ASME SA213 TP321 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP321 Stainless Steel Tube

ASME SA213 TP321 / UNS S32100 titanium-stabilized seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–12.0%, Ti ≥5×(C+N) ≤0.70%, no Mo requirement, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnotes F, H). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the titanium formula result.
Grade
TP321 / UNS S32100
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP321 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers, superheaters, or heat exchangers invoke that adoption by name, SA-213 is the governing product standard for this titanium-stabilized 18-8 tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP321 / UNS S32100 is the titanium-stabilized austenitic row inside that stainless family. Melting carbon is capped at 0.08%, chromium sits at 17.0–19.0%, nickel at 9.0–12.0%, and titanium must satisfy ≥5 × (C + N) with a 0.70% ceiling — molybdenum has no requirement on this row. Table 4 sets tensile at 75 ksi [515 MPa] / 30 ksi [205 MPa] with elongation 35% minimum and hardness max 192 HBW / 90 HRB. Buyers who write “321 HX tube” on a bill of materials still need to name SA-213 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the titanium formula together.

SHH STEEL can supply ASME SA213 TP321 as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report the titanium formula result together with the 75/30 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP321.

Shop names include “321,” “S32100,” and “Ti-stabilized 18-8 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP321 / UNS S32100, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements (S1 / S2 when needed). Sister SA213 pages include SA213 TP321H, SA213 TP304L, SA213 TP316Ti, and SA213 TP347. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP321

Two chemistry layers matter for TP321 under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The defining line for a reviewer is titanium ≥5 × (C + N) with a 0.70% ceiling — not a low-carbon max alone, and not a molybdenum addition. Chromium is 17.0–19.0% and nickel 9.0–12.0%, a slightly lower Cr window than the classic 18–20 / 8–11 304 family.

The tables below reproduce the melt limits for TP321 / UNS S32100, the product-analysis limits from A480 Table A1.1 practice, and a short stabilizer snapshot against TP304L, TP316Ti, and TP347. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP321 (UNS S32100) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 12.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement; analysis method by agreement when reported for the Ti formula)
Titanium (Ti) ≥ 5 × (C + N), ≤ 0.70

Source: public SA-213 / A213 stainless chemistry table for Grade TP321 / UNS S32100 (same grade text family). Confirm the ordered edition. When nitrogen is reported for the titanium formula, the analysis method is a matter of agreement (Footnote B). UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 12.0 0.10 under / 0.15 over 8.90 – 12.15
Titanium (Ti) ≥ 5 × (C+N), ≤ 0.70 0.05 over on max (Ti to 1.00 band practice) max ≤ 0.75 product; min tied to heat C+N

UNCERTAIN: A480 Ti max product-tolerance digits (0.05 over on ≤0.70 / Ti-to-1.00 band practice) — confirm against the ordered A480 edition when product analysis is invoked. Footnotes F/H and S2 full negotiated A262 / stabilization wording — confirm ordered edition.

Snapshot versus TP304L, TP316Ti, and TP347

Element TP304L (S30403) TP321 (S32100) TP316Ti (S31635) TP347 (S34700)
C ≤ 0.035 ≤ 0.08 ≤ 0.08 ≤ 0.08
Cr / Ni 18–20 / 8–12 17–19 / 9–12 16–18 / 10–14 17–20 / 9–13
Mo … … 2.00 – 3.00 …
Stabilizer low C Ti ≥5×(C+N) ≤0.70 Ti ≥5×(C+N) ≤0.70 Nb 10×C – 1.10

Titanium stabilization is not the same lever as L-carbon or niobium stabilization. Compare SA213 TP304L, SA213 TP316Ti, and SA213 TP347 before swapping on a familiar “321” PMI reading alone.

Mechanical Properties of SA213 TP321

ASME SA-213 Table 4 sets the tensile acceptance floor for TP321 / UNS S32100 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB. That is the same room-temperature pair as TP321H and many other 18-8 austenitics — titanium stabilization does not raise the room-temperature tensile floor; it changes sensitization framing and the chemistry check on the MTC.

Property TP321 requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

Source: public SA-213 / A213 Table 4 for UNS S32100 / TP321. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits the titanium formula result is incomplete for TP321. For H-grade carbon floor and grain-size control, open SA213 TP321H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP321 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and heat-exchanger datasheets that pick titanium-stabilized tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Titanium chemistry does not change the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 TP321 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX / boiler datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the titanium formula check.

Equivalent Grades

Equivalence language around 321 tube often treats it as “304 with titanium” or collapses it with 321H. ASME SA-213 Grade TP321 / UNS S32100 is the governing designation for this article; EN 1.4541 / X6CrNiTi18-10 family names and JIS SUS321 / SUS321TB are approximate wrought names that point to similar titanium-stabilized 18-8 families but are not automatic substitutes on an SA-213 MTC.

Designation Notes
ASME SA-213 / SA-213M Grade TP321 Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S32100 Unified number in the stainless chemistry table
ASTM A213 TP321 Separate ASTM product specification — twin page A213 TP321; dual-mark only when the PO asks
EN 1.4541 family (approx.) Approximate wrought Ti-stabilized designation; order EN tube forms under the relevant EN tube specs
Related H-grade SA213 TP321H — C 0.04–0.10, Ti ≥4×(C+N), grain size No. 7
Related L-carbon / Mo-Ti / Nb SA213 TP304L, SA213 TP316Ti, SA213 TP347
Related plate A240 / SA240 flat product in the same UNS family

Dual SA-213/A213 marking is a purchase-order option. Compare TP321H before swapping non-H 321 tube into a creep-range H-grade list.

Heat Treatment and Delivery Condition

TP321 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. Public heat-treatment language for this grade references Footnotes F and H on quench / subsequent exposure paths — confirm the full footnote text in the ordered edition. The public heat-treatment table does not print a mandatory ASTM grain-size number for non-H TP321.

Supplementary Requirement S2 lists TP321 among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. Supplementary Requirement S1 allows stress-relieved annealed TP321 (1500–1650 °F [815–900 °C] after roll straightening) for certain chloride stress-corrosion services when ordered. Neither S1 nor S2 is automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP321 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and titanium result on the EN 10204 3.1 certificate. For H-grade carbon and grain-size controls open SA213 TP321H. UNCERTAIN: S2 stabilizing hold full temperature/time wording and Footnotes F/H full negotiated A262 wording when ordered.

Corrosion Resistance

ASME SA213 TP321 is selected when titanium stabilization is preferred over low-carbon chemistry for resistance to intergranular attack after welding or exposure in the sensitizing range, while keeping a standard 18-8 austenitic alloy without molybdenum. The Ti ≥5 × (C + N) rule ties up carbon as titanium carbides/carbonitrides so chromium stays available for the passive film.

It is not a molybdenum grade and is not automatically better than TP304L in every chloride service — in many wet cooling-water lists, L-carbon or Mo-bearing grades remain the better match. Titanium stabilization also does not replace H-grade carbon floor and grain-size control for creep-range boiler duty; that path is SA213 TP321H.

SHH STEEL reports the titanium formula result on the 3.1 certificate so inspectors can verify stabilization rather than accepting a plain 304 heat stamped as 321 on a Ti PMI trace alone.

Applications of SA213 TP321 Tube

Typical ASME SA213 TP321 uses include Code-stamped heat-exchanger and condenser tubes where titanium stabilization is specified, process heaters that see intermittent sensitizing temperatures, and selected boiler / superheater services that name TP321 rather than the H grade. It is also quoted for replacement tube when original 321 MTCs must be matched on the titanium formula.

  • Heat-exchanger / condenser tubes naming Ti-stabilized 321
  • Process heaters with intermittent sensitizing exposure
  • Boiler / superheater tube when the datasheet names SA-213 TP321 (not H)
  • Replacement bundles matching original S32100 certificates

For creep-range H-grade duty with grain-size control, compare SA213 TP321H. For Mo + Ti, compare SA213 TP316Ti. For Nb stabilization, compare SA213 TP347.

Weldability

TP321 welds with matching titanium-stabilized austenitic filler practices — commonly ER321 / E321 family wires selected to the project WPS. Titanium in the base metal supports as-welded intergranular framing; still follow qualified procedures for heat input, interpass, and purge on thin HX tube, and watch titanium burnout / cleanliness that can deplete stabilization in the weld zone.

Autogenous orbital welds on thin-wall exchanger tube need purge discipline; Ti stabilization does not remove those controls. When S2 stabilization heat treatment is required after welding or mill anneal, put it on the purchase order — it is not automatic with the grade stamp.

Do not dual-stamp a TP304L weld procedure as TP321 without reopening the titanium formula and filler selection on the WPS / PQR.

Surface Finishes

Standard mill delivery for ASME SA213 TP321 is solution annealed and pickled, leaving a clean matte finish suitable for boiler and heat-exchanger tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the titanium formula check. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP321 includes heat analysis (C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–12.0%, Ti ≥5 × (C + N) ≤0.70%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm the titanium formula result rather than trusting a “304 family” PMI without Ti. Product analysis, when ordered, applies A480 tolerances including the Ti max window noted as UNCERTAIN digit confirmation above. S1 / S2 and A262 practices apply only when named on the PO.

EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP321 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP321, UNS S32100, heat number, size, and wall basis so receivers can match the 3.1 certificate — including the titanium formula — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP321 only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP321 as a Code Book titanium-stabilized product with enforceable C ≤0.08%, Cr 17–19%, Ni 9–12%, Ti ≥5 × (C + N) ≤0.70%, 75/30 ksi tensile, 35% elongation, hardness, and marking rules — not as “304 with a titanium trace” checked only by a Ti PMI peak. Enquiry review verifies the titanium formula before release.

That stops silent substitution with TP304 or TP304L heats on datasheets that actually require S32100. We keep SA-213 and A213 independent, dual-mark only on request, and put Ti on the 3.1 certificate so inspectors can verify stabilization.

Cross-links: SA213 TP321H, SA213 TP304L, SA213 TP316Ti, SA213 TP347, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP321 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for titanium-stabilized boiler and heat-exchanger tube.

Item SHH STEEL capability for TP321
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP321 / UNS S32100
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / HX bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Ti formula result; S1 / S2 / A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP321 against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for titanium-stabilized boiler and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common boiler / HX band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX / boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route, and whether dual A213 marking, S1 / S2, or A262 is required. We reply with available mill / stock options for ASME SA213 TP321 and the matching document set.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP321?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–12.0%, and Ti ≥5 × (C + N) ≤0.70% — tensile 75/30 ksi, elongation 35%, and hardness floors align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP321 include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
What is the UNS number and chemistry focus of ASME SA213 TP321?
UNS S32100. Check C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–12.0%, and titanium ≥5 × (C + N) with a 0.70% ceiling. Molybdenum has no requirement on this row. When nitrogen is reported for the Ti formula, the analysis method is by agreement (Footnote B). A heat without enough titanium for the formula is not TP321 even when Cr/Ni look like 18-8.
TP321 vs TP304L — when do I need titanium instead of low carbon under SA213?
Order TP321 when the datasheet wants titanium stabilization (Ti ≥5 × (C + N)) rather than L-carbon chemistry for sensitizing-range or as-welded intergranular framing. Order TP304L when C ≤0.035% without a stabilizer is the named path. They are different levers — not dual stamps — and Cr/Ni windows also differ slightly. Compare SA213 TP304L before swapping on a familiar 18-8 PMI reading alone.
TP321 vs TP316Ti — why choose one over the other under SA213?
TP316Ti adds molybdenum 2.00–3.00% with Ti stabilization; TP321 has no Mo requirement. Order TP316Ti when chloride-leaning or Mo-specified duty needs both Mo and Ti. Order TP321 when the datasheet wants Ti-stabilized 18-8 without molybdenum. Compare SA213 TP316Ti before stretching a 321 heat into a Mo claim.
TP321 vs TP321H — when do I need the H grade under SA213?
Order TP321H when the datasheet needs carbon 0.04–0.10%, Ti ≥4 × (C + N) ≤0.70%, finish-route solution temperatures (CF 2000 °F / HR 1925 °F), and ASTM grain size No. 7 or coarser for creep-range boiler / superheater duty. Non-H TP321 keeps C ≤0.08%, Ti ≥5 × (C + N), 1900 °F solution anneal, and no mandatory grain-size. Room-temperature tensile is the same 75/30 ksi pair on both.
What do Footnotes F and H mean for TP321 heat treatment under SA213?
Public SA-213 / A213 heat-treatment language for TP321 references Footnotes F and H on quench and subsequent-exposure paths. Full negotiated wording — including any A262 capability notes — must be read from the ordered edition; this pack labels that detail UNCERTAIN rather than inventing footnote text. Put A262 Practice E or S2 on the PO when demonstration or stabilization is required.
What is Supplementary Requirement S2 for TP321 under SA213?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. S1 separately allows stress-relieved annealed TP321 after roll straightening for certain chloride SCC services. Neither S1 nor S2 is automatic with the TP321 grade stamp; name them on the purchase order when needed.
Does SA-213 set a hardness limit for TP321?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Grade distinction versus TP304L or TP347 is the titanium formula (and Cr/Ni window), not a harder product. Versus TP321H the room-temperature tensile pair is the same; the H path adds carbon floor, grain size, and finish-route heat-treatment temperatures.
Minimum wall vs average wall — which should I order for SA213 TP321?
Most boiler and heat-exchanger datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in.; other diameters by agreement. Prefer OD × wall / BWG language over ASME B36.19 pipe schedules as the primary size story on tube RFQs.
Can you dual-certify ASME SA-213 and ASTM A213 TP321?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including C ≤0.08%, Cr 17–19%, Ni 9–12%, Ti ≥5 × (C + N) ≤0.70%, 75/30 ksi, and 35% elongation. Dual marking is stencil and documentation practice, not a claim that SA-213 and A213 are one document. Dual 321/321H on the same heat is a separate chemistry and grain-size question.
Is TP321 a good choice for chloride-rich cooling water under SA213?
Not automatically. Titanium stabilization addresses sensitizing-range intergranular framing; it does not add molybdenum for chloride pitting/crevice performance. Many wet cooling-water lists prefer L-carbon Mo-bearing grades or superaustenitics. Evaluate temperature, chloride, and deposit with the project corrosion engineer before defaulting to 321 on a familiar Ti PMI reading alone.

Conclusion

ASME SA213 TP321 / UNS S32100 is the titanium-stabilized seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–12.0%, Ti ≥5 × (C + N) ≤0.70%, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the titanium formula result. Compare sister grades on the same Code Book spine, or start from SA213/SA213M. Enquire with OD × wall, wall basis, quantity, and document needs at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X