ASME SA312 UNS S31002 Stainless Steel Pipe | ASME SA312 Stainless Steel - SHH STEEL

ASME SA312 UNS S31002 Stainless Steel Pipe | SA 312/SA 312M

ASME SA312 UNS S31002 stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M), no TP designation: seamless (SML), welded (WLD) and heavily cold-worked (HCW); C ≤0.015%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%; Table 4 minima 73/30 ksi; solution annealed. SHH STEEL supplies with EN 10204 3.1 MTCs.
Grade
UNS S31002
Standard
ASME SA312 / SA 312M (ASTM A312 / A312M)
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA312 UNS S31002 Stainless Steel Pipe

ASME SA-312/SA-312M covers seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. UNS S31002 appears in Table 1 with no TP designation—the grade column shows only an ellipsis—so the pipe is ordered, marked, and certified by UNS number alone. It is the ultra-low-carbon, low-silicon member of the 25Cr–20Ni (310) family: chromium 24.0–26.0%, nickel 19.0–22.0%, carbon ≤0.015%, silicon ≤0.15%, molybdenum ≤0.10%, nitrogen ≤0.10%, with tight phosphorus ≤0.020% and sulfur ≤0.015%. Commercially the same product may be called 310L, low-carbon 310, or low-silicon 310 pipe, but those nicknames are not SA-312 grade names. For pressure piping and code work, cite UNS S31002 and the edition of SA-312 or A312 on the purchase order and on the mill test certificate—do not rely on a bare “310L” market label.

The chemistry exists because ultra-low carbon and ultra-low silicon reduce sensitization risk and improve resistance in certain oxidizing aqueous services (notably strong nitric acid lines in some process plants), while the 25Cr–20Ni base keeps high-temperature oxidation capability in the same class as ASME SA312 TP310S Stainless Steel Pipe. Table 4 sets S31002 at 73 ksi [500 MPa] tensile and 30 ksi [205 MPa] yield—two ksi below the 75/30 ksi floors of TP310S—because the very low carbon softens the room-temperature strength slightly. Heat treatment follows the Table 2 default of 1900 °F [1040 °C] (S31002 is not individually listed). It is not an H grade: there is no carbon floor, no Table 5 grain-size rule, and no clause 6.2 reheat requirement. Table 6 lists no AWS filler class for S31002, so filler selection is by agreement on the WPS. Silicon at ≤0.15% is the commercial trap—ordinary TP310S allows Si ≤1.00%, so commodity 310S heats will never meet S31002 and must be refused when the datasheet names this UNS.

SHH STEEL can supply ASME SA312 UNS S31002 stainless steel pipe to the edition named on the enquiry, including seamless (SML), welded (WLD), and heavily cold-worked (HCW) routes; ASME B36.19 schedules and special OD/wall by agreement; EN 10204 3.1 mill test certificates that report the full Table 1 window—including C ≤0.015%, Si ≤0.15%, Mo ≤0.10%, and N ≤0.10%; and dual SA-312/A312 marking when the heat analysis, heat treatment, mechanical tests, and marking satisfy both editions named on the purchase order. Confirm NPS, wall or schedule, finish, length practice, and any product-analysis or supplementary tests on enquiry.

Common commercial names and how they map to the ordered product are listed below—use the full SA-312/A312 designation plus UNS S31002 on the purchase order rather than market shorthand alone.

  • ASME SA312 UNS S31002 / SA-312 Grade UNS S31002 — preferred marking language for ASME-code and dual-marked pipe (no TP name exists)
  • ASTM A312 UNS S31002 — same grade tables for chemistry and tensile when the ASTM edition is referenced
  • UNS S31002 — unified numbering system identity used on MTCs, stencils, and cross-reference tables
  • 310L / low-carbon 310 / low-silicon 310 — market shorthand; confirm C ≤0.015%, Si ≤0.15%, Mo ≤0.10%, P ≤0.020%, S ≤0.015%, and N ≤0.10% on the order before accepting any heat

UNS S31002 is not a drop-in for ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 TP310H Stainless Steel Pipe, or ASME SA312 TP310Cb Stainless Steel Pipe on a shared “310” market label—each has its own Table 1 row. Versus TP310S (UNS S31008), S31002 tightens carbon from ≤0.08% to ≤0.015%, silicon from ≤1.00% to ≤0.15%, molybdenum from ≤0.75% to ≤0.10%, and P/S, adds an N ≤0.10% ceiling, and carries a 73 ksi tensile floor instead of 75 ksi. Versus TP310H, S31002 is the opposite design intent: ultra-low carbon without H-grade grain control or reheat, while TP310H requires C 0.04–0.10% plus Table 5 grain size for creep service. Versus TP310Cb, S31002 uses ultra-low carbon rather than niobium stabilization and keeps the tight Si/Mo residual ceilings. Dual marking with TP310S is usually impossible because the Si and Mo ceilings of S31002 sit below typical TP310S practice. Hub: ASME SA 312/SA 312M.

Manufacturing Types (SML / WLD / HCW)

ASME SA-312 defines three manufacturing routes that may be marked on finished UNS S31002 pipe. Selecting the route is a purchase-order decision driven by design code, size range, wall thickness, and inspection preference. It does not change the Table 1 chemistry of S31002—melting must still meet C ≤0.015%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, and S ≤0.015%—and every route must still pass through the solution anneal required by SA-312.

  • Seamless (SML) — no welding at any stage of manufacture. Seamless is preferred for small-bore nitric-acid and oxidizing-process lines, thick-wall process tubing, and pressure parts when the project specification excludes welded pipe or when piping-class documentation is written around seamless product only. Hot-finished or cold-finished seamless must still be solution annealed to the Table 2 default practice and rapidly cooled.
  • Welded (WLD) — automatic welding without filler metal. The weld is finished so that the pipe meets dimensional and mechanical requirements after the final heat treatment required by SA-312. Welded product is widely used for larger NPS/schedule combinations and headers where the code accepts welded austenitic pipe; the plate heat must itself meet S31002 chemistry including the ultra-low silicon and carbon ceilings.
  • Heavily cold-worked (HCW) — welded pipe that is cold worked to a reduction of area of wall and weld of at least 35% before the final anneal, again without filler metal in the longitudinal weld. The weld is radiographed before cold work. HCW is ordered when the buyer wants the HCW marking and the process controls written into SA-312 for that route; clause 11.5 capability for S9 weld-decay testing still applies to HCW when S9 is ordered.

Each finished length is hydrostatically tested or nondestructively electrically tested; the manufacturer may choose the method unless the purchase order fixes one. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser agrees to a system test in lieu of hydrotest. Lot definitions follow clause 11.1. Clause 17 heat-treatment lot marking is not mandatory for S31002 (it is not an H grade and not S30815), but buyers often request heat and lot identity on the stencil for traceability through fabrication. Ultra-low-carbon, low-silicon melts need careful AOD/VOD practice so C and Si land inside the tight windows without drifting Mo above 0.10%; grouping project sizes onto one heat improves consistency and often helps meet mill minimum order quantities that are higher than for commodity TP310S.

Lead times are typically longer than for ASME SA312 TP310S Stainless Steel Pipe because specialty melting capacity for S31002 is thinner and mills often treat it as a made-to-order grade. Remnant fills from prior S31002 heats can still cut weeks off small urgent lots when sizes match. Plan procurement early for seamless heavy-wall sizes, and confirm route, edition, Si/C reporting, and any supplementary tests (S1, S5, S7, S9) before placing a mill order so the certificate matches the design basis. Where only hot oxidation matters and the Si ≤0.15% ceiling is not required, switch the conversation to ASME SA312 TP310S Stainless Steel Pipe; where creep governs, move to ASME SA312 TP310H Stainless Steel Pipe instead of stretching an ultra-low-carbon heat into an H-grade application.

Chemical Composition of SA312 UNS S31002

Two chemistry layers matter: melting (heat / ladle) analysis—mandatory per heat under ASME SA-312/ASTM A312 Table 1—and product analysis when ordered (Suppl. S1 / PO). SA-312/A312 defer product-analysis tolerances through ASTM A999/A999M §6.3 to ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle and, when ordered, product values—never unpublished tighter windows. On heat analysis, every certificate must show carbon ≤0.015% and silicon ≤0.15%; spot-check those two values first on receipt, because they are the commercial traps that separate S31002 from ordinary TP310S.

Melting analysis (heat / ladle analysis) — Table 1

Heat analysis for UNS S31002 from ASME SA-312/SA-312M (ASTM A312/A312M) Table 1 is summarized below. Values are maximum unless a range is shown; ellipses (…) mean no requirement in the ordered edition. The grade column in Table 1 shows “…” (no TP designation).

Element UNS S31002 melting analysis
Carbon (C) ≤ 0.015
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.020
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 0.15
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) ≤ 0.10
Nitrogen (N) ≤ 0.10

Source: SA-312 Table 1, UNS S31002 (grade column “…”). Footnote C: nitrogen determination method by agreement.

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

When product analysis is ordered, apply A480 Table A1.1 tolerances to the Table 1 limits. Plan the Mo acceptance path before the heat is poured, because A480 Mo tolerances begin at “over 0.20%” and do not publish a band at the 0.10% S31002 ceiling.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.015 0.005 over ≤ 0.020
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.020 0.005 over ≤ 0.025
Sulfur (S) ≤ 0.015 0.005 over ≤ 0.020
Silicon (Si) ≤ 0.15 0.05 over ≤ 0.20
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20
Molybdenum (Mo) ≤ 0.10 No A480 row below/at 0.20 start Not established—by agreement
Nitrogen (N) ≤ 0.10 0.01 over ≤ 0.11

Mo ≤0.10%: A480 Table A1.1 Mo tolerances begin at “over 0.20%,” so no published product tolerance applies at the 0.10% max—close the gap by written agreement on the quotation and PO. Vs TP310S: S31002 has C ≤0.015 (vs ≤0.08), Si ≤0.15 (vs ≤1.00), Mo ≤0.10 (vs ≤0.75), tighter P and S, and N ≤0.10 (TP310S has no N requirement). Cr and Ni ranges match TP310S (24–26 / 19–22). Product Cr uses the 0.25 band; Ni uses 0.15 under / 0.20 over (10–20% vs 20–30% rows). Carbon at 0.015% max needs combustion analysis with a low blank; silicon at 0.15% max needs careful OES calibration. Nitrogen ≤0.10% is a Table 1 requirement—Footnote C allows the determination method to be agreed; most mills use inert-gas fusion, and leaving N off the MTC is a nonconformance even when C and Si are correct.

Element TP310S TP310H TP310Cb UNS S31002
C ≤ 0.08 0.04 – 0.10 ≤ 0.08 ≤ 0.015
Si ≤ 1.00 ≤ 1.00 ≤ 1.00 ≤ 0.15
Mo ≤ 0.75 … ≤ 0.75 ≤ 0.10
Nb … … 10×C – 1.10 …
N … … … ≤ 0.10
H controls No Yes No No

The side-by-side table above shows why a shared “310” or “310L” market label is dangerous: ASME SA312 TP310S Stainless Steel Pipe allows Si to 1.00% and C to 0.08%; ASME SA312 TP310H Stainless Steel Pipe adds H-grade carbon and grain rules without the ultra-low Si ceiling; ASME SA312 TP310Cb Stainless Steel Pipe stabilizes with niobium rather than ultra-low carbon; S31002 is the only row that combines C ≤0.015% with Si ≤0.15% and Mo ≤0.10%. Buyers who need only oxidation resistance should say so early; those needs usually push the conversation toward TP310S instead of forcing an S31002 melt when the Si limit is not required.

Mechanical Properties of SA312 UNS S31002

Room-temperature tensile requirements for UNS S31002 come from ASME SA-312/ASTM A312 Table 4. Ultra-low carbon improves welded corrosion behaviour and reduces sensitization risk; it does not raise the room-temperature tensile floor—in fact Table 4 sets S31002 two ksi below the sister 310 grades. Actual mill values are often higher than the minima, but design still uses Table 4 for ambient checks and the governing code allowables for elevated-temperature design of S31002.

Property UNS S31002
Tensile strength, min 73 ksi [500 MPa]
Yield strength, min 30 ksi [205 MPa]
Elongation, min 35% longitudinal / 25% transverse
Hardness No Table 4 maximum

Source: SA-312 Table 4 for UNS S31002. Yield matches ASME SA312 TP310S Stainless Steel Pipe; tensile is 2 ksi lower (73 vs 75 ksi). Elongation follows the Table 4 row for the ordered edition. No Table 5 grain-size requirement (not an H grade).

Base mechanical testing includes tension on a lot basis and flattening (or the alternate bend where the standard permits) typically on 5% of the lot, plus hydrotest or NDE on every length. Elevated-temperature tensile and rupture tests are purchase-order options, not base SA-312 requirements. For pressure-retaining parts, use the governing Section II Part D or project-code allowables for UNS S31002 where listed—do not copy TP310S / S31008 allowable-stress tables into an S31002 calculation package. Where the code lists only TP310 / S31008, the engineer of record must justify use of S31002 with the lower tensile floor. Annealed S31002 retains austenitic toughness to low temperature; impact testing is a construction-code or PO matter, not an SA-312 base test.

Although Table 4 has no hardness maximum, fabricators sometimes set a Rockwell limit for bending or expanding—put any such limit on the PO and verify it on the MTC if required. Like other 310 grades, S31002 hardens when cold worked; intermediate anneals may be needed for severe forming, and those anneals must still meet the Table 2 default practice. After long high-temperature service, expect reduced room-temperature ductility from carbides and possible sigma—evaluate before cold repair. For creep-range service without the ultra-low-Si chemistry case, see ASME SA312 TP310H Stainless Steel Pipe rather than stretching an S31002 heat into an H-grade application.

Dimensions and Tolerances

Dimensional supply for SA312 UNS S31002 pipe follows ASME B36.19 schedules for common NPS/schedule combinations, with special OD and wall by agreement when nitric-acid coolers, condensers, or process heaters need a non-standard section. Outside-diameter variations follow ASTM A999/A999M; wall-thickness variations follow SA-312 Table 3 as summarized below. State whether wall is nominal or minimum (Suppl. S8) on the purchase order so the mill does not ship the wrong interpretation.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Source: SA-312 Table 3; outside diameter variations per A999/A999M.

  • Lengths — NPS 1/8–8 commonly furnished up to 24 ft unless otherwise agreed; SRL, DRL, or cut-to-length on order
  • Cut lengths — typically ≤1/4 in. [6 mm] over unless the PO states a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face when the WPS is already frozen

Process industries often order by OD × wall rather than by NPS/schedule. Special OD × wall combinations are common in nitric-acid coolers and condensers where ASME B36.19 schedules leave gaps—state whether wall is minimum or nominal before the mill rolls. Straightness, end finish, and length tolerance should be written explicitly for export projects so receiving inspection has a clear acceptance basis. For socket-weld or threaded ends on thin schedules, confirm the wall remains adequate after the 12.5% under-tolerance. Jointers are not permitted unless the purchase order expressly allows them; cut-to-length programmes should include an allowance for fit-up scrap so the mill does not ship under-length pieces.

Equivalent Grades

Equivalence for UNS S31002 is primarily an ASME/ASTM identity question. The governing pipe designation is ASME SA-312 UNS S31002 (no TP name); market names and plate counterparts must be mapped back to that row before a mill is asked to dual-mark or substitute.

Designation Notes
ASME SA-312 UNS S31002 Governing pipe grade (no TP designation)
ASTM A312 UNS S31002 Same Table 1 / Table 4 when the ASTM edition is referenced
310L / low-carbon 310 / low-silicon 310 Trade names; confirm S31002 chemistry, especially C ≤0.015 and Si ≤0.15
SA-240 / A240 S31002 Plate/sheet counterpart when listed—not a pipe specification by itself
EN / JIS No one-to-one equivalent asserted in this pack (EN 1.4335-type mappings are engineering judgments, not SA-312 equivalences)

Related SA-312 grades on steelspecs.com: ASME SA312 TP310S Stainless Steel Pipe, ASME SA312 TP310H Stainless Steel Pipe, ASME SA312 TP310Cb Stainless Steel Pipe, ASME SA312 TP310HCb Stainless Steel Pipe, ASME SA312 TP309S Stainless Steel Pipe, ASME SA312 UNS S30815 Stainless Steel Pipe. Versus ASME SA312 TP310S Stainless Steel Pipe, S31002 is the specialty low-C/low-Si row—not a cheaper synonym. Versus ASME SA312 TP310H Stainless Steel Pipe, the design intents are opposite (ultra-low C vs controlled H-grade carbon). Versus ASME SA312 TP310Cb Stainless Steel Pipe, S31002 uses ultra-low carbon rather than Nb stabilization. Versus ASME SA312 UNS S30815 Stainless Steel Pipe, S31002 lacks the intentional silicon and rare-earth additions that S30815 uses for high-temperature strength. Always re-check C, Si, Mo, P, S, and N against Table 1 before accepting a substitute heat, and do not treat “310L” and “S31002” as automatically interchangeable on the purchase order.

Heat Treatment and Delivery Condition

UNS S31002 is not individually listed in Table 2, so the grade follows the Table 2 default of 1900 °F [1040 °C] minimum with rapid cooling. Because S31002 is not an H grade, clause 6.2 reheat language does not apply and direct quench after hot forming is accepted the way it is for non-H grades such as ASME SA312 TP310S Stainless Steel Pipe. There is no Table 5 grain-size rule. Delivery remains the solution-annealed condition required by SA-312 unless the ordered edition and purchase order state otherwise.

  • Solution anneal ≥1900 °F [1040 °C] — Table 2 default; rapid cool
  • No Table 5 grain-size rule — not an H grade
  • Clause 17 lot marking — not mandatory for S31002; often requested for traceability
  • Free of scale and exogenous iron — descaled / pickled or equivalent as ordered
  • Bright anneal / passivation — available on request when the end-user specification requires a scale-free or passivated surface for oxidizing acid service

Annealing at the Table 2 default dissolves residual carbides and restores corrosion resistance after hot work; rapid cooling is required. Bright annealing under hydrogen or vacuum can deliver a scale-free surface preferred for oxidizing acid service; pickled finishes are acceptable when fully rinsed. Owner-specified stabilization or post-fabrication heat treatments are purchaser requirements, not SA-312 base rules—write temperature and time on the PO if needed. Cite the ordered edition’s Table 2 default practice on the enquiry so the mill does not apply a neighboring H-grade reheat habit, or a different anneal temperature, to an S31002 heat by mistake.

Corrosion Resistance

UNS S31002 is chosen when the project needs 310-level hot-gas oxidation resistance and, on the same line list, an ultra-low-carbon / ultra-low-silicon chemistry for oxidizing aqueous service. Chromium at 24.0–26.0% supports hot-air and flue-gas oxidation performance similar in class to ASME SA312 TP310S Stainless Steel Pipe; carbon ≤0.015% and silicon ≤0.15% reduce sensitization risk and are often preferred in strong nitric acid and related oxidizing chemical services—validate concentration, temperature, and oxidizing potential with the project corrosion engineer.

  • Nitric and oxidizing acids — low C / low Si grades are often preferred; validate with corrosion engineering (SA-312 itself publishes no corrosion data)
  • Intergranular attack — C ≤0.015% strongly limits chromium-carbide sensitization in weld heat-affected zones
  • High-temperature oxidation — 24–26% Cr, similar class to TP310S for hot-air and flue-gas duty
  • Chlorides — Mo ≤0.10% is a residual ceiling, not intentional alloying; S31002 is not a 316 substitute for aqueous chloride or seawater service
  • Sigma-phase risk — high-Cr grades can still form sigma after long intermediate-temperature exposure; design dwell times accordingly

Verify intergranular resistance with Suppl. S7 (ASTM A262 Practice E) when the service case is critical, and use Suppl. S9 weld-decay testing when welded pipe must demonstrate comparable weld and base-metal loss rates. Neither test is automatic—order them when the corrosion case needs proof. Compared with ASME SA312 TP310S Stainless Steel Pipe, S31002 trades a slightly lower tensile floor and tighter melt practice for the aqueous-side benefits of ultra-low C and Si. If only hot oxidation matters and the Si ≤0.15% ceiling is not required, TP310S is usually the more available and economical choice; specify S31002 only when the low-C/low-Si chemistry is actually needed.

Applications of SA312 UNS S31002 Pipe

Buyers typically select UNS S31002 when the project already wants 310-level oxidation resistance and the corrosion review adds an oxidizing aqueous or nitric-acid case that ordinary TP310S (Si ≤1.00%, C ≤0.08%) cannot answer cleanly. The grade earns its keep by protecting both hot-gas oxidation performance and welded HAZ integrity under ultra-low carbon and silicon.

Application Why S31002 Note
Nitric acid and oxidizing chemical lines Ultra-low C and Si Confirm concentration / temperature with corrosion engineering
High-temperature process with welded aqueous exposure Low sensitization risk Compare TP310S if Si ≤0.15% is not required
Furnace / hot gas with corrosion-critical shutdowns 310 oxidation + low C Not a carburization specialist
Condensers and coolers in oxidizing service Low C / low Si + 25Cr–20Ni Often ordered by OD × wall
Welded process piping needing as-welded IGC resistance C ≤0.015% limits HAZ sensitization Order S7 if proof is required

If only hot oxidation matters, see ASME SA312 TP310S Stainless Steel Pipe—it is usually more available and carries the higher 75 ksi tensile floor. If creep or stress-rupture governs, see ASME SA312 TP310H Stainless Steel Pipe rather than forcing an ultra-low-carbon heat into an H-grade design basis. If welded HAZ integrity is the driver but ultra-low silicon is not required, compare ASME SA312 TP310Cb Stainless Steel Pipe (niobium stabilization). Typical enquiry packages list design temperature, medium, whether field welding will be performed, and whether intergranular-corrosion testing (S7) is mandatory—adding S7 early avoids late schedule slips. When replacing TP310S with S31002 in an existing unit, review weld procedures, filler selections, and receiving checklists for Si and C—the base-metal change alone does not update the WPS.

Weldability

UNS S31002 welds with GTAW, GMAW, SMAW, and SAW using practices familiar to fabricators of other 310 grades. Ultra-low carbon improves as-welded intergranular resistance in the heat-affected zone; low silicon can change weld-pool fluidity relative to ordinary TP310S, so procedures should be qualified on S31002 chemistry rather than assumed from a TP310S PQR. Mill WLD and HCW longitudinal welds are autogenous (no filler); Table 6 guidance applies to joining with filler, not to the mill seam.

Filler and Table 6: S31002 is listed with AWS class “…”—no classification is given in the extracted edition. Filler selection is by agreement and must be recorded on the WPS. Low-carbon 310-type fillers are typical shop practice so the deposited metal stays close to the ultra-low-carbon intent; do not assume a high-carbon 310 filler preserves the as-welded IGC benefit that buyers paid for in the base metal. Freeze the AWS (or EN) class on the WPS/PQR before production welds.

  • Moderate heat input; clean joints free of oil, paint, and exogenous iron
  • Argon shielding and backing gas for GTAW root passes
  • Remove heat tint; pickle when aqueous or oxidizing acid service follows
  • Mill seams autogenous; clause 15 repairs must identify any filler used

Qualify welding procedures to ASME Section IX on S31002 material (or on a heat with matching C and Si). A PQR on ASME SA312 TP310S Stainless Steel Pipe without review can miss the low-silicon effect on weld-pool behaviour and the need for low-carbon filler. Dissimilar welds of S31002 to carbon steel still commonly use 309-type fillers for dilution control; if the weld must also resist intergranular attack in oxidizing condensate, decide whether the filler itself needs ultra-low carbon or whether a barrier butter layer is required, and capture that decision in the WPS. After high-temperature service exposure, clean thoroughly before repair welding and follow producer guidance for low-carbon 310 repair practice.

Surface Finishes

Surface condition for SA312 UNS S31002 pipe is stated on the purchase order. Cleanliness matters for oxidizing acid service—embedded free iron and chloride-bearing residues defeat the chemistry advantage the buyer paid for. Typical mill finishes available from SHH STEEL supply include the following options:

  • Annealed and pickled (AP) — solution annealed, descaled in acid pickle or an equivalent process, producing a matte gray finish common for process pipe
  • Blasted and pickled — often used for heavy-wall seamless where scale removal benefits from blast first
  • Bright annealed (BA) — annealed in a protective atmosphere to a brighter, scale-free surface preferred for many oxidizing acid services where mill capability exists for the size; temperature must still meet the Table 2 default
  • As-annealed light oxide — sometimes accepted for furnace parts by agreement when the protective scale will form in service anyway
  • Mechanically polished — grit or Ra-controlled polish on OD and/or ID when ordered; polishing does not replace solution annealing
  • Bead-finished welded OD — weld bead rolled or ground flush as agreed for WLD/HCW product

Passivation after pickle or polish can be added when the end-user specification requires it—often specified for nitric-acid service even though SA-312 itself does not mandate passivation. Electropolishing is available for special clean-service needs by agreement. Use low-halide marking inks when the project specification bans chloride-bearing inks. State finish, passivation, and any ink restriction on the order so the mill does not ship a default AP finish into a BA or polished requirement.

Inspection and Testing

Base inspection and testing for SA-312 UNS S31002 pipe combines chemistry (especially C, Si, Mo, and N), mechanical, and integrity checks. The following items form the usual acceptance package; supplementary requirements apply only when written on the purchase order.

  • Heat (melting) analysis — mandatory per heat against Table 1 for UNS S31002, including C ≤0.015%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, and S ≤0.015%
  • Product analysis — when ordered (Suppl. S1 / purchase-order language), using A480 Table A1.1 tolerances via A999 §6.3; Mo product tolerance is by agreement (A480 gap below 0.20%)
  • Tension test — Table 4 tensile, yield, and elongation on a lot basis (73/30 ksi minima)
  • Flattening test — or alternate bend where the standard permits (typically on 5% of the lot)
  • Hydrostatic test or nondestructive electric test — each length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against ordered NPS/schedule or OD/wall and the applicable tolerance clauses; confirm UNS S31002 (not a TP name) on every stencil

Mill test certificates: EN 10204 3.1 is the standard documentation package from SHH STEEL supply. The certificate must report silicon ≤0.15% and carbon ≤0.015% so receiving inspection can verify the two commercial traps that separate S31002 from TP310S; nitrogen and molybdenum should also appear. EN 10204 3.2 or third-party witness (SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency) is arranged when specified and should be booked before final testing. Dual ASME SA-312 / ASTM A312 certification is available when chemistry, heat treatment, mechanical tests, and marking satisfy the edition(s) named on the order.

Option Purpose
S1 product analysis Confirms C, Si, Mo (by agreement), N, and other elements on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates
OES / combustion Si and C verification; handheld XRF is limited for light elements

Receiving review should confirm C ≤0.015, Si ≤0.15, Mo ≤0.10, N ≤0.10, Cr 24–26, Ni 19–22, P ≤0.020, S ≤0.015, tensile ≥73 ksi, yield ≥30 ksi, elongation, and hydro or NDE method. Third-party inspectors should verify that the grade stencil reads UNS S31002—not merely “310L,” “310S,” or “310SS.” PMI by OES on a sample length is a useful receiving check when multiple 310 variants share a laydown area; guns that only report Cr and Ni are insufficient to release S31002 stock. Mechanical tests follow clause 11.1 lot rules; for specialty low-C/low-Si heats made in short campaigns, a lot may be only a few dozen lengths, so base test frequency is effectively high.

Packaging and Shipping

Export and domestic shipments of SA312 UNS S31002 pipe are packed for handling and ocean or land transport. Typical packing practices from SHH STEEL supply include:

  • Seaworthy bundles — pipes strapped or cradled in bundles sized for container or break-bulk handling, with non-metallic separators where needed to protect finish; cradles or individual supports for heavy headers
  • End caps / protectors — plastic or metal caps on plain or beveled ends to reduce damage and contamination during transit
  • Marking — durable marking of specification, grade (UNS S31002—no TP name), heat number, size (NPS or OD × wall / schedule), manufacturing type (SML / WLD / HCW), test letters, and mill identity as required by SA-312 and the purchase order
  • Export packing — waterproof wrapping or desiccant as agreed for polished or bright-annealed finishes; container stuffing photos on request; low-chloride inks on request

Segregate UNS S31002 from TP310S, TP310H, and TP310Cb on the packing list and in the yard so stencil mix-ups do not travel with the shipment—mix-ups discovered after fabrication are expensive because the Si and C ceilings cannot be converted by heat treatment alone. Shipping S31002 in crates labeled only “310SS” or “310L” risks warehouse confusion with commodity TP310S. When S31002 ships with TP310S on the same vessel, use separate bundles and distinctly colored tags. Receiving inspectors should compare stencil heat numbers against the MTC for every length and verify that Si ≤0.15% and C ≤0.015% are reported before release to fabrication. Keep interiors dry and capped so chloride-bearing moisture does not stain or pit the surface before installation. Shipment docs typically include packing list, invoice, B/L or AWB, and MTC (3.1 or 3.2) with full Table 1 chemistry reported, plus origin/customs papers per Incoterms.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless plate and pipe. For ASME SA312 UNS S31002 we quote against the edition you name, report the full Table 1 window on the MTC—including C ≤0.015%, Si ≤0.15%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, and S ≤0.015%—and keep heat identity unbroken from melt through finished length. Receiving inspection then clears the heat against Table 1 and Table 4 rather than against a vague “310L” catalog sheet. We flag missing Si or C fields, Mo above 0.10%, or absent nitrogen on supplier MTCs before shipment, so non-conforming paperwork is caught at the mill—not at the fabricator. We also stay honest about the Mo product-analysis gap (A480 has no published band at 0.10% max) and about Table 6 (no AWS filler class listed), so those items stay closed by agreement on the quotation and WPS.

  • Specification fidelity — chemistry and tensile to SA-312/A312 Table 1 and Table 4 for UNS S31002; C ≤0.015% and Si ≤0.15% reported and checked; no commodity TP310S sold as 310L / S31002
  • Mill resources — SML, WLD, and HCW from qualified stainless pipe mills with heat traceability; cutting and beveling on confirmed orders
  • Documentation — EN 10204 3.1 MTCs standard with full Table 1 chemistry including Si, C, Mo, and N; 3.2 or third-party inspection on request
  • Dual marking — ASME SA-312 and ASTM A312 when the heat and tests meet both requirements you name
  • Related grades — sister 310-family SA-312 grades (TP310S / TP310H / TP310Cb) when projects buy matched high-temperature packages
  • Export packing — seaworthy bundles, end protectors, and durable UNS/heat/size/type marking

Quotations follow your purchase-order language for edition year, manufacturing type, size, finish, and any supplementary tests you name (S1, S5, S7, S8, S9). Ask for coordinated plate-and-pipe heats when a project needs matching ultra-low C/Si levels across SA-240 and SA-312 forms. Grade hub: ASME SA 312/SA 312M.

Supply Capability

SHH STEEL can supply ASME SA312 UNS S31002 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade.

Item SHH STEEL capability for UNS S31002
Standard ASME SA-312/SA-312M and/or ASTM A312/A312M UNS S31002 (no TP designation)
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension, flattening/bend, hydro or NDE per length; Si/C/Mo/N on MTC; S1/S5/S7/S8/S9 on order
Documents EN 10204 3.1 with full Table 1 chemistry reported; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

UNS S31002 is less common in distributor stock than TP310S, so mill-run orders are typical and lead times track specialty melt schedules for ultra-low-carbon, low-silicon 310. Common sizes may occasionally be available from remnant lengths of prior S31002 heats; heavy walls and special OD/wall combinations are mill-order items. Enquiries should state the SA-312 edition, UNS S31002 (not a bare “310L”), SML/WLD/HCW, NPS or OD×wall (nominal or minimum), length practice, finish, Si/C reporting expectation, and any product-analysis or 3.2 requirements so mill slots align with your need date. Cut lengths, beveling, and packing-list marking are available on confirmed orders. Combining project sizes into one heat improves C/Si consistency and helps meet mill minima without over-ordering. For urgent small quantities, ask about remnant lengths from recent S31002 heats before authorizing a new melt—remnants can cut weeks from the schedule when sizes match.

FAQ

Is ASME SA312 the same as ASTM A312?
For chemistry (Table 1), tensile (Table 4), manufacturing types, and most testing language, ASME SA-312/SA-312M matches ASTM A312/A312M of the referenced edition. Dual SA312/A312 marking is common when ordered. Name both editions on the purchase order and mill test certificate so inspectors can verify the heat against the exact books you cited—do not assume a bare market grade stamp covers dual certification.
What is the UNS number for this grade?
Table 1 lists S31002 as the unified number for this pipe grade, with an ellipsis in the TP column—there is no separate TP designation. Cite UNS S31002 on the purchase order, stencil, packing list, and mill test certificate so chemistry and tensile rows cannot be confused with a neighboring 310 grade that shares a “310L” commercial nickname.
UNS S31002 vs TP310S — which should I order?
TP310S (UNS S31008) is the workhorse 310 grade with C ≤0.08%, Si ≤1.00%, Mo ≤0.75%, and 75/30 ksi floors. UNS S31002 tightens C to ≤0.015%, Si to ≤0.15%, Mo to ≤0.10%, adds N ≤0.10%, and carries a 73 ksi tensile floor. Order S31002 only when the ultra-low C/Si chemistry is required—do not treat “310L” and TP310S as interchangeable. Put the design-code grade and UNS on the purchase order before you compare price.
UNS S31002 vs TP310H — which should I order?
TP310H is an H grade with C 0.04–0.10%, Table 5 grain-size control, clause 6.2 reheat, and lot marking for creep service. UNS S31002 is the opposite design intent: ultra-low carbon (≤0.015%) without H-grade grain or reheat rules, plus the tight Si ≤0.15% and Mo ≤0.10% ceilings. They solve different problems—do not substitute one for the other on a shared “310” label. Put the design-code grade and UNS on the purchase order before you compare price.
UNS S31002 vs TP310Cb — which should I order?
TP310Cb uses niobium stabilization (Nb 10×C min to 1.10% max) with C ≤0.08% and Si ≤1.00% on the same 25Cr–20Ni base. UNS S31002 uses ultra-low carbon and ultra-low silicon instead of Nb, with Mo ≤0.10% and N ≤0.10%. Choose Nb stabilization or ultra-low C/Si based on the corrosion and welding case—they are not drop-in substitutes. Put the design-code grade and UNS on the purchase order before you compare price.
Seamless vs welded UNS S31002 — which is better?
Neither is universally better. Choose the manufacturing type your design code and datasheet allow; both are legitimate SA-312 forms when tested to the standard, and both must still meet S31002 chemistry including C ≤0.015% and Si ≤0.15%. State SML, WLD, or HCW on the purchase order and confirm the same letters on the pipe marking and MTC—mixing offers that differ only in manufacturing type is a common bid-evaluation trap.
Can you dual-certify SA312 / A312 UNS S31002?
Yes, when heat analysis (including C ≤0.015%, Si ≤0.15%, Mo ≤0.10%, and N ≤0.10%), solution anneal, mechanical tests, and marking meet both editions named on the order. Write the ASME and ASTM edition years on the PO, and require the MTC to reference both books so receiving inspection can clear the heat without a second paperwork chase after shipment. Dual marking with TP310S is usually impossible because the Si and Mo ceilings differ.
Hydrostatic test vs NDE — which do I get?
Each length is hydrotested or nondestructively electrically tested. Manufacturer may choose unless the purchase order fixes the method. If your piping class or client specification locks one method, state it on the PO and verify the chosen test appears on the MTC for every length—silent mill option is not the same as an approved project method.
What heat treatment / anneal temperature applies to UNS S31002?
Table 2 default 1900 °F [1040 °C] minimum with rapid cooling—S31002 is not individually listed. It is not an H grade, so clause 6.2 reheat and Table 5 grain size do not apply; direct quench after hot forming is accepted. Delivery remains the solution-annealed condition required by SA-312 unless the edition and PO state otherwise. Cite the ordered edition’s Table 2 default on the enquiry so the mill does not apply a neighboring grade’s anneal practice by habit.
What Table 1 chemistry defines UNS S31002?
Table 1: C ≤0.015%, Mn ≤2.00%, P ≤0.020%, S ≤0.015%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10% (no TP designation). Values are melting-analysis limits from the ordered edition—do not invent tighter catalog windows. When product analysis is needed, order it explicitly (Suppl. S1 / PO language) and close the Mo product-tolerance gap by agreement, because A480 has no published band at 0.10% max.
What are the Table 4 tensile requirements for UNS S31002?
Table 4 minima are 73 ksi [500 MPa] tensile and 30 ksi [205 MPa] yield (elongation 35% longitudinal / 25% transverse). Yield matches TP310S; tensile is 2 ksi lower. Design to Table 4 for ambient checks and to the governing code allowables for S31002—do not copy TP310S / S31008 allowable-stress tables. Actual MTC readings are often above the floor; still use Table 4 minima unless the PO states higher guarantees the mill has accepted.
What filler metal should I use to weld UNS S31002 pipe?
Table 6 lists no filler class for S31002—filler by agreement. Low-carbon 310-type fillers are typical practice so deposited metal stays close to the ultra-low-carbon intent; do not assume a high-carbon 310 filler preserves the as-welded IGC benefit. Freeze the AWS (or EN) class on the WPS/PQR before production welds, and remember mill WLD/HCW longitudinal welds are autogenous—Table 6 guidance applies to joining with filler, not to the mill seam.

Conclusion

ASME SA312 UNS S31002 is the TP-less ultra-low-carbon, low-silicon member of the 25Cr–20Ni family: C ≤0.015%, Si ≤0.15%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, S ≤0.015%, Cr 24.0–26.0%, Ni 19.0–22.0%, Table 4 minima 73/30 ksi, and a Table 2 default 1900 °F [1040 °C] anneal. It is not a drop-in for TP310S (higher C/Si ceilings, 75 ksi floor), TP310H (H-grade creep controls), or TP310Cb (Nb stabilization)—each has its own Table 1 row. Table 6 lists no AWS filler class (filler by agreement). Order the manufacturing type (SML/WLD/HCW), schedule or wall, finish, Si/C reporting, and any product analysis or supplementary tests explicitly. For stock checks, mill certificates, or dual SA-312/A312 supply questions, contact SHH STEEL at admin@steelspecs.com or browse the ASME SA 312/SA 312M category on steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X