ASME SA213 TP348H Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP348H Stainless Steel Tube

ASME SA213 TP348H / UNS S34809 H-grade cobalt- and tantalum-controlled niobium-stabilized seamless boiler, superheater and heat-exchanger tube — C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8×C ≤1.10% (chemistry Footnote H), Co ≤0.20%, Ta ≤0.10%, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, finish-route solution anneal (CF 2000 °F / HR 1925 °F) with Footnote H, grain size ASTM No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb+Ta, Co, Ta, and grain size.
Grade
TP348H / UNS S34809
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP348H Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers or superheaters invoke that adoption by name, SA-213 is the governing product standard for this H-grade cobalt- and tantalum-controlled niobium-stabilized tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP348H / UNS S34809 is the H-grade Co/Ta-controlled austenitic row inside that stainless family. Melting carbon sits in a 0.04–0.10% band, chromium at 17.0–19.0%, nickel at 9.0–13.0%, and niobium plus tantalum must satisfy ≥8 × C with a 1.10% ceiling under chemistry Footnote H, while cobalt is held to ≤0.20% and tantalum alone to ≤0.10%. Table 4 keeps tensile at 75 ksi [515 MPa] / 30 ksi [205 MPa] with elongation 35% minimum and hardness max 192 HBW / 90 HRB, but the carbon band, the lower Nb+Ta multiplier, the finish-route solution anneal, and mandatory grain size No. 7 or coarser are what make the H-grade stamp. Buyers who write “348H superheater tube” still need to name SA-213 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the H-grade Co/Ta package together. This is not a dual stamp of TP348, TP347H, or TP347.

SHH STEEL can supply ASME SA213 TP348H as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report Nb+Ta, cobalt, tantalum, and grain size together with the 75/30 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP348H.

Shop names include “348H,” “S34809,” and “H-grade low-cobalt Nb-stabilized tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP348H / UNS S34809, wall basis, OD × wall or BWG, finish route (cold-worked vs hot-rolled anneal path), and any Supplementary Requirement S2 when needed — S1 is not listed for TP348H in the public excerpt. Sister SA213 pages include SA213 TP348, SA213 TP347H, SA213 TP347, and SA213 TP321H. Seamless only — no Manufacturing Types (SML / WLD / HCW) product-form split on this page.

Chemical Composition of SA213 TP348H

Two chemistry layers matter for TP348H under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The defining package for a reviewer is C 0.04–0.10%, Nb+Ta ≥8 × C ≤1.10% (chemistry Footnote H), cobalt ≤0.20%, and tantalum ≤0.10%. That Nb+Ta multiplier is deliberately lower than the 10 × C rule on non-H TP348, so do not copy a TP348 niobium check onto a TP348H heat without recalculating against the actual carbon. Chromium 17.0–19.0% and nickel 9.0–13.0% match the non-H twin’s windows.

The tables below reproduce the melt limits for TP348H / UNS S34809, the product-analysis limits from A480 Table A1.1 practice (with Co and Ta tolerance digits labeled UNCERTAIN pending the ordered A480 edition), and a short C/stabilizer/Co snapshot against TP348, TP347H, and TP347. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP348H (UNS S34809) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium + Tantalum (Nb + Ta) ≥ 8 × C, ≤ 1.10 (chemistry Footnote H)
Cobalt (Co) ≤ 0.20
Tantalum (Ta) ≤ 0.10
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for Grade TP348H / UNS S34809 (same grade text family). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text; full chemistry Footnote H wording on the ordered text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Nb + Ta ≥ 8 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C
Cobalt (Co) ≤ 0.20 0.03 over (UNCERTAIN — confirm A480) ≤ 0.23
Tantalum (Ta) ≤ 0.10 0.02 over (UNCERTAIN — confirm A480) ≤ 0.12

Product analysis is not automatic — order it when the project needs finished-tube chemistry, especially the carbon band and Co/Ta ceilings. UNCERTAIN: A480 product-tolerance digits for Co and Ta are applied from sister-pack practice pending the ordered A480 edition.

C / stabilizer / Co snapshot — TP348 / TP348H / TP347H / TP347

Element TP348 (S34800) TP348H (S34809) TP347H (S34709) TP347 (S34700)
C ≤ 0.08 0.04 – 0.10 0.04 – 0.10 ≤ 0.08
Cr 17.0 – 19.0 17.0 – 19.0 17.0 – 19.0 17.0 – 20.0
Stabilizer Nb+Ta ≥ 10 × C, ≤ 1.10 Nb+Ta ≥ 8 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10 Nb ≥ 10 × C, ≤ 1.10
Co / Ta Co ≤ 0.20; Ta ≤ 0.10 Co ≤ 0.20; Ta ≤ 0.10 not listed not listed
Grain size no mandatory number No. 7 or coarser No. 7 or coarser no mandatory number

Reading tip: a heat that clears non-H TP348 still fails TP348H if carbon sits below 0.04%, if the stabilizer was calculated on a 10 × C rule without checking the 8 × C H-grade minimum, or if grain size No. 7 or coarser is not reported. Do not accept a verbal “348 with H marking” note as proof of the carbon band and grain-size window.

Mechanical Properties of SA213 TP348H

Table 4 of the public SA-213 / A213 grade text family sets TP348H tensile strength at 75 ksi [515 MPa] minimum and yield (0.2% offset) at 30 ksi [205 MPa] minimum — the same floors as non-H TP348 and TP347H. Elongation in 2 in. or 50 mm is 35% minimum, and hardness is capped at 192 HBW / 200 HV or 90 HRB. The H-grade distinction is carried by carbon band, stabilizer multiplier, finish-route heat treatment, and mandatory grain size — not by a higher tensile floor.

Property TP348H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size (Table 3) ASTM No. 7 or coarser

Grain size ASTM No. 7 or coarser is mandatory for TP348H and should appear on the EN 10204 3.1 certificate with the tensile and hardness results. Certificate reviewers should reject a TP348H claim that only shows 75/30 ksi without grain size, or that shows a fine-grain number finer than No. 7 without project-specific agreement. Flattening and flaring follow the general requirements for the ordered size; hydrostatic or nondestructive examination follows the path selected on the PO.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP348H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and superheater datasheets that pick H-grade TP348H usually assume minimum wall for remaining-life calculations — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The H-grade Co/Ta package does not change the dimensional tolerance tables; it changes which heat clears the grade stamp and which anneal path applies.

Item Typical SA213 TP348H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for boiler / superheater datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. Name the finish route on the RFQ because cold-worked and hot-rolled paths carry different solution-temperature minima under SA-213.

Equivalent Grades

Equivalence talk for TP348H should start from the Code Book product standard and the UNS, not from a shop nickname. ASME SA-213 Grade TP348H / UNS S34809 is the governing designation on this page. ASTM A213 TP348H is the separate ASTM twin used when dual marking or a non-Code purchase is agreed — it is not a substitute lead standard for an SA-213 order. Related grades include non-H Co/Ta TP348 and H-grade Nb-without-Co/Ta TP347H — sister options under the same hub, not automatic dual stamps.

Designation Notes
ASME SA-213 / SA-213M Grade TP348H Governing Code Book seamless boiler / HX tube product standard for this article
UNS S34809 Unified number listed in the stainless chemistry table
ASTM A213 TP348H Separate ASTM product specification — dual-mark only when the PO asks; twin page A213 TP348H
Related grades TP348 / S34800 (non-H Co/Ta); TP347H / S34709 (H-grade Nb without Co/Ta)
Related plate A240 / SA240 flat product in related UNS families — order plate and tube under their own product standards

Hub entry point: SA213/SA213M. When a bill of materials only says “348H,” ask whether cobalt/tantalum ceilings and grain size No. 7 or coarser are actually required before shipping TP348H or a TP347H / TP348 alternative.

Heat Treatment and Delivery Condition

TP348H under ASME SA-213 is furnished solution treated on a finish-route schedule: cold-worked tube at a minimum of 2000 °F [1100 °C], hot-rolled tube at a minimum of 1925 °F [1050 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table marks the hot-rolled path with Footnote H — the same footnote family that warns a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. ASTM grain size No. 7 or coarser is mandatory for TP348H.

Supplementary Requirement S2 lists TP348H among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. For niobium/tantalum-bearing H grades, S2 may also be necessary and is permitted to meet Supplementary Requirement S4 (A262 Practice E). Supplementary Requirement S1 does not list TP348H in the public A213–13 excerpt (S1 names TP304L, TP316L, TP321, TP347, and TP348). Do not assume S1 from a verbal “treat like 348” note.

Delivery condition for SHH STEEL TP348H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, finish route, and grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment. UNCERTAIN: full negotiated Footnote H / S2 wording on the ordered edition, and any buyer-insisted S1 language beyond the public list — confirm against the Code Book text named on the PO.

Corrosion Resistance

TP348H under ASME SA-213 is selected for high-temperature H-grade service with cobalt and tantalum ceilings — creep-leaning boiler and superheater framing — not as a general wet-chloride upgrade over TP304. The Nb+Ta stabilizer and Footnote H heat-treatment path support intergranular resistance when the carbon band and grain-size window are respected. The grade is not a duplex or molybdenum-bearing superaustenitic for aggressive aqueous chlorides.

Where a datasheet mixes “348H” with wet process condensates or chloride deposits, ask whether the service is actually looking for a molybdenum-bearing tube and whether S2 stabilization is intended. SHH STEEL will not treat an H-grade stamp alone as proof of aqueous corrosion suitability — chemistry, grain size, heat treatment, and the intended medium have to be read together.

Applications of SA213 TP348H Tube

Typical ASME SA213 TP348H placements are Code-stamped boiler and superheater tubes where the material list names S34809 or explicitly requires an H-grade carbon band, Co/Ta ceilings, and grain size No. 7 or coarser — not generic “348” or “347H” replacements. Power and process plants that already distinguish TP348H from TP348 for creep service are the natural fit.

When the enquiry only says “348H” without Co/Ta or grain-size language, confirm whether the buyer actually needs SA213 TP348 or SA213 TP347H before substituting. SHH STEEL quotes TP348H when the enquiry names the UNS or the H-grade Co/Ta package explicitly.

Weldability

TP348H welds as an H-grade niobium-plus-tantalum stabilized austenitic. Matching or near-matching Nb-stabilized fillers (ER347 / ER347H / ER348 family practice) are the usual starting point; confirm cobalt and tantalum pickup against the WPS when the project treats Co/Ta as contractual on the weld metal as well as the tube.

Autogenous welds and thin-wall boiler tube joints need heat-input control to protect the grain-size window and intergranular resistance near the HAZ. Post-weld stabilization is not a default SA-213 requirement — if the vessel code or the buyer wants S2-style stabilization after welding, write that as a separate ordered step. SHH STEEL can coordinate weld coupons when the PO asks.

Surface Finishes

Standard mill delivery for ASME SA213 TP348H is solution annealed and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the H-grade chemistry check or the grain-size window. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP348H includes heat analysis (C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8 × C ≤1.10%, Co ≤0.20%, Ta ≤0.10%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, grain size ASTM No. 7 or coarser, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm the carbon band, the 8 × C Nb+Ta result, cobalt / tantalum ceilings, and grain size rather than trusting a “348 family” PMI without Co or an H stamp without grain size. Product analysis, when ordered, applies A480 tolerances with Co/Ta digits labeled UNCERTAIN above. S2 and A262 practices apply only when named on the PO; S1 is not on the public list for this grade. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP348H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP348H, UNS S34809, heat number, size, and wall basis so receivers can match the 3.1 certificate — including Nb+Ta, Co, Ta, and grain size — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP348H only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP348H as a Code Book H-grade cobalt- and tantalum-controlled product with enforceable C 0.04–0.10%, Cr 17–19%, Ni 9–13%, Nb+Ta ≥8 × C ≤1.10%, Co ≤0.20%, Ta ≤0.10%, 75/30 ksi tensile, 35% elongation, hardness, grain size No. 7 or coarser, and marking rules — not as “348 with an H suffix” checked only by a carbon PMI peak. Enquiry review verifies the carbon band, Co/Ta ceilings, and grain size before release.

That stops silent substitution with TP348 or TP347H heats on datasheets that actually require S34809. We keep SA-213 and A213 independent, dual-mark only on request, and put Nb+Ta, Co, Ta, and grain size on the 3.1 certificate so inspectors can verify the grade.

Cross-links: SA213 TP348, SA213 TP347H, SA213 TP347, SA213 TP321H, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP348H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for H-grade Co/Ta-controlled boiler and superheater tube.

Item SHH STEEL capability for TP348H
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP348H / UNS S34809
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Nb+Ta / Co / Ta and grain size; S2 / A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP348H against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for H-grade Co/Ta-controlled boiler and superheater tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 14–10 / ~0.083–0.134 in. Small superheater / instrument sizes
1-1/4 – 2 BWG 12–8 / ~0.109–0.165 in. Common boiler / superheater band
2-1/2 – 3 0.150 – 0.280 in. min wall Heavier-wall H-grade enquiry
3-1/2 – 5 0.200 – 0.320 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, length mix, finish route (CF vs HR anneal path), and any dual-mark or S2 needs with the RFQ so we can align mill capacity to the H-grade Co/Ta package on the first reply.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP348H?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8 × C ≤1.10%, Co ≤0.20%, and Ta ≤0.10% — tensile 75/30 ksi, elongation 35%, hardness, and grain size No. 7 or coarser align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does SA213 TP348H cover welded or HCW tube?
No. ASME SA-213 for this stainless series is a seamless boiler, superheater, and heat-exchanger tube product standard. SHH STEEL supplies TP348H as seamless cold-finished or hot-finished tube only. Welded (WLD) or heavily cold-worked welded (HCW) manufacturing types are outside this page’s product form and are not offered as a Manufacturing Types split under the SA213 TP348H listing.
How does SA213 TP348H differ from SA213 TP348?
TP348H requires C 0.04–0.10%, Nb+Ta ≥8 × C ≤1.10% under chemistry Footnote H, a finish-route solution anneal (cold-worked 2000 °F / hot-rolled 1925 °F), and mandatory grain size No. 7 or coarser. Non-H TP348 keeps C ≤0.08%, Nb+Ta ≥10 × C, a 1900 °F path with Footnotes F/H, and no mandatory grain-size number. Both share Co ≤0.20% and Ta ≤0.10%, but they are not interchangeable dual stamps under SA-213.
How does SA213 TP348H differ from SA213 TP347H?
Both are H-grades with C 0.04–0.10% and an 8 × C stabilizer rule, and both carry grain size No. 7 or coarser. TP348H reports stabilizer as Nb+Ta and adds cobalt ≤0.20% and tantalum ≤0.10% ceilings; TP347H reports Nb alone without mandatory Co/Ta limits. If the material list names S34809 or requires low cobalt, order TP348H — do not assume a TP347H heat clears the Co/Ta package.
What chemistry defines ASME SA213 TP348H?
Melting limits are C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8 × C ≤1.10% (chemistry Footnote H), Co ≤0.20%, and Ta ≤0.10%, with no Mo or N requirement on the public row. Recalculate the stabilizer minimum against the actual heat carbon — do not reuse a 10 × C TP348 check on an H-grade heat.
What heat treatment and grain size apply to SA213 TP348H?
Cold-worked tube is solution treated at a minimum of 2000 °F [1100 °C]; hot-rolled tube at a minimum of 1925 °F [1050 °C]; then rapidly cooled. Footnote H applies on the public heat-treatment path. ASTM grain size No. 7 or coarser is mandatory and should appear on the certificate. Name the finish route on the purchase order so the mill applies the correct solution-temperature minimum.
Is Supplementary Requirement S2 available for TP348H? What about S1?
S2 lists TP348H among grades that shall receive a stabilization heat treatment when specified, and for Nb/Ta-bearing H grades S2 may also support S4 (A262 Practice E). S1 does not list TP348H in the public A213–13 excerpt — S1 names TP304L, TP316L, TP321, TP347, and TP348. Do not assume S1 from a verbal “treat like 348” note; write negotiated language if the project insists.
What hardness limit applies to ASME SA213 TP348H tube?
Table 4 caps TP348H hardness at 192 HBW / 200 HV or 90 HRB — the same ceiling as TP348 and TP347H. Hardness is checked together with the 75/30 ksi tensile set, 35% elongation, and grain size No. 7 or coarser. A hardness result alone does not prove H-grade Co/Ta compliance or the carbon band.
Should I order minimum wall or average wall for TP348H?
Boiler and superheater datasheets that pick TP348H usually assume minimum wall for remaining-life and design calculations. Average wall is acceptable when the purchase order says so and the general requirements for the ordered finish are applied. State wall basis, OD × wall or BWG, finish route, and length mix on the RFQ so the mill does not default to a basis your inspector will reject.
Can SHH STEEL dual-certify SA-213 and A213 for TP348H?
Yes, when the purchase order asks for dual marking and the heat meets both product standards’ grade text for TP348H / UNS S34809 — including carbon band, Nb+Ta formula, Co/Ta ceilings, finish-route anneal, and grain size. Dual marking is a documentation and stencil option — it does not merge the two standards. For the ASTM twin alone, see A213 TP348H.
Can a mill dual-stamp TP348 and TP348H on the same heat?
Only when the heat chemistry and heat-treatment path actually satisfy both grade rows — including the H-grade carbon band, the 8 × C stabilizer rule, the finish-route anneal minima, and mandatory grain size for TP348H. Most Co/Ta heats aimed at non-H TP348 will not automatically clear TP348H. Ask for an honest single-grade stamp unless the MTC proves both rows.
Is TP348H suitable for wet chloride heat-exchanger service?
Not as a default upgrade. TP348H is framed for high-temperature H-grade boiler and superheater service with Co/Ta ceilings. Aggressive aqueous chlorides usually need molybdenum-bearing, duplex, or other project-specified alloys. Ask for a corrosion review before substituting TP348H into a wet-chloride HX datasheet that never named S34809.

Conclusion

ASME SA213 TP348H / UNS S34809 is the H-grade cobalt- and tantalum-controlled niobium-stabilized seamless stainless steel tube grade for Code boiler and superheater service when C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8 × C ≤1.10%, Co ≤0.20%, Ta ≤0.10%, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, a finish-route solution anneal, and grain size ASTM No. 7 or coarser are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report Nb+Ta, Co, Ta, and grain size. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X