ASME SA312 UNS S31266 Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 UNS S31266 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 UNS S31266 super-austenitic stainless steel pipe (no TP name) in SML, WLD and HCW, with Mo 5.2–6.2%, W 1.50–2.50% and N 0.35–0.60%, a 109/61 ksi Table 4 floor and a 2100 °F anneal, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
UNS S31266
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Dimensions
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 UNS S31266 Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe for high-temperature and general corrosive service. UNS S31266 sits in Table 1 with no TP designation, so it is ordered, marked, and certified by its UNS number alone. It is one of the most heavily alloyed super-austenitic grades in the standard: C ≤0.030%, Mn 2.00–4.00%, P ≤0.035%, S ≤0.020%, Si ≤1.00%, Cr 23.0–25.0%, Ni 21.0–24.0%, Mo 5.2–6.2%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%. The manganese, tungsten, and high nitrogen are specified ranges rather than residuals, and a certificate that leaves any of them out does not describe S31266.

That chemistry buys a much higher strength floor than the classic 6Mo grade. Table 4 sets 109 ksi [750 MPa] tensile and 61 ksi [420 MPa] yield as a single row with no thickness split, and elongation follows the general austenitic rule of 35% longitudinal / 25% transverse. Table 2 requires a solution anneal at 2100 °F [1150 °C] minimum with rapid cooling. Unlike many high-alloy rows, Table 6 does list fillers for S31266: ERNiCrMo-4, ERNiCrMo-10, ERNiCrMo-13, ERNiCrMo-14, and ERNiCrMo-17 (UNS N10276, N06022, N06059, N06686, N06200). It is not an H grade, so there is no carbon floor, no Table 5 grain-size rule, and no clause 6.2 reheat. In practice engineers specify S31266 for seawater, brine, and acidic chloride duty where they want 6Mo-class pitting resistance and also need a yield floor well above the 45 ksi of ASME SA312 UNS S31254 Stainless Steel Pipe.

SHH STEEL can supply ASME SA312 UNS S31266 stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) form. We quote ASME B36.19 schedules and special OD/wall by agreement, ship with EN 10204 3.1 mill test certificates that report every Table 1 element including Mn, N, Cu, and W, state the 109/61 ksi Table 4 results and the 2100 °F anneal, and offer dual SA-312/A312 marking when the heat analysis, heat treatment, mechanical tests, and marking satisfy both editions on the purchase order. Please confirm NPS, wall or schedule, finish, length practice, filler preference, and any product-analysis or corrosion-test extras when you enquire.

The market uses several names for this alloy, and the list below shows how they map to what should actually appear on the order and certificate. Proprietary trade names are useful for conversation, but only the UNS number carries the Table 1 and Table 4 rows.

  • ASME SA312 UNS S31266 / SA-312 Grade UNS S31266 — the marking language for ASME-code and dual-marked pipe
  • ASTM A312 UNS S31266 — same chemistry and tensile tables when the ASTM edition is referenced
  • “Super austenitic”, “6Mo+W”, or mill trade names — informal labels only; insist on UNS S31266 on stencil and MTC

Sister grades buyers often weigh against S31266 include ASME SA312 UNS S31254 Stainless Steel Pipe (lower Mn and N, no W, 98/95 ksi tensile and 45 ksi yield), ASME SA312 UNS S31277 Stainless Steel Pipe (Mo 6.5–8.0%, Ni 26–28%, 112/52 ksi, 40% elongation), and ASME SA312 TP316L Stainless Steel Pipe for duties that do not need super-austenitic alloying. None of them is a drop-in replacement, because each has its own Table 1 row, its own tensile floor, and its own anneal practice. Grade hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 recognizes three manufacturing routes for UNS S31266 pipe, and the route is a purchase-order decision driven by the design code, the size range, wall thickness, and how the owner wants the pipe inspected. The route never changes the chemistry: whichever way the pipe is made, the heat must still meet C ≤0.030%, Mn 2.00–4.00%, P ≤0.035%, S ≤0.020%, Si ≤1.00%, Cr 23.0–25.0%, Ni 21.0–24.0%, Mo 5.2–6.2%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%, and every length must still go through the solution anneal at 2100 °F [1150 °C] minimum before it is released.

  • Seamless (SML) — no welding at any stage. Seamless dominates high-pressure seawater and brine lines and thick-wall pressure parts where the project excludes welded pipe. The high Mo, W, and N content raises hot-working loads, so every seamless length must be solution annealed at 2100 °F minimum and rapidly cooled before release.
  • Welded (WLD) — automatic welding without filler metal, with the weld finished so the pipe meets dimensional and mechanical requirements after the final heat treatment. The strip or plate heat must itself carry the full UNS S31266 chemistry, so ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked to at least 35% reduction of wall and weld before the final anneal, again without filler in the longitudinal seam, with the weld radiographed before cold work. Order HCW when the project specifically wants that marking and the process controls SA-312 writes around it.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser accepts a system test in place of the hydrotest, and lots for mechanical testing follow clause 11.1. Clause 17 heat-treatment lot marking is not mandatory because S31266 is not an H grade, but seawater and offshore projects nearly always want heat and lot identity on the stencil anyway. Dual certification to UNS S31254 is generally not possible: the Mn, N, Cu, and W windows of the two grades do not overlap.

Mill availability is thinner than for ASME SA312 UNS S31254 Stainless Steel Pipe, and most S31266 is made to order from specialty melt campaigns, so lead times are longer than for commodity 316L or 310S. Enquire early with OD, wall, route, anneal evidence requirements, and filler preference, and group project sizes onto one heat where possible to keep chemistry consistent and meet mill minimums. HCW can help dimensional control on welded sizes because the cold work is followed by the full 2100 °F anneal.

Chemical Composition of SA312 UNS S31266

Two chemistry layers matter for UNS S31266. The melting (heat or ladle) analysis is mandatory for every heat under SA-312/A312 Table 1, while product analysis on finished pipe applies only when it is ordered through Supplementary Requirement S1 or purchase-order wording. Product tolerances are not printed in SA-312 itself; they come through ASTM A999/A999M §6.3 from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values and, when ordered, the product values, and never quotes tighter catalogue windows that the standard does not publish.

Melting analysis (heat / ladle analysis) — Table 1

The table below is the heat analysis for UNS S31266 from SA-312/SA-312M Table 1. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element. The grade column shows “…”, confirming there is no TP name.

Element UNS S31266 melting analysis
Carbon (C) ≤ 0.030
Manganese (Mn) 2.00 – 4.00
Phosphorus (P) ≤ 0.035
Sulfur (S) ≤ 0.020
Silicon (Si) ≤ 1.00
Chromium (Cr) 23.0 – 25.0
Nickel (Ni) 21.0 – 24.0
Molybdenum (Mo) 5.2 – 6.2
Nitrogen (N) 0.35 – 0.60
Copper (Cu) 1.00 – 2.50
Tungsten (W) 1.50 – 2.50

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.030 0.005 over ≤ 0.035
Manganese (Mn) 2.00 – 4.00 0.04 under / 0.05 over 1.96 – 4.05
Phosphorus (P) ≤ 0.035 0.005 over ≤ 0.040
Sulfur (S) ≤ 0.020 0.005 over ≤ 0.025
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 23.0 – 25.0 0.25 under / over 22.75 – 25.25
Nickel (Ni) 21.0 – 24.0 0.20 under / over 20.80 – 24.20
Molybdenum (Mo) 5.2 – 6.2 0.10 under / over 5.10 – 6.30
Nitrogen (N) 0.35 – 0.60 see gap note By agreement above 0.55% max band
Copper (Cu) 1.00 – 2.50 0.10 under / over 0.90 – 2.60
Tungsten (W) 1.50 – 2.50 0.05 under / over (to 2.00 band); above 2.00 by agreement 1.45 – 2.55 with gap flag

Source: SA-312 Table 1, UNS S31266. Mn is a range, not a maximum, and W is required. N max 0.60 exceeds the highest tabulated A480 N band (0.45–0.55 → 0.05), and W max 2.50 exceeds the tabulated W band to 2.00, so product N and W above those bands are by agreement.

Three elements separate S31266 from the 6Mo family on receipt. Manganese at 2–4% is intentional, unlike S31254 where Mn is capped at 1.00%; tungsten at 1.50–2.50% works with molybdenum on pitting resistance and has to be on the MTC; and nitrogen at 0.35–0.60% is far above the 0.18–0.25% of S31254 and is what drives the 61 ksi yield floor. Check those three values first, alongside Cr 23.0–25.0% and Ni 21.0–24.0%, because a handheld PMI gun that reports only Cr and Ni will not reliably tell these grades apart.

For product analysis, manganese uses the A480 over 1–3% (0.04) and over 3–6% (0.05) bands, and this pack applies 0.04 under / 0.05 over as a practical split across the range. Copper at 1.00–2.50% uses the over 1–3% band (0.10), and molybdenum at 5.2–6.2% uses the over 2–8% band (0.10). Nitrogen above 0.55% and tungsten above 2.00% fall outside the published A480 rows, so if you order product analysis, agree the method and acceptance limits for those two elements on the purchase order rather than leaving it to the lab to improvise.

Mechanical Properties of SA312 UNS S31266

Room-temperature tensile requirements for UNS S31266 come from SA-312 Table 4 and are summarized below. These are minimum release values for the lot, not typical values, and design allowables must always be taken from the governing code tables for UNS S31266 rather than from a neighbouring grade.

Property S31266
Tensile, min 109 ksi [750 MPa]
Yield, min 61 ksi [420 MPa]
Elongation 35% L / 25% T
Hardness No Table 4 max asserted

The 109/61 ksi row applies to every wall thickness, which is simpler than ASME SA312 UNS S31254 Stainless Steel Pipe, where Table 4 splits at 0.187 in. [5.00 mm]. Elongation is the general 35% longitudinal / 25% transverse requirement. Table 4 does not set a hardness maximum for S31266, so any hardness limit has to come from the piping class or the purchase order. Design allowables must come from the code tables listed for UNS S31266; borrowing S31254’s 45 ksi yield line would understate the grade, and borrowing anything from a leaner grade would be simply wrong.

Actual certificate results are usually above the minima, but the minima are what the design basis should use unless the mill has accepted higher guaranteed values in writing. Delivery is the solution-annealed condition, and a cold-worked final condition should not be assumed unless both the edition and the purchase order allow it. Because S31266 is fully austenitic, low-temperature toughness is normally favourable, but impact testing is a project extra when the specification asks for it, not part of the SA-312 base package.

Dimensions and Tolerances

Dimensional supply for SA312 UNS S31266 pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow SA-312 Table 3 as summarized below. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M.

  • Lengths — single random, double random, or cut-to-length on order
  • Cut lengths — typically no more than 1/4 in. [6 mm] over the ordered length unless the PO states a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face when the WPS is already frozen

Many seawater, brine, and chloride-process buyers order by OD × wall rather than NPS and schedule, which is fine as long as the enquiry says so clearly. Straightness, end finish, and length tolerance should be written into export orders so receiving inspection has an agreed acceptance basis instead of arguing after arrival. On thin schedules with threaded or socket-weld ends, check that the remaining wall is still adequate after the 12.5% under-tolerance. Jointers are not permitted unless the purchase order allows them, so cut-to-length programmes should include an allowance for fit-up scrap rather than expecting the mill to ship short pieces.

Equivalent Grades

UNS S31266 has no TP name in SA-312, and there is no simple one-to-one equivalent in other standards. Proprietary trade designations and EN numbers exist for similar W-bearing super-austenitic alloys, but any cross-reference has to be checked element by element against Table 1.

Designation Notes
SA-312 UNS S31266 Governing
EN / proprietary maps Recheck W, N, Mn, Cu

Dual certification is only valid when every Table 1 element, including W and Mn, passes, and when the tensile results meet the 109/61 ksi row. Treat EN or proprietary mappings as commercial shorthand rather than a substitution approval, because a heat can meet a trade-name window and still miss the S31266 nitrogen or tungsten range. Related SA-312 pages: ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 UNS S31277 Stainless Steel Pipe, ASME SA312 UNS S31050 Stainless Steel Pipe, and ASME SA312 TP316L Stainless Steel Pipe.

Heat Treatment and Delivery Condition

Table 2 requires UNS S31266 to be solution annealed at 2100 °F [1150 °C] minimum, followed by rapid cooling in water or by other rapid means. The high temperature is there to dissolve intermetallic phases such as sigma and chi that Mo-, W-, and N-rich alloys form readily, and rapid cooling keeps them from reforming as the pipe passes through the 1300–1800 °F range. A commodity 1900 °F cycle that is perfectly suitable for TP310S or TP316 is nonconforming for S31266, so make sure the mill’s anneal record and the MTC both quote the 2100 °F practice.

S31266 is not an H grade, so there is no clause 6.2 reheat, no Table 5 grain-size requirement, and no mandatory heat-treatment lot marking under clause 17. Bright annealing is possible by agreement where the mill can hold the temperature in a protective atmosphere for the size. If pipe is hot bent or formed after delivery, plan a full re-anneal at the same 2100 °F practice rather than a stress relief, since the intermetallic risk is the same for fittings and bends as for straight pipe.

Corrosion Resistance

SA-312 does not contain a corrosion table, so everything in this section is engineering commentary rather than a specification guarantee. With Cr 23–25%, Mo 5.2–6.2%, W 1.5–2.5%, and N 0.35–0.60%, S31266 sits at the top of the austenitic range for pitting and crevice resistance in chlorides. Buyers usually choose it for warm seawater, brines, bleach-plant filtrates, and acidic chloride process streams where 316L and even 904L-type alloys pit, and where the design also benefits from the 61 ksi yield floor.

  • Seawater and brine — a candidate where S31254 would also work on corrosion but higher yield allows thinner walls
  • Acidic chloride process — copper in the specified range helps in some reducing acid environments
  • Stress corrosion cracking — high nickel gives far better chloride SCC resistance than 300-series grades
  • Toughness — fully austenitic, with no duplex-type 475 °C embrittlement limit

Critical pitting and crevice temperatures depend on surface condition, weld quality, and the test method, so if the project needs them, write ASTM G48 or a CPT/CCT test into the purchase order as a contractual extra. Weld metal is usually the weak point in service, which is why Table 6 points to overalloyed Ni-Cr-Mo fillers rather than a matching composition. A poorly pickled weld or heat tint left in place will lose much of the alloy advantage, so post-weld cleaning deserves the same attention as the base-metal choice.

Applications of SA312 UNS S31266 Pipe

Applications for UNS S31266 pipe are driven by chloride severity combined with pressure. The table below summarizes where buyers typically specify the grade and what they should check before committing.

Application Why S31266 Note
High-pressure seawater / brine lines 109/61 ksi + Mo/W/N Confirm vs S31254 economics
Aggressive chloride process Super-austenitic envelope WPS using Table 6 fillers

Typical users include offshore seawater systems, desalination high-pressure lines, flue-gas desulphurization circuits, pulp bleach plants, and chemical plants handling chloride-bearing acids. Enquiries should say whether the owner has already frozen a Table 6 filler class, whether a post-weld anneal is required on fabricated spools, and whether G48 or CPT testing is part of acceptance. Where the corrosion duty is moderate and 61 ksi yield is not needed, ASME SA312 UNS S31254 Stainless Steel Pipe is often cheaper and easier to source, while very high Mo duty may point toward ASME SA312 UNS S31277 Stainless Steel Pipe.

Weldability

Table 6 assigns fillers for UNS S31266: ERNiCrMo-4, ERNiCrMo-10, ERNiCrMo-13, ERNiCrMo-14, and ERNiCrMo-17, corresponding to UNS N10276, N06022, N06059, N06686, and N06200. These are overalloyed nickel-chromium-molybdenum consumables, chosen so that the segregated weld metal still matches or exceeds the pitting resistance of the base pipe. Pick one class by agreement with the owner and freeze it on the WPS and PQR before production welding; do not improvise with 316L or other 300-series wire.

  • Qualify on S31266 — procedure qualification on the actual grade, not on S31254 or 316L coupons
  • Control heat input and interpass temperature — to limit intermetallic precipitation in the HAZ
  • Back-purge roots — to avoid ID oxidation and heat tint on corrosion-critical lines
  • Clean after welding — pickle or mechanically remove heat tint where the owner specification requires it

Mill longitudinal welds on WLD and HCW pipe are autogenous, made without filler, so Table 6 applies to fabrication joints rather than the mill seam. A post-weld solution anneal is not normally required for girth welds but may be specified for formed fittings or for very aggressive duty, and if it is, it must follow the 2100 °F practice. NDE extent for girth welds is a fabrication-code decision, separate from the hydro or electric test the mill applies to each length.

Surface Finishes

Surface condition for SA312 UNS S31266 pipe should be stated on the purchase order rather than left to mill default. For stainless pipe, embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts, so the finish is part of the material performance and not just appearance. The finishes we regularly quote for this grade are listed below.

  • Annealed and pickled (AP) — solution annealed at 2100 °F [1150 °C] minimum, then descaled in acid pickle or an equivalent process to a matte grey finish; the standard choice for process pipe
  • Blasted and pickled — common on heavy-wall seamless where blasting first makes scale removal more reliable
  • Bright annealed (BA) — annealed in a protective atmosphere where mill capability exists for the size; the anneal temperature still has to meet the Table 2 practice for UNS S31266
  • Mechanically polished — OD and/or ID polish to an agreed grit or Ra when ordered; polishing never replaces the solution anneal
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed on WLD and HCW product

For S31266 the pickle has to remove the Mo- and W-rich scale completely, because residual scale is a common crevice initiation site in chloride service. Passivation after pickling or polishing can be added when the end-user specification calls for it, even though SA-312 itself does not require it. If the project bans chloride-bearing marking inks, say so on the order; otherwise the mill will apply its normal stencil practice and ship its default AP finish.

Inspection and Testing

The base acceptance package for SA-312 UNS S31266 pipe combines chemistry, tensile testing, heat-treatment evidence, and a pressure or electrical integrity test on every length. The items below make up the usual package; supplementary requirements and project corrosion tests only apply when they are written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for UNS S31266: C ≤0.030%, Mn 2.00–4.00%, P ≤0.035%, S ≤0.020%, Si ≤1.00%, Cr 23.0–25.0%, Ni 21.0–24.0%, Mo 5.2–6.2%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%
  • Product analysis — when ordered (Suppl. S1 or PO wording), using A480 Table A1.1 tolerances via A999 §6.3; product N above 0.55% and W above 2.00% by agreement
  • Tension test — 109 ksi [750 MPa] tensile and 61 ksi [420 MPa] yield minimum, single row for all walls, plus 35% L / 25% T elongation on a lot basis
  • Flattening test — or the alternate bend test where the standard permits
  • Hydrostatic or nondestructive electric test — every length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD × wall, with UNS S31266 (no TP name exists) on every stencil

Mill test certificates: EN 10204 3.1 is the standard documentation from SHH STEEL supply. For S31266 the certificate must report all eleven Table 1 elements, with Mn, N, Cu, and W shown as actual values, together with 109/61 ksi tensile results, 35%/25% elongation, the hydro or NDE method, and a 2100 °F anneal statement. EN 10204 3.2 or third-party witness by SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency is arranged when specified, and it should be booked before final testing rather than after the heat has been released. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy both editions named on the order.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Receiving review should confirm Mn 2.00–4.00, Mo 5.2–6.2, N 0.35–0.60, Cu 1.00–2.50, and W 1.50–2.50 on the heat, plus Cr and Ni, the 109/61 ksi results, the elongation, and the anneal statement. Third-party inspectors should check that the stencil reads UNS S31266 rather than “6Mo” or a trade name. If several super-austenitic grades share a laydown area, use OES or XRF PMI that reports Mo and W, since Cr and Ni alone will not separate S31266 from S31254 or S31277.

Packaging and Shipping

Export and domestic shipments of SA312 UNS S31266 pipe are packed for handling and for ocean or land transport. The packing we normally apply is summarized below, and anything beyond it can be agreed on the order.

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where the finish needs protecting
  • End caps — plastic or metal caps on plain or beveled ends to keep out damage and contamination in transit
  • Marking — specification, grade (UNS S31266 (no TP name exists)), heat number, size, manufacturing type (SML / WLD / HCW), test letters, and mill identity as SA-312 and the purchase order require
  • Export protection — waterproof wrapping or desiccant as agreed for polished or bright-annealed finishes, with low-chloride inks on request

Segregate UNS S31266 from ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 UNS S31277 Stainless Steel Pipe, and ASME SA312 TP316L Stainless Steel Pipe on the packing list and in the yard, because mix-ups found after fabrication are expensive and the Mn, N, and W bands cannot be fixed by heat treatment. When S31266 ships with other stainless grades on the same vessel, use separate bundles and distinct tags, and have receiving inspectors check stencil heat numbers against the MTC for every length before release. Keep interiors dry and capped so chloride-bearing moisture cannot stain or pit the surface before installation. Shipping documents normally include the packing list, invoice, bill of lading or air waybill, and the 3.1 or 3.2 MTC with full Table 1 chemistry, plus origin and customs papers to suit the agreed Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe, and for SA312 UNS S31266 we quote against the edition you name rather than a generic catalogue sheet. We report every Table 1 element on the MTC—including Mn 2.00–4.00%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%—together with the 109/61 ksi Table 4 results and the 2100 °F anneal statement. Heat identity stays unbroken from the melt to the finished length, so receiving inspection can clear each heat against Table 1 and Table 4 without chasing paperwork after the pipe has arrived.

We check supplier certificates before shipment for missing tungsten or nitrogen values, wrong tensile row, and a missing anneal statement, so problems are caught at the mill rather than at the fabricator. We are also open about the limits of the published tolerances: product nitrogen above 0.55% and tungsten above 2.00% have no A480 row, and we put the agreed acceptance on the quotation instead of hiding it. When you ask about filler, we list the five Table 6 options and leave the final choice with your welding engineer.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for UNS S31266; Mn/N/Cu/W reported; 109/61 ksi confirmed; 2100 °F anneal stated; A480 N/W gaps disclosed
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs as standard with full Table 1 chemistry; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both editions you name
  • Related grades — ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 UNS S31277 Stainless Steel Pipe, and ASME SA312 TP316L Stainless Steel Pipe when a project buys a matched package
  • Export packing — seaworthy bundles, end protectors, and durable grade, heat, size, and type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, wall, finish, and any supplementary tests you name (S1, S5, S7, S8, S9). If the same project also needs plate or fittings, ask for coordinated heats so the chemistry lines up across product forms. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 UNS S31266 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for UNS S31266
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M UNS S31266 (no TP designation)
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension (109/61 ksi), flattening/bend, hydro or NDE per length; Mn/Mo/N/Cu/W on MTC; 2100 °F anneal stated; S1/S5/S7/S8/S9 and corrosion tests on order
Documents EN 10204 3.1 with full Table 1 chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

UNS S31266 is rarely held in distributor stock, so most orders are mill runs and lead times follow specialty melt schedules. Occasional remnant lengths from recent heats can cover small urgent quantities when sizes match, and it is worth asking before authorizing a new melt. Enquiries should state the SA-312 edition, UNS S31266 (no TP name exists), SML/WLD/HCW, NPS or OD × wall (and whether wall is nominal or minimum), length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirements, so mill slots line up with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders, and grouping project sizes onto one heat keeps the chemistry consistent while helping meet mill minimums without over-ordering.

FAQ

Is ASME SA312 the same as ASTM A312 for UNS S31266?
For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition, and S31266 has the same row in both. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and the mill test certificate so inspectors can verify the heat against the books you actually cited.
Why does UNS S31266 have no TP name?
Table 1 lists S31266 with an ellipsis in the TP column, so the unified number is the only grade identity. Put UNS S31266 on the purchase order, stencil, packing list, and MTC. Trade names and “6Mo” style labels are not grade designations and can easily be confused with UNS S31254 or S31277, which share similar commercial nicknames but have different Table 1 rows.
UNS S31266 vs UNS S31254 — which should I order?
S31254 is the classic 6Mo grade with Mo 6.0–6.5%, N 0.18–0.25%, no tungsten, and a 45 ksi yield floor. S31266 adds Mn 2–4% and W 1.5–2.5%, raises N to 0.35–0.60%, Cr to 23–25% and Ni to 21–24%, and lifts Table 4 to 109/61 ksi. Choose S31266 when the extra yield lets you save wall or when the owner already specifies it; otherwise S31254 is easier to source.
UNS S31266 vs UNS S31277 — which should I order?
S31277 pushes molybdenum to 6.5–8.0% with Ni 26–28%, N 0.30–0.40%, no tungsten, a 112/52 ksi floor, 40% longitudinal elongation, and a 2050 °F anneal. S31266 relies on Mo 5.2–6.2% plus W, has higher N and a higher 61 ksi yield, and anneals at 2100 °F. The chemistries do not overlap, so order the exact UNS your datasheet names.
Seamless vs welded UNS S31266 — which is better?
Neither is universally better. Seamless is typical for high-pressure and heavy-wall lines, while welded and HCW pipe are economical in larger diameters and thinner walls when seam quality and the full 2100 °F anneal are controlled. Choose the route your design code and datasheet allow, and confirm the same SML, WLD, or HCW letters on the marking and the MTC.
Can you dual-certify SA312 / A312 UNS S31266?
Yes, when the heat analysis, heat treatment, mechanical tests, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the purchase order and ask for the MTC to reference both books. Dual certification to UNS S31254 is a different matter and is generally impossible, because the Mn, N, Cu, and W windows conflict.
Hydrostatic test vs NDE — which do I get on S31266 pipe?
Each length is either hydrostatically tested or nondestructively electrically tested, and the manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification requires one method, state it on the PO and check that the chosen test appears on the MTC for every length. NPS 10 and larger may be marked NH only when you accept a system test.
What anneal temperature applies to UNS S31266?
Table 2 requires a solution anneal at 2100 °F [1150 °C] minimum with rapid cooling. That is higher than the 1900 °F used for many 300-series grades, because the Mo-, W-, and N-rich chemistry needs the higher temperature to dissolve sigma and chi phases. Ask for the anneal temperature on the MTC and reject paperwork that quotes a generic 1900 °F cycle.
What Table 1 chemistry defines UNS S31266?
Table 1 sets C ≤0.030%, Mn 2.00–4.00%, P ≤0.035%, S ≤0.020%, Si ≤1.00%, Cr 23.0–25.0%, Ni 21.0–24.0%, Mo 5.2–6.2%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%. These are melting-analysis limits. If you need product analysis, order it explicitly and agree acceptance for N above 0.55% and W above 2.00%, which have no A480 tolerance rows.
What are the Table 4 tensile requirements for UNS S31266?
Table 4 requires 109 ksi [750 MPa] tensile and 61 ksi [420 MPa] yield minimum as a single row with no wall-thickness split, with the general 35% longitudinal and 25% transverse elongation. Certificate values are usually higher, but design allowables should still come from the code tables for UNS S31266 unless the mill has accepted higher guaranteed values in writing.
What filler metal should I use to weld UNS S31266 pipe?
Table 6 lists ERNiCrMo-4, ERNiCrMo-10, ERNiCrMo-13, ERNiCrMo-14, and ERNiCrMo-17 (UNS N10276, N06022, N06059, N06686, N06200). Agree one class with the owner and freeze it on the WPS and PQR before production. Mill longitudinal seams on WLD and HCW pipe are autogenous, so Table 6 applies to fabrication joints rather than the mill weld.
How should I check UNS S31266 pipe on receipt?
Start with the elements that make S31266 unique: Mn 2.00–4.00%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%, then Cr, Ni, and Mo. Confirm 109/61 ksi results, elongation, the 2100 °F anneal statement, and the hydro or NDE method. PMI must read Mo and W, because Cr and Ni alone will not separate S31266 from neighbouring super-austenitic grades.

Conclusion

ASME SA312 UNS S31266 is a TP-less, tungsten-bearing super-austenitic pipe grade with C ≤0.030%, Mn 2.00–4.00%, Cr 23.0–25.0%, Ni 21.0–24.0%, Mo 5.2–6.2%, N 0.35–0.60%, Cu 1.00–2.50%, and W 1.50–2.50%, a single 109/61 ksi Table 4 floor with 35% L / 25% T elongation, and a 2100 °F [1150 °C] Table 2 anneal. Table 6 lists five ERNiCrMo filler options. It is not a drop-in for ASME SA312 UNS S31254 Stainless Steel Pipe or ASME SA312 UNS S31277 Stainless Steel Pipe, because each has its own Table 1 row and tensile floor. Order the manufacturing type, size and wall, finish, Mn/N/Cu/W reporting, anneal proof, filler class, and any product-analysis or corrosion tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X