ASME SA312 TP348H Stainless Steel Pipe | SA 312/SA 312M
What is ASME SA312 TP348H Stainless Steel Pipe
ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. Grade TP348H is listed in Table 1 as UNS S34809. Clause 1.2 groups it with the other H grades—TP304H, TP309H, TP309HCb, TP310H, TP310HCb, TP316H, TP321H, TP347H, and TP348H—as modifications intended for temperatures where creep and stress-rupture properties are important. Commercially the same product may be called SA312 TP348H pipe, ASTM A312 TP348H pipe, A312 Grade TP348H, or 348H stainless steel pipe when the purchase order clearly references SA-312 or A312. For pressure piping and code work, cite the full grade designation, the UNS number, and the edition of the standard on the purchase order and on the mill test certificate—do not rely on a bare “348H” market label.
TP348H is the high-carbon, elevated-temperature sister of ASME SA312 TP348 Stainless Steel Pipe, carrying the same explicit Ta ≤0.10% ceiling plus footnote H (Nb ≥8×C and ≤1.0%) on a 0.04–0.10% carbon band. The controlled carbon and the coarse-grain requirement support creep strength, while niobium still stabilizes carbon so grain-boundary sensitization after welding is reduced. Table 1 sets C 0.04–0.10%, Nb at least 8×C with a 1.0% ceiling, and Ta ≤0.10%, with chromium at 17.0–19.0% and nickel at 9.0–13.0%; molybdenum is not required. Table 4 minima are 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield with 35% longitudinal / 25% transverse elongation. As an H grade, Table 2 calls for 2000 °F [1100 °C] minimum for cold-finished and 1925 °F [1050 °C] minimum for hot-finished pipe, clause 6.2 reheating rules and lot marking apply, and Table 5 requires an average grain size of ASTM No. 7 or coarser. Table 6 filler guidance is ER347, and supplementary requirement S6 applies only when the purchase order calls for it.
SHH STEEL can supply ASME SA312 TP348H stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) routes, in ASME B36.19 schedules as well as special OD and wall combinations by agreement. Every shipment carries EN 10204 3.1 mill test certificates that report Nb, Ta, carbon, the measured grain size, and the Table 2 anneal temperature, and dual SA-312/A312 marking is available when chemistry, heat treatment, mechanical tests, and marking satisfy both editions named on the order. Send NPS, wall or schedule, finish, length practice, and any product-analysis or supplementary tests with the enquiry so we can quote the right mill route first time.
The common commercial names below all point to the same product, provided the order clearly references SA-312 or A312 and the grade rules are met:
- ASME SA312 TP348H / SA-312 Grade TP348H — preferred marking language for ASME-code and dual-marked pipe
- ASTM A312 TP348H — same chemistry and tensile tables when the ASTM edition is referenced
- UNS S34809 — unified number used on MTCs and in allowable-stress tables
- 348H stainless steel pipe — market shorthand; confirm C 0.04–0.10%, Nb ≥8×C, Ta ≤0.10%, and grain-size control on the order
TP348H and ASME SA312 TP348 Stainless Steel Pipe are separate Table 1 rows with different carbon bands and stabilizer multipliers, so a heat certified to one does not automatically qualify as the other unless the MTC proves both sets of limits and the order asks for dual grading. Related grades: ASME SA312 TP347H Stainless Steel Pipe, ASME SA312 TP347LN Stainless Steel Pipe, ASME SA312 TP347 Stainless Steel Pipe. Hub: ASME SA 312/SA 312M.
Manufacturing Types (SML / WLD / HCW)
ASME SA-312 defines three manufacturing routes that may be marked on finished TP348H pipe. Selecting the route is a purchase-order decision driven by design code, size range, wall thickness, and inspection preference. It does not change the Table 1 chemistry of Grade TP348H—melting must still meet C 0.04–0.10%, Nb at least 8×C with a 1.0% ceiling, and Ta ≤0.10%.
- Seamless (SML) — no welding at any stage of manufacture. Seamless is preferred when the project specification excludes welded pipe, when thick walls favor seamless production, or when the piping class documentation is written around seamless product only.
- Welded (WLD) — automatic welding without filler metal. The weld is finished so that the pipe meets dimensional and mechanical requirements after the final heat treatment required by SA-312. Welded product is widely used for common NPS and schedule combinations where the code accepts welded austenitic pipe.
- Heavily cold-worked (HCW) — welded pipe that is cold worked to a reduction of area of wall and weld of at least 35% before the final anneal, again without filler metal in the longitudinal weld. HCW is ordered when the buyer wants the HCW marking and the process controls written into SA-312 for that route.
Each finished length is hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Marking on the pipe typically includes the manufacturer, grade (TP348H), heat number, NPS or outside diameter and schedule or wall thickness, and the manufacturing type letters SML, WLD, or HCW. When comparing seamless versus welded TP348H offers, check manufacturing type and the hydro or NDE method on the mill test certificate—not only the grade stamp.
Chemical Composition of SA312 TP348H
Two chemistry layers matter for TP348H: the melting (heat or ladle) analysis, which is mandatory for every heat under ASME SA-312/ASTM A312 Table 1, and product analysis on finished pipe, which applies only when ordered through Supplementary Requirement S1 or PO wording. Product-analysis tolerances are referenced from A999/A999M §6.3 to ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values and, when ordered, product values—never unpublished tighter windows.
Melting analysis (heat / ladle analysis) — Table 1
Heat analysis for Grade TP348H / UNS S34809 from ASME SA-312/SA-312M (ASTM A312/A312M) Table 1 is summarized below. Values are maximum unless a range is shown, and ellipses (…) mean the ordered edition places no requirement on that element.
| Element | TP348H / UNS S34809 melting analysis |
|---|---|
| Carbon (C) | 0.04 – 0.10 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 17.0 – 19.0 |
| Nickel (Ni) | 9.0 – 13.0 |
| Molybdenum (Mo) | No requirement (…) |
| Niobium (Nb) | ≥ 8 × C and ≤ 1.0% (footnote H) |
| Tantalum (Ta) | ≤ 0.10 |
| Nitrogen (N) | No requirement (…) |
Source: ASME SA-312/SA-312M ≡ ASTM A312/A312M Table 1 for Grade TP348H, including footnote H (Nb ≥8×C and ≤1.0%) and Ta ≤0.10%. The niobium minimum moves with the actual carbon of each heat. Example: at C = 0.08%, Nb must be at least 0.64%; even at the top of the carbon band (C = 0.10%) the 8×C minimum is 0.80%, still under the 1.0% cap. Also confirm Ta ≤0.10%. Do not apply TP348’s 10×C factor to H heats.
Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1
When product analysis is ordered, finished-pipe chemistry shall meet Table 1 as modified by the tolerances in ASTM A480/A480M Table A1.1. The resulting limits used for TP348H receiving inspection are:
| Element | Melting (Table 1) | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | 0.04 – 0.10 | 0.01 under / over | 0.03 – 0.11 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 17.0 – 19.0 | 0.20 under / over | 16.80 – 19.20 |
| Nickel (Ni) | 9.0 – 13.0 | 0.10 under / 0.15 over | 8.90 – 13.15 |
| Niobium (Nb) | ≥ 8 × C, ≤ 1.0 | 0.05 under / over on applicable limit | Per heat calculation |
| Tantalum (Ta) | ≤ 0.10 | 0.05 over | ≤ 0.15 |
Versus TP348: carbon moves to a 0.04–0.10% band, the Nb multiplier drops from 10×C to 8×C, and grain-size control, clause 6.2 reheating, lot marking, and higher anneal temperatures are added; Ta ≤0.10% stays. Carbon carries a ±0.01 product tolerance, giving a 0.03–0.11% band on finished pipe when product analysis is ordered. Versus TP347H: chemistry is essentially the same H-grade Nb window, but TP348H adds the explicit Ta ≤0.10% ceiling. If an enquiry only says “348H stainless pipe”, confirm Ta reporting, grain-size evidence, and the Table 1 limits before the mill books a rolling slot.
Mechanical Properties of SA312 TP348H
Tensile requirements for TP348H are given in ASME SA-312/SA-312M (ASTM A312/A312M) Table 4. Specimens and orientation follow the testing clauses of the standard and the referenced general requirements in A999/A999M.
| Property | TP348H |
|---|---|
| Tensile, min | 75 ksi [515 MPa] |
| Yield, min | 30 ksi [205 MPa] |
| Elongation | 35% L / 25% T |
| Grain size (Table 5) | No. 7 or coarser |
TP348H uses a single 75/30 ksi row regardless of route and wall, plus the Table 5 grain-size requirement of ASTM No. 7 or coarser. These are the mandatory acceptance floors; actual MTC values are usually higher, but design should still use Table 4 and the allowable-stress tables for UNS S34809 unless the purchase order states higher guaranteed values that the mill has accepted in writing. The No. 7 or coarser grain size is part of what makes the H grade an elevated-temperature material, so ask for the measured grain size on the MTC rather than a bare “complies”.
Hardness: Table 4 does not list a separately mandated hardness maximum for TP348H. If hardness matters for fabrication or end-user acceptance, state the limit on the purchase order and verify it on the MTC. Flattening or bend and tension tests run on a lot basis, and supplementary tests apply only when they are listed on the order.
Dimensions and Tolerances
Dimensional practice for austenitic stainless steel pipe ordered to SA-312 typically follows ASME B36.19 / B36.19M stainless-steel pipe schedules. Outside diameter and wall thickness are stated as NPS and schedule, or as OD and specified wall. Common schedules for TP348H enquiry include Schedule 5S, 10S, 40S, and 80S. Other walls and non-standard OD/wall combinations are available by agreement when both the mill and the order accept them.
Size coverage in commercial practice is summarized below. Confirm large NPS and heavy walls against mill capability for the chosen manufacturing type before you lock the purchase order.
- NPS / DN: commonly from NPS 1/8 upward; large NPS and heavy walls depend on manufacturing type (SML versus WLD/HCW) and mill capability—confirm on enquiry
- Schedules: 5S, 10S, 40S, 80S and special walls by agreement
- Length: single random (SRL), double random (DRL), or fixed cut lengths as stated on the purchase order
- Ends: plain end (PE), beveled end (BE), or other end preparations by agreement
Wall-thickness variation limits from SA-312 Table 3 (t/D = specified wall / ordered OD) are the acceptance bands used on mill test certificates and receiving inspection for TP348H:
| NPS designator | Wall over | Wall under |
|---|---|---|
| 1/8 to 2-1/2 incl., all t/D | 20.0% | 12.5% |
| 3 to 18 incl., t/D up to 5% | 22.5% | 12.5% |
| 3 to 18 incl., t/D over 5% | 15.0% | 12.5% |
| 20 and larger, welded, all t/D | 17.5% | 12.5% |
| 20 and larger, seamless, t/D up to 5% | 22.5% | 12.5% |
| 20 and larger, seamless, t/D over 5% | 15.0% | 12.5% |
Source: SA-312 Table 3; outside diameter variations per A999/A999M. OD, wall, and length tolerances follow SA-312 via ASTM A999/A999M and the dimensional standard on the order. SHH STEEL quotes the applicable clause rather than dumping entire A999 tables. Confirm max wall and NPS near the edge of B36.19 practice before acceptance.
Equivalent Grades
Equivalence for TP348H has to be stated carefully. Regional designations help selection discussions, but they are not automatic one-to-one substitutes for ASME pressure-code pipe without an approved material specification and design-code acceptance.
| Designation | Notes |
|---|---|
| ASME SA-312 / ASTM A312 Grade TP348H | Governing pipe product standard for this article |
| UNS S34809 | Unified number listed in Table 1 |
| TP348 (UNS S34800) | Standard-carbon sister; C ≤0.08%, Nb ≥10×C, Ta ≤0.10%, default 1900 °F anneal |
| TP347H (UNS S34709) | Nb-stabilized H grade without the Ta ≤0.10% ceiling |
| TP347LN (UNS S34751) | Low-carbon, nitrogen-bearing Nb grade |
| TP321H (UNS S32109) | Ti-stabilized H grade |
Within SA-312, do not swap TP348H for a sister grade just because they share a “348H” or “347H” market label—each has its own Table 1 and Table 4 / Table 5 rules, and only the 348 family carries the explicit Ta control. Related pages: ASME SA312 TP348 Stainless Steel Pipe, ASME SA312 TP347H Stainless Steel Pipe, ASME SA312 TP347LN Stainless Steel Pipe, ASME SA312 TP321H Stainless Steel Pipe. Hub: ASME SA 312/SA 312M.
Pressure-code caution: EN, JIS, or proprietary approximations do not authorize B31 or Section VIII substitution without engineered approval and an accepted material specification on the design documents.
Heat Treatment and Delivery Condition
All pipe furnished to ASME SA-312 shall be heat treated. For TP348H, Table 2 sets a minimum solution-annealing temperature of 2000 °F [1100 °C] for cold-finished pipe and 1925 °F [1050 °C] for hot-finished pipe, followed by water quenching or another rapid cool. These are higher than the 1900 °F default used for TP348, because the anneal also has to develop the coarse grain that Table 5 requires.
As an H grade, TP348H must meet the Table 5 average grain size of ASTM No. 7 or coarser, the clause 6.2 reheating rules, and lot-marking requirements. Supplementary requirement S6 (stabilization heat treatment) applies only when the purchase order specifies it—do not assume S6 on every shipment, and if it is ordered, agree the temperature and confirm it on the MTC. HCW cold reduction is done before the final anneal; delivery remains the annealed condition.
Commercial delivery condition for TP348H typically includes the following unless the purchase order or ordered edition states otherwise:
- Solution annealed to SA-312 Table 2 requirements for TP348H
- Pickled and descaled, or bright annealed, as ordered (see Surface Finishes)
- Straightened and cut to the ordered length practice
- Hydrotested or NDE-tested per length as required by the standard and the purchase order
Corrosion Resistance
TP348H is chosen where welded construction or service in the sensitizing range would put an unstabilized grade at risk of intergranular attack. Niobium combines with carbon before chromium can, so the chromium-depleted zones that cause weld decay are much less likely to form. The H grade trades some of that margin for the higher carbon needed for creep strength, which is why the stabilizer rule and anneal temperatures matter so much on the MTC. The purchase specification for this grade also wants tantalum residual controlled at ≤0.10%, which is the practical difference from TP347H on the same H-grade stabilizer concept.
Versus sister grades: ASME SA312 TP348 Stainless Steel Pipe and ASME SA312 TP321H Stainless Steel Pipe share the stabilized 18–10 concept but differ in carbon band, stabilizer element, or nickel range. They are not automatic drop-in replacements when the datasheet fixed UNS S34809.
Versus Mo-bearing grades: stabilization does not add pitting resistance. When chloride pitting, crevice attack, or reducing media dominate, molybdenum-bearing austenitics such as ASME SA312 TP316L Stainless Steel Pipe are usually the better choice. Mill annealed-and-pickled pipe already has a descaled surface; site welds and grinding should be cleaned and passivated when the end-user specification requires it, and intergranular-corrosion testing applies only when written on the order.
Applications of SA312 TP348H Pipe
TP348H pipe is selected where austenitic stainless behavior, SA-312 product form, and creep-range strength with stabilized chemistry are all needed. Typical application areas include:
| Application area | Typical use of TP348H pipe | Selection note |
|---|---|---|
| Superheater and reheater piping | Elevated-temperature steam lines where creep strength is in the design basis | Confirm grain size and Table 2 anneal on the MTC |
| Refinery heater and hydroprocessing lines | Hot hydrocarbon service with welded joints | Check allowable stresses for UNS S34809 at design temperature |
| Petrochemical furnace outlets | Transfer and header piping in the creep range | Agree S6 at enquiry if the licensor requires it |
| Code piping packages | Dual SA-312/A312 projects with heat traceability | Name edition, route, and UNS on the enquiry |
Plants that already run TP348 or TP321H sometimes buy TP348H in the same package, which is sensible for logistics but only when each line’s datasheet actually allows the grade being shipped to it. Match the grade to the corrosion and code case first; commercial convenience comes second.
Weldability
TP348H is generally weldable by common austenitic fusion processes with suitable heat input, interpass control, and joint cleanliness. Typical processes used on this grade include:
- GTAW (TIG) — preferred for root passes and thin-wall pipe where weld metal cleanliness and heat-input control matter
- GMAW (MIG) — productive for fill and cap passes on thicker walls when procedures are qualified
- SMAW — widely used for field girth welds with coated austenitic electrodes selected by agreement
- Automatic orbital or mechanized GTAW — common for repetitive high-integrity girth joints
Higher carbon in the H band makes heat-input and interpass control more important, especially on heavy walls that will see creep-range service. These are engineering choices on the WPS, not automatic SA-312 requirements on every order.
Filler metal: SA-312 Table 6 maps TP348H to ER347. Qualify the AWS (or EN) classification on the WPS/PQR using actual TP348H base metal and freeze it before production welds. Mill longitudinal welds on WLD and HCW product are made without filler metal, so Table 6 applies to joining with filler, not to the mill seam.
Girth welds follow the piping/vessel code (e.g. ASME B31 / Section IX) and are separate from mill hydro/NDE. Specify girth NDE on fabrication documents when required. Keep joints clean of oil, paint, and carbon-steel contamination.
Surface Finishes
Surface condition for SA312 TP348H pipe is stated on the purchase order. Typical mill finishes available from SHH STEEL supply include the following options:
- Annealed and pickled (AP) — solution annealed, descaled in acid pickle or an equivalent process, producing a matte gray finish common for process and utility pipe
- Bright annealed (BA) — annealed in a protective atmosphere to a brighter surface where the order allows and mill capability exists for the size
- Mechanically polished — for example 180#, 320#, or 400# grit, or Ra-controlled polish on OD and/or ID for hygienic or architectural duty; polishing does not replace solution annealing
- Bead-finished welded OD — weld bead rolled or ground flush as agreed for WLD/HCW product
Passivation after pickle or polish can be added when the end-user specification requires it. For hygienic or high-purity lines, state both the Ra (or grit) target and the documentation package—including any surface roughness reports—on the enquiry. SHH STEEL will not imply a polished hygienic finish on standard AP pipe unless the purchase order says so. End preparation (plain or beveled) should be ordered together with finish so that bevel faces and ID cleanliness meet the same acceptance language.
Inspection and Testing
Base inspection and testing for SA-312 TP348H pipe combines chemistry, mechanical, and integrity checks. The following items form the usual acceptance package; supplementary requirements apply only when written on the purchase order.
- Heat (melting) analysis — mandatory per heat against Table 1 for TP348H (UNS S34809), including C 0.04–0.10%, Nb at least 8×C with a 1.0% ceiling, and Ta ≤0.10%
- Product analysis — when ordered (Suppl. S1 / purchase-order language), using A480 Table A1.1 tolerances via A999 §6.3
- Tension test — Table 4 tensile, yield, and elongation on a lot basis (75/30 ksi minima, plus grain size)
- Flattening test — or alternate bend where the standard permits for certain welded pipe
- Hydrostatic test or nondestructive electric test — each length; manufacturer’s option unless the order fixes the method
- Visual and dimensional check — against ordered NPS/schedule or OD/wall and the applicable tolerance clauses
Mill test certificates: EN 10204 3.1 is the standard documentation package from SHH STEEL supply. EN 10204 3.2 or third-party witness (SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency) is arranged when specified and should be booked before final testing. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy the edition(s) named on the order.
Optional / supplementary: PMI, RT/UT, intergranular corrosion or weld-decay tests, tighter straightness, special marking—only when listed on the PO. Keep heat numbers on cut pieces for MTC traceability.
Packaging and Shipping
Export and domestic shipments of SA312 TP348H pipe are packed for handling and ocean or land transport. Typical packing practices from SHH STEEL supply include:
- Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with separators where needed to protect finish
- End caps / protectors — plastic or metal caps on plain or beveled ends to reduce damage and contamination during transit
- Marking — durable marking of grade (TP348H), UNS S34809 when required, heat number, size (NPS or OD × wall / schedule), manufacturing type (SML / WLD / HCW), and mill identity as required by SA-312 and the purchase order
- Export packing — waterproof wrapping as agreed for polished or sensitive finishes; container stuffing photos on request
Segregate TP348H from TP348 and TP321H on the packing list and in the yard so stencil mix-ups do not travel with the shipment. Shipment docs typically include packing list, invoice, B/L or AWB, and MTC (3.1 or 3.2), plus origin/customs papers per Incoterms. State destination, packing preference, and extra marking at enquiry.
Why Choose SHH STEEL
SHH STEEL supplies specification-driven stainless pipe and plate. For ASME SA312 TP348H / UNS S34809 we quote against the edition you name, report the carbon and niobium (columbium) values the stabilizer rule depends on, state the measured grain size and the Table 2 anneal temperature on the MTC, and keep heat identity unbroken from melt to finished length, so receiving inspection can clear each heat against Table 1 and Table 4 instead of a generic “348H” catalog sheet.
- Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for TP348H (S34809), not unpublished tighter windows
- Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability
- Documentation — EN 10204 3.1 MTCs standard; 3.2 or third-party inspection on request
- Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both requirements you name
- Related grades — TP348, TP321H, and other stabilized austenitic SA-312 grades for matched packages
- Export packing — seaworthy bundles, end protectors, and durable grade/heat/size/type marking
Quotations follow your purchase-order language for edition year, manufacturing type, size, finish, and any supplementary tests such as S6, so the documents that arrive with the pipe match the documents your inspector expects. Grade hub: ASME SA 312/SA 312M.
Supply Capability
SHH STEEL can supply ASME SA312 TP348H / UNS S34809 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.
| Item | SHH STEEL capability for TP348H |
|---|---|
| Standard | ASME SA-312/SA-312M and/or ASTM A312/A312M Grade TP348H (UNS S34809) |
| Manufacturing types | SML, WLD, HCW |
| Size | NPS 1/8 and up per ASME B36.19; special OD/wall by agreement |
| Schedules | 5S, 10S, 40S, 80S and non-standard walls |
| Length | SRL, DRL, or cut-to-length |
| Finish | Annealed and pickled; bright annealed or polished by agreement |
| Testing | Tension, flattening/bend, hydro or NDE per length; grain size; S6 when ordered; supplementary tests on order |
| Documents | EN 10204 3.1; third-party inspection / 3.2 on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock moves with mill rolling cycles. Enquiries should state the SA-312 edition, SML/WLD/HCW, NPS or OD×wall, length practice, and any product-analysis or 3.2 requirements so mill slots align with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders.
FAQ
-
Is ASME SA312 the same as ASTM A312?
- For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and mill test certificate so inspectors can verify the heat against the exact books you cited—do not assume a bare market grade stamp covers dual certification.
-
What is the UNS number for TP348H?
- Table 1 lists TP348H as UNS S34809. Use that UNS on the purchase order, stencil, and MTC so the chemistry, grain-size, and tensile rows stay unambiguous. TP348 has its own UNS (S34800) and should never be assumed from a shared “348” market name.
-
TP348H vs TP348 — which should I order?
- TP348H uses C 0.04–0.10% with Nb ≥8×C, Ta ≤0.10%, grain size No. 7 or coarser, and higher anneal temperatures, while TP348 uses C ≤0.08% with Nb ≥10×C and the default 1900 °F anneal. Choose the H grade when the design is creep-governed; otherwise the standard grade is usually adequate. Fix the grade and UNS on the datasheet before comparing prices.
-
TP348H vs TP347H — which should I order?
- Both are H-grade Nb-stabilized grades with C 0.04–0.10%, Nb ≥8×C, grain size No. 7 or coarser, and CF 2000 / HF 1925 °F anneal. TP348H adds the explicit Ta ≤0.10% ceiling that TP347H does not publish. Order TP348H when the datasheet names S34809 or requires Ta control; otherwise TP347H is the more common commercial H-grade choice.
-
Seamless vs welded TP348H — which is better?
- Neither is universally better. Choose the manufacturing type your design code and datasheet allow; both are legitimate SA-312 forms when tested to the standard. State SML, WLD, or HCW on the order and confirm the same letters on the marking and MTC, along with the grain-size and anneal evidence that the H grade requires.
-
Can you dual-certify SA312 / A312 TP348H?
- Yes, when the heat analysis, heat treatment, mechanical tests, grain size, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the PO and require the MTC to reference both books. Dual certification with TP348 is only possible when the heat also proves the standard-grade limits.
-
Hydrostatic test vs NDE — which do I get?
- Each length is hydrotested or nondestructively electrically tested. Manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification locks one method, state it on the PO and verify the chosen test appears on the MTC for every length—silent mill option is not the same as an approved project method.
-
What heat treatment applies to TP348H?
- Table 2 requires 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe, followed by rapid cooling. As an H grade, TP348H also has to meet Table 5 grain size No. 7 or coarser, clause 6.2 reheating, and lot marking. S6 stabilization applies only when the purchase order specifies it.
-
What Table 1 chemistry defines TP348H?
- Table 1 sets C 0.04–0.10%, Nb ≥8×C and ≤1.0% (footnote H), Ta ≤0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Mn ≤2.00%, Si ≤1.00%, P ≤0.045%, and S ≤0.030%; molybdenum is not required. These are melting-analysis limits, and product analysis on finished pipe must be ordered explicitly if receiving inspection needs it.
-
What are the Table 4 tensile requirements for TP348H?
- Table 4 minima are 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield with 35% longitudinal / 25% transverse elongation, plus Table 5 grain size ASTM No. 7 or coarser. Actual MTC values are often higher, but design still uses Table 4 and the code allowables for UNS S34809 unless the PO states higher guarantees.
-
What filler metal should I use to weld TP348H pipe?
- SA-312 Table 6 maps TP348H to ER347. Qualify and freeze the AWS or EN class on the WPS/PQR before production welds. Mill WLD and HCW longitudinal welds are autogenous, so Table 6 applies to joining with filler in fabrication, not to the mill seam.
-
Does TP348H require grain-size control?
- Yes. As an H grade, TP348H must meet Table 5 average grain size of ASTM No. 7 or coarser, and the MTC should report the measured result rather than a bare “complies.” Combined with the CF 2000 / HF 1925 °F anneal and clause 6.2 reheating rules, grain size is part of what makes the grade suitable for creep-range design—do not clear a heat that omits it.
Conclusion
ASME SA312 TP348H (UNS S34809) is the elevated-temperature H-grade Nb-stabilized austenitic pipe grade in SA-312 that adds an explicit Ta ≤0.10% ceiling to footnote H (Nb ≥8×C and ≤1.0%) on a 0.04–0.10% carbon band. Table 4 minima are 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield; heat treatment follows CF 2000 °F / HF 1925 °F; grain size must be ASTM No. 7 or coarser; Table 6 filler guidance is ER347; and S6 stabilization applies only when specified. Order the manufacturing type (SML/WLD/HCW), schedule or wall, finish, grain-size evidence, Ta reporting, and any product analysis or supplementary tests explicitly, and keep TP348 and TP347H heats segregated. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.