness, tension, and grain-size specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP310H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes — including the grain-size reporting expectation that distinguishes H-grade release packages.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP310H as a Code Book product standard with enforceable chemistry, tensile, hardness, heat-treatment, grain-size, and marking rules — not as a catalogue nickname for “any 310H tube.” The MTC reports the full ladle chemistry, the tensile/hardness acceptance set, and the E112 grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 310-family conversation honest for creep-range boiler and furnace duty. If the specification only needs C ≤0.08% without grain-size controls, we open SA213 TP310S. If niobium stabilization on the same 25Cr-20Ni balance is specified without the H package, we open SA213 TP310Cb. If both H-grade carbon/grain-size and Nb are required, we open SA213 TP310HCb. If a step down in chromium–nickel is enough on an H path, we open SA213 TP309H. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 310H into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME H-grade callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP310H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this H grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for creep-range boiler, superheater, and furnace tube duty.

Item SHH STEEL capability for TP310H
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP310H / UNS S31009
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / furnace / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size ASTM No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry and grain-size result; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310H tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for creep-range high-temperature oxidation-resistant boiler and furnace tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP310H
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/furnace/HX ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative creep-range boiler/furnace sizes, confirm min vs average wall
Length Cut lengths for boiler, superheater, and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, grain-size reporting confirmation, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), grain-size reporting expectation, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP310S, SA213 TP310HCb, and SA213 TP309H sit on the same hub when the datasheet steps beyond TP310H.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP310H?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP310H include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP310H under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP310H?
TP310H is UNS S31009. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 24.0–26.0%, and nickel 19.0–22.0%, with molybdenum, nitrogen, and niobium as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the general-requirements path. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP310H vs TP310S — which SA213 grade should I order?
Order TP310H when the boiler or superheater datasheet needs carbon 0.04–0.10% and ASTM No. 7 or coarser grain size on the same 24–26% Cr / 19–22% Ni balance. Order TP310S when the specification calls for the standard C ≤0.08% path without H-grade carbon and grain-size controls. Both share a 75/30 ksi tensile floor, so tensile equality alone is not a reason to swap; confirm the carbon band and grain-size callout before substituting either grade for the other.
TP310H vs TP309H — when do I need the higher Cr–Ni H grade under SA213?
Order TP310H when the datasheet needs the higher 24–26% Cr / 19–22% Ni oxidation balance on an H-grade carbon and grain-size path. Order TP309H when 22–24% Cr / 12–15% Ni is enough for the design metal temperature and atmosphere. Both carry C 0.04–0.10% and ASTM No. 7 or coarser grain size, so the Cr–Ni step — not the H package alone — is the deciding comparison.
Why does SA-213 require grain size for TP310H?
The H-grade heat-treatment row requires ASTM No. 7 or coarser grain size per heat-treatment lot because coarse grain is part of the elevated-temperature / creep-oriented acceptance package that distinguishes TP310H from ordinary TP310S. A tensile-only certificate that omits the E112 result is incomplete for TP310H release. Ask for the grain-size number on the EN 10204 3.1 mill test certificate before releasing the heat to fabrication.
Does SA-213 set a hardness limit for TP310H?
Yes. Public mechanical-table summaries for TP310H set a hardness maximum of 192 HBW / 200 HV or 90 HRB alongside the 75 ksi tensile and 30 ksi yield floors. Hardness testing sits on a lot basis with tension, flattening, and flaring. If a project quotes a tighter hardness window, put it on the purchase order as a contractual extra — the product-standard ceiling remains the acceptance floor unless the mill accepts a tighter guarantee in writing.
What heat treatment does ASME SA-213 require for TP310H?
TP310H is solution treated at a minimum of 1900 °F [1040 °C] and quenched in water or cooled rapidly by other means. The same heat-treatment row carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot. Cold-finished versus hot-finished is a dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition is typically solution annealed and pickled, with anneal temperature, quench method, and E112 result on the MTC.
Minimum wall vs average wall — which should I order for SA213 TP310H?
Boiler and superheater datasheets almost always assume minimum wall because remaining wall after high-temperature oxidation and creep is a design input. Average wall is acceptable when the purchase order says so and the general-requirements tolerances for that finish route are understood. State the wall basis explicitly on the enquiry so mill and stock lengths are rolled and accepted to the correct table — do not leave wall basis implied by a BWG number alone.
Is TP310H a good choice for chloride-rich cooling water under SA213?
Usually no. TP310H is built for high-temperature oxidation and creep-oriented service from its 24–26% Cr / 19–22% Ni balance and H-grade carbon path; molybdenum is a no-requirement ellipsis. For chloride-rich cooling water and wet brine-leaning exchangers, open molybdenum grades such as SA213 TP316 / TP316L or higher rather than treating 310H as a chloride upgrade. Higher chromium and nickel are not a molybdenum substitute.
Can you dual-certify ASME SA213 TP310S and TP310H?
Sometimes. Heats that meet the TP310S carbon ceiling and also clear the TP310H carbon band, tensile, hardness, and grain-size requirements can be dual-certified TP310S/TP310H when the purchase order asks for both grade marks. Dual marking is not automatic from a PMI reading — ask for it on the PO so the MTC and stencil carry both designations under ASME SA-213.
Can you dual-certify ASME SA-213 and ASTM A213 TP310H?
Yes, when the purchase order asks for both independent standards on the stencil and mill test certificate. ASME SA-213 and ASTM A213 remain separate documents even when chemistry and tensile floors align for a referenced edition. Dual-mark only when both names are required; do not assume an A213-only certificate substitutes for an SA-213 Code callout, or the reverse.

Conclusion

ASME SA213 TP310H / UNS S31009 is the H-grade 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for Code boiler, superheater, and furnace heat-exchanger service when creep-range carbon control, ASTM No. 7 or coarser grain size, and high-temperature oxidation resistance above the 309H family matter together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F, tested to the 75/30 ksi tensile and hardness acceptance floors with grain-size reporting, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, grain-size reporting expectation, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X