ASME SA312 UNS S30415 Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 UNS S30415 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 UNS S30415 heat-resisting austenitic stainless steel pipe to SA-312/SA-312M (ASTM A312/A312M), no TP designation: SML, WLD and HCW; Si 1.00–2.00%, N 0.12–0.18%, Ce 0.03–0.08%; tensile 87 ksi min, yield 42 ksi min; ASME B36.19 schedules; MTCs from SHH STEEL.
Grade
UNS S30415
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 UNS S30415 Stainless Steel Pipe

UNS S30415 is one of the grades in ASME SA-312/SA-312M (ASTM A312/A312M) Table 1 that has no TP designation—the grade column shows only an ellipsis, so the pipe is identified and marked by its UNS number alone. It is a micro-alloyed, heat-resisting austenitic stainless steel built on an 18Cr–9.5Ni base, modified with silicon 1.00–2.00%, nitrogen 0.12–0.18%, a controlled carbon window of 0.04–0.06%, and cerium 0.03–0.08%.

Each addition has a purpose at high temperature. Silicon and the rare-earth element cerium work together to form a thin, tightly adherent oxide scale that resists spalling during thermal cycling. Nitrogen and controlled carbon strengthen the austenite and support creep resistance. Manganese is held low (≤0.80%) because it would otherwise degrade the oxide. The result is a lean, economical alloy that is widely described as delivering oxidation resistance at higher service temperatures than standard 304-type grades, together with markedly higher strength.

That strength shows in Table 4: S30415 must meet 87 ksi [600 MPa] tensile and 42 ksi [290 MPa] yield minimum, compared with 75 / 30 ksi for ASME SA312 TP304 Stainless Steel Pipe and ASME SA312 TP304H Stainless Steel Pipe. S30415 is not one of the “H” grades listed in clause 1.2, and it has no grain size requirement in Table 5, yet its chemistry is explicitly designed for elevated-temperature duty.

SHH STEEL can supply ASME SA312 UNS S30415 stainless steel pipe to the edition named on the enquiry, including seamless (SML), welded (WLD), and heavily cold-worked (HCW) routes; ASME B36.19 schedules and special OD/wall by agreement; EN 10204 3.1 mill test certificates; and dual SA-312/A312 marking when the heat analysis, heat treatment, mechanical tests, and marking satisfy both editions named on the purchase order. Because the grade has no TP name, we mark and certify it by UNS S30415 alone, and we confirm a heat inside the narrow C 0.04–0.06%, Si 1.00–2.00%, N 0.12–0.18%, and Ce 0.03–0.08% windows before quoting a date. Confirm NPS, wall or schedule, finish, length practice, and any product-analysis or supplementary tests on enquiry.

The alloy reaches us under several labels, including proprietary trade names. The list below shows how each relates to the ordered product; because SA-312 gives no TP designation, the UNS number is the only reliable identity on the purchase order and MTC.

  • ASME SA312 UNS S30415 / SA-312 S30415 — correct Code form, since no TP name exists
  • ASTM A312 S30415 — ASTM parent, same Table 1 and Table 4 rows
  • EN 1.4818 — European heat-resisting steel commonly cross-referenced to S30415 (confirm against the EN product standard)
  • Proprietary names — producers sell this chemistry under trade names; order by UNS S30415 to stay specification-based

Why a lean heat-resisting grade? Traditional answers to high-temperature oxidation have been to add more chromium and nickel—moving from 304 to 309 or 310 types. Those alloys work, but they use much more nickel and can be prone to sigma embrittlement. S30415 takes a different route: it keeps an 18-9 base and relies on small, precisely controlled additions of silicon, nitrogen, and a rare-earth element to improve oxide behaviour and strength. For many furnace and heat-recovery components this gives a useful step up from 304H without the cost of higher-alloy grades.

A PO that says “TP304 modified” or “304 heat-resisting” is not sufficient—use UNS S30415 and the SA-312 edition. S30415 is not a drop-in for ASME SA312 TP304H Stainless Steel Pipe: it has higher Table 4 floors (87/42 vs 75/30 ksi), Si-Ce-N micro-alloying, Mn ≤0.80%, and a tighter carbon window, while TP304H carries a Table 5 grain-size rule that S30415 does not. Moving to ASME SA312 TP309H Stainless Steel Pipe or ASME SA312 TP310H Stainless Steel Pipe buys more chromium and nickel for hotter or harsher atmospheres at higher alloy cost. Grade hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

S30415 may be furnished in any of the three SA-312 product forms:

  • Seamless (SML) — hot extruded or pierced and cold finished. Suits heavy-wall furnace and radiant tubes and high-temperature transfer piping.
  • Welded (WLD) — strip or plate formed and welded without filler, then annealed. Widely used for ducting-type piping, recuperators, and large thin-wall sizes.
  • Heavily cold-worked (HCW) — welded and cold reduced at least 35% in wall and weld before anneal, with the weld radiographed first.

The higher silicon content gives S30415 a slightly different hot-working and welding behaviour from 304, but this is managed at the mill. Buyers should simply confirm route and size availability early: S30415 is a specialty grade with fewer producers than the common 300-series, and most pipe is made from rolled plate or strip produced in campaigns.

For large-diameter heat-resisting ducts and headers, welded pipe made from S30415 plate is often the only practical form. In that case, the plate heat analysis carries through to the pipe certificate, and the pipe mill’s anneal after welding is what governs the final structure. Ask the supplier to state both the plate heat number and the pipe lot on the MTC.

All lengths are hydrostatically tested or tested by nondestructive electric methods per A999, and marked SML, WLD, or HCW. Unlike H grades, SA-312 does not require heat-treatment lot marking for S30415, though many buyers request it for traceability.

Chemical Composition of SA312 UNS S30415

Heat analysis to Table 1 is mandatory for every heat. Product analysis (S1) uses ASTM A480/A480M Table A1.1 tolerances through A999—with one exception discussed below.

Melting analysis (heat / ladle analysis) — Table 1

Heat analysis for UNS S30415. Values are maximum unless a range is shown; ellipses (…) mean no requirement.

Element UNS S30415 melting analysis
Carbon (C) 0.04 – 0.06
Manganese (Mn) ≤ 0.80
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) 1.00 – 2.00
Chromium (Cr) 18.0 – 19.0
Nickel (Ni) 9.0 – 10.0
Nitrogen (N) 0.12 – 0.18
Cerium (Ce) 0.03 – 0.08
Molybdenum (Mo) … (no requirement)

Source: ASME SA-312/SA-312M ≡ ASTM A312/A312M Table 1, UNS S30415 (grade column “…”, no TP designation). Nitrogen method by agreement.

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.06 0.01 under / over 0.03 – 0.07
Manganese (Mn) ≤ 0.80 0.03 over ≤ 0.83
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) 1.00 – 2.00 0.05 under / 0.10 over 0.95 – 2.10
Chromium (Cr) 18.0 – 19.0 0.20 under / over 17.80 – 19.20
Nickel (Ni) 9.0 – 10.0 0.10 under / over 8.90 – 10.10
Nitrogen (N) 0.12 – 0.18 0.01 under / over 0.11 – 0.19
Cerium (Ce) 0.03 – 0.08 Not listed in A480 Table A1.1 Not established—by agreement

Cerium tolerance gap: A480 Table A1.1 does not include a row for cerium. The specification therefore provides no product-analysis tolerance for Ce, and any check analysis of cerium should be judged by agreement between purchaser and manufacturer. SHH STEEL reports the heat analysis value as certified and does not apply an unpublished tolerance.

Element by element:

  • Carbon 0.04–0.06% — a narrow window: enough for creep strength, low enough to limit carbide networks
  • Silicon 1.00–2.00% — strengthens the protective oxide layer beneath the chromia scale
  • Nitrogen 0.12–0.18% — solid-solution strengthening and austenite stability
  • Cerium 0.03–0.08% — rare-earth addition that improves scale adhesion under cycling
  • Manganese ≤0.80% — kept low because Mn-rich oxides are less protective
  • Chromium 18.0–19.0% and nickel 9.0–10.0% — tight ranges around the 18-9 base

Silicon is the other element that needs care. Its range straddles two A480 rows: the 1.00 minimum falls in the “to 1.00 incl” row (0.05 under), while the 2.00 maximum is in the “over 1.00 to 3.00” row (0.10 over). The narrow carbon window of 0.04–0.06% takes 0.01 each way.

S30415 vs TP304H, side by side (Table 1):

Element TP304H (S30409) S30415
C 0.04 – 0.10 0.04 – 0.06
Mn ≤ 2.00 ≤ 0.80
Si ≤ 1.00 1.00 – 2.00
Cr 18.0 – 20.0 18.0 – 19.0
Ni 8.0 – 11.0 9.0 – 10.0
N … 0.12 – 0.18
Ce … 0.03 – 0.08

Mechanical Properties of SA312 UNS S30415

Property (SA-312 Table 4) UNS S30415
Tensile strength, min 87 ksi [600 MPa]
Yield strength (0.2% offset), min 42 ksi [290 MPa]
Elongation in 2 in. or 50 mm (or 4D), min 35% longitudinal / 25% transverse
Hardness No maximum in Table 4
Grain size Not listed in Table 5

The 42 ksi yield floor is 40% higher than TP304H’s 30 ksi, and the 87 ksi tensile floor 12 ksi higher. Nitrogen in solid solution and the fine dispersion of nitrides and carbides that the micro-alloying promotes account for the difference.

At elevated temperature, the alloy’s producers publish creep and rupture data that are generally higher than those of 304H, which is the basis for thinner walls in furnace components. For pressure design, however, use the allowable stresses listed for S30415 in ASME Section II Part D or the applicable B31 table; if the code lists none for the intended temperature, the producer data cannot substitute.

Testing per SA-312: tension test per heat-treatment lot (one per 100 pipes or fewer, two for larger lots), flattening or permitted bend tests on 5% of pipes. Elevated-temperature tests, stress-rupture tests, and hardness are not in the base requirement.

Comparison of SA-312 strength floors:

Grade UNS Tensile min, ksi [MPa] Yield min, ksi [MPa]
TP304 S30400 75 [515] 30 [205]
TP304H S30409 75 [515] 30 [205]
— S30415 87 [600] 42 [290]
TP316 S31600 75 [515] 30 [205]

Note the absence of a grain size requirement. Unlike TP304H, S30415 has no Table 5 entry. Projects that rely on creep properties sometimes add a grain size report as a PO requirement; that is a purchaser option, not a specification rule.

Dimensions and Tolerances

S30415 pipe is supplied to ASME B36.19 stainless schedules (5S, 10S, 40S, 80S) and special OD/wall by agreement. SA-312 Table 3 wall tolerances:

  • NPS 1/8–2-1/2: +20.0% / −12.5%
  • NPS 3–18: +22.5% (t/D ≤5%) or +15.0% (t/D >5%) / −12.5%
  • NPS 20 and larger welded: +17.5% / −12.5%
  • NPS 20 and larger seamless: +22.5% (t/D ≤5%) or +15.0% (t/D >5%) / −12.5%

OD tolerances follow A999/A999M. NPS 1/8–8 are normally supplied up to 24 ft (15–24 ft range); cut lengths no more than 1/4 in. [6 mm] over.

Heat-resisting applications often use non-standard sizes—large thin-wall welded pipe for ducts, recuperator tubes to OD × wall, and heavy seamless for radiant tubes. When ordering by OD and wall, say whether wall is nominal or minimum (S8). Thermal growth at high temperature should be considered in length planning for furnace installations; S30415 has an expansion coefficient typical of austenitic stainless.

Equivalent Grades

Designation Relationship to S30415
ASME SA-312 / ASTM A312, UNS S30415 Governing pipe grade (no TP name)
ASME SA-240 / ASTM A240 S30415 Plate and sheet for fabricated heat-resisting parts (separate specification)
ASME SA-213 S30415 Boiler and heat-exchanger tube (separate specification)
EN 1.4818 (X6CrNiSiNCe19-10) Commonly cited European equivalent; verify chemistry against EN 10095 or EN 10302
Proprietary trade names Sold by several producers; order by UNS S30415

Distinguish S30415 from its relatives in SA-312:

  • ASME SA312 TP304H Stainless Steel Pipe (S30409) — higher C ceiling, no Si/N/Ce additions, lower strength floors, grain size controlled
  • ASME SA312 TP304 Stainless Steel Pipe (S30400) — general-purpose 18-8 with no heat-resisting modification
  • S30416 — the next row in Table 1, a different micro-alloyed composition with Mo and low S; not interchangeable
  • Higher-alloy heat-resisting grades such as S30815 — more Cr and Ni for even higher temperatures

Related: ASME SA312 TP304L Stainless Steel Pipe, ASME SA312 TP316 Stainless Steel Pipe, ASME SA240 304 Stainless Steel Plate.

Heat Treatment and Delivery Condition

S30415 is not individually listed in SA-312 Table 2. It therefore falls under the general row: solution anneal at 1900 °F [1040 °C] minimum, then quench in water or rapidly cool by other means at a rate sufficient to prevent carbide re-precipitation (demonstrable by A262 Practice E if S7 is ordered).

Under ASME clause 6.2, S30415 is not among the grades that must be reheated (H grades, S33228, S30815, S31272), so seamless pipe may be quenched directly after hot forming provided its temperature is not below the Table 2 minimum.

Producers of this chemistry frequently anneal at temperatures above the 1900 °F minimum to fully dissolve nitrides and develop the intended grain structure. The specification sets only the minimum; if a project requires a particular anneal range, write it into the PO and ask for it on the MTC.

  • Delivery: solution annealed and quenched, pickled or bright annealed
  • Surface: free of scale and exogenous iron; passivation on request
  • In service: the alloy forms its protective oxide during operation; no special pre-oxidation is required by SA-312

Corrosion Resistance

S30415 is fundamentally a heat-resisting alloy. Its corrosion resistance at ambient temperature is generally comparable to 304-type stainless in mild environments, but it is not chosen for aqueous corrosion.

High-temperature oxidation: Silicon and cerium modify the oxide that forms on the surface, producing a thin, adherent scale that resists cracking and spalling during heating and cooling cycles. Producers commonly quote service in air up to about 1920 °F [1050 °C]; actual limits depend on atmosphere, cycling, and load, and the figure is general guidance rather than an SA-312 value.

Carburizing and nitriding atmospheres: silicon improves resistance to carbon and nitrogen pickup compared with plain 304. Severe carburizing conditions still need higher-nickel alloys.

Sulfidizing atmospheres: moderate nickel content limits the risk of low-melting nickel sulfides compared with high-nickel alloys, but reducing sulfur-bearing gases remain aggressive for all stainless steels.

Aqueous service: no Mo; chloride pitting and SCC resistance are in the 304 range. Condensation during shutdowns, especially of acidic or chloride-bearing deposits, can attack any austenitic grade.

Embrittlement: long exposure in the intermediate temperature range can precipitate phases that reduce room-temperature toughness; the lean chemistry of S30415 is generally regarded as less prone to sigma formation than higher-Cr heat-resisting grades.

Applications of SA312 UNS S30415 Pipe

Application Role of S30415 Note
Furnace radiant and muffle tubes Oxidation resistance with high strength allows thinner walls Check code listing if pressure retaining
Recuperators and heat exchangers Thermal cycling resistance of the Ce-Si oxide Watch for condensate corrosion at cold end
Hot-gas ducting and stacks Lightweight welded pipe in hot flue gas Sulfur levels in fuel influence life
Petrochemical heaters Convection-section piping and supports Compare with TP304H or higher alloys
Kilns, calciners, incinerators Burner tubes, thermowells, protection tubes Abrasion and ash chemistry matter
Heat-treatment equipment Radiant tubes, retorts, fixtures made from pipe Carburizing atmospheres may need higher Ni

Selecting between S30415 and alternatives: if the component is mainly a non-pressure part exposed to hot air or flue gas with frequent thermal cycling, S30415’s oxide behaviour is the main reason to choose it. If the part is a code pressure line, availability of code allowable stresses for S30415 at the design temperature must be confirmed first. If the atmosphere is strongly carburizing, sulfidizing, or contains molten salts, higher-nickel alloys may be required. A materials engineer’s review is recommended for new furnace designs.

Where the service is a code pressure line in the creep range but oxidation is moderate, ASME SA312 TP304H Stainless Steel Pipe may be the more familiar choice. For ambient corrosive service, use ASME SA312 TP304L Stainless Steel Pipe or ASME SA312 TP316L Stainless Steel Pipe instead.

Weldability

S30415 is weldable with GTAW, GMAW, SMAW, and SAW using practices similar to other austenitic stainless steels, with attention to its silicon content and nitrogen.

Filler metal and Table 6: UNS S30415 is not listed in SA-312 Table 6. The standard therefore names no AWS A5.9 classification, and filler selection is by agreement and must be recorded on the WPS (and, for seam repairs under clause 15, on the certificate). Producers of this alloy offer matching-chemistry consumables for full high-temperature performance; where those are not used, the joint’s oxidation resistance and strength will reflect the filler chosen, so the fabricator and designer should decide together.

  • Hot cracking: higher silicon can increase solidification cracking sensitivity; matching fillers are formulated with controlled ferrite to counter this
  • Heat input: moderate; keep interpass temperature controlled
  • Shielding: argon or argon-helium; argon backing for roots
  • Cleaning: remove heat tint; at very high service temperatures this matters less for function but remains good practice

Dissimilar welds: S30415 is often joined to 304H, 309, or 310 type components in furnace assemblies. In those cases a 309-type or nickel-base filler may be selected for dilution tolerance; the trade-off is reduced oxidation performance at the joint compared with a matching filler. The choice should be documented on the WPS and agreed with the designer.

Qualify procedures under ASME Section IX on S30415 base metal. Mill longitudinal welds are made autogenously.

Surface Finishes

  • Annealed and pickled — standard; the starting surface for in-service oxide growth
  • Bright annealed — small OD tubing
  • Blasted — heavy-wall seamless
  • Polished — rarely needed for heat-resisting duty, available by agreement

Unlike decorative or sanitary applications, heat-resisting service will transform the surface within hours of operation as the protective scale forms. The value of the delivered finish is therefore mainly in cleanliness and inspection, not appearance. A uniform pickled surface makes visual and penetrant inspection easier and gives the oxide a consistent starting point.

For high-temperature service, a clean, pickled surface free of embedded iron and contaminants gives the most uniform oxide. Avoid marking paints or tapes that contain low-melting metals or high halide content.

Inspection and Testing

Base SA-312 requirements for S30415:

  • Heat analysis to Table 1, including C 0.04–0.06, Si 1.00–2.00, N 0.12–0.18, and Ce 0.03–0.08
  • Tension test per lot to the 87/42 ksi floors
  • Flattening or permitted bend test on 5% of the lot
  • Hydrostatic or nondestructive electric test per length
  • Visual and dimensional examination
Option Use
S1 product analysis Confirms Si and N; Ce tolerance by agreement (not in A480)
S5 radiography Weld soundness on WLD pipe
Grain size report (PO) Optional for creep-sensitive applications
Elevated-temperature tensile (PO) Project-specific verification
PMI (OES preferred) Handheld XRF can confirm Cr/Ni/Si but not C, N, or reliably Ce

Lot rules and sampling: lots are defined by clause 11.1—same size, heat, furnace, temperature, time, and speed for continuous furnaces. For specialty grades made in short campaigns, a heat may be split into several lots by size, each needing its own tension and flattening results. Check that every size on the order has its own test results on the MTC.

Certificates: EN 10204 3.1 standard, 3.2 on request. The MTC should explicitly report cerium; a certificate without a Ce value cannot demonstrate conformance to Table 1.

Packaging and Shipping

  • Strapped bundles with non-metallic separators; cases for small OD
  • End caps or bevel protectors
  • Marking: specification, “S30415” (no TP grade), heat number, size and wall, SML/WLD/HCW, test letters, manufacturer’s mark
  • Waterproof export wrap

For export to furnace builders, pipe is often cut to fabrication lengths before shipment. Cut lengths should keep the heat number transferred to each piece, either by stencil or by tagging, so that the MTC link is never lost.

Since there is no TP name, stencils read the UNS number. Warehouses that sort stock by TP grade should be told explicitly so S30415 is not shelved as generic 304.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe, and with S30415 the critical point is that every one of its small additions is a controlled window, not a nice-to-have. We quote UNS S30415 against the edition you name and report the full Table 1 row on the MTC—C 0.04–0.06%, Mn ≤0.80%, Si 1.00–2.00%, Cr 18.0–19.0%, Ni 9.0–10.0%, N 0.12–0.18%, Ce 0.03–0.08%—with heat identity unbroken from melt through finished length, so receiving inspection clears the heat against Table 1 and the 87/42 ksi Table 4 floors rather than a proprietary data sheet. We are also clear about the gaps: Table 6 lists no filler for S30415, and A480 Table A1.1 has no cerium tolerance, so both are handled by agreement and stated as such.

  • Specification fidelity — Table 1 and Table 4 for UNS S30415, Ce reported; marked by UNS because no TP name exists
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs standard; 3.2 or third-party inspection on request
  • Dual marking — SA-312/A312 when the heat meets both editions you name
  • Purchaser options — grain-size report, specific anneal range, or elevated-temperature data when written on the PO
  • Export packing — seaworthy bundles, end protectors, and durable UNS/heat/size/type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, finish, and supplementary tests. If the pipe is pressure-retaining in a furnace or heater, check first that your code lists allowable stresses for S30415 at the design temperature; if it does not, producer creep data cannot fill the gap, and we will tell you so before you order.

Supply Capability

SHH STEEL can supply ASME SA312 UNS S30415 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for UNS S30415
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M UNS S30415 (no TP designation)
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; bright annealed or polished by agreement
Testing Tension, flattening/bend, hydro or NDE per length; supplementary tests on order
Documents EN 10204 3.1; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

S30415 is a specialty heat-resisting melt, so pipe stock is limited and lead time usually follows the mill melt schedule. Welded pipe is common in larger, thinner sizes used for ducting and furnace parts; seamless and heavy-wall sizes are mill-order items. Enquiries should state the SA-312 edition, UNS S30415, SML/WLD/HCW, NPS or OD×wall, length practice, finish, and any grain-size, anneal-range, product-analysis, or 3.2 requirements so mill slots match your need date. If matching welding consumables are needed for fabrication, mention it at enquiry so they can be sourced together. Cut lengths, beveling, and packing-list marking are available on confirmed orders.

FAQ

Does S30415 have a TP grade name in SA-312?
No. Table 1 shows an ellipsis in the grade column for S30415, so the pipe is ordered, marked, and certified as UNS S30415 alone. Purchase orders that say “TP304 modified” or “304 heat-resisting” are not enough; write SA-312 UNS S30415 with the edition year so the MTC ties to the right Table 1 row.
What are the Table 4 minima for S30415?
Table 4 sets 87 ksi [600 MPa] tensile and 42 ksi [290 MPa] yield minimum, with 35% longitudinal and 25% transverse elongation. That is 12 ksi more tensile and 40% more yield than TP304H at 75/30 ksi. Table 4 lists no hardness maximum, and there is no Table 5 grain-size requirement for this grade.
What makes S30415 heat resisting?
Silicon 1.00–2.00% and cerium 0.03–0.08% work together to form a thin, adherent oxide that resists spalling in thermal cycling, while nitrogen 0.12–0.18% and controlled carbon of 0.04–0.06% strengthen the austenite. Manganese is held at ≤0.80% because it would degrade the oxide. The 18Cr–9.5Ni base keeps alloy cost moderate.
Is S30415 an H grade?
No. S30415 is not listed among the H grades in clause 1.2, it has no Table 5 grain-size requirement, and the ASME clause 6.2 reheat rule does not apply to it. Its chemistry is still designed for elevated-temperature duty. Projects relying on creep properties sometimes add a grain-size report to the PO as a purchaser option.
What heat treatment applies to S30415?
S30415 is not individually listed in Table 2, so the default applies: solution anneal at 1900 °F [1040 °C] minimum, then water quench or rapid cooling. Producers often anneal hotter to dissolve nitrides fully and set the grain structure; if your project needs a specific range, write it on the PO and ask for it on the MTC.
Which filler metal is specified for S30415?
None. S30415 is not in SA-312 Table 6, so filler is by agreement and must be recorded on the WPS and, for any seam repair, on the certificate. Matching-chemistry consumables from the alloy producers give full high-temperature performance; 309-type or nickel-base fillers are sometimes used for dissimilar joints, at some cost to joint oxidation behaviour.
Is there a product-analysis tolerance for cerium?
No. A480 Table A1.1 has no cerium row, so a product tolerance for Ce is not established in the specification and any Ce check analysis is by agreement. The other elements follow A480: for example C 0.03–0.07%, Si 0.95–2.10%, and N 0.11–0.19% on product analysis. State any Ce verification you need on the PO.
How does S30415 compare with TP304H?
S30415 has higher strength floors (87/42 vs 75/30 ksi), Si-Ce-N micro-alloying for better oxide adherence, lower Mn, and a narrower carbon window. TP304H has a wider carbon range and a Table 5 grain-size requirement. For code pressure lines, TP304H may be the more familiar choice; check which grade your code lists at temperature.
Is S30415 good for aqueous corrosion?
It is chosen for high-temperature service. At ambient temperature it behaves broadly like 304-type stainless and has no Mo, so chloride pitting and SCC resistance are in the 304 range. Watch for acidic or chloride-bearing condensate at cold ends and during shutdowns. For ambient corrosive service, TP304L or TP316L is usually the better buy.
What is the European equivalent of S30415?
EN 1.4818 is commonly cross-referenced to S30415, but it is a European heat-resisting steel designation, not an SA-312 grade. Verify the chemistry in the applicable EN product standard before treating them as equal, and remember that ASME code work still needs pipe ordered and certified to SA-312 UNS S30415.
Can S30415 be supplied seamless and welded?
Yes. SA-312 permits SML, WLD, and HCW for S30415. Welded pipe is common in the larger, thinner sizes used for ducting and furnace components, while seamless is typically chosen for heavier walls or when the specification excludes welded pipe. Each length is hydrotested or electrically NDE-tested as the standard requires.
What service temperature can S30415 handle?
Producers commonly quote oxidation service in air up to about 1920 °F [1050 °C], but that is producer guidance, not an SA-312 value. Real limits depend on atmosphere, thermal cycling, and load. For pressure parts, the governing limit is the code allowable-stress table for S30415, so confirm that first.

Conclusion

ASME SA312 UNS S30415 is the lean heat-resisting austenitic pipe grade in SA-312 with no TP designation: C 0.04–0.06%, Mn ≤0.80%, Si 1.00–2.00%, Cr 18.0–19.0%, Ni 9.0–10.0%, N 0.12–0.18%, Ce 0.03–0.08%, Table 4 floors of 87 ksi [600 MPa] tensile and 42 ksi [290 MPa] yield, and a Table 2 default 1900 °F [1040 °C] anneal. It is not an H grade, has no Table 5 grain-size rule, and Table 6 lists no filler, so consumables are by agreement. It is not a drop-in for TP304H, TP309H, or TP310H. Order by UNS number with the manufacturing type (SML/WLD/HCW), schedule or wall, finish, and any product analysis or supplementary tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response