ASME SA312 TP304N / UNS S30451 nitrogen-strengthened stainless steel pipe in SML, WLD and HCW, with N 0.10–0.16%, an 80/35 ksi Table 4 floor and a 1900 °F solution anneal, supplied by SHH STEEL to ASME B36.19 with EN 10204 3.1 MTCs.
Grade
TP304N / UNS S30451
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Dimensions
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 TP304N Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe for high-temperature and general corrosive service, and it is the ASME Code adoption of ASTM A312/A312M. TP304N / UNS S30451 is classic 18-8 stainless with one deliberate change: a required nitrogen content. It keeps the chromium, nickel, and carbon limits of ASME SA312 TP304 Stainless Steel Pipe and uses nitrogen to lift the strength floor, so buyers get a stronger 304 that welds, forms, and corrodes like 304 in almost every other respect.

Table 1 sets C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16%, with footnote C leaving the nitrogen method to agreement. Table 4 sets 80 ksi [550 MPa] tensile and 35 ksi [240 MPa] yield minimum with 35% longitudinal / 25% transverse elongation, against 75/30 ksi for TP304. TP304N is not individually listed in Table 2, so the default 1900 °F [1040 °C] minimum anneal applies, and Table 6 lists ER308 as the filler. Nitrogen strengthens the austenite interstitially without forming grain-boundary carbides and helps keep the structure stable during cold work and at cryogenic temperature.

SHH STEEL can supply ASME SA312 TP304N stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) form. We quote ASME B36.19 schedules and special OD/wall by agreement, ship with EN 10204 3.1 mill test certificates reporting nitrogen inside the 0.10–0.16% band and the 80/35 ksi results, and offer dual SA-312/A312 marking when the heat and tests meet both editions. TP304N is usually a mill-order grade, so please confirm NPS, wall or schedule, finish, and any supplementary tests early.

The names below are the ones buyers commonly use, and they map to the ordered product as shown. Put both TP304N and S30451 on the order, because “304N” is easily misread as 304 or 304LN somewhere between purchasing, the mill, and the yard.

  • ASME SA312 TP304N / UNS S30451 — preferred marking language for ASME-code and dual-marked pipe
  • ASTM A312 TP304N — same grade tables when the ASTM edition is referenced
  • “304N” pipe — common shorthand; the certificate must show the nitrogen band and the 80/35 ksi results
  • EN 1.4315 / JIS SUS304N1 — commonly cited regional equivalents, approximate only

Sister grades buyers compare with TP304N include ASME SA312 TP304 Stainless Steel Pipe (no nitrogen requirement and 75/30 ksi), ASME SA312 TP304LN Stainless Steel Pipe (low carbon with the same nitrogen band and 75/30 ksi), ASME SA312 TP304L Stainless Steel Pipe, and ASME SA312 TP316LN Stainless Steel Pipe when molybdenum is also wanted. It is also distinct from high-manganese nitrogen grades such as ASME SA312 TP201 Stainless Steel Pipe. Grade hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 recognizes three manufacturing routes for TP304N pipe, and the route is a purchase-order decision driven by the design code, the size range, wall thickness, and how the owner wants the pipe inspected. The route never changes the chemistry: whichever way the pipe is made, the heat must still meet C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16%, and every length must still go through the solution anneal at 1900 °F [1040 °C] minimum before it is released.

  • Seamless (SML) — no welding at any stage. Seamless is typical for heavy walls, power-plant lines, and piping classes written around seamless product; it still has to be solution annealed before release.
  • Welded (WLD) — automatic welding without filler metal, with the weld finished so the pipe meets dimensional and mechanical requirements after the final heat treatment. The strip or plate heat must itself carry the full TP304N chemistry, so ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked to at least 35% reduction of wall and weld before the final anneal, again without filler in the longitudinal seam, with the weld radiographed before cold work. Order HCW when the project specifically wants that marking and the process controls SA-312 writes around it.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser accepts a system test in place of the hydrotest, and lots for mechanical testing follow clause 11.1. Clause 18.1.3 lists TP304N among the grades covered by the government-procurement provisions, which matters on some public projects. Check the SML, WLD, or HCW letters and the hydro or NDE method on the certificate when comparing offers, and make sure the mill has a reliable nitrogen analysis method for the heat.

TP304N is far less common in stock than TP304 or TP304L, so most orders are planned mill runs, and minimum quantities can apply on seamless sizes. Give us the route, sizes, wall, edition year, and need date early, and we will tell you honestly whether a mill slot or a substitute discussion with your designer makes more sense.

Chemical Composition of SA312 TP304N

Two chemistry layers matter for TP304N. The melting (heat or ladle) analysis is mandatory for every heat under SA-312/A312 Table 1, while product analysis on finished pipe applies only when it is ordered through Supplementary Requirement S1 or purchase-order wording. Product tolerances are not printed in SA-312 itself; they come through ASTM A999/A999M §6.3 from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values and, when ordered, the product values, and never quotes tighter catalogue windows that the standard does not publish.

The tables below reproduce the Table 1 heat analysis for TP304N, the product-analysis limits that result from applying the A480 Table A1.1 tolerances, and a comparison with the other 304-family rows. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element.

Melting analysis (heat / ladle analysis) — Table 1

Element TP304N (UNS S30451) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Nitrogen (N) 0.10 – 0.16
Molybdenum (Mo) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 11.0 0.10 under / 0.15 over 7.90 – 11.15
Nitrogen (N) 0.10 – 0.16 0.01 under / over 0.09 – 0.17
Grade UNS C Ni N
TP304 S30400 ≤ 0.08 8.0 – 11.0 …
TP304L S30403 ≤ 0.035 8.0 – 13.0 …
TP304H S30409 0.04 – 0.10 8.0 – 11.0 …
TP304N S30451 ≤ 0.08 8.0 – 11.0 0.10 – 0.16
TP304LN S30453 ≤ 0.035 8.0 – 12.0 0.10 – 0.16

Nitrogen at 0.10–0.16% is the defining element and the first value to check on receipt. Ordinary 304 heats carry some residual nitrogen, but not enough to meet this band, which is why TP304N has to be melted on purpose rather than picked from 304 stock. Because carbon and nickel are the same as ASME SA312 TP304 Stainless Steel Pipe, dual TP304/TP304N certification is possible when the nitrogen is in the band and the tensile results meet 80/35 ksi; the comparison table shows how ASME SA312 TP304LN Stainless Steel Pipe differs only in its 0.035% carbon ceiling and 8.0–12.0% nickel window.

On product analysis the finished pipe may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20%, Ni 7.90–11.15%, and N 0.09–0.17%. Footnote C leaves the nitrogen method to agreement between purchaser and manufacturer, so if your inspector wants a particular method, write it on the purchase order before the heat is tested.

Mechanical Properties of SA312 TP304N

Room-temperature tensile requirements for TP304N come from SA-312 Table 4 and are summarized below. These are minimum release values for the lot, not typical values, and design allowables must always be taken from the governing code tables for UNS S30451 rather than from a neighbouring grade.

Property (SA-312 Table 4) TP304N
Tensile strength, min 80 ksi [550 MPa]
Yield strength (0.2% offset), min 35 ksi [240 MPa]
Elongation in 2 in. or 50 mm (or 4D), min 35% longitudinal / 25% transverse
Hardness No maximum listed in Table 4
Grade Tensile min, ksi [MPa] Yield min, ksi [MPa]
TP304L 70 [485] 25 [170]
TP304 / TP304H 75 [515] 30 [205]
TP304LN 75 [515] 30 [205]
TP304N 80 [550] 35 [240]

The 80/35 ksi floor is the main commercial reason to choose TP304N, and it is higher than both ASME SA312 TP304 Stainless Steel Pipe and ASME SA312 TP304LN Stainless Steel Pipe at 75/30 ksi. Higher code allowables for UNS S30451 can allow a thinner wall at the same pressure, but that is a design decision that must use the code tables for S30451, not an assumption made at purchasing. Table 4 lists no hardness maximum for TP304N.

Certificate results are normally above the minima, but design should still use Table 4 and the code tables unless the mill has accepted higher guarantees in writing. Elongation stays at 35% longitudinal and 25% transverse, so formability for bending and flaring is not given up in exchange for the extra strength.

Dimensions and Tolerances

Dimensional supply for SA312 TP304N pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow SA-312 Table 3 as summarized below. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M.

  • Lengths — single random, double random, or cut-to-length on order
  • Cut lengths — typically no more than 1/4 in. [6 mm] over the ordered length unless the PO states a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face when the WPS is already frozen

Many power, cryogenic, and process buyers order by OD × wall rather than NPS and schedule, which is fine as long as the enquiry says so clearly. Straightness, end finish, and length tolerance should be written into export orders so receiving inspection has an agreed acceptance basis instead of arguing after arrival. On thin schedules with threaded or socket-weld ends, check that the remaining wall is still adequate after the 12.5% under-tolerance. Jointers are not permitted unless the purchase order allows them, so cut-to-length programmes should include an allowance for fit-up scrap rather than expecting the mill to ship short pieces.

Equivalent Grades

TP304N / UNS S30451 has commonly cited equivalents in European and Japanese standards, but the nitrogen bands and strength floors of those designations do not always match. Any cross-reference is a materials discussion, not a substitution approval for pressure-code pipe.

Designation Relationship to TP304N
ASME SA-312 / ASTM A312 TP304N Governing pipe grade
UNS S30451 Unified number in Table 1
ASME SA-240 / A240 304N Plate and sheet counterpart (separate specification)
EN 1.4315 (X5CrNiN19-9) Commonly cited European nitrogen-alloyed 304; verify chemistry and strength in the EN standard
JIS SUS304N1 Commonly cited Japanese counterpart; verify against JIS

EN 1.4315 and JIS SUS304N1 are commonly cited approximate equivalents that were not verified against the EN or JIS texts for this page, and they do not authorize B31 or Section VIII substitution without engineered approval. Within SA-312, ASME SA312 TP304 Stainless Steel Pipe lacks the nitrogen requirement and ASME SA312 TP304LN Stainless Steel Pipe adds low carbon at a lower 75/30 ksi floor. Related: ASME SA312 TP304L Stainless Steel Pipe and ASME SA312 TP316LN Stainless Steel Pipe.

Heat Treatment and Delivery Condition

All pipe furnished to SA-312 has to be heat treated. TP304N is not individually listed in Table 2, so it takes the default solution anneal at 1900 °F [1040 °C] minimum, followed by water quenching or another rapid cool. The anneal dissolves carbides and nitrides and restores the fully austenitic structure on which the 80/35 ksi floor and the corrosion behaviour depend, and the anneal statement belongs on the certificate for every lot.

Seamless pipe may be quenched directly after hot forming when the edition allows it and the finishing temperature is not below the minimum anneal; TP304N is not an H grade, so the clause 6.2 reheat rule does not apply. HCW cold reduction is done before the final anneal, so delivery is always the annealed condition. In practice the pipe ships solution annealed, pickled or bright annealed as ordered, straightened, cut to the ordered length practice, and hydrotested or NDE-tested on every length.

Corrosion Resistance

SA-312 has no corrosion table, so this section is engineering commentary rather than a specification requirement. TP304N corrodes broadly like ASME SA312 TP304 Stainless Steel Pipe in most media, with nitrogen giving a modest improvement in pitting resistance rather than a change of class. With carbon up to 0.08%, welded joints can still sensitize, so TP304N does not replace a low-carbon grade where as-welded corrosion resistance is specified.

  • Chlorides — still no molybdenum; ASME SA312 TP316LN Stainless Steel Pipe or the 316 family is the better choice for seawater and brine
  • Welded joints — ASME SA312 TP304LN Stainless Steel Pipe combines the nitrogen with low carbon when sensitization matters
  • Cryogenic duty — nitrogen helps keep the austenite stable at low temperature; confirm code acceptance for the service
  • Magnetism — nitrogen reduces cold-work martensite, so TP304N tends to stay less magnetic after forming

As with every 304-family grade, deposits, stagnant pockets, and contamination cause most field failures, so drainage and cleanliness matter as much as the grade. Site welds and ground areas should be cleaned and passivated when the end-user specification asks for it, and the S7 intergranular test can be ordered when the owner wants evidence rather than assumption.

Applications of SA312 TP304N Pipe

Applications for TP304N pipe come from the combination of 304-family corrosion behaviour with an 80/35 ksi strength floor and stable austenite. The table below summarizes where buyers typically specify the grade and what to check on the enquiry.

Application Why TP304N Note
Pressure piping in plants standardized on 304 Higher allowables allow lighter walls with familiar chemistry Check code listing at design temperature
Cryogenic and LNG auxiliaries Nitrogen stabilizes austenite and keeps toughness Impact tests per governing code
Nuclear and power auxiliaries Nitrogen-strengthened 304 variants used where strength and stability needed Owner specifications often add requirements
Food, beverage, pharma utilities 304 hygiene with more strength Specify finish and passivation
Heat exchangers and pressure vessels Shell and connection pipe Tube and plate under separate specs
High-pressure gas lines Strength in a weldable 18-8 Weld procedure qualified on S30451

Typical users include power-plant and nuclear-related piping where the owner specifies S30451, cryogenic and liquefied-gas equipment, and pressure lines where the higher allowables are used to save wall. Enquiries should state the design code, whether TP304N allowables are being used, the nitrogen method if one is required, and any dual marking. Where welded corrosion resistance matters, look at ASME SA312 TP304LN Stainless Steel Pipe instead.

Weldability

TP304N welds by the same processes and much the same procedures as ASME SA312 TP304 Stainless Steel Pipe. SA-312 Table 6 lists ER308 (given in the pack source as S30880 / W30840) as the filler for TP304N, and the choice should be recorded on the WPS and PQR. A standard ER308 deposit does not carry the nitrogen of the base metal, so welds are not necessarily as strong as the 80/35 ksi pipe; where the design relies on the higher allowables across the joint, ask the welding engineer to confirm weld-metal properties during qualification.

  • Qualify on TP304N — rather than borrowing a plain TP304 procedure without review
  • Control heat input and interpass temperature — to limit HAZ sensitization with carbon up to 0.08%
  • Back-purge roots — on thin wall and critical lines
  • Clean joints — free of oil, paint, and carbon-steel contamination before welding

Mill longitudinal welds on WLD and HCW pipe are made without filler, so Table 6 applies to repairs and fabrication joints. Girth-weld NDE extent follows the piping or vessel code and is separate from the hydro or electric test the mill applies to each length. Avoid shielding practices that strip nitrogen from the weld pool where the weld properties matter to the design.

Surface Finishes

Surface condition for SA312 TP304N pipe should be stated on the purchase order rather than left to mill default. For stainless pipe, embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts, so the finish is part of the material performance and not just appearance. The finishes we regularly quote for this grade are listed below.

  • Annealed and pickled (AP) — solution annealed at 1900 °F [1040 °C] minimum, then descaled in acid pickle or an equivalent process to a matte grey finish; the standard choice for process pipe
  • Blasted and pickled — common on heavy-wall seamless where blasting first makes scale removal more reliable
  • Bright annealed (BA) — annealed in a protective atmosphere where mill capability exists for the size; the anneal temperature still has to meet the Table 2 practice for TP304N
  • Mechanically polished — OD and/or ID polish to an agreed grit or Ra when ordered; polishing never replaces the solution anneal
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed on WLD and HCW product

For TP304N the usual choice is annealed and pickled, since most orders are for pressure and power piping where a clean, scale-free surface matters more than appearance. Passivation after pickling or polishing can be added when the end-user specification calls for it, even though SA-312 itself does not require it. If the project bans chloride-bearing marking inks, say so on the order; otherwise the mill will apply its normal stencil practice and ship its default AP finish.

Inspection and Testing

The base acceptance package for SA-312 TP304N pipe combines chemistry, tensile testing, heat-treatment evidence, and a pressure or electrical integrity test on every length. The items below make up the usual package; supplementary requirements and project corrosion tests only apply when they are written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for TP304N: C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16%
  • Product analysis — when ordered (Suppl. S1 or PO wording), using A480 Table A1.1 tolerances via A999 §6.3
  • Tension test — 80 ksi [550 MPa] tensile and 35 ksi [240 MPa] yield minimum, plus 35% L / 25% T elongation on a lot basis
  • Flattening test — or the alternate bend test where the standard permits
  • Hydrostatic or nondestructive electric test — every length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD × wall, with TP304N (UNS S30451) on every stencil

Mill test certificates: EN 10204 3.1 is the standard documentation from SHH STEEL supply. For TP304N the certificate reports the full Table 1 chemistry with nitrogen shown inside 0.10–0.16%, the 80/35 ksi tensile results with 35%/25% elongation, the hydro or NDE method, and the 1900 °F anneal statement. EN 10204 3.2 or third-party witness by SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency is arranged when specified, and it should be booked before final testing rather than after the heat has been released. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy both editions named on the order.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Receiving review should confirm N 0.10–0.16%, C ≤0.08%, Cr 18.0–20.0%, Ni 8.0–11.0%, tensile at or above 80/35 ksi, the anneal statement, and the test method, and that the stencil reads TP304N rather than TP304 or TP304LN. Handheld PMI guns cannot measure nitrogen, so the certified analysis is the only practical evidence of the grade.

Packaging and Shipping

Export and domestic shipments of SA312 TP304N pipe are packed for handling and for ocean or land transport. The packing we normally apply is summarized below, and anything beyond it can be agreed on the order.

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where the finish needs protecting
  • End caps — plastic or metal caps on plain or beveled ends to keep out damage and contamination in transit
  • Marking — specification, grade (TP304N (UNS S30451)), heat number, size, manufacturing type (SML / WLD / HCW), test letters, and mill identity as SA-312 and the purchase order require
  • Export protection — waterproof wrapping or desiccant as agreed for polished or bright-annealed finishes, with low-chloride inks on request

Segregate TP304N from ASME SA312 TP304 Stainless Steel Pipe and ASME SA312 TP304LN Stainless Steel Pipe on the packing list and in the yard, because these grades look identical and nitrogen cannot be checked with a handheld PMI gun. Use separate bundles and distinct tags on mixed shipments, and have receiving check stencil heat numbers against the MTC. Keep interiors dry and capped so chloride-bearing moisture cannot stain or pit the surface before installation. Shipping documents normally include the packing list, invoice, bill of lading or air waybill, and the 3.1 or 3.2 MTC with full Table 1 chemistry, plus origin and customs papers to suit the agreed Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe, and for SA312 TP304N we quote against the edition you name rather than a generic catalogue sheet. We report the full Table 1 chemistry on the MTC with nitrogen shown inside the 0.10–0.16% band and the 80/35 ksi results, and we quote against the edition you name rather than a generic catalogue sheet. Heat identity stays unbroken from the melt to the finished length, so receiving inspection can clear each heat against Table 1 and Table 4 without chasing paperwork after the pipe has arrived.

The commonest problems we see with TP304N are ordinary 304 offered as “304N” with residual nitrogen below 0.10%, certificates that omit nitrogen, and tensile results reported against the TP304 floor instead of 80/35 ksi. We check supplier certificates before shipment so those issues are caught at the mill rather than at the fabricator.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for TP304N (S30451); N 0.10–0.16% reported; 80/35 ksi verified; 1900 °F anneal stated
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs as standard with full Table 1 chemistry; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both editions you name
  • Related grades — ASME SA312 TP304 Stainless Steel Pipe, ASME SA312 TP304LN Stainless Steel Pipe, ASME SA312 TP304L Stainless Steel Pipe, and ASME SA312 TP316LN Stainless Steel Pipe when a project buys a matched package
  • Export packing — seaworthy bundles, end protectors, and durable grade, heat, size, and type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, wall, finish, and any supplementary tests you name (S1, S5, S7, S8, S9). If the same project also needs plate or fittings, ask for coordinated heats so the chemistry lines up across product forms. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 TP304N stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for TP304N
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M Grade TP304N / UNS S30451
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension (80/35 ksi), flattening/bend, hydro or NDE per length; N 0.10–0.16% reported on MTC; S1/S5/S7/S8/S9 on order
Documents EN 10204 3.1 with full Table 1 chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

TP304N is rarely held in stock in the range that TP304 is, so most orders are mill runs grouped by heat. Tell us the full size list and need date early so mill slots can be matched, and we will be clear about lead time rather than promise stock that does not exist. Enquiries should state the SA-312 edition, TP304N (UNS S30451), SML/WLD/HCW, NPS or OD × wall (and whether wall is nominal or minimum), length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirements, so mill slots line up with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders, and grouping project sizes onto one heat keeps the chemistry consistent while helping meet mill minimums without over-ordering.

FAQ

Is ASME SA312 the same as ASTM A312 for TP304N?
For chemistry (Table 1), tensile (Table 4), manufacturing types, heat treatment, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when it is ordered. Name both editions on the purchase order and make sure the mill test certificate repeats them, so inspectors can verify the heat against the books you cited.
Seamless vs welded TP304N — which is better?
Neither is universally better. Seamless is the usual choice for heavy walls, high-pressure lines, and piping classes written around seamless product, while WLD and HCW are fully legitimate SA-312 forms when they are tested and annealed to the standard and usually cost less in common sizes. Choose the route your design code and datasheet allow, and check that SML, WLD, or HCW appears on both the stencil and the MTC.
Hydrostatic test vs NDE — which do I get on TP304N pipe?
Every length is either hydrostatically tested or nondestructively electrically tested, and the manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification requires one of them, state it on the PO and confirm the chosen test on the MTC for each length. NPS 10 and larger may be marked NH only when you accept a system test instead.
Does SA-312 Table 4 set a hardness limit for TP304N?
No. Table 4 lists tensile strength, yield strength, and elongation for TP304N, but no hardness maximum, so catalogue Brinell or Rockwell figures are not specification requirements. If hardness matters for your fabrication or for an end-user rule, write the limit and the test method on the purchase order, and we will make sure the mill reports it on the certificate.
What is the UNS number and chemistry of TP304N?
Table 1 lists TP304N as UNS S30451 with C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16%, with no molybdenum requirement. Nitrogen is the defining element. Put TP304N and S30451 on every document so the pipe is not confused with TP304 or TP304LN.
How does TP304N differ from TP304?
The two grades share the same carbon, chromium, and nickel limits, but TP304N requires N 0.10–0.16%, which raises the Table 4 floor to 80/35 ksi from 75/30 ksi. Ordinary 304 carries some residual nitrogen but not enough to meet the band. Dual TP304/TP304N is possible when nitrogen and tensile results satisfy both rows.
What is the difference between TP304N and TP304LN?
Both require N 0.10–0.16%. TP304N keeps carbon at up to 0.08% and reaches an 80/35 ksi floor, while TP304LN limits carbon to 0.035%, widens nickel to 8.0–12.0%, and has a 75/30 ksi floor. Choose TP304LN when as-welded sensitization resistance matters and TP304N when you want the highest strength in the 304 family.
Is TP304N more corrosion resistant than TP304?
Only modestly. Nitrogen gives a small improvement in pitting resistance, but TP304N has no molybdenum and the same carbon ceiling as TP304, so it is not a chloride grade and welded joints can still sensitize. For chlorides look at the 316 family such as TP316LN, and for as-welded corrosion resistance use TP304LN or TP304L.
Can higher-strength TP304N allow a thinner wall?
It can, because the ASME Code gives UNS S30451 higher allowable stresses than TP304, but that is a design calculation using the code tables for S30451, not a purchasing shortcut. Weld-metal strength, corrosion allowance, and the 12.5% under-tolerance on wall all have to be checked before the schedule is reduced, so involve the piping designer first.
How is nitrogen measured on TP304N pipe?
Table 1 footnote C leaves the nitrogen analysis method to agreement between purchaser and manufacturer, and handheld PMI guns cannot measure it. Mills normally use inert-gas fusion or a similar laboratory method on the heat. If your inspector requires a specific method or witness, write it on the purchase order before the heat is tested.
What filler and heat treatment apply to TP304N?
SA-312 Table 6 lists ER308 for TP304N, and the grade takes the default Table 2 solution anneal at 1900 °F [1040 °C] minimum with rapid cooling. An ER308 deposit does not carry the base-metal nitrogen, so confirm weld-metal properties during procedure qualification when the design relies on the higher TP304N allowables across the joint.

Conclusion

ASME SA312 TP304N / UNS S30451 is the nitrogen-strengthened member of the 304 family, with C ≤0.08%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16% in Table 1, an 80/35 ksi Table 4 floor with 35% L / 25% T elongation, the default 1900 °F [1040 °C] solution anneal, and ER308 filler from Table 6. It is stronger than ASME SA312 TP304 Stainless Steel Pipe and ASME SA312 TP304LN Stainless Steel Pipe but not a low-carbon or chloride grade. Order the manufacturing type, size and wall, finish, nitrogen reporting and method, any dual marking, and supplementary tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X