ASME SA312 UNS S31277 Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 UNS S31277 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 UNS S31277 super-austenitic stainless steel pipe (no TP name) in SML, WLD and HCW, with Mo 6.5–8.0%, Ni 26.0–28.0% and N 0.30–0.40%, a 112/52 ksi Table 4 floor with 40% elongation and a 2050 °F anneal, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
UNS S31277
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Dimensions
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 UNS S31277 Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe for high-temperature and general corrosive service. UNS S31277 is listed in Table 1 with no TP designation, so it is ordered, marked, and certified by UNS number alone. It is the highest-molybdenum super-austenitic pipe grade in the family: C ≤0.020%, Mn ≤3.00%, P ≤0.030%, S ≤0.010%, Si ≤0.50%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, and Cu 0.50–1.50%. The nickel level is well above the 6Mo grades, and it is what keeps such a high molybdenum content stable in an austenitic matrix.

Table 4 sets 112 ksi [770 MPa] tensile and 52 ksi [360 MPa] yield as a single row with no thickness split, one of the highest tensile floors in SA-312. Elongation is a special case: S31277 is grouped with N08925, N08028, and N08029 at 40% longitudinal, not the 35% default that inspectors apply by habit. Table 2 calls for a solution anneal at 2050 °F [1120 °C] minimum with rapid cooling. Table 6 in the extracted edition assigns no AWS filler class to S31277, so filler is by agreement. It is not an H grade: no carbon floor, no Table 5 grain size, and no clause 6.2 reheat. Engineers usually specify it for severe chloride and acid chloride duty where even 6Mo grades are marginal.

SHH STEEL can supply ASME SA312 UNS S31277 stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) form. We quote ASME B36.19 schedules and special OD/wall by agreement, ship with EN 10204 3.1 mill test certificates that report every Table 1 element with Mo, Ni, N, and Cu as actual values, state the 112/52 ksi results with 40% elongation and the 2050 °F anneal, and offer dual SA-312/A312 marking when chemistry, heat treatment, mechanical tests, and marking satisfy both editions on the purchase order. Please confirm NPS, wall or schedule, finish, length practice, filler basis, and any product-analysis or corrosion-test extras when you enquire.

The list below shows how the names used in the market map to what should appear on the order and certificate. Trade names are useful shorthand, but only the UNS number carries the Table 1 and Table 4 rows.

  • ASME SA312 UNS S31277 / SA-312 Grade UNS S31277 — the marking language for ASME-code and dual-marked pipe
  • ASTM A312 UNS S31277 — same chemistry and tensile tables when the ASTM edition is referenced
  • “7Mo”, “super austenitic”, or mill trade names — informal labels only; insist on UNS S31277 on stencil and MTC

Sister grades buyers compare with S31277 include ASME SA312 UNS S31254 Stainless Steel Pipe (Mo 6.0–6.5%, Ni 17.5–18.5%, thickness-split 98/95 ksi tensile and 45 ksi yield, 2100 °F anneal) and ASME SA312 UNS S31266 Stainless Steel Pipe (W-bearing, Mn 2–4%, N 0.35–0.60%, 109/61 ksi, 2100 °F). For moderate chloride duty, ASME SA312 TP316L Stainless Steel Pipe or ASME SA312 TP317L Stainless Steel Pipe may be enough. None of these is a drop-in replacement for S31277. Grade hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 recognizes three manufacturing routes for UNS S31277 pipe, and the route is a purchase-order decision driven by the design code, the size range, wall thickness, and how the owner wants the pipe inspected. The route never changes the chemistry: whichever way the pipe is made, the heat must still meet C ≤0.020%, Mn ≤3.00%, P ≤0.030%, S ≤0.010%, Si ≤0.50%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, and Cu 0.50–1.50%, and every length must still go through the solution anneal at 2050 °F [1120 °C] minimum before it is released.

  • Seamless (SML) — no welding at any stage. Seamless dominates high-pressure chloride process lines and thick-wall pressure parts where welded pipe is excluded. The very high Mo content raises segregation and hot-working risk, so every seamless length must be solution annealed at 2050 °F minimum and rapidly cooled.
  • Welded (WLD) — automatic welding without filler metal, with the weld finished so the pipe meets dimensional and mechanical requirements after the final heat treatment. The strip or plate heat must itself carry the full UNS S31277 chemistry, so ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked to at least 35% reduction of wall and weld before the final anneal, again without filler in the longitudinal seam, with the weld radiographed before cold work. Order HCW when the project specifically wants that marking and the process controls SA-312 writes around it.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser accepts a system test in place of the hydrotest, and lots for mechanical testing follow clause 11.1. Clause 17 heat-treatment lot marking is not mandatory because S31277 is not an H grade, but projects buying this alloy almost always want heat and lot identity on the stencil. Dual certification to S31254 or S31266 is not possible because the Mo, Ni, and N windows do not overlap.

S31277 is one of the least common grades in SA-312 and is essentially always made to order from specialty melt campaigns. Lead times are longer than for ASME SA312 UNS S31254 Stainless Steel Pipe, and mill minimums can be significant, so enquire early with route, sizes, wall, anneal evidence requirements, and filler basis, and group all project sizes onto a single heat where you can.

Chemical Composition of SA312 UNS S31277

Two chemistry layers matter for UNS S31277. The melting (heat or ladle) analysis is mandatory for every heat under SA-312/A312 Table 1, while product analysis on finished pipe applies only when it is ordered through Supplementary Requirement S1 or purchase-order wording. Product tolerances are not printed in SA-312 itself; they come through ASTM A999/A999M §6.3 from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values and, when ordered, the product values, and never quotes tighter catalogue windows that the standard does not publish.

Melting analysis (heat / ladle analysis) — Table 1

The table below is the heat analysis for UNS S31277 from SA-312/SA-312M Table 1. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element. The grade column shows “…”, confirming there is no TP name.

Element UNS S31277 melting analysis
Carbon (C) ≤ 0.020
Manganese (Mn) ≤ 3.00
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.010
Silicon (Si) ≤ 0.50
Chromium (Cr) 20.5 – 23.0
Nickel (Ni) 26.0 – 28.0
Molybdenum (Mo) 6.5 – 8.0
Nitrogen (N) 0.30 – 0.40
Copper (Cu) 0.50 – 1.50

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.020 0.005 over ≤ 0.025
Manganese (Mn) ≤ 3.00 0.04 over ≤ 3.04
Phosphorus (P) ≤ 0.030 0.005 over ≤ 0.035
Sulfur (S) ≤ 0.010 0.005 over ≤ 0.015
Silicon (Si) ≤ 0.50 0.05 over ≤ 0.55
Chromium (Cr) 20.5 – 23.0 0.25 under / over 20.25 – 23.25
Nickel (Ni) 26.0 – 28.0 0.20 under / over 25.80 – 28.20
Molybdenum (Mo) 6.5 – 8.0 0.10 under / over 6.40 – 8.10
Nitrogen (N) 0.30 – 0.40 0.03 under / 0.04 over 0.27 – 0.44
Copper (Cu) 0.50 – 1.50 0.05 under / 0.10 over 0.45 – 1.60

Source: SA-312 Table 1, UNS S31277. Mo uses the A480 over 2–8% band (0.10). N 0.30–0.40 uses over 0.25–0.35 (0.03) / over 0.35–0.45 (0.04). Cu spans the 0.50–1.00 (0.05) and 1.00–3.00 (0.10) bands.

The values to check first on receipt are molybdenum 6.5–8.0%, which sits above the 6.0–6.5% window of S31254, nickel 26.0–28.0%, far higher than any 6Mo grade, and nitrogen 0.30–0.40%, which falls between S31254 (0.18–0.25%) and S31266 (0.35–0.60%). Carbon is capped at 0.020% and silicon at 0.50%, both tighter than commodity stainless. A heat that reports Mo at 6.3% may be fine S31254 but is not S31277, which is why “6Mo” on a purchase order without the UNS is a genuine risk.

For product analysis, molybdenum uses the A480 0.10 band and nitrogen uses 0.03 under and 0.04 over across the 0.30–0.40% window. Copper straddles two A480 bands, so this pack applies 0.05 under at the low end and 0.10 over at the high end. If product analysis is ordered, state those bases on the purchase order so the mill and the receiving laboratory work from the same limits.

Mechanical Properties of SA312 UNS S31277

Room-temperature tensile requirements for UNS S31277 come from SA-312 Table 4 and are summarized below. These are minimum release values for the lot, not typical values, and design allowables must always be taken from the governing code tables for UNS S31277 rather than from a neighbouring grade.

Property S31277
Tensile, min 112 ksi [770 MPa]
Yield, min 52 ksi [360 MPa]
Elongation 40% longitudinal (special Table 4 group)

The 112/52 ksi row applies to all walls, so there is no 0.187 in. thickness split to check, unlike ASME SA312 UNS S31254 Stainless Steel Pipe. The important trap is elongation: S31277 belongs to the special Table 4 group with N08925, N08028, and N08029 that requires 40% longitudinal, and a result of 37% that would pass ordinary 316L fails here. Table 4 does not set a hardness maximum for S31277. Design allowables must come from the code tables listed for UNS S31277; borrowing S31254’s 45 ksi yield or S31266’s 61 ksi yield misrepresents the grade.

Certificate values are normally above the minima, but the design basis should still use Table 4 and the code allowables unless the mill has accepted higher guaranteed values in writing. Delivery is the solution-annealed condition. The fully austenitic, high-nickel structure gives good toughness at low temperature, though impact testing remains a project extra rather than part of the SA-312 base package.

Dimensions and Tolerances

Dimensional supply for SA312 UNS S31277 pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow SA-312 Table 3 as summarized below. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M.

  • Lengths — single random, double random, or cut-to-length on order
  • Cut lengths — typically no more than 1/4 in. [6 mm] over the ordered length unless the PO states a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face when the WPS is already frozen

Many seawater, chemical, and chloride-process buyers order by OD × wall rather than NPS and schedule, which is fine as long as the enquiry says so clearly. Straightness, end finish, and length tolerance should be written into export orders so receiving inspection has an agreed acceptance basis instead of arguing after arrival. On thin schedules with threaded or socket-weld ends, check that the remaining wall is still adequate after the 12.5% under-tolerance. Jointers are not permitted unless the purchase order allows them, so cut-to-length programmes should include an allowance for fit-up scrap rather than expecting the mill to ship short pieces.

Equivalent Grades

UNS S31277 has no TP name in SA-312, and cross-references to proprietary or EN grades are approximate at best. Any mapping has to be checked element by element against Table 1, with particular care on Mo, Ni, N, and Cu.

Designation Notes
SA-312 UNS S31277 Governing
Proprietary maps Recheck Mo 6.5–8, Ni 26–28, N, Cu

Treat trade-name equivalents as commercial shorthand rather than a substitution approval, because a heat can satisfy a trade window and still miss the S31277 molybdenum or nickel range. Dual certification is valid only when every Table 1 element passes and the tensile results meet 112/52 ksi with 40% elongation. Related SA-312 pages: ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 UNS S31266 Stainless Steel Pipe, ASME SA312 TP316L Stainless Steel Pipe, and ASME SA312 TP317L Stainless Steel Pipe.

Heat Treatment and Delivery Condition

Table 2 requires UNS S31277 to be solution annealed at 2050 °F [1120 °C] minimum, followed by rapid cooling. This is its own listing, distinct from the 2100 °F used for S31254 and S31266 and far above the 1900 °F typical of 316 practice, so the MTC should quote the S31277 row specifically. The high temperature dissolves intermetallic phases that molybdenum-rich alloys form easily, and rapid cooling keeps them from returning as the pipe cools through the sensitive range.

S31277 is not an H grade, so clause 6.2 reheat, Table 5 grain size, and mandatory clause 17 lot marking do not apply. Bright annealing is possible by agreement where the mill can hold temperature in a protective atmosphere for the size. If pipe is hot formed or bent after delivery, plan a full re-anneal at the 2050 °F practice rather than a stress relief, because formed parts carry the same intermetallic risk as straight lengths.

Corrosion Resistance

SA-312 does not include a corrosion table, so this section is engineering commentary rather than a guarantee. With Mo 6.5–8.0%, Cr 20.5–23.0%, N 0.30–0.40%, and Ni 26–28%, S31277 offers very high resistance to chloride pitting and crevice corrosion and, thanks to the high nickel, very good resistance to chloride stress corrosion cracking. Copper in the specified range helps in some reducing acid environments. Calculated PREN values using specification minima are commonly quoted in the high 40s or above, but that figure is commentary, not a Table 1 value.

  • Severe chloride process — where S31254 or S31266 are marginal in service or in testing
  • Seawater upgrades — for warm or polluted seawater where higher Mo justifies the cost
  • Acid chloride streams — Cu and high Ni support resistance in some sulfuric and mixed-acid duties
  • Stress corrosion cracking — high nickel gives a large margin over 300-series grades

Critical pitting and crevice temperatures depend on surface condition, weld quality, and the test method, so if they matter, write ASTM G48 or a CPT/CCT test into the purchase order. Welds are usually the weakest point, which is why overalloyed Ni-Cr-Mo fillers and careful post-weld cleaning are standard practice for this grade.

Applications of SA312 UNS S31277 Pipe

Applications for UNS S31277 pipe are driven by chloride severity and by the need for high strength and ductility in the same material. The table below summarizes where buyers typically specify the grade.

Application Why Note
Severe chloride process / seawater upgrades Mo 6.5–8 + 112/52 ksi Confirm vs S31266
High-pressure chloride lines needing ductility 40% elong min Owner spec

Typical users include chemical plants handling chloride-bearing acids, flue-gas desulphurization and scrubber systems, pulp bleach plants, and offshore or desalination projects with aggressive seawater. Before committing, compare the duty against ASME SA312 UNS S31266 Stainless Steel Pipe, which may offer adequate resistance with a higher yield, and confirm the owner specification on filler class, post-weld cleaning, and corrosion testing. For moderate duties, ASME SA312 UNS S31254 Stainless Steel Pipe is easier to source and cheaper.

Weldability

Table 6 in the extracted edition does not assign an AWS filler class to UNS S31277, so the filler is by agreement. Industry practice is to use an overalloyed nickel-chromium-molybdenum consumable so that the segregated weld metal keeps at least the pitting resistance of the base pipe. Whatever is chosen, name it specifically on the WPS and PQR and qualify it on S31277 base metal before production welding.

  • Qualify on S31277 — not on S31254 or 316L coupons
  • Control heat input and interpass temperature — to limit intermetallic precipitation in the HAZ
  • Back-purge roots — to prevent ID oxidation on corrosion-critical lines
  • Remove heat tint — by pickling or mechanical cleaning where the owner specification requires it

Mill longitudinal welds on WLD and HCW pipe are autogenous, so the filler question applies only to fabrication joints. NDE extent for girth welds is a fabrication-code decision, separate from the mill hydro or electric test on each length. If a post-weld anneal is specified for formed parts, it must follow the 2050 °F practice.

Surface Finishes

Surface condition for SA312 UNS S31277 pipe should be stated on the purchase order rather than left to mill default. For stainless pipe, embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts, so the finish is part of the material performance and not just appearance. The finishes we regularly quote for this grade are listed below.

  • Annealed and pickled (AP) — solution annealed at 2050 °F [1120 °C] minimum, then descaled in acid pickle or an equivalent process to a matte grey finish; the standard choice for process pipe
  • Blasted and pickled — common on heavy-wall seamless where blasting first makes scale removal more reliable
  • Bright annealed (BA) — annealed in a protective atmosphere where mill capability exists for the size; the anneal temperature still has to meet the Table 2 practice for UNS S31277
  • Mechanically polished — OD and/or ID polish to an agreed grit or Ra when ordered; polishing never replaces the solution anneal
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed on WLD and HCW product

For S31277 the pickle must remove all Mo-rich scale, because residual scale becomes a crevice initiation site and can waste the alloy advantage in chloride service. Passivation after pickling or polishing can be added when the end-user specification calls for it, even though SA-312 itself does not require it. If the project bans chloride-bearing marking inks, say so on the order; otherwise the mill will apply its normal stencil practice and ship its default AP finish.

Inspection and Testing

The base acceptance package for SA-312 UNS S31277 pipe combines chemistry, tensile testing, heat-treatment evidence, and a pressure or electrical integrity test on every length. The items below make up the usual package; supplementary requirements and project corrosion tests only apply when they are written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for UNS S31277: C ≤0.020%, Mn ≤3.00%, P ≤0.030%, S ≤0.010%, Si ≤0.50%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, and Cu 0.50–1.50%
  • Product analysis — when ordered (Suppl. S1 or PO wording), using A480 Table A1.1 tolerances via A999 §6.3
  • Tension test — 112 ksi [770 MPa] tensile and 52 ksi [360 MPa] yield minimum, single row, plus 40% longitudinal elongation (special Table 4 group) on a lot basis
  • Flattening test — or the alternate bend test where the standard permits
  • Hydrostatic or nondestructive electric test — every length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD × wall, with UNS S31277 (no TP name exists) on every stencil

Mill test certificates: EN 10204 3.1 is the standard documentation from SHH STEEL supply. For S31277 the certificate must report all ten Table 1 elements, with Mo, Ni, N, and Cu shown as actual values, together with 112/52 ksi tensile results, 40% longitudinal elongation, the hydro or NDE method, and a 2050 °F anneal statement. EN 10204 3.2 or third-party witness by SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency is arranged when specified, and it should be booked before final testing rather than after the heat has been released. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy both editions named on the order.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Receiving review should confirm Mo 6.5–8.0, Ni 26.0–28.0, N 0.30–0.40, Cu 0.50–1.50, Cr 20.5–23.0, and C ≤0.020 on the heat, then 112/52 ksi tensile, 40% longitudinal elongation, and the 2050 °F anneal statement. Third-party inspectors should check that the stencil reads UNS S31277 rather than “6Mo” or a trade name. Use PMI that reports Mo and Ni when super-austenitic grades share a laydown area.

Packaging and Shipping

Export and domestic shipments of SA312 UNS S31277 pipe are packed for handling and for ocean or land transport. The packing we normally apply is summarized below, and anything beyond it can be agreed on the order.

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where the finish needs protecting
  • End caps — plastic or metal caps on plain or beveled ends to keep out damage and contamination in transit
  • Marking — specification, grade (UNS S31277 (no TP name exists)), heat number, size, manufacturing type (SML / WLD / HCW), test letters, and mill identity as SA-312 and the purchase order require
  • Export protection — waterproof wrapping or desiccant as agreed for polished or bright-annealed finishes, with low-chloride inks on request

Segregate UNS S31277 from ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 UNS S31266 Stainless Steel Pipe, and ASME SA312 TP316L Stainless Steel Pipe on the packing list and in the yard, because the grades look identical and a mix-up found after fabrication cannot be corrected by heat treatment. Use separate bundles and distinct tags on mixed shipments, and have receiving inspectors check stencil heat numbers against the MTC for every length. Keep interiors dry and capped so chloride-bearing moisture cannot stain or pit the surface before installation. Shipping documents normally include the packing list, invoice, bill of lading or air waybill, and the 3.1 or 3.2 MTC with full Table 1 chemistry, plus origin and customs papers to suit the agreed Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe, and for SA312 UNS S31277 we quote against the edition you name rather than a generic catalogue sheet. We report every Table 1 element on the MTC—including Mo 6.5–8.0%, Ni 26.0–28.0%, N 0.30–0.40%, and Cu 0.50–1.50%—together with the 112/52 ksi Table 4 results, the 40% elongation, and the 2050 °F anneal statement. Heat identity stays unbroken from the melt to the finished length, so receiving inspection can clear each heat against Table 1 and Table 4 without chasing paperwork after the pipe has arrived.

We check supplier certificates before shipment for a Mo value that would really make the heat S31254, a 35% elongation habit instead of the 40% requirement, and an anneal statement copied from a neighbouring grade. We are also open about what the standard leaves open: Table 6 assigns no filler class, and corrosion figures such as PREN or CPT are commentary or contractual extras, not SA-312 values.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for UNS S31277; Mo/Ni/N/Cu reported; 112/52 ksi with 40% elongation confirmed; 2050 °F anneal stated
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs as standard with full Table 1 chemistry; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both editions you name
  • Related grades — ASME SA312 UNS S31254 Stainless Steel Pipe, ASME SA312 UNS S31266 Stainless Steel Pipe, and ASME SA312 TP316L Stainless Steel Pipe when a project buys a matched package
  • Export packing — seaworthy bundles, end protectors, and durable grade, heat, size, and type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, wall, finish, and any supplementary tests you name (S1, S5, S7, S8, S9). If the same project also needs plate or fittings, ask for coordinated heats so the chemistry lines up across product forms. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 UNS S31277 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for UNS S31277
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M UNS S31277 (no TP designation)
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension (112/52 ksi, 40% L elongation), flattening/bend, hydro or NDE per length; Mo/Ni/N/Cu on MTC; 2050 °F anneal stated; S1/S5/S7/S8/S9 and corrosion tests on order
Documents EN 10204 3.1 with full Table 1 chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

UNS S31277 is not a distributor stock grade, so orders are mill runs and lead times follow specialty melt schedules and mill minimums. Enquiries should state the SA-312 edition, UNS S31277 (no TP name exists), SML/WLD/HCW, NPS or OD × wall (and whether wall is nominal or minimum), length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirements, so mill slots line up with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders, and grouping project sizes onto one heat keeps the chemistry consistent while helping meet mill minimums without over-ordering.

FAQ

Is ASME SA312 the same as ASTM A312 for UNS S31277?
For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition, and S31277 has the same row in both. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and the mill test certificate so inspectors can verify the heat against the books you cited.
Why does UNS S31277 have no TP name?
Table 1 lists S31277 with an ellipsis in the TP column, so the unified number is its only identity in SA-312. Put UNS S31277 on the purchase order, stencil, packing list, and MTC. Labels such as 7Mo or super austenitic are not grade names and can be confused with S31254 or S31266, which have different chemistry and tensile rows.
UNS S31277 vs UNS S31254 — which should I order?
S31254 has Mo 6.0–6.5%, Ni 17.5–18.5%, N 0.18–0.25%, a thickness-split 98/95 ksi tensile with 45 ksi yield, 35% elongation, and a 2100 °F anneal. S31277 raises Mo to 6.5–8.0% and Ni to 26–28%, with a 112/52 ksi floor, 40% elongation, and a 2050 °F anneal. Choose S31277 when S31254 is marginal for the duty.
UNS S31277 vs UNS S31266 — which should I order?
S31266 relies on Mo 5.2–6.2% plus W 1.5–2.5%, Mn 2–4%, and N 0.35–0.60%, giving 109/61 ksi and a 2100 °F anneal. S31277 has more Mo and Ni, no tungsten requirement, 112/52 ksi with 40% elongation, and a 2050 °F anneal. The windows do not overlap, so order the exact UNS your datasheet names.
Seamless vs welded UNS S31277 — which is better?
Neither is universally better. Seamless suits high-pressure and heavy-wall lines, while WLD and HCW are economical for larger diameters and thinner walls when seam quality and the full 2050 °F anneal are controlled. Choose the route your design code and datasheet allow, and confirm the same SML, WLD, or HCW letters on the marking and MTC.
Can you dual-certify SA312 / A312 UNS S31277?
Yes, when the heat analysis, heat treatment, mechanical tests, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the purchase order and ask for the MTC to reference both. Dual certification with S31254 or S31266 is not possible because the Mo, Ni, and N windows conflict.
Hydrostatic test vs NDE — which do I get on S31277 pipe?
Each length is either hydrostatically tested or nondestructively electrically tested, and the manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification requires one, state it on the PO and confirm the chosen test on the MTC for every length. NPS 10 and larger may be marked NH only when you accept a system test.
What anneal temperature applies to UNS S31277?
Table 2 lists S31277 at 2050 °F [1120 °C] minimum with rapid cooling. That is a separate listing from the 2100 °F used for S31254 and S31266 and well above the 1900 °F typical of 316 grades. Ask for the S31277 anneal temperature on the MTC and reject paperwork that copies a neighbouring grade’s practice.
What Table 1 chemistry defines UNS S31277?
Table 1 sets C ≤0.020%, Mn ≤3.00%, P ≤0.030%, S ≤0.010%, Si ≤0.50%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, and Cu 0.50–1.50%. These are melting-analysis limits. If you need product analysis, order it explicitly and state the A480 tolerance basis for Mo, N, and Cu on the purchase order.
What are the Table 4 tensile requirements for UNS S31277?
Table 4 requires 112 ksi [770 MPa] tensile and 52 ksi [360 MPa] yield minimum as a single row, and S31277 belongs to the special group requiring 40% longitudinal elongation together with N08925, N08028, and N08029. Do not apply the 35% habit from 300-series grades, and design to the code allowables listed for UNS S31277.
What filler metal should I use to weld UNS S31277 pipe?
Table 6 in the extracted edition assigns no AWS class to S31277, so filler is by agreement. Common practice is an overalloyed nickel-chromium-molybdenum consumable that keeps weld-metal pitting resistance at or above the base pipe. Name the specific consumable on the WPS and PQR and qualify it on S31277 base metal before production welding.
How should I check UNS S31277 pipe on receipt?
Start with molybdenum 6.5–8.0% and nickel 26.0–28.0%, since those separate S31277 from 6Mo grades, then check N, Cu, Cr, and C ≤0.020%. Confirm 112/52 ksi results, 40% longitudinal elongation, the 2050 °F anneal statement, and the hydro or NDE method. Make sure the stencil reads UNS S31277, not a trade name.

Conclusion

ASME SA312 UNS S31277 is a TP-less, high-molybdenum super-austenitic pipe grade with C ≤0.020%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, and Cu 0.50–1.50%, a single 112/52 ksi Table 4 floor with a special 40% longitudinal elongation requirement, and a 2050 °F [1120 °C] Table 2 anneal. Table 6 assigns no filler class, so the consumable is by agreement. It is not a drop-in for ASME SA312 UNS S31254 Stainless Steel Pipe or ASME SA312 UNS S31266 Stainless Steel Pipe. Order the manufacturing type, size and wall, finish, Mo/Ni/N/Cu reporting, anneal proof, filler basis, and any product-analysis or corrosion tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X