ASME SA213 TP347H Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP347H Stainless Steel Tube

ASME SA213 TP347H / UNS S34709 niobium-stabilized H-grade seamless boiler, superheater and heat-exchanger tube — C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb ≥8×C ≤1.10%, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, ASTM grain size No. 7 or coarser, finish-route solution anneal (CF 2000 °F / HR 1925 °F). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb, carbon floor, and grain size.
Grade
TP347H / UNS S34709
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP347H Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers or superheaters invoke that adoption by name for creep-range niobium-stabilized service, SA-213 is the governing product standard for this H-grade tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP347H / UNS S34709 is the H-grade niobium-stabilized austenitic row. Melting carbon is locked inside 0.04–0.10%, chromium narrows to 17.0–19.0%, nickel stays 9.0–13.0%, and niobium must satisfy ≥8 × C with a 1.10% ceiling — a deliberately lower multiplier than the 10 × C rule on non-H TP347. Table 4 still sets 75/30 ksi with 35% elongation and hardness max 192 HBW / 90 HRB, but grain size must meet ASTM No. 7 or coarser per heat-treatment lot. This is not a dual stamp of TP347, TP347HFG, or TP321H.

SHH STEEL can supply ASME SA213 TP347H as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report carbon inside 0.04–0.10%, the 8 × C niobium result, grain size No. 7 or coarser, and the 75/30 ksi tensile set. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP347H.

Shop names include “347H,” “S34709,” and “H-grade Nb 18-8 tube.” Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP347H / UNS S34709, wall basis, OD × wall or BWG, finish route (which also selects the solution-temperature floor), and any Supplementary Requirements (S2 when needed). Sister SA213 pages include SA213 TP347, SA213 TP347HFG, SA213 TP321H, and SA213 TP347LN. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP347H

Two chemistry layers matter for TP347H under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. Two lines define the grade for a reviewer: the carbon band 0.04–0.10%, and niobium ≥8 × C with a 1.10% ceiling. That Nb multiplier is deliberately lower than the 10 × C rule on non-H SA213 TP347, so do not copy a TP347 niobium check onto a TP347H heat without reopening the formula. Chromium narrows to 17.0–19.0% versus TP347’s 17.0–20.0%.

The tables below reproduce the melt limits for TP347H / UNS S34709, the product-analysis limits from A480 Table A1.1 practice, and a short carbon / niobium snapshot against TP347, TP347HFG, and TP321H. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP347H (UNS S34709) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) ≥ 8 × C, ≤ 1.10
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for Grade TP347H / UNS S34709 (same grade text family). Confirm the ordered edition. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Niobium (Nb) ≥ 8 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C

UNCERTAIN: A480 Nb product-tolerance digits — confirm against the ordered A480 edition when product analysis is invoked. Footnote H / S2 full negotiated wording — confirm ordered edition.

Carbon and stabilizer snapshot — TP347 / TP347H / TP347HFG / TP321H

Element TP347 (S34700) TP347H (S34709) TP347HFG (S34710) TP321H (S32109)
C ≤ 0.08 0.04 – 0.10 0.06 – 0.10 0.04 – 0.10
Cr 17.0 – 20.0 17.0 – 19.0 17.0 – 19.0 17.0 – 19.0
Ni 9.0 – 13.0 9.0 – 13.0 9.0 – 13.0 9.0 – 12.0
Stabilizer Nb ≥ 10 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10 Ti ≥ 4 × (C+N), ≤ 0.70

Heats that also meet the non-H TP347 carbon ceiling while clearing the H-grade floor, the 8 × C niobium floor, tensile, hardness, and grain-size paths can be dual-certified TP347/TP347H when the purchase order asks — do not assume it from a PMI gun. Dual TP347H/TP321H is not a chemistry path: one grade requires niobium, the other titanium. Versus SA213 TP347HFG, TP347H allows a lower carbon floor (0.04% vs 0.06%), does not mandate the fine-grain 7–10 band or Footnote I softening path, and permits both cold-finished and hot-finished routes.

Mechanical Properties of SA213 TP347H

ASME SA-213 Table 4 sets the tensile acceptance floor for TP347H / UNS S34709 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB — the same room-temperature pair as TP347 and TP321H. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112, sitting beside the niobium stabilization chemistry.

Property TP347H requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: public SA-213 / A213 Table 4 for UNS S34709 / TP347H and H-grade grain-size language. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. Note that SA213 TP347HFG carries a higher Table 4 tensile floor (80 ksi [550 MPa]) plus a fine-grain band — do not treat HFG paperwork as interchangeable with TP347H. A tensile-only MTC that omits grain size or niobium is incomplete for TP347H. UNCERTAIN: grain-size table/clause number wording in the ordered edition.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP347H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and superheater datasheets that pick H-grade niobium-stabilized tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Finish route (cold-finished vs hot-finished) also selects which solution-temperature floor applies; it does not change the dimensional tolerance tables.

Item Typical SA213 TP347H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for boiler / superheater datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the carbon floor, Nb formula, or grain-size check.

Equivalent Grades

Equivalence language around 347H tube often collapses it with non-H 347 or with fine-grain HFG. ASME SA-213 Grade TP347H / UNS S34709 is the governing designation for this article; European or Japanese wrought names that mention “347H” point to related families but are not automatic substitutes on an SA-213 mill test certificate.

Designation Notes
ASME SA-213 / SA-213M Grade TP347H Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S34709 Unified number in the stainless chemistry table
ASTM A213 TP347H Separate ASTM product specification — twin page A213 TP347H; dual-mark only when the PO asks
Related non-H Nb SA213 TP347 — C ≤0.08, Nb ≥10×C, no mandatory grain number
Related fine-grain HFG SA213 TP347HFG — C 0.06–0.10, grain 7–10, 80 ksi, cold-finished only
Related Ti H-grade SA213 TP321H — titanium, not niobium
Related plate A240 / SA240 flat product in related UNS families

Dual SA-213/A213 marking is a purchase-order option. Compare TP347HFG before treating fine-grain paperwork as interchangeable with coarse-grain TP347H.

Heat Treatment and Delivery Condition

TP347H under ASME SA-213 is furnished solution treated, then quenched in water or cooled rapidly by other means. The public heat-treatment table sets separate minimum solution temperatures by finish route: cold-worked tube at 2000 °F [1100 °C], and hot-rolled tube at 1925 °F [1050 °C], with Footnote H on the hot-rolled path. Grain size after heat treatment must meet ASTM No. 7 or coarser for the heat-treatment lot. That combination — finish-route solution temperature, niobium chemistry, and coarse-grain control — is what separates TP347H paperwork from a tensile-only TP347 certificate.

Footnote H warns that a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure in the indicated grades, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. Supplementary Requirement S2 lists TP347H among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. S2 is not automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route that also selects which solution-temperature floor applies; it is not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP347H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, niobium result, and grain-size result stated on the EN 10204 3.1 certificate. For non-H niobium stabilization open SA213 TP347; for fine-grain cold-finished HFG open SA213 TP347HFG; for titanium H-grade open SA213 TP321H. UNCERTAIN: Footnote H / S2 full negotiated wording in the ordered edition.

Corrosion Resistance

ASME SA213 TP347H is selected when niobium stabilization plus an H-grade carbon floor and coarse-grain control are required for creep-range boiler and superheater service. The Nb ≥8 × C rule (with the 0.04–0.10% carbon band) ties up carbon as niobium carbides/carbonitrides while the grain-size requirement supports elevated-temperature framing that non-H TP347 does not mandate.

It is not a molybdenum grade and is not automatically better than TP304L in every chloride wet service. It is also not interchangeable with SA213 TP347HFG, which adds a fine-grain 7–10 band, a higher tensile floor, and cold-finished-only manufacture. Versus titanium H-grade SA213 TP321H, TP347H carries niobium rather than titanium.

SHH STEEL reports carbon, niobium, and grain size on the 3.1 certificate so inspectors can verify the full H-grade package rather than accepting a tensile-only 347 heat stamped as 347H.

Applications of SA213 TP347H Tube

Typical ASME SA213 TP347H uses include Code-stamped boiler and superheater tubes in the creep range where niobium H-grade chemistry and grain-size No. 7 or coarser are named, reheater and high-temperature process heaters that specify S34709, and replacement tube matching original 347H MTCs.

  • Boiler / superheater tube naming SA-213 TP347H
  • Reheater and high-temperature process heaters needing Nb H-grade controls
  • Creep-range Code services that reject non-H 347 certificates
  • Replacement bundles matching original S34709 certificates

For non-H Nb stabilization, compare SA213 TP347. For fine-grain cold-finished HFG, compare SA213 TP347HFG. For titanium H-grade, compare SA213 TP321H.

Weldability

TP347H welds with matching niobium-stabilized austenitic filler practices — commonly ER347 / ER347H family wires selected to the project WPS. Niobium in the base metal supports as-welded intergranular framing; still follow qualified procedures for heat input, interpass, and purge on thin boiler / HX tube.

When S2 stabilization heat treatment is required after welding or mill anneal, put it on the purchase order — it is not automatic with the H-grade stamp. Do not dual-stamp a TP347 or TP321H weld procedure as TP347H without reopening carbon floor, Nb formula (8 × C), grain-size acceptance, and filler selection on the WPS / PQR.

H-grade carbon and grain-size controls do not remove purge discipline on thin-wall orbital welds; they add certificate checks the fabricator must verify before release.

Surface Finishes

Standard mill delivery for ASME SA213 TP347H is solution annealed and pickled, leaving a clean matte finish suitable for boiler and superheater tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the carbon floor, Nb formula, or grain-size check. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP347H includes heat analysis (C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb ≥8 × C ≤1.10%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, grain size No. 7 or coarser per heat-treatment lot, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm carbon floor, niobium formula, and E112 grain-size result rather than trusting a “347 family” PMI without those H-grade checks. S2 and A262 practices apply only when named on the PO.

EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP347H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP347H, UNS S34709, heat number, size, and wall basis so receivers can match the 3.1 certificate — including carbon, niobium, and grain size — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP347H only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP347H as a Code Book niobium H-grade product with enforceable C 0.04–0.10%, Cr 17–19%, Ni 9–13%, Nb ≥8 × C ≤1.10%, grain size No. 7 or coarser, finish-route solution temperatures, 75/30 ksi tensile, and marking rules — not as “347 with an H stamped on” checked only by a PMI peak. Enquiry review verifies carbon, Nb, and grain size before release.

That stops silent substitution with non-H TP347 or titanium TP321H heats on datasheets that actually require S34709. We keep SA-213 and A213 independent, dual-mark only on request, and put the full H-grade package on the 3.1 certificate.

Cross-links: SA213 TP347, SA213 TP347HFG, SA213 TP321H, SA213 TP347LN, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP347H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for niobium-stabilized H-grade boiler and superheater tube.

Item SHH STEEL capability for TP347H
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP347H / UNS S34709
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with C, Nb formula, and grain-size result; S2 / A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347H against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for niobium-stabilized H-grade boiler and superheater tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small superheater / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common boiler / superheater band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route (CF or HF), and whether dual A213 marking, S2, or A262 is required. We reply with available mill / stock options for ASME SA213 TP347H and the matching document set.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP347H?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, and Nb ≥8 × C ≤1.10% — tensile 75/30 ksi, elongation 35%, hardness, and grain size No. 7 or coarser align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP347H include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
TP347H vs TP347 — when do I need the H grade under SA213?
Order TP347H when the datasheet needs carbon 0.04–0.10%, Nb ≥8 × C ≤1.10% (not the non-H 10 × C rule), finish-route solution temperatures (CF 2000 °F / HR 1925 °F), and ASTM grain size No. 7 or coarser for creep-range duty. Order non-H TP347 when those H-grade controls are not named. Dual 347/347H is possible only when the heat clears both rows and the PO asks.
What is the UNS number and chemistry focus of ASME SA213 TP347H?
UNS S34709. Check C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, and niobium ≥8 × C with a 1.10% ceiling. Do not apply the non-H TP347 10 × C niobium rule to a TP347H heat. Molybdenum has no requirement on this row. Grain size No. 7 or coarser is part of the H-grade acceptance package beside chemistry.
Does SA-213 set a hardness and grain-size limit for TP347H?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Grain size must meet ASTM No. 7 or coarser per heat-treatment lot. A tensile-and-hardness MTC that omits grain size or niobium is incomplete for TP347H. Compare SA213 TP347HFG if the datasheet wants a fine-grain 7–10 band and 80 ksi tensile instead.
What solution temperatures apply to TP347H under SA213?
Public heat-treatment language sets cold-worked tube at a minimum of 2000 °F [1100 °C] and hot-rolled tube at a minimum of 1925 °F [1050 °C], with Footnote H on the hot-rolled path. Finish route therefore selects which solution-temperature floor applies. Full Footnote H negotiated wording is UNCERTAIN without the ordered edition — confirm before writing contractual language.
What is Supplementary Requirement S2 for TP347H under SA213?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. S2 is listed for TP347H in the public grade text family but is not automatic with the grade stamp; write it explicitly on the purchase order when the project needs it.
TP347H vs TP347HFG — are they interchangeable under SA213?
No. TP347HFG has a higher carbon floor (0.06–0.10% vs 0.04–0.10%), a fine-grain band No. 7–10 (not “7 or coarser”), a higher Table 4 tensile floor (80 ksi vs 75 ksi), cold-finished-only manufacture, and a Footnote I softening-before-cold-work path. Do not treat HFG paperwork as interchangeable with coarse-grain TP347H. Compare SA213 TP347HFG on its own page.
TP347H vs TP321H — why choose Nb over Ti under SA213?
Both are H-grade stabilized 18-8 grades, but TP347H requires niobium ≥8 × C ≤1.10% while TP321H requires titanium ≥4 × (C + N) ≤0.70%. Nickel windows also differ slightly (347H: 9–13; 321H: 9–12). Dual TP347H/TP321H is not a chemistry path. Order the stabilizer the datasheet names.
Minimum wall vs average wall — which should I order for SA213 TP347H?
Most boiler and superheater datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in. State wall basis, OD × wall or BWG, and finish route on the RFQ so the mill applies the correct dimensional table and solution-temperature floor.
Can you dual-certify ASME SA-213 and ASTM A213 TP347H?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including C 0.04–0.10%, Cr 17–19%, Ni 9–13%, Nb ≥8 × C ≤1.10%, grain size No. 7 or coarser, 75/30 ksi, and 35% elongation. Dual marking does not merge the standards into one document. See also the twin page A213 TP347H.
Is TP347H a good choice for chloride-rich cooling water under SA213?
Not automatically. H-grade Nb stabilization and grain-size control address creep-range and sensitizing-range framing; they do not add molybdenum for chloride pitting/crevice performance. Many wet cooling-water lists prefer L-carbon or Mo-bearing grades. Keep TP347H where the datasheet names H-grade Nb boiler / superheater service.

Conclusion

ASME SA213 TP347H / UNS S34709 is the niobium-stabilized H-grade seamless stainless steel tube for Code boiler and superheater service when C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb ≥8 × C ≤1.10%, ASTM grain size No. 7 or coarser, finish-route solution temperatures, a 75/30 ksi tensile floor with 35% elongation, and hardness max 192 HBW / 90 HRB are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report carbon, niobium, and grain size. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X