ASME SA312 TP317 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 TP317 (UNS S31700) high-molybdenum stainless steel pipe in seamless, welded and HCW forms, with Mo 3.0–4.0%, Cr 18–20%, Ni 11–15% and 75/30 ksi minima, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP317 / UNS S31700
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 TP317 Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded and heavily cold-worked austenitic stainless steel pipe for high-temperature and general corrosive service, and it is technically aligned with ASTM A312/A312M of the referenced edition. Grade TP317 is listed in Table 1 as UNS S31700. For pressure piping and code work, cite the grade, the UNS number and the edition of the standard on the purchase order and on the mill test certificate, rather than relying on a market label that several neighbouring grades share.

TP317 is the higher-molybdenum companion to TP316. Table 1 sets Cr 18.0–20.0%, Ni 11.0–15.0%, Mo 3.0–4.0% and C ≤0.08%, with no nitrogen, titanium or copper requirement. The extra point of molybdenum over the 2–3% of TP316 improves resistance to many chloride and reducing-acid process streams where 316 is marginal. Table 4 releases the grade at 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield, the same floors as TP316. It is not an H grade; Table 2 does not list S31700 individually, so the default 1900 °F [1040 °C] anneal with rapid cooling applies. Table 6 lists TP317, but the filler-class pairing is not clearly populated in the edition extract, so the consumable is agreed on the WPS (ER317-type consumables are common industry practice, but that is not asserted here as a Table 6 mandate).

SHH STEEL can supply ASME SA312 TP317 stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD) and heavily cold-worked (HCW) forms. We cover ASME B36.19 schedules and special OD and wall combinations by agreement, issue EN 10204 3.1 mill test certificates as standard, and can dual-mark SA-312/A312 when the heat analysis, heat treatment, mechanical tests and marking satisfy both editions named on the purchase order. Tell us the NPS, wall or schedule, finish, length practice and any product-analysis or supplementary tests at enquiry stage, and we will confirm stock or mill rolling against those details.

Common commercial names and how they map to the ordered product are listed below. Use the full SA-312/A312 designation on the purchase order rather than market shorthand alone, because the shorthand is where grade substitutions usually start.

  • ASME SA312 TP317 / SA-312 Grade TP317 — preferred marking language for ASME-code and dual-marked pipe
  • ASTM A312 TP317 — same chemistry and tensile tables when the ASTM edition is referenced
  • UNS S31700 — unified numbering identity used on MTCs, stencils and ASME Section II Part D cross-references
  • 317 / 317 stainless steel pipe — market shorthand; confirm Mo 3.0–4.0% and UNS S31700 on the order

TP317 is not a drop-in for ASME SA312 TP317L Stainless Steel Pipe, ASME SA312 TP316 Stainless Steel Pipe, ASME SA312 UNS S31725 Stainless Steel Pipe or ASME SA312 UNS S31726 Stainless Steel Pipe. Against TP317L, the only chemistry difference is carbon (0.08% vs 0.035% maximum), but that matters for welded aqueous service. Against TP316, TP317 adds a full point of molybdenum plus higher Cr and Ni. S31725 and S31726 are lower-carbon, higher-Mo developments with their own Table 1 rows and should be compared on their own terms. Hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

SA-312 defines three manufacturing routes that may be marked on finished TP317 pipe. The route is a purchase-order decision driven by design code, size range, wall thickness and inspection preference. It does not change the Table 1 chemistry of UNS S31700, and every route must still finish with the solution anneal required by SA-312.

  • Seamless (SML) — no welding at any stage. Preferred for small-bore and thick-wall pressure pipe, and wherever the piping class excludes welded product.
  • Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment. Common for larger NPS lines where the code accepts welded austenitic pipe.
  • Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, with the weld radiographed before cold work. Ordered when tighter OD and wall consistency matters.

Each finished length is hydrostatically tested or nondestructively electrically tested, and the manufacturer may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser agrees to a system test instead. State SML, WLD or HCW explicitly on the enquiry; bids that differ only in manufacturing type are a common evaluation trap, and the same letters should appear on the stencil and the MTC.

Chemical Composition of SA312 TP317

Melting analysis (heat / ladle analysis) — Table 1

The table below is the SA-312 Table 1 heat analysis for TP317 / UNS S31700. Values are maximum unless a range is shown, and an ellipsis (…) means no requirement. These are the numbers the mill must report on the certificate, and they are the numbers receiving inspection should check first.

Element TP317 / UNS S31700 melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 11.0 – 15.0
Molybdenum (Mo) 3.0 – 4.0

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

When product analysis is ordered (Supplementary Requirement S1 or PO wording), the check analysis may vary from the Table 1 limits by the A480 tolerances below. Product analysis is not automatic, so order it explicitly if your project needs it rather than assuming ladle values will satisfy the client inspector.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 11.0 – 15.0 0.15 under / over 10.85 – 15.15
Molybdenum (Mo) 3.0 – 4.0 0.10 under / over 2.90 – 4.10

Molybdenum is the element that decides whether a heat is TP317, so check that it lands inside 3.0–4.0% on the heat analysis and within the ±0.10 A480 tolerance on any product analysis. Ordering “317” without UNS S31700 invites a 316 heat with a stretched Mo result. Against TP317L, all bands are the same except carbon. Product-analysis limits apply the A480 tolerances shown above.

Mechanical Properties of SA312 TP317

Property TP317
Tensile, min 75 ksi [515 MPa]
Yield, min 30 ksi [205 MPa]
Elongation 35% L / 25% T

The 75/30 ksi row matches the TP316 room-temperature floors. Elevated-temperature design must still use the code allowables for UNS S31700 rather than TP316 numbers, and receiving inspection should check that the certificate cites the TP317 row rather than a sister grade’s strength line.

Actual certificate values are usually comfortably above the minima, but design and acceptance still use the Table 4 row unless the purchase order states higher guaranteed values. Record the row on the datasheet so fabricators and inspectors do not substitute a sister grade’s strength line from memory, and make sure the tension test on the MTC is traceable to the heat and lot that was shipped.

Dimensions and Tolerances

TP317 pipe is normally ordered to ASME B36.19 schedules, with heavier B36.10 walls and special OD and wall combinations available by agreement. Wall thickness tolerance follows SA-312 Table 3, and outside diameter variations follow A999/A999M for the ordered size.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M. Cut lengths should not be shorter than ordered, and random or fixed length practice should be stated on the enquiry. Special walls and non-standard sizes need written mill agreement before rolling slots are booked, so raise them early if your design does not fit a standard schedule.

Equivalent Grades

Designation Notes
ASME SA-312 TP317 / UNS S31700 Governing specification for ASME code work
ASTM A312 TP317 / UNS S31700 Same chemistry and tensile rows for the referenced edition
UNS S31700 Unified numbering identity on MTC and stencil

Cross-references to EN or other national numbers are not given here, because SA-312 does not define them and near-equivalents rarely match every Table 1 limit. If a project needs a cross-standard equivalence, treat it as an engineering decision against both specifications rather than a catalogue lookup. Dual SA-312/A312 certification is straightforward when both editions are named on the order. Related grades for comparison: ASME SA312 TP316 Stainless Steel Pipe, ASME SA312 TP317L Stainless Steel Pipe, ASME SA312 UNS S31725 Stainless Steel Pipe, ASME SA312 UNS S31726 Stainless Steel Pipe.

Heat Treatment and Delivery Condition

UNS S31700 is not individually listed in Table 2, so the default solution-annealing practice applies: heat to a minimum of 1900 °F [1040 °C] and cool rapidly. TP317 is not an H grade, so there is no Table 5 grain-size requirement and no clause 6.2 reheat rule. Pipe is delivered in the solution-annealed condition, and the certificate should state the heat-treatment temperature and cooling method actually used.

Fabricators who hot form or heavily cold work TP317 bends and fittings should re-anneal to the same practice where the governing code requires it. Cite the ordered edition’s Table 2 default on the enquiry so the mill does not apply a neighbouring grade’s anneal by habit.

Corrosion Resistance

Mo 3–4% targets chloride and reducing environments where TP316 runs out of margin, such as some flue-gas, pulp-and-paper and chemical process streams. With carbon up to 0.08%, weld heat-affected zones can sensitize, which is why welded aqueous projects often choose ASME SA312 TP317L Stainless Steel Pipe. TP317 is not a 6Mo seawater alloy; for warm seawater, compare ASME SA312 UNS S31254 Stainless Steel Pipe. SA-312 publishes no corrosion rates, so service suitability needs engineering review.

Intergranular-corrosion testing to A262 or similar is a supplementary requirement and applies only when written on the purchase order, so state the practice and acceptance criteria if your client needs it. The same applies to any pitting or crevice tests requested by the end user.

Applications of SA312 TP317 Pipe

Application Why TP317 Buyer note
Chemical process lines where TP316 is marginal Mo 3.0–4.0% Consider TP317L if welded aqueous
Pulp, paper and flue-gas service Higher Mo, Cr and Ni than 316 Validate against actual medium
Projects specifying 317 by datasheet UNS S31700 identity Confirm Mo on every heat

TP317 is the standard “more molybdenum than 316” grade in SA-312 and is ordered when the corrosion basis needs that extra margin without moving to 6Mo or nickel alloys. It is less widely stocked than TP316, and many mills supply TP317L instead, so enquiries should say whether dual TP317/TP317L certification is acceptable when carbon meets 0.035%.

Weldability

Because the Table 6 filler-class pairing for TP317 is not clearly extracted, freeze the consumable by agreement on the WPS and PQR; ER317-type practice is common, but record it as a project decision. Qualify the procedure on TP317 base metal, and manage heat input to limit sensitization given carbon up to 0.08%. Mill longitudinal welds on WLD and HCW pipe are autogenous and use no filler.

Use stainless-only tooling and back-purge root passes where the specification calls for a clean root, and keep consumable lot records with the weld traveler when Section IX or B31 documentation applies. NDE extent for girth welds is a fabrication-code decision, separate from the mill hydro or electric test on each length.

Surface Finishes

Most TP317 pipe ships pickled and passivated after the solution anneal, which is the normal finish for process piping. Other finishes are order extras and should be stated on the enquiry, together with whether a roughness target applies to the OD, the ID or both.

  • Annealed and pickled (standard)
  • Bright annealed, by agreement
  • Mechanically polished OD, by agreement
  • Electropolished ID for hygienic service, by agreement

Inspection and Testing

SA-312 sets the minimum test package for every heat and length of TP317. Supplementary tests are only applied when written on the order, so the inspection and test plan should list them before production starts.

  • Heat analysis to Table 1, including every element with a limit
  • Tension test to the Table 4 row (75 ksi [515 MPa] / 30 ksi [205 MPa])
  • Flattening and, for welded pipe, the applicable weld tests
  • Hydrostatic or nondestructive electric test on each length
  • Visual and dimensional checks to Table 3 and A999
  • Optional: product analysis, IGC test, PMI, UT/RT of welds, EN 10204 3.2 witness

Packaging and Shipping

Each length is marked with SA-312 (and A312 when dual-certified), TP317 / UNS S31700, the manufacturing type, size, heat number and test method. For export, we pack in a way that protects the stainless surface from carbon steel contact and moisture during ocean transit.

  • Plastic end caps on every length
  • Bundles strapped with non-metallic or protected bands
  • Seaworthy wooden cases or crates for polished or thin-wall pipe
  • Segregation from sister grades so stencils cannot be mixed

Why Choose SHH STEEL

SHH STEEL works with qualified stainless mills to supply TP317 to the edition you name, and our job is to make sure what arrives on site matches the datasheet. That starts with reading the enquiry against the actual SA-312 rows—Table 1 chemistry, the 75 ksi [515 MPa] / 30 ksi [205 MPa] Table 4 row and the Table 2 anneal—and flagging mismatches before an order is placed. We are honest where the standard is silent: if Table 6 does not give a clear filler class, we say so rather than inventing one.

  • Seamless, welded and HCW TP317 to SA-312/A312, with dual marking when both editions are ordered
  • EN 10204 3.1 MTCs as standard; 3.2 and third-party witness by arrangement
  • Full Table 1 reporting, including molybdenum on every heat
  • B36.19 schedules plus special OD and wall by agreement
  • Export packing and heat traceability from mill to site

Supply Capability

We supply TP317 pipe from mill production and selected stock, with lead time depending on size, wall and manufacturing type. The table summarises what we can offer; please confirm the details for your order on enquiry.

Item Supply
Grade TP317 / UNS S31700
Standard ASME SA-312/SA-312M, ASTM A312/A312M (dual by agreement)
Routes SML, WLD, HCW
Sizes ASME B36.19 schedules; special OD and wall by agreement
Filler guidance by agreement (Table 6 pairing not clearly extracted)
Certificates EN 10204 3.1; 3.2 by arrangement

Standard schedules can often ship from stock or short mill runs, while heavy-wall seamless and special sizes need a rolling slot. Send the edition, grade and UNS, size list, quantities and required date, and we will separate stock lengths from made-to-order items in our quotation so your site dates are realistic.

FAQ

Is ASME SA312 the same as ASTM A312?
For chemistry, tensile requirements, manufacturing types and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking for TP317 is common when ordered. Name both editions on the purchase order and the certificate so inspectors can verify the heat against the exact books you cited; a bare market stamp does not prove dual certification.
What is the UNS number for TP317?
Table 1 lists TP317 as UNS S31700. Use that UNS on the purchase order, the stencil and the MTC so the chemistry and tensile rows stay unambiguous. When a project mixes plate, fittings and pipe, carry the same UNS language across all forms, but still order pipe to SA-312/A312 rather than to a plate specification.
TP317 vs TP317L — which should I order?
The chemistry is identical except carbon: TP317 allows C up to 0.08%, TP317L caps it at 0.035%, and both are released at 75/30 ksi. Choose TP317L for welded aqueous service where sensitization matters. Dual TP317/TP317L certification is possible when the heat meets the lower carbon limit; write that acceptance on the purchase order.
TP317 vs TP316 — which should I order?
TP317 carries Mo 3.0–4.0% with Cr 18–20% and Ni 11–15%, against Mo 2–3% in TP316. Both share the 75/30 ksi row. Order TP317 when the corrosion basis needs the extra molybdenum; otherwise TP316 is cheaper and easier to source. Settle the grade on the datasheet before price comparison.
Seamless vs welded TP317 — which is better?
Neither is universally better. Seamless suits small-bore, thick-wall and pressure parts where the piping class excludes welds, while welded and HCW pipe are economical for larger sizes and offer good wall consistency. Choose the route your design code and datasheet allow, state SML, WLD or HCW on the order, and confirm the same letters on the marking and certificate.
Hydrostatic test vs NDE — which do I get?
Each length of TP317 is either hydrotested or nondestructively electrically tested, and the manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification requires one method, state it on the order and check that the chosen test appears on the certificate for every length; a silent mill choice is not an approved project method.
What heat treatment applies to TP317?
UNS S31700 is not individually listed in Table 2, so the default solution anneal at a minimum of 1900 °F [1040 °C] with rapid cooling applies. TP317 is not an H grade, so there is no Table 5 grain-size rule. Delivery is in the solution-annealed condition, and the certificate should state the temperature and cooling used so the record is complete.
What Table 1 chemistry defines TP317?
Table 1 for UNS S31700: C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%. These are melting-analysis limits from the ordered edition, so do not invent tighter catalogue windows. When product analysis is needed, order it explicitly through Supplementary Requirement S1 or PO wording, and the A480 tolerances shown in the chemistry section then apply.
What are the Table 4 tensile requirements for TP317?
Table 4 minima for TP317 are 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield, with elongation of 35% longitudinal and 25% transverse. Actual certificate values are usually higher, but design and acceptance use Table 4 unless the order states higher guarantees. Record the row on the datasheet so nobody substitutes a sister grade’s line from memory.
What filler metal should I use to weld TP317 pipe?
Table 6 lists TP317 in the grade column but the filler-class pairing is not clearly populated in the edition extract, so filler is by agreement. Freeze the AWS or EN class on the WPS and PQR before production welding and qualify the procedure on TP317 base metal. Mill longitudinal welds on WLD and HCW pipe are autogenous, so Table 6 guidance applies only to joints made with filler, not to the mill seam.
How much molybdenum is in TP317?
Table 1 requires Mo 3.0–4.0% for TP317 / UNS S31700, a full point above the TP316 band. Confirm molybdenum on the heat analysis, and on product analysis allow only the ±0.10 A480 tolerance. A certificate showing Mo just under 3.0% on the heat analysis is not TP317, however close it looks.
Is TP317 an H grade for creep service?
No. TP317 has no carbon floor, no Table 5 grain-size rule and no clause 6.2 reheat requirement, so it is not an H grade. It is chosen for corrosion resistance rather than creep strength. Use the code allowables for UNS S31700 at the design temperature and do not apply H-grade assumptions to the order or the certificate review.

Conclusion

ASME SA312 TP317 (UNS S31700) is the higher-molybdenum 316 companion: C ≤0.08%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%, released against 75/30 ksi Table 4 minima with a Table 2 default 1900 °F [1040 °C] anneal. The Table 6 filler pairing is not clearly extracted, so the consumable is agreed on the WPS. It is not an H grade and not interchangeable with TP317L or TP316. State the manufacturing type, schedule or wall and finish on the enquiry, and ask for the heat certificate with molybdenum clearly reported. For stock checks, mill certificates or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X