ASME SA312 TP316H Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 TP316H Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 TP316H / UNS S31609 H-grade stainless steel pipe in SML, WLD and HCW, with C 0.04–0.10% and Mo 2.00–3.00%, Table 5 grain size No. 7 or coarser, a 75/30 ksi Table 4 floor and a 1900 °F anneal, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP316H / UNS S31609
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Dimensions
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 TP316H Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe for high-temperature and general corrosive service. TP316H / UNS S31609 is the controlled-carbon, high-temperature member of the molybdenum-bearing 316 family. Table 1 sets C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 16.0–18.0%, Ni 10.0–14.0%, and Mo 2.00–3.00%. The carbon minimum is the whole point of the grade: it supports creep strength at elevated temperature, and a heat with 0.03% carbon is perfectly good TP316L but is not TP316H.

As an H grade, TP316H carries a package of extra rules beyond chemistry. Table 5 requires an ASTM grain size of No. 7 or coarser (a finer limit number than the No. 6 used for TP309H and TP310H), Table 2 lists the solution anneal at 1900 °F [1040 °C] minimum together with TP304H, clause 6.2 requires a separate solution treatment after hot forming rather than relying on the hot-working heat, and clause 17 requires heat-treatment lot marking. Table 4 sets 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield with 35% longitudinal / 25% transverse elongation, and Table 6 assigns ER316H as the filler. Buyers specify TP316H for heater tubes, hot process lines, and steam service where design temperatures put the pipe into the creep range and where the 316 molybdenum also helps with corrosion.

SHH STEEL can supply ASME SA312 TP316H stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) form. We quote ASME B36.19 schedules and special OD/wall by agreement, ship with EN 10204 3.1 mill test certificates that report the full Table 1 chemistry with carbon shown inside the 0.04–0.10% band, the Table 5 grain size, the 75/30 ksi results, and the 1900 °F anneal and clause 6.2 reheat statements, and offer dual SA-312/A312 marking when the heat and tests meet both editions on the purchase order. Please confirm NPS, wall or schedule, finish, length practice, and any product-analysis or supplementary tests when you enquire.

The names below are the ones buyers commonly use, and they map to the ordered product as shown. Always put both the TP name and the UNS number on the order.

  • ASME SA312 TP316H / UNS S31609 — preferred marking language for ASME-code and dual-marked pipe
  • ASTM A312 TP316H — same grade tables when the ASTM edition is referenced
  • “316H” — common shorthand; acceptable in conversation, but the certificate must show the carbon band and grain size
  • EN 1.4919 type — similar high-temperature 316 grades exist in EN standards; treat as an approximate map only

Sister grades buyers compare with TP316H include ASME SA312 TP316 Stainless Steel Pipe (C ≤0.08% with no minimum and no H rules), ASME SA312 TP316L Stainless Steel Pipe (C ≤0.035% and 70/25 ksi), ASME SA312 TP316Ti Stainless Steel Pipe (titanium-stabilized), ASME SA312 TP316N Stainless Steel Pipe (N 0.10–0.16% and 80/35 ksi without H grain or reheat rules), and ASME SA312 TP304H Stainless Steel Pipe for high-temperature duty without molybdenum. Grade hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 recognizes three manufacturing routes for TP316H pipe, and the route is a purchase-order decision driven by the design code, the size range, wall thickness, and how the owner wants the pipe inspected. The route never changes the chemistry: whichever way the pipe is made, the heat must still meet C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 16.0–18.0%, Ni 10.0–14.0%, and Mo 2.00–3.00%, and every length must still go through the solution anneal at 1900 °F [1040 °C] minimum before it is released.

  • Seamless (SML) — no welding at any stage. Seamless dominates heater tubes, high-pressure steam lines, and thick-wall hot process pipe. Every seamless length must still receive the 1900 °F solution anneal, and hot-finished pipe needs the separate clause 6.2 treatment rather than a quench from the hot-working heat.
  • Welded (WLD) — automatic welding without filler metal, with the weld finished so the pipe meets dimensional and mechanical requirements after the final heat treatment. The strip or plate heat must itself carry the full TP316H chemistry, so ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked to at least 35% reduction of wall and weld before the final anneal, again without filler in the longitudinal seam, with the weld radiographed before cold work. Order HCW when the project specifically wants that marking and the process controls SA-312 writes around it.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser accepts a system test in place of the hydrotest, and lots for mechanical testing follow clause 11.1. Because TP316H is an H grade, clause 17 heat-treatment lot marking is mandatory, and each lot must be traceable to the anneal that produced its grain size. Dual certification TP316/TP316H is common when the carbon is 0.04–0.08% and the grain-size and reheat requirements are met; dual TP316L/TP316H is impossible because the carbon windows do not overlap.

TP316H is widely produced, but not every stockist carries genuine H-grade material with grain-size reporting, so check the certificate before accepting stock offered as “316H”. Mill runs are common for heavy-wall seamless and special sizes. Enquire with route, sizes, wall, edition year, and whether you need TP316/TP316H dual marking, so the mill can target carbon within the overlap band and plan the grain-size control from the start.

Chemical Composition of SA312 TP316H

Two chemistry layers matter for TP316H. The melting (heat or ladle) analysis is mandatory for every heat under SA-312/A312 Table 1, while product analysis on finished pipe applies only when it is ordered through Supplementary Requirement S1 or purchase-order wording. Product tolerances are not printed in SA-312 itself; they come through ASTM A999/A999M §6.3 from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values and, when ordered, the product values, and never quotes tighter catalogue windows that the standard does not publish.

Melting analysis (heat / ladle analysis) — Table 1

The table below is the heat analysis for TP316H from SA-312/SA-312M Table 1. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element. TP316H has no titanium, niobium, or nitrogen requirement in Table 1.

Element TP316H / UNS S31609 melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 10.0 – 14.0
Molybdenum (Mo) 2.00 – 3.00

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 10.0 – 14.0 0.15 under / over 9.85 – 14.15
Molybdenum (Mo) 2.00 – 3.00 0.10 under / over 1.90 – 3.10

Source: SA-312 Table 1 TP316H / S31609. No Ti, Nb, or N requirement.

Carbon at 0.04–0.10% is the defining element and the first value to check on receipt. Compared with ASME SA312 TP316L Stainless Steel Pipe, which has C ≤0.035% and 70/25 ksi, TP316H has the carbon band and the 75/30 ksi floor; compared with ASME SA312 TP316N Stainless Steel Pipe, which adds N 0.10–0.16% and 80/35 ksi, TP316H relies on carbon and grain size instead of nitrogen for elevated-temperature strength. Molybdenum at 2.00–3.00% is the same as the rest of the 316 family, so a PMI gun that reads Cr, Ni, and Mo will not distinguish TP316H from TP316L; carbon has to come from the certified analysis or an OES test.

For product analysis, carbon may read 0.03–0.11% under the A480 ±0.01 tolerance on the 0.04–0.10% band, and molybdenum uses the 0.10 band across 2–3%. If dual TP316/TP316H marking is ordered, the heat carbon must sit within 0.04–0.08% so it satisfies both rows. State any product-analysis requirement on the purchase order so the acceptance basis is agreed before the pipe is made.

Mechanical Properties of SA312 TP316H

Room-temperature tensile requirements for TP316H come from SA-312 Table 4 and are summarized below. These are minimum release values for the lot, not typical values, and design allowables must always be taken from the governing code tables for UNS S31609 rather than from a neighbouring grade.

Property TP316H
Tensile, min 75 ksi [515 MPa]
Yield, min 30 ksi [205 MPa]
Elongation 35% L / 25% T
Grain size (Table 5) No. 7 or coarser

The room-temperature floors of 75/30 ksi match ASME SA312 TP316 Stainless Steel Pipe, which is why the H-grade requirements are easy to overlook. The difference lies in the extra Table 5 grain-size requirement of No. 7 or coarser, which supports creep strength, and in the carbon band. Grain size finer than No. 7 fails the grade regardless of how good the tensile results look. Table 4 does not set a hardness maximum for TP316H.

Elevated-temperature design must use the code allowable stresses listed for UNS S31609. Using TP316L stress values understates the grade, and using TP316 values without H evidence is not appropriate in the creep range. Certificate results are normally above the minima, but design should still use Table 4 and the code tables unless the mill has accepted higher guarantees in writing. Delivery is the solution-annealed condition.

Dimensions and Tolerances

Dimensional supply for SA312 TP316H pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow SA-312 Table 3 as summarized below. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M.

  • Lengths — single random, double random, or cut-to-length on order
  • Cut lengths — typically no more than 1/4 in. [6 mm] over the ordered length unless the PO states a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face when the WPS is already frozen

Many refinery, power, and petrochemical buyers order by OD × wall rather than NPS and schedule, which is fine as long as the enquiry says so clearly. Straightness, end finish, and length tolerance should be written into export orders so receiving inspection has an agreed acceptance basis instead of arguing after arrival. On thin schedules with threaded or socket-weld ends, check that the remaining wall is still adequate after the 12.5% under-tolerance. Jointers are not permitted unless the purchase order allows them, so cut-to-length programmes should include an allowance for fit-up scrap rather than expecting the mill to ship short pieces.

Equivalent Grades

TP316H / UNS S31609 has close equivalents in ASTM A312 and in other ASTM pipe and tube standards, and approximate equivalents in EN high-temperature grades. Any cross-reference has to be checked against carbon, grain size, and heat-treatment requirements, not just Cr, Ni, and Mo.

Designation Notes
SA-312 TP316H / S31609 Governing
ASTM A312 TP316H When editions align

Approximate EN or JIS equivalents are useful for commercial discussion, but they are not substitution approvals because their carbon ranges, grain-size rules, and tensile floors may differ. TP316/TP316H dual certification is valid only when carbon is 0.04–0.08% and the H-grade grain-size and reheat rules are satisfied. Related SA-312 pages: ASME SA312 TP316 Stainless Steel Pipe, ASME SA312 TP316L Stainless Steel Pipe, ASME SA312 TP316Ti Stainless Steel Pipe, ASME SA312 TP304H Stainless Steel Pipe, and ASME SA312 TP321H Stainless Steel Pipe.

Heat Treatment and Delivery Condition

Table 2 lists TP316H with TP304H at 1900 °F [1040 °C] minimum for both cold-finished and hot-finished pipe, followed by rapid cooling, and the hot-finished size notes in the right-hand columns of Table 2 apply as tabulated in the ordered edition. Clause 6.2 requires a separate solution treatment after hot working for H grades, so a direct quench from the hot-working temperature is not acceptable. This anneal is what sets the coarse grain size needed for Table 5, which is why the anneal record and the grain-size result belong together on the certificate.

Clause 17 requires heat-treatment lot marking on TP316H, so each length can be traced to the anneal that produced its grain size. Bright annealing is available by agreement where the mill can hold the temperature in a protective atmosphere. If pipe is hot bent or formed later, a fresh solution anneal is needed to restore the structure, and any post-weld heat treatment for creep service should be specified by the owner rather than improvised.

Corrosion Resistance

SA-312 does not contain a corrosion table, so this section is engineering commentary. TP316H has the same Cr, Ni, and Mo as the rest of the 316 family, so its pitting and general corrosion resistance at ambient temperature is broadly similar to TP316. The higher carbon, however, makes it more prone to sensitization when it sits in roughly the 800–1500 °F range, which is why TP316H is normally chosen for high-temperature strength rather than for aqueous corrosion at low temperature.

  • High-temperature oxidation — good in air and steam at typical 316H service temperatures
  • Intergranular corrosion — higher risk than TP316L after sensitizing exposure; S7 (A262 Practice E) can be ordered when proof is needed
  • Polythionic acid cracking — a known concern in refinery shutdowns; follow the owner’s neutralization practice
  • Chloride stress corrosion cracking — similar susceptibility to other 300-series grades

Where the pipe will see both creep-range temperatures and wet corrosive conditions during shutdowns, discuss the choice between TP316H and stabilized options such as ASME SA312 TP316Ti Stainless Steel Pipe or ASME SA312 TP347H Stainless Steel Pipe with the materials engineer. Do not swap TP316H for TP316L to gain corrosion resistance in creep service, because the allowable stresses and H-grade controls will be lost.

Applications of SA312 TP316H Pipe

Applications for TP316H pipe are driven by elevated design temperature combined with the moderate corrosion resistance of the 316 family. The table below summarizes where buyers typically specify the grade.

Application Why Note
High-T process / heater tubes (creep) H rules + Mo Confirm S31609 allowables
Refinery / chemical hot lines 316 oxidation + H Do not substitute TP316L

Typical users include refinery heater tubes and transfer lines, petrochemical crackers and reformers, power-plant steam and superheater piping, and chemical plants with hot process streams. Enquiries should state the design temperature, whether the owner requires TP316/TP316H dual marking, whether S7 or other supplementary tests apply, and the filler basis for fabrication. When molybdenum is not needed, ASME SA312 TP304H Stainless Steel Pipe may be cheaper; when sensitization during shutdown is a concern, compare with ASME SA312 TP321H Stainless Steel Pipe or ASME SA312 TP347H Stainless Steel Pipe.

Weldability

Table 6 assigns ER316H as the filler for TP316H / UNS S31609, and that consumable should appear on the WPS and PQR. ER316H keeps a carbon level in the deposit that supports creep strength in the weld, which matters when the weld sees the same design temperature as the pipe. Substituting ER316L for H-grade creep welds should only happen after an engineering review, because the low-carbon deposit can become the weak link at temperature.

  • Qualify on TP316H — procedure qualification on the actual H grade
  • Control heat input and interpass temperature — to limit sensitization in the HAZ
  • Back-purge roots — to protect the ID from oxidation
  • Post-weld heat treatment — when the owner specifies it for creep service, to the agreed cycle

Mill longitudinal welds on WLD and HCW pipe are made without filler, so Table 6 applies to fabrication joints. NDE extent for girth welds is a fabrication-code decision, separate from the hydro or electric test the mill applies to each length. For thick-wall creep service, ask the welding engineer whether delta-ferrite limits in the weld metal are required, since the owner specification often controls that.

Surface Finishes

Surface condition for SA312 TP316H pipe should be stated on the purchase order rather than left to mill default. For stainless pipe, embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts, so the finish is part of the material performance and not just appearance. The finishes we regularly quote for this grade are listed below.

  • Annealed and pickled (AP) — solution annealed at 1900 °F [1040 °C] minimum, then descaled in acid pickle or an equivalent process to a matte grey finish; the standard choice for process pipe
  • Blasted and pickled — common on heavy-wall seamless where blasting first makes scale removal more reliable
  • Bright annealed (BA) — annealed in a protective atmosphere where mill capability exists for the size; the anneal temperature still has to meet the Table 2 practice for TP316H
  • Mechanically polished — OD and/or ID polish to an agreed grit or Ra when ordered; polishing never replaces the solution anneal
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed on WLD and HCW product

For TP316H the usual choice is annealed and pickled, because the pipe is bought for high-temperature service where appearance matters less than a clean, scale-free surface. Passivation after pickling or polishing can be added when the end-user specification calls for it, even though SA-312 itself does not require it. If the project bans chloride-bearing marking inks, say so on the order; otherwise the mill will apply its normal stencil practice and ship its default AP finish.

Inspection and Testing

The base acceptance package for SA-312 TP316H pipe combines chemistry, tensile testing, heat-treatment evidence, and a pressure or electrical integrity test on every length. The items below make up the usual package; supplementary requirements and project corrosion tests only apply when they are written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for TP316H: C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 16.0–18.0%, Ni 10.0–14.0%, and Mo 2.00–3.00%
  • Product analysis — when ordered (Suppl. S1 or PO wording), using A480 Table A1.1 tolerances via A999 §6.3
  • Tension test — 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum, plus 35% L / 25% T elongation, with Table 5 grain size No. 7 or coarser on a lot basis
  • Flattening test — or the alternate bend test where the standard permits
  • Hydrostatic or nondestructive electric test — every length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD × wall, with TP316H (UNS S31609) and the heat-treatment lot on every stencil

Mill test certificates: EN 10204 3.1 is the standard documentation from SHH STEEL supply. For TP316H the certificate must report the full Table 1 chemistry with carbon inside 0.04–0.10%, the Table 5 grain size of No. 7 or coarser, 75/30 ksi tensile results, 35%/25% elongation, the hydro or NDE method, the 1900 °F anneal, the clause 6.2 reheat, and the heat-treatment lot identity. EN 10204 3.2 or third-party witness by SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency is arranged when specified, and it should be booked before final testing rather than after the heat has been released. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy both editions named on the order.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Receiving review should confirm carbon 0.04–0.10% (or 0.04–0.08% for dual TP316/TP316H), Mo 2.00–3.00%, Cr and Ni, the grain size of No. 7 or coarser, 75/30 ksi tensile, elongation, the anneal statement, and the lot marking. Third-party inspectors should check that the stencil reads TP316H and not only TP316. PMI guns cannot measure carbon reliably, so OES testing or the certified analysis is needed to separate TP316H from TP316L stock.

Packaging and Shipping

Export and domestic shipments of SA312 TP316H pipe are packed for handling and for ocean or land transport. The packing we normally apply is summarized below, and anything beyond it can be agreed on the order.

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where the finish needs protecting
  • End caps — plastic or metal caps on plain or beveled ends to keep out damage and contamination in transit
  • Marking — specification, grade (TP316H (UNS S31609) and the heat-treatment lot), heat number, size, manufacturing type (SML / WLD / HCW), test letters, and mill identity as SA-312 and the purchase order require
  • Export protection — waterproof wrapping or desiccant as agreed for polished or bright-annealed finishes, with low-chloride inks on request

Segregate TP316H from ASME SA312 TP316 Stainless Steel Pipe, ASME SA312 TP316L Stainless Steel Pipe, and ASME SA312 TP316Ti Stainless Steel Pipe on the packing list and in the yard, because these grades look identical and carbon cannot be checked with a handheld PMI gun. Use separate bundles and distinct tags on mixed shipments, and have receiving inspectors check stencil heat and lot numbers against the MTC for every length. Keep interiors dry and capped so chloride-bearing moisture cannot stain or pit the surface before installation. Shipping documents normally include the packing list, invoice, bill of lading or air waybill, and the 3.1 or 3.2 MTC with full Table 1 chemistry, plus origin and customs papers to suit the agreed Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe, and for SA312 TP316H we quote against the edition you name rather than a generic catalogue sheet. We report the full Table 1 chemistry on the MTC with carbon shown inside the 0.04–0.10% band, together with the Table 5 grain size, the 75/30 ksi results, and the 1900 °F anneal and clause 6.2 reheat statements. Heat identity stays unbroken from the melt to the finished length, so receiving inspection can clear each heat against Table 1 and Table 4 without chasing paperwork after the pipe has arrived.

We check supplier certificates before shipment for missing grain-size results, carbon below 0.04%, absent lot marking, or “316/316L” stock relabelled as 316H, so problems are caught at the mill rather than at the fabricator. Where you need TP316/TP316H dual marking, we confirm before the order that the heat carbon will sit inside the 0.04–0.08% overlap.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for TP316H; C 0.04–0.10% reported; Table 5 grain size No. 7 or coarser; 1900 °F anneal and clause 6.2 reheat stated; lot marking applied
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs as standard with full Table 1 chemistry; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both editions you name
  • Related grades — ASME SA312 TP316 Stainless Steel Pipe, ASME SA312 TP316L Stainless Steel Pipe, ASME SA312 TP304H Stainless Steel Pipe, and ASME SA312 TP321H Stainless Steel Pipe when a project buys a matched package
  • Export packing — seaworthy bundles, end protectors, and durable grade, heat, size, and type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, wall, finish, and any supplementary tests you name (S1, S5, S7, S8, S9). If the same project also needs plate or fittings, ask for coordinated heats so the chemistry lines up across product forms. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 TP316H stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for TP316H
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M TP316H / UNS S31609
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension (75/30 ksi), Table 5 grain size No. 7 or coarser, flattening/bend, hydro or NDE per length; C 0.04–0.10% on MTC; 1900 °F anneal and clause 6.2 reheat stated; S1/S5/S7/S8/S9 on order
Documents EN 10204 3.1 with full Table 1 chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Common TP316H sizes are sometimes available from stock, but check that the stock certificate shows the carbon band, grain size, and lot marking before accepting it. Heavy-wall seamless and special sizes are usually mill-order items. Enquiries should state the SA-312 edition, TP316H (UNS S31609) and the heat-treatment lot, SML/WLD/HCW, NPS or OD × wall (and whether wall is nominal or minimum), length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirements, so mill slots line up with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders, and grouping project sizes onto one heat keeps the chemistry consistent while helping meet mill minimums without over-ordering.

FAQ

Is ASME SA312 the same as ASTM A312 for TP316H?
For chemistry (Table 1), tensile (Table 4), grain size (Table 5), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and the mill test certificate so inspectors can verify the heat against the books you cited.
What is the UNS number for TP316H?
Table 1 lists TP316H as UNS S31609. Cite both TP316H and S31609 on the purchase order, the stencil, and the mill test certificate. Keeping the UNS on every document stops the pipe being confused with TP316 (S31600) or TP316L (S31603), which share the same Cr, Ni, and Mo ranges but have different carbon limits and no H-grade rules.
TP316H vs TP316 — which should I order?
TP316 allows C up to 0.08% with no minimum and carries no grain-size or reheat rules. TP316H requires C 0.04–0.10%, Table 5 grain size No. 7 or coarser, the clause 6.2 reheat, and lot marking. Both have 75/30 ksi floors. Choose TP316H when design temperatures enter the creep range and the code allowables for S31609 are needed.
TP316H vs TP316L — which should I order?
TP316L has C ≤0.035% and a 70/25 ksi floor and is chosen for weld corrosion resistance at ordinary temperatures. TP316H has C 0.04–0.10%, 75/30 ksi, and H-grade grain-size and reheat controls for elevated-temperature strength. The carbon windows do not overlap, so dual TP316L/TP316H certification is impossible; pick the grade that matches the design temperature.
Seamless vs welded TP316H — which is better?
Neither is universally better. Seamless is typical for heater tubes, high-pressure steam lines, and heavy walls, while WLD and HCW are legitimate SA-312 forms when tested and annealed to the H-grade rules. Choose the route your design code and datasheet allow, and check that the same SML, WLD, or HCW letters appear on the marking and MTC.
Can you dual-certify SA312 / A312 TP316H, or TP316/TP316H?
Yes on SA312/A312, when chemistry, heat treatment, mechanical tests, grain size, and marking meet both editions named on the order. TP316/TP316H dual marking is also possible when the heat carbon is 0.04–0.08% and the H-grade grain-size and reheat requirements are met. Write the editions and the dual grade on the PO before the heat is made.
Hydrostatic test vs NDE — which do I get on TP316H pipe?
Each length is either hydrostatically tested or nondestructively electrically tested, and the manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification requires one, state it on the PO and confirm the chosen test on the MTC for every length. NPS 10 and larger may be marked NH only when you accept a system test.
What heat treatment applies to TP316H?
Table 2 lists TP316H with TP304H at 1900 °F [1040 °C] minimum for cold- and hot-finished pipe, followed by rapid cooling. Clause 6.2 requires a separate solution treatment after hot working, and clause 17 requires heat-treatment lot marking. The anneal is what produces the Table 5 grain size, so the anneal and grain-size records should appear together on the MTC.
What Table 1 chemistry defines TP316H?
Table 1 sets C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 16.0–18.0%, Ni 10.0–14.0%, and Mo 2.00–3.00%, with no Ti, Nb, or N requirement. Carbon is the defining element. On product analysis, carbon may read 0.03–0.11% under the A480 ±0.01 tolerance, and molybdenum uses the 0.10 band.
What are the Table 4 tensile requirements for TP316H?
Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum, with 35% longitudinal and 25% transverse elongation. Those floors match TP316, so the H-grade difference shows up in carbon, grain size, and the elevated-temperature allowables for UNS S31609 rather than at room temperature. Design to the code tables listed for S31609.
What filler metal should I use to weld TP316H pipe?
Table 6 assigns ER316H to TP316H. Put ER316H on the WPS and PQR, since its carbon level supports creep strength in the weld. Do not substitute ER316L in creep-range welds without an engineering review. Mill longitudinal seams on WLD and HCW pipe are autogenous, so Table 6 guidance applies to fabrication joints, not to the mill weld.
Does TP316H require grain-size control?
Yes. Table 5 requires an ASTM grain size of No. 7 or coarser for TP316H, which is a finer limit number than the No. 6 used for TP309H and TP310H. A result finer than No. 7 fails the grade even if chemistry and tensile pass. Ask for the grain-size result on the MTC alongside the anneal and lot records.

Conclusion

ASME SA312 TP316H / UNS S31609 is the high-temperature member of the 316 family, with C 0.04–0.10%, Cr 16.0–18.0%, Ni 10.0–14.0%, and Mo 2.00–3.00%, a 75/30 ksi Table 4 floor with 35% L / 25% T elongation, Table 5 grain size No. 7 or coarser, a 1900 °F [1040 °C] Table 2 anneal listed with TP304H, the clause 6.2 reheat, clause 17 lot marking, and ER316H filler from Table 6. It is not a drop-in for ASME SA312 TP316L Stainless Steel Pipe or ASME SA312 TP316 Stainless Steel Pipe. Order the manufacturing type, size and wall, finish, carbon and grain-size reporting, anneal and reheat proof, any dual TP316/TP316H requirement, and supplementary tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X