ASME SA213 TP304 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP304 Stainless Steel Tube

ASME SA213 TP304 / UNS S30400 seamless boiler, superheater and heat-exchanger tube with Cr 18.0–20.0%, Ni 8.0–11.0% and C ≤0.08%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP304 / UNS S30400
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP304 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP304 under that Code Book text is the familiar 18-8 chromium-nickel austenitic listed as UNS S30400, with melting limits of carbon ≤0.08%, chromium 18.0–20.0%, and nickel 8.0–11.0%. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP304, the purchase order and mill test certificate should carry the ASME designation — not only a shop nickname such as “304 HX tube.”

SHH STEEL can supply ASME SA213 TP304 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 304, 18-8, S30400 boiler tube, or SA213 304 HX tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP304L, SA213 TP304H, SA213 TP316 / SA213 TP316L, SA213 TP321, and SA213 TP347. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP304.

Chemical Composition of SA213 TP304

Two chemistry layers matter for TP304 under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements path (commonly ASTM A1016/A1016M as referenced by the ordered SA-213 edition). Product-analysis tolerances are not reprinted as a standalone chemistry table inside SA-213 itself; when ordered, they typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise tighter catalogue chemistry windows that the Code Book text does not publish.

The tables below reproduce the heat analysis for TP304 / UNS S30400 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element, so it need not be determined or reported on the certificate. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP304 / UNS S30400. Confirm the ordered ASME edition on the purchase order.

Element TP304 (UNS S30400) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 11.0 0.10 under / 0.15 over 7.90 – 11.15

The 18–20% chromium and 8–11% nickel balance is why TP304 remains the reference 18-8 austenitic tube grade under SA-213: chromium builds the passive film and nickel keeps the structure fully austenitic after the 1900 °F [1040 °C] solution treatment. Carbon is capped at 0.08% on the melt; heats that also meet the TP304L carbon ceiling and overlapping nickel band can be dual-certified to SA213 TP304L when both tensile floors and hardness limits are satisfied.

When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20% and Ni 7.90–11.15%. Those are the only product limits we quote from the A480 A1.1 path. Put any tighter project carbon or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP304

ASME SA-213 sets the tensile acceptance floor for TP304 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. The same mechanical table also lists a hardness maximum for TP304 of 192 HBW / 200 HV or 90 HRB, and hardness tests are part of the lot acceptance scheme — a point that often surprises buyers who only know ASTM A312 pipe rows for the same UNS number. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP304 / UNS S30400 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP304 requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

Flattening and flaring tests are also required on a lot basis for finished tube; they sit beside tension and hardness rather than replacing them. Actual mill certificates often clear the 75/30 ksi floor with margin, but design calculations should still use the Code Book floor unless the purchase order states higher guaranteed values that the mill has accepted in writing. For creep-range boiler service that needs a controlled carbon floor and grain-size language, open SA213 TP304H rather than stretching standard TP304 beyond its intended framing.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP304 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition — do not treat a catalogue one-liner as a substitute for the table.

Item Typical SA213 TP304 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP304 tube is often looser than a Code or heat-exchanger purchase order can afford. ASME SA-213 Grade TP304 / UNS S30400 is the governing designation for this article; EN 1.4301 and JIS SUS304 are approximate wrought names that point to similar chemistry families but are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 304,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP304 Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30400 Unified number listed with the grade chemistry
ASTM A213 TP304 Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP304
EN 1.4301 (X5CrNi18-10) Approximate wrought stainless designation; order EN tube forms under the relevant EN tube specs, not by EN number alone on an SA-213 MTC
JIS SUS304 Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP304 is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare low-carbon, H-grade, and molybdenum sisters on their own ASME SA213 pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP304 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave a structure that sensitizes in service even when ladle chemistry looked acceptable on paper.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal: cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL TP304 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability (commonly tied to ASTM A262 Practice E on sensitized or as-shipped specimens, depending on grade type) is ordered, the corrosion test report travels with the heat-treatment record. H-grade grain-size rules do not rewrite the TP304 path — use SA213 TP304H when the datasheet calls for H-grade carbon and grain-size controls.

Corrosion Resistance

TP304’s chromium-rich passive film handles a wide band of oxidizing process fluids, clean steam-side and water-side duties, and many organic media that do not lean heavily on chlorides. In chloride-bearing waters, coastal cooling circuits, and many brine-leaning heat-exchanger services, pitting and crevice attack become limiting, and buyers usually step up to SA213 TP316 or SA213 TP316L. Intergranular corrosion risk after tube-to-tubesheet welding or after sensitizing thermal cycles is controlled by ordering SA213 TP304L, by solution treating after fabrication when the sequence allows, or by invoking the contractual corrosion test on the tube PO.

ASME SA-213 itself does not publish a corrosion-rate table for TP304; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note. SHH STEEL will not rank TP304 as equal to 316 in chlorides — that claim is not supported by the product standard.

Applications of SA213 TP304 Tube

Because TP304 is the default austenitic seamless tube grade in so many Code and heat-exchanger specifications, it shows up across power-plant and industrial steam systems, process heat exchangers, condensers, and general corrosive tube duty where molybdenum is not required. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid, temperature, and fabrication route — not only for the familiar “304” name on the BOM.

Application area Typical use of TP304 tube Selection note
Boiler and superheater Seamless generating-bank, screen, and moderate-temperature steam tubing ordered to SA-213 For creep-critical H-grade service open TP304H; confirm design metal temperature
Heat exchangers / condensers Straight and U-bend HX tubes in process and utility exchangers State min vs average wall, BWG, and bend radius on the enquiry
Chemical and process Tube-side or shell-side circuits with oxidizing or mild corrosive media Prefer TP316/TP316L if chlorides dominate
Food / pharmaceutical utilities Utility and process HX where 304 stainless tube is accepted Follow hygiene finish and welding procedure requirements
Cryogenic / low-temperature HX Austenitic toughness in cold-box and LNG-related exchangers Confirm low-temperature Code acceptance for the grade
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe product forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For as-welded tube-to-tubesheet joints in sensitizing service consider TP304L or dual TP304/TP304L; for high-temperature creep-range boiler tubing open TP304H; for chloride-rich cooling water move to the molybdenum grades on the same SA213/SA213M hub.

Weldability

TP304 tube welds readily with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER308 / ER308L (or equivalent covered electrodes) under a qualified WPS; many exchanger fabricators prefer ER308L deposits for lower carbon in the weld metal even when the base tube is standard TP304. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP304 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. For tube that will enter service as-welded in a sensitizing environment, many owners change the base metal to SA213 TP304L rather than relying on a perfect weld procedure alone to protect standard-carbon TP304. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP304 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP304 includes heat analysis, tension tests to the mechanical-table floors, hardness tests to the hardness maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP304 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP304 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP304 as a Code Book product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 304 tube.” The MTC reports the full ladle chemistry and the tensile/hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 304-family conversation honest for boiler and HX duty. If tube-to-tubesheet joints will run as-welded in a sensitizing environment, we steer toward SA213 TP304L or dual TP304/TP304L. If creep-range boiler service needs H-grade carbon and grain-size controls, we open SA213 TP304H. If chlorides dominate the cooling water or process fluid, we open SA213 TP316 / SA213 TP316L. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP304 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.

Item SHH STEEL capability for TP304
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP304 / UNS S30400
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP304 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP304
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP321, SA213 TP347H, and SA213 UNS S30432 sit on the same hub when the datasheet steps beyond standard TP304.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP304?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP304 include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP304 under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
Minimum wall vs average wall — which should I order for SA213 TP304?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from the general requirements.
Hydrostatic test vs NDE — which do I get on SA213 TP304 tube?
ASME SA-213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
Does SA-213 set a hardness limit for TP304?
Yes. The mechanical table for TP304 lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under SA-213, which differs from many SA312 / A312 pipe rows for the same UNS number that omit a hardness cap. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What is the UNS number and chemistry of ASME SA213 TP304?
TP304 is UNS S30400. Melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 18.0–20.0%, and nickel 8.0–11.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the general-requirements path. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP304 vs TP304L — which SA213 tube should I order?
Order TP304 when the specification calls for the standard 75/30 ksi tensile floor, 192 HBW / 90 HRB hardness maximum, and carbon ≤0.08% is acceptable. Order TP304L when as-welded intergranular resistance is the driver and the lower 70/25 ksi floor is acceptable. Dual TP304/TP304L certification is possible on qualifying heats — ask for it on the PO rather than assuming it from a PMI gun reading.
TP304 vs TP304H — when do I need the H grade under SA213?
Order TP304H when the boiler or superheater datasheet needs the H-grade carbon range, grain-size controls, and creep-rupture framing that the H designation carries under SA-213. Standard TP304 remains appropriate for many moderate-temperature HX and general corrosive tube duties. Do not treat "304H" as a synonym stamp for ordinary TP304 on the MTC.
TP304 vs TP316 — which SA213 grade is better in chlorides?
TP316 / TP316L adds molybdenum and generally resists chloride pitting and crevice corrosion better than TP304 in seawater-leaning cooling water, brines, and many process exchangers. TP304 remains appropriate for many oxidizing and low-chloride steam and process services. ASME SA-213 does not publish a chloride ranking table; open the TP316 tube pages on the hub when chlorides dominate.
What heat treatment does ASME SA-213 require for TP304?
TP304 is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
Can you dual-certify ASME SA-213 and ASTM A213 TP304, or TP304/TP304L?
Yes on both axes when the heat and testing support it. Dual SA-213/A213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Dual TP304/TP304L is available when ladle chemistry meets the tighter carbon rules and tensile plus hardness results clear both mechanical-table rows. Spell the required marking on the enquiry so the heat is selected correctly.

Conclusion

ASME SA213 TP304 / UNS S30400 remains the reference 18-8 seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when molybdenum is not required and standard carbon is acceptable. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the tensile and hardness acceptance floors, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X