ASME SA312 TP310H Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 TP310H Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 TP310H (UNS S31009) stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M): seamless (SML), welded (WLD) and heavily cold-worked (HCW); C 0.04–0.10%, Cr 24.0–26.0%, Ni 19.0–22.0%; grain size ASTM No. 6 or coarser; reheated 1900 °F anneal; Table 4 minima 75/30 ksi. SHH STEEL supplies with EN 10204 3.1 MTCs.
Grade
TP310H / UNS S31009
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 TP310H Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. Grade TP310H is listed in Table 1 as UNS S31009. Clause 1.2 groups it with the other H grades—TP304H, TP309H, TP309HCb, TP310HCb, TP316H, TP321H, TP347H, and TP348H—as modifications intended for temperatures where creep and stress-rupture properties are important. Commercially the same product may be called SA312 TP310H pipe, ASTM A312 TP310H pipe, A312 Grade TP310H, or 310H stainless steel pipe when the purchase order clearly references SA-312 or A312. For pressure piping and code work, cite the full grade designation, the UNS number, and the edition of the standard on the purchase order and on the mill test certificate—do not rely on a bare “310H” or “25-20” market label.

TP310H keeps the 24.0–26.0% chromium and 19.0–22.0% nickel of the 310 family, but Table 1 adds a carbon range of 0.04–0.10% (not a ≤0.08% ceiling alone like ASME SA312 TP310S Stainless Steel Pipe). Silicon is ≤1.00%, and Table 1 shows no molybdenum requirement for TP310H—the Mo column is an ellipsis. Table 5 requires grain size ASTM No. 6 or coarser; ASME clause 6.2 requires a reheated solution anneal before quench; and clause 17 requires heat-treatment lot marking on every length. Room-temperature Table 4 floors remain 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield. The H-grade benefit appears in elevated-temperature code allowables and in the carbon floor plus coarse grain that support creep resistance—not in a higher room-temperature tensile number. Table 2 lists the solution temperature at 1900 °F [1040 °C] (with TP309H, TP309HCb, and TP310HCb). Table 6 does not assert a mandatory AWS filler class for TP310H from the packed notes; filler selection is by agreement on the WPS.

SHH STEEL can supply ASME SA312 TP310H stainless steel pipe to the edition named on the enquiry, including seamless (SML), welded (WLD), and heavily cold-worked (HCW) routes; ASME B36.19 schedules and special OD/wall by agreement; EN 10204 3.1 mill test certificates that report grain size and heat-treatment lot; and dual SA-312/A312 marking when the heat analysis, heat treatment, mechanical tests, and marking satisfy both editions named on the purchase order. Confirm NPS, wall or schedule, finish, length practice, and any product-analysis or supplementary tests on enquiry.

Common commercial names and how they map to the ordered product are listed below—use the full SA-312/A312 designation on the purchase order rather than market shorthand alone.

  • ASME SA312 TP310H / SA-312 Grade TP310H — preferred marking language for ASME-code and dual-marked pipe
  • ASTM A312 TP310H — same grade tables for chemistry and tensile when the ASTM edition is referenced
  • UNS S31009 — unified numbering system identity used on MTCs, stencils, and Section II Part D cross-references
  • 310H / 25-20 H-grade stainless steel pipe — market shorthand; confirm C 0.04–0.10%, grain size ASTM No. 6 or coarser, reheat documentation, and lot marking on the order

TP310H is not a drop-in for ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 UNS S31002 Stainless Steel Pipe, ASME SA312 TP310Cb Stainless Steel Pipe, or ASME SA312 TP309H Stainless Steel Pipe on a shared “310” or “25-20” market label—each has its own Table 1 row and (where applicable) H-grade or specialty rules. Versus TP310S, TP310H adds the carbon floor, Table 5 grain-size rule, and clause 6.2 reheat; dual 310S/310H marking is possible only when carbon also meets the 0.04–0.10% H band and grain size is controlled. Versus UNS S31002, TP310H allows C up to 0.10% (vs ≤0.015%), Si ≤1.00% (vs ≤0.15%), and carries H-grade controls rather than ultra-low C/Si aqueous practice. Versus TP310Cb, TP310H has no niobium stabilization—order HCb (ASME SA312 TP310HCb Stainless Steel Pipe) when Nb plus H rules are both required. Versus TP309H (Cr 22–24, Ni 12–15), TP310H sits one step higher in alloy content for hotter oxidation and creep service. Hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 defines three manufacturing routes that may be marked on finished TP310H pipe. Selecting the route is a purchase-order decision driven by design code, size range, wall thickness, and inspection preference. It does not change the Table 1 chemistry of Grade TP310H—melting must still meet C 0.04–0.10%, Cr 24.0–26.0%, and Ni 19.0–22.0%—and every route must still pass through the clause 6.2 reheated solution anneal that produces conforming grain size.

  • Seamless (SML) — no welding at any stage of manufacture. Seamless is preferred for high-temperature pressure parts, heater tubes, radiant coils, and heavy walls when the project specification excludes welded pipe or when the piping class documentation is written around seamless product only. Hot-finished or cold-finished seamless must still be reheated to the solution temperature before quenching; residual heat from piercing is not enough under clause 6.2.
  • Welded (WLD) — automatic welding without filler metal. The weld is finished so that the pipe meets dimensional and mechanical requirements after the final heat treatment required by SA-312. Weld joint quality factors and creep-range weld strength reduction factors may apply under B31 codes. The plate heat must itself meet S31009 chemistry, and the pipe anneal must produce conforming grain size in both base metal and weld zone.
  • Heavily cold-worked (HCW) — welded pipe that is cold worked to a reduction of area of wall and weld of at least 35% before the final anneal, again without filler metal in the longitudinal weld. The weld is radiographed before cold work. HCW is ordered when the buyer wants the HCW marking and the process controls written into SA-312 for that route.

Every length must carry the heat number and the heat-treatment lot identification (clause 17). That lot links each pipe to the anneal that produced its grain size—verify lot numbers on both stencil and MTC. Each finished length is hydrostatically tested or nondestructively electrically tested; the manufacturer may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser agrees to a system test in lieu of hydrotest. Lot definitions follow clause 11.1; grain-size determinations are made on each heat-treatment lot for the same number of pipes as the flattening test (typically 5% of the lot) per clause 11.4.

Because of the reheat and grain-size controls, TP310H lead times are typically longer than for ASME SA312 TP310S Stainless Steel Pipe. Plan procurement early for project-critical heater sizes, and confirm route, edition, and any supplementary tests before placing a mill order so the certificate matches the design basis. Where a component is oxidation-limited rather than creep-limited, switch the conversation to TP310S before the mill melts the heat—oxidation-limited furnace parts and creep-range pressure parts are different selection problems. Where ultra-low C and Si are mandatory for oxidizing aqueous service, move to ASME SA312 UNS S31002 Stainless Steel Pipe instead of stretching an H-grade heat into that chemistry window.

Chemical Composition of SA312 TP310H

Two chemistry layers matter: melting (heat / ladle) analysis—mandatory per heat under ASME SA-312/ASTM A312 Table 1—and product analysis when ordered (Suppl. S1 / PO). SA-312/A312 defer product-analysis tolerances through ASTM A999/A999M §6.3 to ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle and, when ordered, product values—never unpublished tighter windows. Spot-check carbon 0.04–0.10%, chromium 24–26%, and nickel 19–22% first on receipt; those three values, plus the H-grade grain-size and reheat evidence, are what separate TP310H from neighboring 310 rows.

Melting analysis (heat / ladle analysis) — Table 1

Heat analysis for Grade TP310H / UNS S31009 from ASME SA-312/SA-312M (ASTM A312/A312M) Table 1 is summarized below. Values are maximum unless a range is shown; ellipses (…) mean no requirement in the ordered edition.

Element TP310H / UNS S31009 melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)

Source: SA-312 Table 1, TP310H / UNS S31009. Mo column is “…” (no requirement). No Nb, N, Cu, or Ti requirement. Do not treat secondary catalog sheets as a substitute for the ordered edition.

Chromium drives oxidation resistance; nickel stabilizes austenite and supports toughness at the 25Cr–20Ni balance; the 0.04% carbon floor feeds fine, stable carbides that pin dislocations during long high-temperature exposure, while the 0.10% ceiling keeps the alloy weldable and limits excessive carbide networks. Unlike TP310S, Table 1 does not list a molybdenum residual for TP310H—an MTC need not report Mo unless the purchase order asks for it as information.

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

When product analysis is ordered, finished-pipe chemistry shall meet Table 1 as modified by the product-analysis tolerances of ASTM A480/A480M Table A1.1 (via A999 §6.3). The verified product-analysis limits for TP310H are:

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20

Carbon 0.04–0.10%: the defining H-grade band. Heats below 0.04% C are TP310S candidates, not TP310H. Product analysis uses the A480 ±0.01% band (0.03–0.11%). Vs TP310S: TP310S allows C ≤0.08 with no minimum and carries Mo ≤0.75%; TP310H has the carbon band, no Mo requirement, plus Table 5 / clause 6.2. Vs UNS S31002: S31002 tightens C to ≤0.015%, Si to ≤0.15%, Mo to ≤0.10%, and adds N ≤0.10%—commodity or H-grade 310 heats will never meet that window. Vs TP310Cb: TP310Cb adds Nb 10×C min – 1.10 max and Mo ≤0.75% without H-grade grain rules.

Element TP310H TP310S TP310Cb UNS S31002
C 0.04 – 0.10 ≤ 0.08 ≤ 0.08 ≤ 0.015
Si ≤ 1.00 ≤ 1.00 ≤ 1.00 ≤ 0.15
Mo … ≤ 0.75 ≤ 0.75 ≤ 0.10
Nb … … 10×C – 1.10 …
N … … … ≤ 0.10
H controls Yes No No No

The side-by-side table above shows why a shared “310” or “310H” market label is dangerous: ASME SA312 TP310S Stainless Steel Pipe is the commodity low-carbon row; ASME SA312 TP310Cb Stainless Steel Pipe stabilizes with niobium; ASME SA312 UNS S31002 Stainless Steel Pipe combines ultra-low C with ultra-low Si and Mo; TP310H is the creep-service H-grade row with C 0.04–0.10% and grain-size control. Dual-certified TP310S/TP310H heats need carbon in the 0.04–0.08% overlap and conforming H-grade anneal and grain-size evidence—chemistry alone is not enough. Do not invent Table 1 maxima for Ti, Nb, Cu, or Al on TP310H. Residual elements not listed in Table 1 are controlled by melt practice and by any purchase-order limits the buyer adds.

Mechanical Properties of SA312 TP310H

Tensile requirements for TP310H are given in ASME SA-312/SA-312M (ASTM A312/A312M) Table 4. Specimens and orientation follow the testing clauses of the standard and the referenced general requirements (A999/A999M as applicable). Grain size is a separate Table 5 acceptance item that does not appear for TP310S.

Property TP310H (S31009)
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm (or 4D) 35% longitudinal / 25% transverse, min
Grain size (Table 5) ASTM No. 6 or coarser
Hardness No maximum in Table 4

Source: SA-312 Table 4 for TP310H / UNS S31009; Table 5 grain-size rule for H grades. These floors match ASME SA312 TP310S Stainless Steel Pipe and ASME SA312 TP309H Stainless Steel Pipe at room temperature; ASME SA312 UNS S31002 Stainless Steel Pipe is lower at 73 ksi tensile. The H grade is chosen for carbon-floor and coarse-grain practice that support elevated-temperature allowables, not for a higher Table 4 number.

Grain size is measured per ASTM E112 on each heat-treatment lot; a result of No. 7 or finer fails TP310H even if chemistry and tensile results pass. Cite UNS S31009 wherever allowable-stress tables are consulted so fabricators do not pull a sister-grade strength line from memory. ASME Section II Part D lists allowable stresses for S31009 where the part is pressure retaining—do not back-calculate allowables from Table 4 room-temperature minima, and do not copy TP310S stress tables into a TP310H calculation package when the code separates H and non-H entries.

Hardness and optional tests: Table 4 does not list a hardness maximum for TP310H as a separately mandated acceptance item. If hardness matters for fabrication or end-user acceptance, state the limit on the purchase order and verify it on the MTC. Flattening or bend and tension run on a lot basis; grain size uses the same sampling as flattening (typically 5% of the lot). Elevated-temperature tensile, creep, and rupture tests are purchase-order options—not part of base SA-312.

MTC review order for TP310H: carbon 0.04–0.10%; grain size ASTM number ≤6 (coarser); anneal temperature ≥1900 °F with reheat evidence; lot number matching the stencil; tensile ≥75 ksi; yield ≥30 ksi; elongation; hydro or NDE method. Forming loads are similar to TP310S; springback is greater than for 304, so use generous bend radii for furnace tubing. Include corrosion/oxidation allowance and the 12.5% mill under-tolerance (or S8 minimum wall) in the thickness calculation. After long high-temperature service, room-temperature ductility can fall as carbides and sigma form—that is expected ageing behaviour, and used pipe should be evaluated before cold bending or repair welding.

Dimensions and Tolerances

Dimensional practice for austenitic stainless steel pipe ordered to SA-312 typically follows ASME B36.19 / B36.19M stainless-steel pipe schedules. Outside diameter and wall thickness are stated as NPS and schedule, or as OD and specified wall. Common schedules for TP310H enquiry include Schedule 5S, 10S, 40S, and 80S. Heater tubes, radiant coils, and headers are often ordered by OD and wall to the equipment drawing, and heavy walls for heater headers are common. Other walls and non-standard OD/wall combinations are available by agreement when both the mill and the order accept them.

Size coverage in commercial practice is summarized below. Confirm large NPS and heavy walls against mill capability for the chosen manufacturing type before you lock the purchase order—heavy-wall seamless is usually mill-run with longer lead times.

  • NPS / DN: commonly from NPS 1/8 upward; large NPS and heavy walls depend on manufacturing type (SML versus WLD/HCW) and mill capability—confirm on enquiry
  • Schedules: 5S, 10S, 40S, 80S and special walls by agreement
  • Length: single random (SRL), double random (DRL), or fixed cut lengths as stated on the purchase order; NPS 1/8 to 8 commonly up to 24 ft (15–24 ft range) unless agreed; cut lengths ≤1/4 in. [6 mm] over
  • Ends: plain end (PE), beveled end (BE) to B16.25, or machined weld preps by agreement; jointers not permitted unless specified
  • Minimum wall (S8): often ordered so creep-range calculations use the actual minimum rather than nominal wall minus mill under-tolerance

Wall-thickness variation limits from SA-312 Table 3 (t/D = specified wall / ordered OD) are the acceptance bands used on mill test certificates and receiving inspection for TP310H:

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M. OD, wall, and length tolerances follow SA-312 via ASTM A999/A999M and the dimensional standard on the order. State whether wall is nominal or minimum on the PO. For automatic orbital welding, owners may specify tighter OD, wall, and end-squareness tolerances than A999 requires. Thermal expansion of 310-type austenitic pipe is high relative to carbon steel—long hot runs need sliding supports, spring hangers, or expansion loops, and support spacing for thin-wall heater tubes should also consider creep sag over the planned campaign length.

Equivalent Grades

Equivalence for TP310H must be stated carefully. Chemistry approximations across regional designations help material selection discussions; they are not automatic one-to-one substitutes for ASME pressure-code pipe without an approved material specification and design-code acceptance. Do not accept TP310S stock marked as 310H without grain-size results, reheat documentation, and carbon ≥0.04%—the stencil alone is not enough for code work.

Designation Notes
ASME SA-312 / ASTM A312 Grade TP310H Governing pipe product standard for this article
UNS S31009 Unified number listed in Table 1
TP310S (UNS S31008) Parent S grade; C ≤0.08%, Mo ≤0.75%; no Table 5 grain-size mandate
TP310Cb / TP310HCb Columbium (niobium) stabilized sisters; order the exact TP name on the PO
UNS S31002 Ultra-low C/Si specialty; 73 ksi tensile; not an H grade
TP309H (UNS S30909) Lower Cr–Ni H grade; not interchangeable on a “310H” label
ASME SA-213 TP310H Boiler and heat-exchanger tube (separate specification)
ASME SA-240 / A240 310H Plate counterpart (separate specification)
EN 1.4845 / JIS SUS 310S approx. Engineering map only—recheck C band and H rules; not automatic H-grade equivalents

Related product pages: ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 UNS S31002 Stainless Steel Pipe, ASME SA312 TP310Cb Stainless Steel Pipe, ASME SA312 TP310HCb Stainless Steel Pipe, ASME SA312 TP309H Stainless Steel Pipe, ASME SA312 TP309S Stainless Steel Pipe, ASME SA312 TP304H Stainless Steel Pipe. When an enquiry says only “310H pipe,” confirm whether TP310H or TP310HCb is intended—niobium stabilization changes both chemistry and welding practice. Dual TP310S/TP310H certification widens available stock only when carbon, anneal, grain size, and lot marking all satisfy the H-grade rules. Hub: ASME SA 312/SA 312M.

Heat Treatment and Delivery Condition

All pipe furnished to ASME SA-312 shall be heat treated. SA-312 Table 2 lists TP310H (with TP309H, TP309HCb, and TP310HCb) at 1900 °F [1040 °C], cooling note D (water quench or rapid cooling). That temperature is the same number used as the Table 2 default for many non-H grades, but the process path for TP310H is different because of the H-grade reheat rule.

ASME clause 6.2: for H grades, pipe must be reheated to the specified solution temperature for the required time before quenching. Direct quenching after hot forming—allowed for many other grades including TP310S—is not permitted for TP310H. Clause 17 marking: includes heat number and heat-treatment lot identification so each length traces to its anneal. Grain size ASTM No. 6 or coarser must be demonstrated on each heat-treatment lot.

  • Delivered solution annealed by reheating at ≥1900 °F [1040 °C], then rapidly cooled
  • Grain size ASTM No. 6 or coarser on each lot (Table 5)
  • Free of scale and exogenous iron; pickled or blasted as agreed
  • Heat number and heat-treatment lot number on pipe and MTC
  • Bright anneal / passivation available on request when the end-user specification requires a scale-free or passivated surface

Ask mills to retain furnace charts for each lot so time and temperature can be shown on request. Post-fabrication PWHT, if specified, must not refine grain below the Table 5 requirement. Too short a soak or too low a temperature can leave grain finer than No. 6, which fails Table 5 even when the furnace setpoint looks correct on paper—that is why lot-based grain-size testing is mandatory, not optional, for TP310H. If a project wants Nb stabilization plus H rules, order ASME SA312 TP310HCb Stainless Steel Pipe instead. Cite the ordered edition’s Table 2 row on the enquiry so the mill does not apply a neighboring S-grade direct-quench habit to a TP310H heat by mistake.

Corrosion Resistance

TP310H is selected primarily for high-temperature oxidation and creep-range pressure duty, not as a general aqueous corrosion grade. The 24–26% chromium supports a continuous chromia scale similar to ASME SA312 TP310S Stainless Steel Pipe; the higher carbon (up to 0.10%) increases sensitization risk after welding or slow cooling compared with the S grade. Fitness for service depends on atmosphere, temperature, and cycling—SA-312 itself contains no corrosion data.

  • Oxidation: 24–26% Cr supports continuous air and flue-gas duty where classic 18-8 grades scale rapidly; producer guidance often quotes intermittent air service into the 1900–2100 °F range (not an SA-312 value)—always defer to the design code’s temperature limits for S31009
  • Sensitization: C up to 0.10% means HAZ carbides are more likely; for wet corrosive service after furnace exposure, review stabilized ASME SA312 TP310HCb Stainless Steel Pipe or shutdown neutralization
  • Sulfidation and carburization: evaluate case by case; not a Si–Al carburization specialist
  • Chlorides: no Mo requirement in Table 1; not a substitute for ASME SA312 TP316L Stainless Steel Pipe in chloride immersion
  • Sigma phase: long holds near 1100–1650 °F can form sigma and reduce toughness

Versus sister grades: versus ASME SA312 TP309H Stainless Steel Pipe, the extra chromium and nickel raise oxidation resistance by roughly one temperature class for hotter furnace zones. Versus ASME SA312 TP310S Stainless Steel Pipe, the H grade is the SA-312 choice when creep rupture—not oxidation alone—governs life. Versus ASME SA312 UNS S31002 Stainless Steel Pipe, TP310H trades the ultra-low C/Si aqueous advantage for H-grade creep controls and the 75 ksi tensile floor. Polythionic acid stress corrosion during refinery shutdowns is a known concern for sensitized austenitics. Sulfur-bearing fuels can leave acidic condensates that attack sensitized grain boundaries when the unit cools—design for drainage, specify dry-out procedures, and consider whether a stabilized HCb grade is safer for units with frequent shutdowns.

Applications of SA312 TP310H Pipe

TP310H pipe is selected where austenitic stainless behavior, SA-312 product form, and H-grade carbon-floor plus grain-size practice are required for creep-range or highly stressed high-temperature duty at 310-level Cr/Ni. Typical application areas include:

Application area Why TP310H Selection note
Refinery heater tubes and transfer lines Creep allowables plus 310 oxidation resistance Polythionic acid precautions on shutdown
Petrochemical furnace pressure parts Carbon floor and coarse grain at 25Cr–20Ni Confirm code listing for S31009
Power and HRSG hot sections Elevated-temperature strength Compare with ASME SA312 TP304H Stainless Steel Pipe / ASME SA312 TP309H Stainless Steel Pipe
Industrial furnace pressure piping When oxidation and creep both matter at hotter zones Prefer ASME SA312 TP310S Stainless Steel Pipe if non-pressure / oxidation-limited
Radiant coils and reformer-adjacent piping 310-level scale resistance with H controls Document filler and WPS

For non-creep furnace parts prefer ASME SA312 TP310S Stainless Steel Pipe. For ultra-low C/Si aqueous oxidizing duty see ASME SA312 UNS S31002 Stainless Steel Pipe. For Nb-stabilized H-grade practice see ASME SA312 TP310HCb Stainless Steel Pipe. When 310-level Cr/Ni is not required, ASME SA312 TP309H Stainless Steel Pipe is often the more economic H-grade choice. The H-grade premium is justified when code allowables or owner specs require it—not for simple ducts or muffles. Many fired heaters use TP310H or TP310HCb tubes in the radiant or convection section when flue-gas oxidation and metal temperature push beyond 309H capability. Tube metal temperature, not firebox air temperature, governs the grade choice—confirm the design metal temperature against Section II Part D before ordering.

Weldability

TP310H is generally weldable by common austenitic fusion processes with suitable heat input, interpass control, and joint cleanliness. Higher carbon raises HAZ sensitization risk compared with ASME SA312 TP310S Stainless Steel Pipe, so wet corrosive service after welding needs a deliberate review. Typical processes used on this grade include:

  • GTAW (TIG) — preferred for root passes and thin-wall pipe where weld metal cleanliness and heat-input control matter
  • GMAW (MIG) — productive for fill and cap passes on thicker walls when procedures are qualified
  • SMAW — widely used for field girth welds with coated austenitic electrodes selected by agreement
  • SAW / FCAW — used where procedure qualification and joint design support them
  • Automatic orbital or mechanized GTAW — common for repetitive high-integrity girth joints

Filler metal and Table 6: no TP310H AWS class is asserted from the Table 6 extract used for this pack (ellipsis for the matching class). Filler selection is therefore by agreement and must be recorded on the WPS; seam repairs under clause 15 must identify the filler on the certificate. Industry practice often uses ER310 or E310-type consumables—that practice is guidance, not a Table 6 prescription. Mill longitudinal welds for WLD and HCW product are made without filler metal; Table 6 guidance applies to joining with filler, not to the mill autogenous weld.

Elevated-temperature WPSs may limit ferrite to reduce sigma risk in service. Moderate heat input and controlled interpass remain good practice. Dissimilar joints to carbon steel commonly use 309-type fillers for dilution control; to Cr-Mo alloy steels, nickel-base fillers are often specified. PWHT is not normally required; if specified, protect grain size. Qualify procedures to ASME Section IX—weld strength reduction factors in B31 codes may apply in the creep range. TP310H pipe is sometimes used as a transition spool between Cr-Mo headers and stainless tubes; in that case the WPS must address both joints, differential expansion, and carbon migration. Document the full joint design, not only the pipe grade.

Surface Finishes

Surface condition for SA312 TP310H pipe is stated on the purchase order. Typical mill finishes available from SHH STEEL supply include the following options:

  • Annealed and pickled (AP) — solution annealed, descaled in acid pickle or an equivalent process, producing a matte gray finish common for process and heater pipe
  • Blasted and pickled — often used for heavy-wall seamless where scale removal benefits from blast first
  • Bright annealed (BA) — annealed in a protective atmosphere to a brighter surface where the order allows; confirm the bright-anneal line still meets Table 2 temperature and grain-size rules
  • As-annealed light oxide — sometimes accepted for furnace parts by agreement when the protective scale will form in service anyway
  • Mechanically polished — grit or Ra-controlled polish on OD and/or ID when ordered; polishing does not replace solution annealing
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed for WLD/HCW product

Passivation after pickle or polish can be added when the end-user specification requires it. For high-temperature service the protective scale forms in operation; the delivered finish mainly affects inspection and cleanliness. Low-halide marking inks are preferred for high-temperature lines—avoid marking materials with low-melting metals or high halide content. For critical heater tubes, some owners specify a maximum residual scale after pickling or a visual cleanliness class; those are PO requirements beyond SA-312’s scale-free rule. End preparation (plain or beveled) should be ordered together with finish so that bevel faces and ID cleanliness meet the same acceptance language.

Inspection and Testing

Base inspection and testing for SA-312 TP310H pipe combines chemistry, mechanical, grain-size, and integrity checks. The following items form the usual acceptance package; supplementary requirements apply only when written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for TP310H (UNS S31009), including C 0.04–0.10%, Cr 24.0–26.0%, and Ni 19.0–22.0%
  • Product analysis — when ordered (Suppl. S1 / purchase-order language), using A480 Table A1.1 tolerances via A999 §6.3; useful to confirm the carbon floor on finished pipe
  • Grain size — ASTM No. 6 or coarser per heat-treatment lot (Table 5); same sampling as flattening
  • Tension test — Table 4 tensile, yield, and elongation on a lot basis (75/30 ksi minima)
  • Flattening test — or alternate bend where the standard permits (typically on 5% of the lot)
  • Hydrostatic test or nondestructive electric test — each length; manufacturer’s option unless the order fixes the method
  • Heat-treatment lot marking — heat number and lot identification on every length (clause 17)
  • Visual and dimensional check — against ordered NPS/schedule or OD/wall and the applicable tolerance clauses

Mill test certificates: EN 10204 3.1 is the standard documentation package from SHH STEEL supply. The certificate must report grain size and heat-treatment lot. EN 10204 3.2 or third-party witness (SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency) is arranged when specified and should be booked before final testing. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy the edition(s) named on the order.

Option Purpose
S1 product analysis Confirms carbon floor on finished pipe
S5 radiography Weld integrity on WLD pipe
S8 minimum wall Creep design on minimum wall
UT (by agreement) Volumetric check of heavy-wall seamless
PMI Confirms Cr/Ni; carbon needs OES or lab analysis

Power and refining inspectors often witness grain-size specimens and review anneal charts. Keep heat-treatment lot identity unbroken from mill through spool fabrication: when long lengths are cut, transfer heat and lot numbers to every piece. Receiving review should confirm carbon 0.04–0.10, grain size ≤6 (coarser), anneal ≥1900 °F with reheat, lot match, tensile ≥75 ksi, yield ≥30 ksi, elongation, and hydro or NDE method. Third-party inspectors should verify that the grade stencil reads TP310H / S31009—not merely “310H” or “25-20.”

Packaging and Shipping

Export and domestic shipments of SA312 TP310H pipe are packed for handling and ocean or land transport. Typical packing practices from SHH STEEL supply include:

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where needed to protect finish; cradles or individual supports for heavy headers
  • End caps / protectors — plastic or metal caps on plain or beveled ends to reduce damage and contamination during transit
  • Marking — durable marking of specification, grade (TP310H), heat number, heat-treatment lot, size (NPS or OD × wall / schedule), manufacturing type (SML / WLD / HCW), test letters, and mill identity as required by SA-312 and the purchase order
  • Export packing — waterproof wrapping or desiccant as agreed for polished or sensitive finishes; container stuffing photos on request; low-chloride inks on request

Receiving inspectors should compare stencil lot numbers against the MTC for every length before release to fabrication—missing lot fields are a red flag for “310H” paperwork that only dual-certified on chemistry. Segregate TP310H from ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 UNS S31002 Stainless Steel Pipe, ASME SA312 TP310Cb Stainless Steel Pipe, and ASME SA312 TP309H Stainless Steel Pipe on the packing list and in the yard so stencil mix-ups do not travel with the shipment. Long thin-wall heater tubes are vulnerable to bending in transit; ship them in rigid frames or with close-spaced saddles, and keep interiors dry and capped so chloride-bearing moisture does not stain or pit the surface before installation. Shipment docs typically include packing list, invoice, B/L or AWB, and MTC (3.1 or 3.2) with grain size and lot, plus origin/customs papers per Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe. For ASME SA312 TP310H / UNS S31009 we quote against the edition you name, report the full Table 1 window on the MTC—including C 0.04–0.10%, Cr 24.0–26.0%, and Ni 19.0–22.0%—and keep heat and heat-treatment-lot identity unbroken from melt through finished length. Receiving inspection then clears the heat against Table 1, Table 4, Table 5 grain size, and clause 6.2 reheat evidence rather than against a vague “310H” catalog sheet. We flag missing grain-size or lot fields on supplier MTCs before shipment, so non-conforming paperwork is caught at the mill—not at the fabricator. We also stay honest about Table 6: no AWS filler class is asserted for TP310H in the packed notes, so filler selection stays by agreement on the WPS. Dual 310S/310H options are flagged only when carbon, anneal, and grain-size rules actually allow—we do not pretend commodity 310S heats automatically meet H-grade controls.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for TP310H (S31009); grain size No. 6 or coarser per lot; no low-carbon 310S sold as 310H
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat and lot traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs standard with grain size and lot; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both requirements you name; dual 310S/310H when carbon, anneal, and grain-size rules allow
  • Related grades — sister 310-family and 309H SA-312 grades when projects buy matched high-temperature packages
  • Export packing — seaworthy bundles, end protectors, and durable grade/heat/lot/size/type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, finish, and any supplementary tests you name. Ask for dual 310S/310H options when the design temperature is near the creep boundary and carbon can sit in the overlap. Ask for S31002 when the corrosion case actually needs Si ≤0.15% and C ≤0.015%, and ask for TP310HCb when Nb stabilization plus H rules are both required. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 TP310H / UNS S31009 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for TP310H
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M Grade TP310H (UNS S31009); dual 310S/310H on request when rules allow
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Grain size, tension, flattening/bend, hydro or NDE per length; supplementary tests on order
Documents EN 10204 3.1 with grain size and lot; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

TP310H is a regular mill grade for heater and furnace pressure work at 310-level Cr/Ni, but reheat and grain-size controls mean lead times are often longer than for TP310S. Common sizes may be available from dual-certified stock when paperwork already carries grain-size reports; heavy walls and special OD/wall combinations are mill-order items. Enquiries should state the SA-312 edition, SML/WLD/HCW, NPS or OD×wall (nominal or minimum), length practice, finish, grain-size reporting, and any product-analysis or 3.2 requirements so mill slots align with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders. Combining heater-tube sizes into one heat improves chemistry consistency across a project. For dual-certified lots, confirm that grain size and lot marking still appear—chemistry alone does not make a heat TP310H. If the design temperature sits below the creep range and only oxidation matters, ask whether TP310S is preferred before finalising the PO.

FAQ

Is ASME SA312 the same as ASTM A312?
For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and mill test certificate so inspectors can verify the heat against the exact books you cited—do not assume a bare market grade stamp covers dual certification.
What is the UNS number for TP310H?
Table 1 lists TP310H as UNS S31009. Use that UNS on the purchase order, stencil, and MTC so chemistry, grain-size, and tensile rows stay unambiguous against neighboring 310 grades. When the project mixes plate and pipe, carry the same UNS language across forms, but still order pipe to SA-312/A312—not to the plate specification alone.
TP310H vs TP310S — which should I order?
TP310H requires C 0.04–0.10%, Table 5 grain size No. 6 or coarser, and clause 6.2 reheat; TP310S allows C ≤0.08% without those H rules and lists Mo ≤0.75%. Table 4 floors are both 75/30 ksi. Put the design-code grade and UNS on the datasheet and purchase order before you compare price—switching to TP310S after fabrication drawings are frozen usually means a material change notice, not a free mill substitution.
TP310H vs UNS S31002 — which should I order?
UNS S31002 tightens C to ≤0.015%, Si to ≤0.15%, Mo to ≤0.10%, adds N ≤0.10%, and carries a 73 ksi tensile floor without H-grade grain or reheat rules. TP310H uses C 0.04–0.10%, Si ≤1.00%, no Mo requirement, 75/30 ksi, plus Table 5 and clause 6.2. Order S31002 only when the ultra-low C/Si chemistry is required—H-grade 310 heats will never meet S31002. Put the design-code grade and UNS on the purchase order before you compare price.
TP310H vs TP310Cb — which should I order?
TP310Cb adds niobium stabilization (Nb 10×C min to 1.10% max) and Mo ≤0.75% on a C ≤0.08% base without Table 5 grain-size or clause 6.2 reheat mandates. TP310H has the H-grade carbon band and grain/reheat controls but no Nb requirement. Choose Nb stabilization or H-grade creep practice based on the corrosion and design case—they are not drop-in substitutes. Put the design-code grade and UNS on the purchase order before you compare price.
TP310H vs TP309H — which should I order?
Both are H grades with C 0.04–0.10%, Table 5 grain-size control, and clause 6.2 reheat. TP310H carries higher Cr (24–26%) and Ni (19–22%) than TP309H (22–24% Cr, 12–15% Ni) for hotter oxidation and creep service. Table 4 floors are both 75/30 ksi. Put the design-code grade and UNS on the datasheet and purchase order before you compare price—switching after fabrication drawings are frozen usually means a material change notice, not a free mill substitution.
Seamless vs welded TP310H — which is better?
Neither is universally better. Choose the manufacturing type your design code and datasheet allow; both are legitimate SA-312 forms when tested to the standard and both must still pass the clause 6.2 reheated anneal. State SML, WLD, or HCW on the purchase order and confirm the same letters on the pipe marking and MTC—mixing offers that differ only in manufacturing type is a common bid-evaluation trap.
Can you dual-certify SA312 / A312 TP310H?
Yes, when heat analysis, heat treatment, mechanical tests, grain size, lot marking, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the PO, and require the MTC to reference both books so receiving inspection can clear the heat without a second paperwork chase after shipment. Dual marking with TP310S needs the H-grade carbon band and grain-size rules as well—most commodity 310S heats will not qualify.
Hydrostatic test vs NDE — which do I get?
Each length is hydrotested or nondestructively electrically tested. Manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification locks one method, state it on the PO and verify the chosen test appears on the MTC for every length—silent mill option is not the same as an approved project method.
What heat treatment / anneal temperature applies to TP310H?
Table 2 lists 1900 °F [1040 °C] with TP309H, TP309HCb, and TP310HCb, cooling note D. Clause 6.2 reheat before quench and clause 17 lot marking both apply—direct quench after hot forming is not allowed. Delivery remains the solution-annealed condition required by SA-312 unless the edition and PO state otherwise. Cite the ordered edition’s Table 2 row on the enquiry so the mill does not apply a neighboring S-grade anneal practice by habit.
What Table 1 chemistry defines TP310H?
Table 1: C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 24.0–26.0%, Ni 19.0–22.0%; Mo has no requirement (UNS S31009). Values are melting-analysis limits from the ordered edition—do not invent tighter catalog windows. When product analysis is needed, order it explicitly (Suppl. S1 / PO language) rather than assuming ladle values alone will satisfy receiving inspection.
Does TP310H require grain-size control?
Yes. Table 5 requires ASTM No. 6 or coarser for TP310H / UNS S31009 on each heat-treatment lot—a result of No. 7 or finer fails even when chemistry and tensile pass. Confirm the grain-size number and lot identity on the MTC against the ordered edition of SA-312/A312, and put the same wording on the purchase order and receiving checklist so inspectors do not invent a tighter window or accept chemistry-only dual marks.

Conclusion

ASME SA312 TP310H (UNS S31009) is the creep-service 25Cr–20Ni grade in SA-312: carbon 0.04–0.10%, grain size ASTM No. 6 or coarser, reheated 1900 °F [1040 °C] anneal with clause 17 lot marking, and 75/30 ksi room-temperature minima. It is not a drop-in for TP310S—the H-grade carbon band and grain-size practice are mandatory for creep-range pressure parts, while oxidation-limited furnace duty often stays on the S grade. It is also not a substitute for UNS S31002 (ultra-low C/Si), TP310Cb (Nb stabilization without H rules), or TP309H (lower Cr/Ni H grade). Table 6 lists no AWS filler class (filler by agreement). Order the manufacturing type (SML/WLD/HCW), schedule or wall, finish, grain-size reporting, and any product analysis or supplementary tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X