ASME SA312 UNS S31050 Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 UNS S31050 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 UNS S31050 stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M), no TP designation: seamless (SML), welded (WLD) and heavily cold-worked (HCW); C ≤0.025%, Si ≤0.40%, Cr 24.0–26.0%, Ni 20.5–23.5%, Mo 1.60–2.60%, N 0.09–0.15%; Table 4 thickness-split 84/39 or 78/37 ksi; solution annealed. SHH STEEL supplies with EN 10204 3.1 MTCs.
Grade
UNS S31050
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 UNS S31050 Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. UNS S31050 appears in Table 1 with no TP designation—the grade column shows only an ellipsis—so the pipe is ordered, marked, and certified by UNS number alone. It is the low-carbon, low-silicon, nitrogen-alloyed 25Cr-22Ni-2Mo member of the 310 family, often called 310MoLN in trade: chromium 24.0–26.0%, nickel 20.5–23.5%, carbon ≤0.025%, silicon ≤0.40%, molybdenum 1.60–2.60%, nitrogen 0.09–0.15%, with tight phosphorus ≤0.020% and sulfur ≤0.015%. Commercially the same product may be labelled 310MoLN or 25-22-2 pipe, but those nicknames are not SA-312 grade names. For pressure piping and code work, cite UNS S31050 and the edition of SA-312 or A312 on the purchase order and on the mill test certificate—do not rely on a bare “310MoLN” market label.

The intentional molybdenum and nitrogen distinguish S31050 from ASME SA312 TP310S Stainless Steel Pipe / UNS S31008 (Mo ≤0.75% residual, no N requirement) and from ASME SA312 UNS S31002 Stainless Steel Pipe (Mo ≤0.10%, N ≤0.10% ceilings without a 2% Mo band). Table 4 tensile requirements are thickness-dependent: 84 ksi [580 MPa] / 39 ksi [270 MPa] for wall t ≤ 0.250 in. [6.35 mm], and 78 ksi [540 MPa] / 37 ksi [255 MPa] for thicker product. Elongation is special at 25% longitudinal (grouped with S32615)—not the usual 35% L family default. Heat treatment follows the Table 2 default of 1900 °F [1040 °C] (S31050 is not individually listed). It is not an H grade: there is no carbon floor, no Table 5 grain-size rule, and no clause 6.2 reheat requirement. Table 6 lists no AWS filler class for S31050, so filler selection is by agreement on the WPS—urea projects often freeze a matching consumable. The primary service niche is urea synthesis and other strongly oxidizing/carbamate environments where 316L urea grade is insufficient; calling it “310 stainless” on a urea PO is a specification error.

SHH STEEL can supply ASME SA312 UNS S31050 stainless steel pipe to the edition named on the enquiry, including seamless (SML), welded (WLD), and heavily cold-worked (HCW) routes; ASME B36.19 schedules and special OD/wall by agreement; EN 10204 3.1 mill test certificates that report the full Table 1 window—including C ≤0.025%, Si ≤0.40%, Mo 1.60–2.60%, and N 0.09–0.15%—plus the correct Table 4 thickness row; and dual SA-312/A312 marking when the heat analysis, heat treatment, mechanical tests, and marking satisfy both editions named on the purchase order. Confirm NPS, wall or schedule, finish, length practice, licensor extras, and any product-analysis or supplementary tests on enquiry.

Common commercial names and how they map to the ordered product are listed below—use the full SA-312/A312 designation plus UNS S31050 on the purchase order rather than market shorthand alone.

  • ASME SA312 UNS S31050 / SA-312 Grade UNS S31050 — preferred marking language for ASME-code and dual-marked pipe (no TP name exists)
  • ASTM A312 UNS S31050 — same grade tables for chemistry and tensile when the ASTM edition is referenced
  • UNS S31050 — unified numbering system identity used on MTCs, stencils, and cross-reference tables
  • 310MoLN / 25-22-2 — market shorthand; confirm Mo 1.60–2.60%, N 0.09–0.15%, C ≤0.025%, Si ≤0.40%, Ni 20.5–23.5%, and the thickness-split Table 4 floors before accepting any heat

UNS S31050 is not a drop-in for ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 UNS S31002 Stainless Steel Pipe, or ASME SA312 UNS S31254 Stainless Steel Pipe on a shared “310” or “urea stainless” market label—each has its own Table 1 row. Versus TP310S, S31050 raises Mo from a ≤0.75% residual to an intentional 1.60–2.60% band, requires N 0.09–0.15%, tightens C and Si, lifts Ni to 20.5–23.5%, and carries thickness-split tensile floors well above the 75/30 ksi TP310S row. Versus S31002, the design intents are opposite: S31002 keeps Mo and N as tight ceilings for nitric/oxidizing aqueous service, while S31050 alloys Mo and N for urea/carbamate duty. Versus S31254 (6Mo), S31050 has far less molybdenum and targets carbamate/oxidizing service rather than warm-seawater PREN. Dual marking with TP310S is usually impossible because Mo, N, Si, and tensile rows differ. Hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 defines three manufacturing routes that may be marked on finished UNS S31050 pipe. Selecting the route is a purchase-order decision driven by design code, size range, wall thickness, and inspection preference. It does not change the Table 1 chemistry of S31050—melting must still meet C ≤0.025%, Si ≤0.40%, Cr 24.0–26.0%, Ni 20.5–23.5%, Mo 1.60–2.60%, N 0.09–0.15%, P ≤0.020%, and S ≤0.015%—and every route must still pass through the solution anneal required by SA-312.

  • Seamless (SML) — no welding at any stage of manufacture. Seamless dominates high-pressure urea stripper and condenser tubing, thick-wall process pipe, and pressure parts when the project specification or licensor list excludes welded pipe. Hot-finished or cold-finished seamless must still be solution annealed to the Table 2 default practice and rapidly cooled.
  • Welded (WLD) — automatic welding without filler metal. The weld is finished so that the pipe meets dimensional and mechanical requirements after the final heat treatment required by SA-312. Welded S31050 may appear in lower-duty lines when the licensor permits it—confirm before bidding; the plate heat must itself meet S31050 chemistry including Mo and N bands.
  • Heavily cold-worked (HCW) — welded pipe that is cold worked to a reduction of area of wall and weld of at least 35% before the final anneal, again without filler metal in the longitudinal weld. The weld is radiographed before cold work. HCW is ordered when the buyer wants the HCW marking and the process controls written into SA-312 for that route.

Each finished length is hydrostatically tested or nondestructively electrically tested; the manufacturer may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser agrees to a system test in lieu of hydrotest. Lot definitions follow clause 11.1. Clause 17 heat-treatment lot marking is not mandatory for S31050 (it is not an H grade), but urea projects usually demand full heat and lot identity on the stencil for traceability through fabrication. Low silicon and controlled nitrogen need careful AOD/VOD practice so Mo and N land inside the intentional bands without drifting C or Si above their ceilings; grouping project sizes onto one heat improves consistency and often helps meet mill minimum order quantities that are higher than for commodity TP310S.

Lead times are typically longer than for ASME SA312 TP310S Stainless Steel Pipe because specialty melting capacity for Mo- and N-bearing 310MoLN-type heats is thinner and mills often treat S31050 as a made-to-order grade. Remnant fills from prior S31050 heats can still cut weeks off small urgent lots when sizes match. Plan procurement early for seamless heavy-wall urea sizes, and confirm route, edition, wall (because Table 4 is thickness-split), Mo/N reporting, and any licensor extras (Huey, corrosion coupons) before placing a mill order so the certificate matches the design basis. Where only hot oxidation matters and intentional Mo/N are not required, switch the conversation to ASME SA312 TP310S Stainless Steel Pipe; where warm seawater PREN governs, move to ASME SA312 UNS S31254 Stainless Steel Pipe instead of stretching a ~2% Mo heat into a 6Mo application.

Chemical Composition of SA312 UNS S31050

Two chemistry layers matter: melting (heat / ladle) analysis—mandatory per heat under ASME SA-312/ASTM A312 Table 1—and product analysis when ordered (Suppl. S1 / PO). SA-312/A312 defer product-analysis tolerances through ASTM A999/A999M §6.3 to ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle and, when ordered, product values—never unpublished tighter windows. On heat analysis, every certificate must show molybdenum 1.60–2.60% and nitrogen 0.09–0.15%; spot-check those two values first on receipt, together with C ≤0.025% and Si ≤0.40%, because they are the commercial traps that separate S31050 from ordinary TP310S.

Melting analysis (heat / ladle analysis) — Table 1

Heat analysis for UNS S31050 from ASME SA-312/SA-312M (ASTM A312/A312M) Table 1 is summarized below. Values are maximum unless a range is shown; ellipses (…) mean no requirement in the ordered edition. The grade column in Table 1 shows “…” (no TP designation).

Element UNS S31050 melting analysis
Carbon (C) ≤ 0.025
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.020
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 0.40
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 20.5 – 23.5
Molybdenum (Mo) 1.60 – 2.60
Nitrogen (N) 0.09 – 0.15

Source: SA-312 Table 1, UNS S31050 (TP column “…”). Si printed as 0.4 in table—treated as ≤0.40%. Footnote C style method-by-agreement practice for N determination should be settled on the PO.

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

When product analysis is ordered, apply A480 Table A1.1 tolerances to the Table 1 limits. Product Mo uses A480 bands that split across 2.00% (0.05 under/over for over 0.60 to 2.00; 0.10 under/over above 2.00)—this pack applies 0.05 under/over across the stated 1.60–2.60 range as a practical single band and flags the band split as UNCERTAIN.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.025 0.005 over ≤ 0.030
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.020 0.005 over ≤ 0.025
Sulfur (S) ≤ 0.015 0.005 over ≤ 0.020
Silicon (Si) ≤ 0.40 0.05 over ≤ 0.45
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 20.5 – 23.5 0.20 under / over 20.30 – 23.70
Molybdenum (Mo) 1.60 – 2.60 0.05 under / over 1.55 – 2.65
Nitrogen (N) 0.09 – 0.15 0.01 under / over 0.08 – 0.16

Vs TP310S: much lower C and Si; Mo raised to 1.60–2.60%; Ni raised to 20.5–23.5%; N required. Vs S31002: S31002 has Mo ≤0.10 and Si ≤0.15 without the 2% Mo / N band—different specialty. Nickel 20.5–23.5% uses the A480 20–30% Ni band (0.20 under/over). Chromium uses the 0.25 band. Nitrogen 0.09–0.15% must appear on the MTC; leaving N off the certificate is a nonconformance even when Mo is correct. Silicon at 0.40% max is easy to miss when mills quote commodity 310S Si ≤1.00%.

Element TP310S UNS S31002 UNS S31050 UNS S31254
C ≤ 0.08 ≤ 0.015 ≤ 0.025 ≤ 0.020
Si ≤ 1.00 ≤ 0.15 ≤ 0.40 ≤ 0.80
Ni 19.0 – 22.0 19.0 – 22.0 20.5 – 23.5 17.5 – 18.5
Mo ≤ 0.75 ≤ 0.10 1.60 – 2.60 6.0 – 6.5
N … ≤ 0.10 0.09 – 0.15 0.18 – 0.22
Primary niche Hot oxidation Nitric / low C-Si Urea / carbamate Seawater / 6Mo

The side-by-side table above shows why a shared “310” or “urea stainless” market label is dangerous: ASME SA312 TP310S Stainless Steel Pipe keeps Mo as a residual; ASME SA312 UNS S31002 Stainless Steel Pipe caps Mo and N for nitric duty; ASME SA312 UNS S31254 Stainless Steel Pipe pushes Mo to ~6% for chloride PREN; S31050 is the only row that combines intentional ~2% Mo with a required N band on the 25Cr–22Ni base for urea/carbamate service. Buyers who need only oxidation resistance should say so early; those needs usually push the conversation toward TP310S instead of forcing an S31050 melt when Mo and N bands are not required.

Mechanical Properties of SA312 UNS S31050

Room-temperature tensile requirements for UNS S31050 come from ASME SA-312/ASTM A312 Table 4 and are thickness-dependent. Intentional molybdenum and nitrogen raise the tensile floor well above the 75/30 ksi sister-310 defaults, but the floor drops when wall exceeds 0.250 in. [6.35 mm]. Always match the tensile row to actual ordered wall—a certificate showing only 84/39 for 0.300 in. wall is nonconforming. Actual mill values are often higher than the minima, but design still uses Table 4 for ambient checks and the governing code allowables for elevated-temperature design of S31050.

Wall thickness t Tensile min Yield min
t ≤ 0.250 in. [6.35 mm] 84 ksi [580 MPa] 39 ksi [270 MPa]
t > 0.250 in. [6.35 mm] 78 ksi [540 MPa] 37 ksi [255 MPa]

Source: SA-312 Table 4 for UNS S31050. Elongation: 25% longitudinal (Table 4 note: S31050 with S32615). Transverse elongation is not given a separate Table 4 number for this pair in the extract. Hardness: no Table 4 maximum asserted here. No Table 5 grain-size requirement (not an H grade).

Elongation 25% L is intentionally lower than the 35% family default; do not fail a heat for “only” 28% when 25% is the Table 4 minimum for S31050. Base mechanical testing includes tension on a lot basis and flattening (or the alternate bend where the standard permits) typically on 5% of the lot, plus hydrotest or NDE on every length. Elevated-temperature tensile and rupture tests are purchase-order options, not base SA-312 requirements. For pressure-retaining parts, use the governing Section II Part D or project-code allowables for UNS S31050 where listed—do not copy TP310S / S31008 allowable-stress tables into an S31050 calculation package, and do not mix thin-wall and heavy-wall Table 4 rows in the same release. Annealed S31050 retains austenitic toughness to low temperature; impact testing is a construction-code or PO matter, not an SA-312 base test.

Although Table 4 has no hardness maximum, fabricators sometimes set a Rockwell limit for bending or expanding—put any such limit on the PO and verify it on the MTC if required. Like other 310 grades, S31050 hardens when cold worked; intermediate anneals may be needed for severe forming, and those anneals must still meet the Table 2 default practice. After long high-temperature service, expect reduced room-temperature ductility from carbides and possible sigma—evaluate before cold repair. For creep-range service without the Mo/N urea chemistry case, see ASME SA312 TP310H Stainless Steel Pipe rather than stretching an S31050 heat into an H-grade application.

Dimensions and Tolerances

Dimensional supply for SA312 UNS S31050 pipe follows ASME B36.19 schedules for common NPS/schedule combinations, with special OD and wall by agreement when urea exchangers, strippers, or condensers need a non-standard section. Outside-diameter variations follow ASTM A999/A999M; wall-thickness variations follow SA-312 Table 3 as summarized below. Wall thickness also drives the Table 4 tensile row—state ordered wall clearly, and state whether wall is nominal or minimum (Suppl. S8) on the purchase order so the mill does not ship the wrong interpretation.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M.

  • Lengths — NPS 1/8–8 commonly furnished up to 24 ft unless otherwise agreed; SRL, DRL, or cut-to-length on order
  • Cut lengths — typically ≤1/4 in. [6 mm] over unless the PO states a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face when the WPS is already frozen

Urea and oxidizing-chemical industries often order by OD × wall rather than by NPS/schedule. Special OD × wall combinations are common in strippers and condensers where ASME B36.19 schedules leave gaps—state whether wall is minimum or nominal before the mill rolls, because the Table 4 thickness split makes wall a mechanical as well as a dimensional decision. Straightness, end finish, and length tolerance should be written explicitly for export projects so receiving inspection has a clear acceptance basis. For socket-weld or threaded ends on thin schedules, confirm the wall remains adequate after the 12.5% under-tolerance. Jointers are not permitted unless the purchase order expressly allows them; cut-to-length programmes should include an allowance for fit-up scrap so the mill does not ship under-length pieces.

Equivalent Grades

Equivalence for UNS S31050 is primarily an ASME/ASTM identity question. The governing pipe designation is ASME SA-312 UNS S31050 (no TP name); market names and plate counterparts must be mapped back to that row before a mill is asked to dual-mark or substitute.

Designation Notes
ASME SA-312 UNS S31050 Governing pipe grade (no TP designation)
ASTM A312 UNS S31050 Same Table 1 / Table 4 when the ASTM edition is referenced
310MoLN (trade) Confirm full Table 1 incl. Si ≤0.40, Mo 1.60–2.60, and N 0.09–0.15
EN 1.4466 / X1CrNiMoN25-22-2 approx. Engineering map—recheck every limit before dual certification
SA-240 / A240 S31050 Plate/sheet counterpart when listed—not a pipe specification by itself

Related SA-312 grades on steelspecs.com: ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 UNS S31002 Stainless Steel Pipe, ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 TP310H Stainless Steel Pipe, ASME SA312 TP310Cb Stainless Steel Pipe, ASME SA312 TP309S Stainless Steel Pipe. Versus ASME SA312 TP310S Stainless Steel Pipe, S31050 is the Mo- and N-bearing urea-grade row—not a synonym. Versus ASME SA312 UNS S31002 Stainless Steel Pipe, the design intents are opposite (intentional Mo/N vs tight Mo/N ceilings). Versus ASME SA312 UNS S31254 Stainless Steel Pipe, S31050 has far less Mo and targets carbamate/oxidizing service rather than warm seawater. Always re-check C, Si, Mo, N, Ni, and the thickness-split tensile row against Table 1 / Table 4 before accepting a substitute heat, and do not treat “310MoLN” and “TP310S” as automatically interchangeable on the purchase order.

Heat Treatment and Delivery Condition

UNS S31050 is not individually listed in Table 2, so the grade follows the Table 2 default of 1900 °F [1040 °C] minimum with rapid cooling. Because S31050 is not an H grade, clause 6.2 reheat language does not apply and direct quench after hot forming is accepted the way it is for non-H grades such as ASME SA312 TP310S Stainless Steel Pipe. There is no Table 5 grain-size rule. Delivery remains the solution-annealed condition required by SA-312 unless the ordered edition and purchase order state otherwise.

  • Solution anneal ≥1900 °F [1040 °C] — Table 2 default; rapid cool
  • No Table 5 grain-size rule — not an H grade
  • Clause 17 lot marking — not mandatory for S31050; urea projects usually request heat/lot identity
  • Free of scale and exogenous iron — descaled / pickled or equivalent as ordered
  • Bright anneal / high-cleanliness finish — available on request when the end-user or licensor specification requires a scale-free surface for urea/carbamate service

Annealing at the Table 2 default dissolves residual carbides and restores corrosion resistance after hot work; rapid cooling is required. Bright annealing under hydrogen or vacuum can deliver a scale-free surface preferred for clean urea service; pickled finishes are acceptable when fully rinsed. Owner-specified stabilization or post-fabrication heat treatments are purchaser requirements, not SA-312 base rules—write temperature and time on the PO if needed. Cite the ordered edition’s Table 2 default practice on the enquiry so the mill does not apply a neighboring H-grade reheat habit, or a different anneal temperature, to an S31050 heat by mistake.

Corrosion Resistance

UNS S31050 is aimed at urea / carbamate and strongly oxidizing services. Low carbon, controlled silicon, intentional molybdenum 1.60–2.60%, and nitrogen 0.09–0.15% support resistance where 316L urea grade is marginal. SA-312 itself publishes no corrosion rates—licensor specifications (Stamicarbon, Saipem, and others) govern urea plants and may add Huey tests or other corrosion trials beyond SA-312; those extras are contractual, not Table 4.

  • Urea strippers / condensers — primary niche; validate grade list and any corrosion coupons with the process licensor
  • Nitric / oxidizing acids — often considered; engineer confirmation of concentration and temperature is required
  • Intergranular attack — C ≤0.025% limits chromium-carbide sensitization in weld heat-affected zones relative to higher-carbon 310
  • Seawater chlorides — Mo ~2% is below 6Mo PREN; use ASME SA312 UNS S31254 Stainless Steel Pipe for warm seawater rather than stretching S31050
  • Sigma-phase risk — high-Cr grades can still form sigma after long intermediate-temperature exposure; design dwell times accordingly

Verify intergranular resistance with Suppl. S7 (ASTM A262 Practice E) when the service case is critical, and use Suppl. S9 weld-decay testing when welded pipe must demonstrate comparable weld and base-metal loss rates. Neither test is automatic—order them when the corrosion case needs proof. Compared with ASME SA312 TP310S Stainless Steel Pipe, S31050 trades commodity availability for intentional Mo/N chemistry and thickness-split tensile floors aimed at urea duty. If only hot oxidation matters and Mo/N bands are not required, TP310S is usually the more available and economical choice; specify S31050 only when the urea/carbamate chemistry is actually needed.

Applications of SA312 UNS S31050 Pipe

Buyers typically select UNS S31050 when the project already wants 310-level chromium with intentional molybdenum and nitrogen for urea synthesis or other strongly oxidizing/carbamate service that ordinary TP310S (Mo ≤0.75% residual, no N requirement) cannot answer cleanly. The grade earns its keep by protecting both high-pressure urea piping integrity and welded HAZ behaviour under low carbon and controlled silicon.

Application Why S31050 Note
Urea plant high-pressure piping 310MoLN chemistry (Mo + N) Follow licensor grade list
Urea strippers / condensers Low C/Si + intentional Mo/N Often seamless; confirm wall for Table 4 row
Oxidizing chemical lines Low C/Si + Mo/N Confirm concentration / temperature
Carbamate service Designed urea-grade alloy Not a seawater 6Mo substitute
Welded process piping needing as-welded IGC resistance C ≤0.025% limits HAZ sensitization Order S7 if proof is required

If only hot oxidation matters, see ASME SA312 TP310S Stainless Steel Pipe—it is usually more available and carries a simpler single tensile row. If warm seawater or high PREN governs, see ASME SA312 UNS S31254 Stainless Steel Pipe rather than forcing a ~2% Mo heat into a 6Mo design basis. If ultra-low C/Si nitric duty without intentional Mo is the driver, compare ASME SA312 UNS S31002 Stainless Steel Pipe. Typical enquiry packages list design pressure, urea service duty, wall (for the Table 4 thickness split), whether field welding will be performed, and whether licensor corrosion trials or S7 are mandatory—adding those extras early avoids late schedule slips. When replacing TP310S with S31050 in an existing unit, review weld procedures, filler selections, and receiving checklists for Mo and N—the base-metal change alone does not update the WPS.

Weldability

UNS S31050 welds with GTAW, GMAW, SMAW, and SAW using low-carbon austenitic practices familiar to fabricators of other 310 grades. Low carbon improves as-welded intergranular resistance in the heat-affected zone; intentional Mo and N mean procedures should be qualified on S31050 chemistry rather than assumed from a TP310S PQR. Mill WLD and HCW longitudinal welds are autogenous (no filler); Table 6 guidance applies to joining with filler, not to the mill seam.

Filler and Table 6: S31050 is listed with AWS class “…”—no classification is given in the extracted edition. Filler selection is by agreement and must be recorded on the WPS. Urea projects often freeze a specific matching consumable so deposited metal stays close to the Mo/N intent; do not improvise from 316L or commodity 310 stock. Freeze the AWS (or EN) class on the WPS/PQR before production welds.

  • Moderate heat input; clean joints free of oil, paint, and exogenous iron
  • Argon shielding and backing gas for GTAW root passes
  • Remove heat tint; pickle or passivate when urea/carbamate service follows
  • Mill seams autogenous; clause 15 repairs must identify any filler used

Qualify welding procedures to ASME Section IX on S31050 material (or on a heat with matching Mo and N). A PQR on ASME SA312 TP310S Stainless Steel Pipe without review can miss the Mo/N effect on weld-pool behaviour and the need for a matching filler. Dissimilar welds of S31050 to carbon steel still commonly use 309-type fillers for dilution control; if the weld must also resist carbamate attack, decide whether the filler itself needs matching Mo/N or whether a barrier butter layer is required, and capture that decision in the WPS. After high-temperature service exposure, clean thoroughly before repair welding and follow producer guidance for 310MoLN-type repair practice.

Surface Finishes

Surface condition for SA312 UNS S31050 pipe is stated on the purchase order. Cleanliness matters for urea and carbamate service—embedded free iron and chloride-bearing residues defeat the chemistry advantage the buyer paid for. Typical mill finishes available from SHH STEEL supply include the following options:

  • Annealed and pickled (AP) — solution annealed, descaled in acid pickle or an equivalent process, producing a matte gray finish common for process pipe
  • Blasted and pickled — often used for heavy-wall seamless where scale removal benefits from blast first
  • Bright annealed (BA) — annealed in a protective atmosphere to a brighter, scale-free surface preferred for many urea services where mill capability exists for the size; temperature must still meet the Table 2 default
  • High-cleanliness for urea service — by agreement when licensor or end-user specs demand extra cleanliness beyond standard pickle
  • Mechanically polished — grit or Ra-controlled polish on OD and/or ID when ordered; polishing does not replace solution annealing
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed for WLD/HCW product

Passivation after pickle or polish can be added when the end-user specification requires it—often specified for urea/carbamate service even though SA-312 itself does not mandate passivation. Electropolishing is available for special clean-service needs by agreement. Use low-halide marking inks when the project specification bans chloride-bearing inks. State finish, passivation, and any ink restriction on the order so the mill does not ship a default AP finish into a BA or high-cleanliness requirement.

Inspection and Testing

Base inspection and testing for SA-312 UNS S31050 pipe combines chemistry (especially C, Si, Mo, and N), mechanical (correct thickness row and 25% elongation), and integrity checks. The following items form the usual acceptance package; supplementary requirements and licensor extras apply only when written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for UNS S31050, including C ≤0.025%, Si ≤0.40%, Cr 24.0–26.0%, Ni 20.5–23.5%, Mo 1.60–2.60%, N 0.09–0.15%, P ≤0.020%, and S ≤0.015%
  • Product analysis — when ordered (Suppl. S1 / purchase-order language), using A480 Table A1.1 tolerances via A999 §6.3; Mo product band split across 2.00% flagged as UNCERTAIN (pack uses 0.05 under/over)
  • Tension test — Table 4 tensile and yield on the correct thickness row (84/39 or 78/37 ksi) plus 25% longitudinal elongation on a lot basis
  • Flattening test — or alternate bend where the standard permits (typically on 5% of the lot)
  • Hydrostatic test or nondestructive electric test — each length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD/wall and the applicable tolerance clauses; confirm UNS S31050 (not a TP name) on every stencil

Mill test certificates: EN 10204 3.1 is the standard documentation package from SHH STEEL supply. The certificate must report molybdenum 1.60–2.60%, nitrogen 0.09–0.15%, silicon ≤0.40%, and carbon ≤0.025% so receiving inspection can verify the commercial traps that separate S31050 from TP310S; the correct Table 4 thickness row and 25% elongation must also appear. EN 10204 3.2 or third-party witness (SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency) is arranged when specified and should be booked before final testing. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy the edition(s) named on the order.

Option Purpose
S1 product analysis Confirms C, Si, Mo, N, and other elements on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal (also affects Table 4 row)
S9 weld decay Compares weld and base-metal loss rates
Licensor extras Huey / corrosion coupons when urea licensor specs require them

Receiving review should confirm C ≤0.025, Si ≤0.40, Mo 1.60–2.60, N 0.09–0.15, Cr 24–26, Ni 20.5–23.5, P ≤0.020, S ≤0.015, the correct thickness-row tensile/yield, 25% elongation, and hydro or NDE method. Third-party inspectors should verify that the grade stencil reads UNS S31050—not merely “310MoLN,” “310S,” or “310SS.” PMI by OES on a sample length is a useful receiving check when multiple 310 variants share a laydown area; guns that only report Cr and Ni are insufficient to release S31050 stock. Mechanical tests follow clause 11.1 lot rules; for specialty Mo/N heats made in short campaigns, a lot may be only a few dozen lengths, so base test frequency is effectively high.

Packaging and Shipping

Export and domestic shipments of SA312 UNS S31050 pipe are packed for handling and ocean or land transport. Typical packing practices from SHH STEEL supply include:

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where needed to protect finish; cradles or individual supports for heavy headers
  • End caps / protectors — plastic or metal caps on plain or beveled ends to reduce damage and contamination during transit
  • Marking — durable marking of specification, grade (UNS S31050—no TP name), heat number, size (NPS or OD × wall / schedule), manufacturing type (SML / WLD / HCW), test letters, and mill identity as required by SA-312 and the purchase order
  • Export packing — waterproof wrapping or desiccant as agreed for polished or bright-annealed finishes; container stuffing photos on request; low-chloride inks on request

Segregate UNS S31050 from ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 UNS S31002 Stainless Steel Pipe, and ASME SA312 UNS S31254 Stainless Steel Pipe on the packing list and in the yard so stencil mix-ups do not travel with the shipment—mix-ups discovered after fabrication are expensive because Mo and N bands cannot be converted by heat treatment alone. Shipping S31050 in crates labeled only “310SS” or “310MoLN” without the UNS risks confusion with commodity TP310S. When S31050 ships with TP310S on the same vessel, use separate bundles and distinctly colored tags. Receiving inspectors should compare stencil heat numbers against the MTC for every length and verify that Mo 1.60–2.60%, N 0.09–0.15%, and the correct Table 4 thickness row are reported before release to fabrication. Keep interiors dry and capped so chloride-bearing moisture does not stain or pit the surface before installation. Shipment docs typically include packing list, invoice, B/L or AWB, and MTC (3.1 or 3.2) with full Table 1 chemistry reported, plus origin/customs papers per Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe. For ASME SA312 UNS S31050 we quote against the edition you name, report the full Table 1 window on the MTC—including C ≤0.025%, Si ≤0.40%, Mo 1.60–2.60%, N 0.09–0.15%, P ≤0.020%, and S ≤0.015%—and keep heat identity unbroken from melt through finished length. Receiving inspection then clears the heat against Table 1 and the correct Table 4 thickness row rather than against a vague “310MoLN” catalog sheet. We flag missing Mo or N fields, Si above 0.40%, wrong tensile row for wall, or absent 25% elongation on supplier MTCs before shipment, so non-conforming paperwork is caught at the mill—not at the fabricator. We also stay honest about the Mo product-analysis band split across 2.00% and about Table 6 (no AWS filler class listed), so those items stay closed by agreement on the quotation and WPS.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for UNS S31050; Mo/N/Si/C reported and checked; correct 84/39 or 78/37 row; no commodity TP310S sold as 310MoLN / S31050
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs standard with full Table 1 chemistry including Mo and N; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both requirements you name
  • Related grades — sister 310-family and specialty SA-312 grades (ASME SA312 TP310S Stainless Steel Pipe / ASME SA312 UNS S31002 Stainless Steel Pipe / ASME SA312 UNS S31254 Stainless Steel Pipe) when projects buy matched packages
  • Export packing — seaworthy bundles, end protectors, and durable UNS/heat/size/type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, wall (for the Table 4 split), finish, licensor extras, and any supplementary tests you name (S1, S5, S7, S8, S9). Ask for coordinated plate-and-pipe heats when a project needs matching Mo/N levels across SA-240 and SA-312 forms. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 UNS S31050 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for UNS S31050
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M UNS S31050 (no TP designation)
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or high-cleanliness by agreement
Testing Tension (correct t row), flattening/bend, hydro or NDE per length; Mo/N/Si/C on MTC; S1/S5/S7/S8/S9 and licensor extras on order
Documents EN 10204 3.1 with full Table 1 chemistry reported; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

UNS S31050 is less common in distributor stock than TP310S, so mill-run orders are typical and lead times track specialty melt schedules for Mo- and N-bearing 310MoLN-type heats. Common sizes may occasionally be available from remnant lengths of prior S31050 heats; heavy walls and special OD/wall combinations for urea exchangers are mill-order items. Enquiries should state the SA-312 edition, UNS S31050 (not a bare “310MoLN”), SML/WLD/HCW, NPS or OD×wall (nominal or minimum—wall drives Table 4), length practice, finish, Mo/N reporting expectation, licensor extras, and any product-analysis or 3.2 requirements so mill slots align with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders. Combining project sizes into one heat improves Mo/N consistency and helps meet mill minima without over-ordering. For urgent small quantities, ask about remnant lengths from recent S31050 heats before authorizing a new melt—remnants can cut weeks from the schedule when sizes match.

FAQ

Is ASME SA312 the same as ASTM A312?
For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and mill test certificate so inspectors can verify the heat against the exact books you cited—do not assume a bare market grade stamp covers dual certification for UNS S31050.
What is the UNS number for this grade?
Table 1 lists S31050 as the unified number for this pipe grade, with an ellipsis in the TP column—there is no separate TP designation. Cite UNS S31050 on the purchase order, stencil, packing list, and mill test certificate so chemistry and tensile rows cannot be confused with a neighboring 310 grade that shares a “310MoLN” commercial nickname.
UNS S31050 vs TP310S — which should I order?
TP310S (UNS S31008) is the workhorse 310 grade with C ≤0.08%, Si ≤1.00%, Mo ≤0.75% residual, no N requirement, and 75/30 ksi floors. UNS S31050 adds intentional Mo 1.60–2.60% and N 0.09–0.15%, tightens C and Si, raises Ni to 20.5–23.5%, and carries thickness-split 84/39 or 78/37 ksi floors with 25% elongation. Order S31050 when urea/carbamate Mo+N chemistry is required—do not treat “310MoLN” and TP310S as interchangeable. Put the design-code grade and UNS on the purchase order before you compare price.
UNS S31050 vs UNS S31002 — which should I order?
S31002 is the ultra-low-carbon, low-silicon 310 UNS with Mo ≤0.10% and N ≤0.10% ceilings aimed at nitric/oxidizing aqueous service and a 73/30 ksi floor. S31050 is the opposite specialty: intentional Mo 1.60–2.60% and N 0.09–0.15% for urea/carbamate duty, with thickness-split tensile floors. They solve different problems—do not substitute one for the other on a shared “310” label. Put the design-code grade and UNS on the purchase order before you compare price.
UNS S31050 vs UNS S31254 — which should I order?
S31254 is a 6Mo superaustenitic (Mo ~6%, high N) aimed at warm seawater and high-PREN chloride service. S31050 carries only ~2% Mo and targets urea/carbamate and oxidizing duty on a 25Cr–22Ni base. They are not drop-in substitutes—choose by corrosion case, not by a shared “specialty stainless” nickname. Put the design-code grade and UNS on the purchase order before you compare price.
Seamless vs welded UNS S31050 — which is better?
Neither is universally better. Choose the manufacturing type your design code, datasheet, and urea licensor allow; both are legitimate SA-312 forms when tested to the standard, and both must still meet S31050 chemistry including Mo 1.60–2.60% and N 0.09–0.15%. High-pressure urea piping is almost always seamless. State SML, WLD, or HCW on the purchase order and confirm the same letters on the pipe marking and MTC—mixing offers that differ only in manufacturing type is a common bid-evaluation trap.
Can you dual-certify SA312 / A312 UNS S31050?
Yes, when heat analysis (including Mo 1.60–2.60% and N 0.09–0.15%), solution anneal, mechanical tests on the correct Table 4 thickness row, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the PO, and require the MTC to reference both books so receiving inspection can clear the heat without a second paperwork chase after shipment. Dual marking with TP310S is usually impossible because Mo, N, Si, and tensile rows differ.
Hydrostatic test vs NDE — which do I get?
Each length is hydrotested or nondestructively electrically tested. Manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification locks one method, state it on the PO and verify the chosen test appears on the MTC for every length—silent mill option is not the same as an approved project method for UNS S31050.
What heat treatment / anneal temperature applies to UNS S31050?
Table 2 default 1900 °F [1040 °C] minimum with rapid cooling—S31050 is not individually listed. It is not an H grade, so clause 6.2 reheat and Table 5 grain size do not apply; direct quench after hot forming is accepted. Delivery remains the solution-annealed condition required by SA-312 unless the edition and PO state otherwise. Cite the ordered edition’s Table 2 default on the enquiry so the mill does not apply a neighboring grade’s anneal practice by habit.
What Table 1 chemistry defines UNS S31050?
Table 1: C ≤0.025%, Mn ≤2.00%, P ≤0.020%, S ≤0.015%, Si ≤0.40%, Cr 24.0–26.0%, Ni 20.5–23.5%, Mo 1.60–2.60%, N 0.09–0.15% (no TP designation). Values are melting-analysis limits from the ordered edition—do not invent tighter catalog windows. When product analysis is needed, order it explicitly (Suppl. S1 / PO language) and note the Mo A480 band split across 2.00% (this pack applies 0.05 under/over as a practical single band).
What are the Table 4 tensile requirements for UNS S31050?
Table 4 is thickness-dependent: t ≤ 0.250 in. [6.35 mm] uses 84 ksi [580 MPa] / 39 ksi [270 MPa]; thicker product uses 78 ksi [540 MPa] / 37 ksi [255 MPa]; elongation is 25% longitudinal (with S32615). Always match the row to ordered wall—do not release heavy wall to the thin-wall 84/39 floor alone. Design to Table 4 unless the mill has accepted higher guaranteed values in writing. Actual MTC readings are often above the floor; still use Table 4 minima for allowable-stress calculations unless the PO states higher guarantees.
What filler metal should I use to weld UNS S31050 pipe?
Table 6 lists no AWS class for S31050—filler by agreement. Urea projects often freeze a matching Mo/N-bearing consumable so deposited metal stays close to the base-metal intent; do not improvise from 316L or commodity 310 stock. Freeze the AWS (or EN) class on the WPS/PQR before production welds, and remember mill WLD/HCW longitudinal welds are autogenous—Table 6 guidance applies to joining with filler, not to the mill seam.

Conclusion

ASME SA312 UNS S31050 is the TP-less 25Cr-22Ni-2Mo-N (310MoLN-type) pipe grade: C ≤0.025%, Si ≤0.40%, Mo 1.60–2.60%, N 0.09–0.15%, Ni 20.5–23.5%, Cr 24.0–26.0%, thickness-split Table 4 floors of 84/39 or 78/37 ksi with 25% longitudinal elongation, and a Table 2 default 1900 °F [1040 °C] anneal. It is not a drop-in for TP310S (Mo residual, no N, 75/30 ksi), UNS S31002 (Mo/N ceilings for nitric duty), or UNS S31254 (6Mo seawater)—each has its own Table 1 row. Table 6 lists no AWS filler class (filler by agreement). Order the manufacturing type (SML/WLD/HCW), schedule or wall (wall drives Table 4), finish, Mo/N reporting, and any product analysis, licensor extras, or supplementary tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X