ASME SA312 TP348 Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 TP348 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 TP348 (UNS S34800) Nb-stabilized stainless steel pipe with Ta ≤0.10% to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with footnote G Nb ≥10×C, 75/30 ksi Table 4 minima and EN 10204 3.1 MTCs.
Grade
TP348 / UNS S34800
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 TP348 Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. Grade TP348 is listed in Table 1 as UNS S34800. Commercially the same product is often called SA312 TP348 pipe, ASTM A312 TP348 pipe, A312 Grade TP348, or 348 stainless steel pipe, but for code work the purchase order and mill test certificate should carry the full grade, the UNS number, and the edition of the standard rather than a bare market label.

TP348 is the niobium-stabilized sister of ASME SA312 TP347 Stainless Steel Pipe, with the same footnote G rule (Nb ≥10×C and ≤1.00%) and the same 17.0–19.0% chromium / 9.0–13.0% nickel window, plus an explicit tantalum ceiling of 0.10% that TP347 does not carry. Niobium forms very stable carbides, which keeps chromium in solution next to welds and makes the grade a long-standing choice for welded service in the sensitizing temperature range; the Ta limit exists because some nuclear and specialty specifications want that residual controlled on the heat. Table 1 sets C ≤0.08%, Nb at least 10×C with a 1.00% ceiling, and Ta ≤0.10%; molybdenum is not required. Table 4 minima are 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield with 35% longitudinal / 25% transverse elongation. It is not an H grade: Table 2 uses the default 1900 °F [1040 °C] minimum solution-annealing temperature, and there is no Table 5 grain-size mandate. Table 6 filler guidance is ER347, and supplementary requirement S6 (stabilization heat treatment) applies only when the purchase order calls for it.

SHH STEEL can supply ASME SA312 TP348 stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) routes, in ASME B36.19 schedules as well as special OD and wall combinations by agreement. Every shipment carries EN 10204 3.1 mill test certificates that report Nb, Ta, and carbon so the stabilizer rule and Ta ceiling can be checked, and dual SA-312/A312 marking is available when the heat analysis, heat treatment, mechanical tests, and marking satisfy both editions named on the order. Send NPS, wall or schedule, finish, length practice, and any product-analysis or supplementary tests with the enquiry so we can quote the right mill route first time.

The common commercial names below all point to the same product, provided the order clearly references SA-312 or A312 and the grade rules are met:

  • ASME SA312 TP348 / SA-312 Grade TP348 — preferred marking language for ASME-code and dual-marked pipe
  • ASTM A312 TP348 — same chemistry and tensile tables when the ASTM edition is referenced
  • UNS S34800 — unified number used on MTCs and in allowable-stress tables
  • 348 stainless steel pipe — market shorthand; confirm the Nb ≥10×C / Ta ≤0.10% rules and carbon band on the order

TP348 and ASME SA312 TP348H Stainless Steel Pipe are separate Table 1 rows with different carbon bands and stabilizer multipliers, so a heat certified to one does not automatically qualify as the other unless the MTC proves both sets of limits and the order asks for dual grading. Related grades: ASME SA312 TP347 Stainless Steel Pipe, ASME SA312 TP347LN Stainless Steel Pipe, ASME SA312 TP348H Stainless Steel Pipe. Hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 defines three manufacturing routes that may be marked on finished TP348 pipe. Selecting the route is a purchase-order decision driven by design code, size range, wall thickness, and inspection preference. It does not change the Table 1 chemistry of Grade TP348—melting must still meet C ≤0.08%, Nb at least 10×C with a 1.00% ceiling, and Ta ≤0.10%.

  • Seamless (SML) — no welding at any stage of manufacture. Seamless is preferred when the project specification excludes welded pipe, when thick walls favor seamless production, or when the piping class documentation is written around seamless product only.
  • Welded (WLD) — automatic welding without filler metal. The weld is finished so that the pipe meets dimensional and mechanical requirements after the final heat treatment required by SA-312. Welded product is widely used for common NPS and schedule combinations where the code accepts welded austenitic pipe.
  • Heavily cold-worked (HCW) — welded pipe that is cold worked to a reduction of area of wall and weld of at least 35% before the final anneal, again without filler metal in the longitudinal weld. HCW is ordered when the buyer wants the HCW marking and the process controls written into SA-312 for that route.

Each finished length is hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Marking on the pipe typically includes the manufacturer, grade (TP348), heat number, NPS or outside diameter and schedule or wall thickness, and the manufacturing type letters SML, WLD, or HCW. When comparing seamless versus welded TP348 offers, check manufacturing type and the hydro or NDE method on the mill test certificate—not only the grade stamp.

Chemical Composition of SA312 TP348

Two chemistry layers matter for TP348: the melting (heat or ladle) analysis, which is mandatory for every heat under ASME SA-312/ASTM A312 Table 1, and product analysis on finished pipe, which applies only when ordered through Supplementary Requirement S1 or PO wording. Product-analysis tolerances are referenced from A999/A999M §6.3 to ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values and, when ordered, product values—never unpublished tighter windows.

Melting analysis (heat / ladle analysis) — Table 1

Heat analysis for Grade TP348 / UNS S34800 from ASME SA-312/SA-312M (ASTM A312/A312M) Table 1 is summarized below. Values are maximum unless a range is shown, and ellipses (…) mean the ordered edition places no requirement on that element.

Element TP348 / UNS S34800 melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) No requirement (…)
Niobium (Nb) ≥ 10 × C and ≤ 1.00% (footnote G)
Tantalum (Ta) ≤ 0.10
Nitrogen (N) No requirement (…)

Source: ASME SA-312/SA-312M ≡ ASTM A312/A312M Table 1 for Grade TP348, including footnote G (Nb ≥10×C and ≤1.00%) and Ta ≤0.10%. The niobium minimum is not a fixed number; it moves with the actual carbon of each heat. Example: at C = 0.05%, Nb must be at least 0.50% and no more than 1.00%. Also confirm Ta ≤0.10% on the same heat analysis. Footnote M confirms that niobium (Nb) and columbium (Cb) are the same element. OCR of some editions may show the Nb cell as an ellipsis with Ta listed separately—treat Nb via footnote G and the Ta 0.10% ceiling as ASTM practice for 348.

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

When product analysis is ordered, finished-pipe chemistry shall meet Table 1 as modified by the tolerances in ASTM A480/A480M Table A1.1. The resulting limits used for TP348 receiving inspection are:

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.10 under / 0.15 over 8.90 – 13.15
Niobium (Nb) ≥ 10 × C, ≤ 1.00 0.05 under / over on applicable limit Per heat calculation
Tantalum (Ta) ≤ 0.10 0.05 over ≤ 0.15

Versus TP347: chemistry is essentially the same Nb-stabilized 18–10 window, but TP348 adds the explicit Ta ≤0.10% ceiling that TP347 does not publish. Versus TP348H: the H grade uses footnote H (Nb ≥8×C, 1.0% max) with a 0.04–0.10% carbon band, grain-size control, and higher anneal temperatures. Versus TP347LN: LN uses a low-carbon, nitrogen-bearing Nb band rather than the carbon-ratio rule. If an enquiry only says “348 stainless pipe”, confirm Ta reporting, the Table 1 limits, manufacturing type, and whether product analysis is needed before the mill books a rolling slot.

Mechanical Properties of SA312 TP348

Tensile requirements for TP348 are given in ASME SA-312/SA-312M (ASTM A312/A312M) Table 4. Specimens and orientation follow the testing clauses of the standard and the referenced general requirements in A999/A999M.

Property TP348
Tensile, min 75 ksi [515 MPa]
Yield, min 30 ksi [205 MPa]
Elongation 35% L / 25% T

TP348-family pipe uses a single 75/30 ksi row regardless of route and wall. These are the mandatory acceptance floors; actual MTC values are usually higher, but design should still use Table 4 and the allowable-stress tables for UNS S34800 unless the purchase order states higher guaranteed values that the mill has accepted in writing.

Hardness: Table 4 does not list a separately mandated hardness maximum for TP348. If hardness matters for fabrication or end-user acceptance, state the limit on the purchase order and verify it on the MTC. Flattening or bend and tension tests run on a lot basis, and supplementary tests apply only when they are listed on the order.

Dimensions and Tolerances

Dimensional practice for austenitic stainless steel pipe ordered to SA-312 typically follows ASME B36.19 / B36.19M stainless-steel pipe schedules. Outside diameter and wall thickness are stated as NPS and schedule, or as OD and specified wall. Common schedules for TP348 enquiry include Schedule 5S, 10S, 40S, and 80S. Other walls and non-standard OD/wall combinations are available by agreement when both the mill and the order accept them.

Size coverage in commercial practice is summarized below. Confirm large NPS and heavy walls against mill capability for the chosen manufacturing type before you lock the purchase order.

  • NPS / DN: commonly from NPS 1/8 upward; large NPS and heavy walls depend on manufacturing type (SML versus WLD/HCW) and mill capability—confirm on enquiry
  • Schedules: 5S, 10S, 40S, 80S and special walls by agreement
  • Length: single random (SRL), double random (DRL), or fixed cut lengths as stated on the purchase order
  • Ends: plain end (PE), beveled end (BE), or other end preparations by agreement

Wall-thickness variation limits from SA-312 Table 3 (t/D = specified wall / ordered OD) are the acceptance bands used on mill test certificates and receiving inspection for TP348:

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M. OD, wall, and length tolerances follow SA-312 via ASTM A999/A999M and the dimensional standard on the order. SHH STEEL quotes the applicable clause rather than dumping entire A999 tables. Confirm max wall and NPS near the edge of B36.19 practice before acceptance.

Equivalent Grades

Equivalence for TP348 has to be stated carefully. Regional designations help selection discussions, but they are not automatic one-to-one substitutes for ASME pressure-code pipe without an approved material specification and design-code acceptance.

Designation Notes
ASME SA-312 / ASTM A312 Grade TP348 Governing pipe product standard for this article
UNS S34800 Unified number listed in Table 1
TP347 (UNS S34700) Nb-stabilized sister without the Ta ≤0.10% ceiling
TP348H (UNS S34809) H grade: C 0.04–0.10%, Nb ≥8×C, Ta ≤0.10%, grain size No. 7 or coarser
TP347LN (UNS S34751) Low-carbon, nitrogen-bearing Nb grade with Nb 0.20–0.50%
TP321 (UNS S32100) Ti-stabilized sister; Ni up to 12.0%

Within SA-312, do not swap TP348 for a sister grade just because they share a “348” or “347” market label—each has its own Table 1 row, and only the 348 family carries the explicit Ta control. Related pages: ASME SA312 TP347 Stainless Steel Pipe, ASME SA312 TP348H Stainless Steel Pipe, ASME SA312 TP347LN Stainless Steel Pipe, ASME SA312 TP321 Stainless Steel Pipe. Hub: ASME SA 312/SA 312M.

Pressure-code caution: EN, JIS, or proprietary approximations do not authorize B31 or Section VIII substitution without engineered approval and an accepted material specification on the design documents. EN maps for 348 are soft in this pack and should be rechecked against the ordered edition.

Heat Treatment and Delivery Condition

All pipe furnished to ASME SA-312 shall be heat treated. TP348 does not carry an individual temperature row in Table 2, so the default minimum solution-annealing temperature of 1900 °F [1040 °C] applies, followed by water quenching or another rapid cool sufficient to prevent harmful carbide reprecipitation. That default is SHH STEEL’s delivery baseline unless the ordered edition states otherwise.

TP348 is not an H grade, so there is no Table 5 grain-size mandate or clause 6.2 reheating requirement. When the purchase order invokes supplementary requirement S6, a stabilization heat treatment at an agreed temperature below the solution anneal is required; it is not automatic, and it is worth deciding at enquiry stage because it adds a furnace step. HCW cold reduction is done before the final anneal; delivery remains the annealed condition.

Commercial delivery condition for TP348 typically includes the following unless the purchase order or ordered edition states otherwise:

  • Solution annealed to SA-312 Table 2 requirements for TP348
  • Pickled and descaled, or bright annealed, as ordered (see Surface Finishes)
  • Straightened and cut to the ordered length practice
  • Hydrotested or NDE-tested per length as required by the standard and the purchase order

Corrosion Resistance

TP348 is chosen where welded construction or service in the sensitizing range would put an unstabilized grade at risk of intergranular attack. Niobium combines with carbon before chromium can, so the chromium-depleted zones that cause weld decay are much less likely to form. SA-312 itself does not publish corrosion rates, so fitness for a given fluid, temperature, and velocity still has to come from the project corrosion specification. The purchase specification for this grade also wants tantalum residual controlled at ≤0.10%, which is the practical difference from TP347 on the same stabilizer concept.

Versus sister grades: ASME SA312 TP348H Stainless Steel Pipe and ASME SA312 TP321 Stainless Steel Pipe share the stabilized 18–10 concept but differ in carbon band, stabilizer element, or nickel range. They are not automatic drop-in replacements when the datasheet fixed UNS S34800.

Versus Mo-bearing grades: stabilization does not add pitting resistance. When chloride pitting, crevice attack, or reducing media dominate, molybdenum-bearing austenitics such as ASME SA312 TP316L Stainless Steel Pipe are usually the better choice. Mill annealed-and-pickled pipe already has a descaled surface; site welds and grinding should be cleaned and passivated when the end-user specification requires it, and intergranular-corrosion testing applies only when written on the order.

Applications of SA312 TP348 Pipe

TP348 pipe is selected where austenitic stainless behavior, SA-312 product form, and stabilized chemistry for welded or sensitizing service are all needed. Typical application areas include:

Application area Typical use of TP348 pipe Selection note
Welded process lines Lines exposed to the sensitizing range during welding or service Prove the stabilizer rule on the MTC
Exhaust, expansion-joint and heater piping Intermittent elevated-temperature duty without H-grade creep design Use TP348H when the design is creep-governed
Chemical and refining utility Oxidizing or mildly corrosive service specified with stabilized 18–10 chemistry Prefer Mo grades if chlorides dominate
Code piping packages Dual SA-312/A312 projects with heat traceability Name edition, route, and UNS on the enquiry

Plants that already run TP348H or TP321 sometimes buy TP348 in the same package, which is sensible for logistics but only when each line’s datasheet actually allows the grade being shipped to it. Match the grade to the corrosion and code case first; commercial convenience comes second.

Weldability

TP348 is generally weldable by common austenitic fusion processes with suitable heat input, interpass control, and joint cleanliness. Typical processes used on this grade include:

  • GTAW (TIG) — preferred for root passes and thin-wall pipe where weld metal cleanliness and heat-input control matter
  • GMAW (MIG) — productive for fill and cap passes on thicker walls when procedures are qualified
  • SMAW — widely used for field girth welds with coated austenitic electrodes selected by agreement
  • Automatic orbital or mechanized GTAW — common for repetitive high-integrity girth joints

Stabilization lowers HAZ sensitization risk compared with unstabilized 304-type heats, but low heat input and controlled interpass are still good practice. These are engineering choices on the WPS, not automatic SA-312 requirements on every order.

Filler metal: SA-312 Table 6 maps TP348 to ER347. Qualify the AWS (or EN) classification on the WPS/PQR using actual TP348 base metal and freeze it before production welds. Mill longitudinal welds on WLD and HCW product are made without filler metal, so Table 6 applies to joining with filler, not to the mill seam.

Girth welds follow the piping/vessel code (e.g. ASME B31 / Section IX) and are separate from mill hydro/NDE. Specify girth NDE on fabrication documents when required. Keep joints clean of oil, paint, and carbon-steel contamination.

Surface Finishes

Surface condition for SA312 TP348 pipe is stated on the purchase order. Typical mill finishes available from SHH STEEL supply include the following options:

  • Annealed and pickled (AP) — solution annealed, descaled in acid pickle or an equivalent process, producing a matte gray finish common for process and utility pipe
  • Bright annealed (BA) — annealed in a protective atmosphere to a brighter surface where the order allows and mill capability exists for the size
  • Mechanically polished — for example 180#, 320#, or 400# grit, or Ra-controlled polish on OD and/or ID for hygienic or architectural duty; polishing does not replace solution annealing
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed for WLD/HCW product

Passivation after pickle or polish can be added when the end-user specification requires it. For hygienic or high-purity lines, state both the Ra (or grit) target and the documentation package—including any surface roughness reports—on the enquiry. SHH STEEL will not imply a polished hygienic finish on standard AP pipe unless the purchase order says so. End preparation (plain or beveled) should be ordered together with finish so that bevel faces and ID cleanliness meet the same acceptance language.

Inspection and Testing

Base inspection and testing for SA-312 TP348 pipe combines chemistry, mechanical, and integrity checks. The following items form the usual acceptance package; supplementary requirements apply only when written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for TP348 (UNS S34800), including C ≤0.08%, Nb at least 10×C with a 1.00% ceiling, and Ta ≤0.10%
  • Product analysis — when ordered (Suppl. S1 / purchase-order language), using A480 Table A1.1 tolerances via A999 §6.3
  • Tension test — Table 4 tensile, yield, and elongation on a lot basis (75/30 ksi minima)
  • Flattening test — or alternate bend where the standard permits for certain welded pipe
  • Hydrostatic test or nondestructive electric test — each length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD/wall and the applicable tolerance clauses

Mill test certificates: EN 10204 3.1 is the standard documentation package from SHH STEEL supply. EN 10204 3.2 or third-party witness (SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency) is arranged when specified and should be booked before final testing. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy the edition(s) named on the order.

Optional / supplementary: PMI, RT/UT, intergranular corrosion or weld-decay tests, tighter straightness, special marking—only when listed on the PO. Keep heat numbers on cut pieces for MTC traceability.

Packaging and Shipping

Export and domestic shipments of SA312 TP348 pipe are packed for handling and ocean or land transport. Typical packing practices from SHH STEEL supply include:

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with separators where needed to protect finish
  • End caps / protectors — plastic or metal caps on plain or beveled ends to reduce damage and contamination during transit
  • Marking — durable marking of grade (TP348), UNS S34800 when required, heat number, size (NPS or OD × wall / schedule), manufacturing type (SML / WLD / HCW), and mill identity as required by SA-312 and the purchase order
  • Export packing — waterproof wrapping as agreed for polished or sensitive finishes; container stuffing photos on request

Segregate TP348 from TP348H and TP321 on the packing list and in the yard so stencil mix-ups do not travel with the shipment. Shipment docs typically include packing list, invoice, B/L or AWB, and MTC (3.1 or 3.2), plus origin/customs papers per Incoterms. State destination, packing preference, and extra marking at enquiry.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe and plate. For ASME SA312 TP348 / UNS S34800 we quote against the edition you name, report the carbon and niobium (columbium) values the stabilizer rule depends on, and keep heat identity unbroken from melt to finished length, so receiving inspection can clear each heat against Table 1 and Table 4 instead of a generic “348” catalog sheet.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for TP348 (S34800), not unpublished tighter windows
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability
  • Documentation — EN 10204 3.1 MTCs standard; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both requirements you name
  • Related grades — TP348H, TP321, and other stabilized austenitic SA-312 grades for matched packages
  • Export packing — seaworthy bundles, end protectors, and durable grade/heat/size/type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, finish, and any supplementary tests such as S6, so the documents that arrive with the pipe match the documents your inspector expects. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 TP348 / UNS S34800 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for TP348
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M Grade TP348 (UNS S34800)
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; bright annealed or polished by agreement
Testing Tension, flattening/bend, hydro or NDE per length; S6 when ordered; supplementary tests on order
Documents EN 10204 3.1; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock moves with mill rolling cycles. Enquiries should state the SA-312 edition, SML/WLD/HCW, NPS or OD×wall, length practice, and any product-analysis or 3.2 requirements so mill slots align with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders.

FAQ

Is ASME SA312 the same as ASTM A312?
For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and mill test certificate so inspectors can verify the heat against the exact books you cited—do not assume a bare market grade stamp covers dual certification.
What is the UNS number for TP348?
Table 1 lists TP348 as UNS S34800. Use that UNS on the purchase order, stencil, and MTC so the chemistry and tensile rows stay unambiguous, and so designers pull allowable stresses for the right material. TP348H has its own UNS (S34809) and should never be assumed from a shared “348” market name.
TP348 vs TP347 — which should I order?
Both use footnote G (Nb ≥10×C, ≤1.00%) with C ≤0.08%, Cr 17–19%, and Ni 9–13%. TP348 adds the explicit Ta ≤0.10% ceiling that TP347 does not publish. Order TP348 when the datasheet or owner specification names S34800 or requires Ta control; otherwise TP347 is the more common commercial choice for the same stabilizer concept.
TP348 vs TP348H — which should I order?
TP348 uses C ≤0.08% with Nb ≥10×C, while TP348H uses C 0.04–0.10% with Nb ≥8×C, Ta ≤0.10%, grain size No. 7 or coarser, and higher Table 2 anneal temperatures. Choose the H grade when the design is creep-governed; otherwise the standard grade is usually adequate. Fix the grade and UNS on the datasheet before comparing prices.
Seamless vs welded TP348 — which is better?
Neither is universally better. Choose the manufacturing type your design code and datasheet allow; both are legitimate SA-312 forms when tested to the standard. State SML, WLD, or HCW on the order and confirm the same letters on the marking and MTC, because the tensile row for this grade does not change with route but the owner class often does.
Can you dual-certify SA312 / A312 TP348?
Yes, when the heat analysis, heat treatment, mechanical tests, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the PO and require the MTC to reference both books, so receiving inspection can clear the heat without a second paperwork chase after shipment.
Hydrostatic test vs NDE — which do I get?
Each length is hydrotested or nondestructively electrically tested. Manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification locks one method, state it on the PO and verify the chosen test appears on the MTC for every length—silent mill option is not the same as an approved project method.
What heat treatment applies to TP348?
TP348 uses the Table 2 default of 1900 °F [1040 °C] minimum with rapid cooling. It is not an H grade, so there is no grain-size mandate. S6 stabilization at an agreed temperature below the solution anneal applies only when the purchase order invokes it, and the MTC should then record it.
What Table 1 chemistry defines TP348?
Table 1 sets C ≤0.08%, Nb ≥10×C and ≤1.00% (footnote G), Ta ≤0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Mn ≤2.00%, Si ≤1.00%, P ≤0.045%, and S ≤0.030%; molybdenum is not required. These are melting-analysis limits, and product analysis on finished pipe must be ordered explicitly if receiving inspection needs it.
What are the Table 4 tensile requirements for TP348?
Table 4 minima are 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield with 35% longitudinal / 25% transverse elongation. Actual MTC values are often higher, but design still uses Table 4 unless the PO states higher guarantees. Record the correct row on the datasheet so fabricators do not substitute a sister-grade strength line from memory.
What filler metal should I use to weld TP348 pipe?
SA-312 Table 6 maps TP348 to ER347. Qualify and freeze the AWS or EN class on the WPS/PQR before production welds. Mill WLD and HCW longitudinal welds are autogenous, so Table 6 applies to joining with filler in fabrication, not to the mill seam.
Why does TP348 control tantalum?
Table 1 sets Ta ≤0.10% for TP348 (and TP348H) as an explicit residual limit alongside the Nb stabilizer rule. Some nuclear and specialty specifications want that residual controlled on the heat; TP347 does not publish the same Ta ceiling. Ask for Ta as an actual value on the MTC, and treat OCR editions that show Nb as an ellipsis with Ta listed separately as still governed by footnote G plus the 0.10% Ta max.

Conclusion

ASME SA312 TP348 (UNS S34800) is the standard-carbon Nb-stabilized austenitic pipe grade in SA-312 that adds an explicit Ta ≤0.10% ceiling to the same footnote G rule used by TP347 (Nb ≥10×C and ≤1.00%). Table 4 minima are 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield with 35% L / 25% T elongation; heat treatment follows the default 1900 °F [1040 °C] minimum; Table 6 filler guidance is ER347; and S6 stabilization applies only when specified. Order the manufacturing type (SML/WLD/HCW), schedule or wall, finish, Ta reporting, and any product analysis or supplementary tests explicitly, and keep TP347 and TP348H heats segregated. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X