ASTM A312 TP304N Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 TP304N Stainless Steel Pipe

ASTM A312 TP304N / UNS S30451 nitrogen-strengthened 18-8 pipe with an 80/35 ksi Table 4 floor, in SML, WLD and HCW, supplied by SHH STEEL with EN 10204 3.1 MTCs for pressure piping, cryogenic, and high-strength 304-family service.
Grade
TP304N / UNS S30451
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP304N Stainless Steel Pipe

ASTM A312 / A312M is the ASTM International product standard for seamless (SML), welded (WLD), and heavily cold-worked (HCW) austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a materials specification; ASME SA-312 / SA-312M is a separate Code Book adoption used when a piping or boiler code requires an ASME-listed material, and the two documents are not interchangeable titles even when their grade tables align. This page covers TP304N / UNS S30451 under ASTM A312 / A312M as the primary ordering standard.

Table 1 of ASTM A312 lists TP304N with C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16%. Table 4 sets the room-temperature tensile floor at 80 ksi [550 MPa] tensile and 35 ksi [240 MPa] yield minimum, with 35% longitudinal / 25% transverse elongation Because TP304N is not individually listed in Table 2, the default solution-anneal minimum of 1900 °F [1040 °C] applies, followed by water quenching or another rapid cool. Table 6 identifies ER308 (UNS S30880 / W30840) as the matching filler metal for fabrication and repair welds.

SHH STEEL can supply ASTM A312 TP304N stainless steel pipe to the edition named on the enquiry, in seamless (SML), welded (WLD), and heavily cold-worked (HCW) form. We quote ASME B36.19 schedules together with special OD/wall by agreement, ship with EN 10204 3.1 mill test certificates that report the full Table 1 chemistry and the 80/35 ksi tensile results, and offer dual A312/SA-312 marking only when the purchase order asks for it — never as a default synonym. Please confirm NPS, wall or schedule, finish, any owner restrictions, and supplementary requirements when you enquire.

Common names for the same ordered product are listed below; put both TP grade and UNS number on the order and certificate.

  • ASTM A312 TP304N / UNS S30451 — preferred marking language for ASTM-ordered pipe
  • A312 Grade TP304N — shortened specification reference when the edition year is stated elsewhere on the PO
  • “304N” stainless pipe — common shorthand; the certificate must still show the ASTM grade and the controlling chemistry limits
  • EN 1.4315 / JIS SUS304N1 — commonly cited regional equivalents, approximate only and not code substitutes

When a project is written to an ASME Section I, III, VIII, or B31 Code Book material listing, the sister page SA312 TP304NASME SA312 TP304N stainless steel pipe explains SA-312 marking as a separate standard; do not merge the two titles on the same line item. Sister ASTM grades buyers compare with TP304N include A312 TP304ASTM A312 TP304, A312 TP304LNASTM A312 TP304LN, A312 TP304LASTM A312 TP304L, A312 TP304HASTM A312 TP304H. Grade hub: A312/A312MASTM A312 / A312M product hub.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 defines three manufacturing routes that may be marked on finished TP304N pipe. Selecting the route is a purchase-order decision driven by design code, size range, wall thickness, and inspection preference; it does not change the Table 1 chemistry of TP304N / UNS S30451.

  • Seamless (SML) — no welding at any stage of manufacture. Seamless suits heavy walls and specifications that exclude welded pipe. SML TP304N still has to be solution annealed before release.
  • Welded (WLD) — automatic welding without filler metal, followed by cold working of the weld (when required by the edition) and full solution annealing. WLD is economical in thinner walls and larger diameters.
  • Heavily cold-worked (HCW) — welded pipe that is cold worked to a high reduction before the final anneal, producing a wrought structure across the weld.

Chemical Composition of ASTM A312 TP304N

Two chemistry layers matter on every ASTM A312 TP304N order: melting (heat / ladle) analysis — mandatory per heat under Table 1 — and product analysis when ordered under Supplementary Requirement S1 or an equivalent purchase-order clause. A312 defers product-analysis tolerances through ASTM A999/A999M to ASTM A480/A480M Table A1.1.

Melting analysis (heat / ladle analysis) — Table 1

Heat analysis for Grade TP304N / UNS S30451 from ASTM A312 / A312M Table 1 is reproduced below. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element.

Element TP304N (UNS S30451) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Nitrogen (N) 0.10 – 0.16
Molybdenum (Mo) … (no requirement)

Read the melting table against the certificate ladle line: carbon must satisfy ≤0.08%, chromium must sit inside 18.0–20.0%, and nickel must sit inside 8.0–11.0%. Nitrogen must fall inside 0.10–0.16% — that band is what separates this grade from ordinary residual nitrogen in the same family.

Product analysis limits (A480 Table A1.1 tolerances applied)

When product analysis is ordered, the finished-pipe limits below are the melting limits plus the A480 A1.1 tolerances.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 11.0 0.10 under / 0.15 over 7.90 – 11.15
Nitrogen (N) 0.10 – 0.16 0.01 under / over 0.09 – 0.17

On product analysis the finished pipe may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20%, Ni 7.90–11.15%, and N 0.09–0.17%. State any owner-tighter carbon, cobalt, ferrite, or residual limits on the purchase order before the heat is selected.

The comparison table below places TP304N next to its closest ASTM A312 sister grades so buyers can see which chemistry and tensile floor they are actually ordering.

Grade UNS C Ni N
TP304 S30400 ≤ 0.08 8.0 – 11.0 …
TP304L S30403 ≤ 0.035 8.0 – 13.0 …
TP304H S30409 0.04 – 0.10 8.0 – 11.0 …
TP304N S30451 ≤ 0.08 8.0 – 11.0 0.10 – 0.16
TP304LN S30453 ≤ 0.035 8.0 – 12.0 0.10 – 0.16

Use the comparison as a reading aid only; the grade on the stencil and the MTC is what ships.

Mechanical Properties of ASTM A312 TP304N

Room-temperature tensile requirements for TP304N are set in ASTM A312 Table 4. The floors below are acceptance minima for the ordered grade; they are not design allowables, which come from the governing piping or vessel code and the edition of the allowable-stress tables listed for UNS S30451.

Property (ASTM A312 Table 4) TP304N
Tensile strength, min 80 ksi [550 MPa]
Yield strength (0.2% offset), min 35 ksi [240 MPa]
Elongation in 2 in. or 50 mm (or 4D), min 35% longitudinal / 25% transverse
Hardness No maximum listed in Table 4

The 80/35 ksi floor, together with 35% longitudinal / 25% transverse elongation, is the mechanical identity of TP304N under A312. Table 4 lists no hardness maximum for this grade, so write any hardness limit on the purchase order if fabrication or owner rules need one — do not invent a catalog HB or HRB value and treat it as a specification number.

The sister-grade tensile comparison below shows how TP304N sits inside its ASTM A312 family at room temperature.

Grade Tensile min, ksi [MPa] Yield min, ksi [MPa]
TP304L 70 [485] 25 [170]
TP304 / TP304H 75 [515] 30 [205]
TP304LN 75 [515] 30 [205]
TP304N 80 [550] 35 [240]

The 80/35 ksi floor is the highest room-temperature tensile pair in the basic 304 family under A312, sitting above the 75/30 ksi of A312 TP304ASTM A312 TP304 / A312 TP304LNASTM A312 TP304LN and the 70/25 ksi of A312 TP304LASTM A312 TP304L. That strength comes from the required nitrogen band, not from cold work left in the pipe — delivery is still the annealed condition. Higher room-temperature floors do not automatically authorize a thinner wall; check the allowable-stress tables for UNS S30451 at the design temperature before changing schedule.

Dimensions and Tolerances

ASTM A312 pipe is commonly ordered to ASME B36.19 stainless-steel pipe schedules (Sch 5S, 10S, 40S, 80S and others) and may also be ordered to special outside diameter and wall combinations by agreement. Outside-diameter and wall-thickness tolerances follow the tables referenced by A312 through the general requirements specifications; the wall-thickness tolerance summary below is the Table 3 pattern buyers use when checking nominal wall on receipt.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Read “wall over” and “wall under” as percentages of the ordered nominal wall. Light-wall and large-diameter sizes carry the wider bands; if the purchase order invokes Supplementary Requirement S8, wall is interpreted as minimum rather than nominal, and that choice must be visible on the order and the MTC.

Representative stock sizes and common OD × wall examples are listed in the Stock / available sizes table under Supply Capability below; special OD/wall and cut lengths are quoted on enquiry rather than promised from a fixed warehouse list.

Equivalent Grades

Cross-references help purchasing conversations, but they do not authorize substitution on a pressure-code line item. The governing product standard for pipe ordered from this page is ASTM A312 / A312M Grade TP304N / UNS S30451. The table lists related designations as approximate relationships only.

Designation Relationship to TP304N
ASTM A312 / A312M TP304N Governing pipe grade for this article
UNS S30451 Unified number in Table 1
ASME SA-312 TP304N Separate Code Book adoption; dual-mark only when the PO asks
ASTM A240 / ASME SA-240 304N Plate/sheet counterpart (separate specification)
EN 1.4315 Commonly cited European designation — approximate only; verify in the EN text
JIS SUS304N1 Commonly cited Japanese counterpart — approximate only

EN 1.4315 and JIS SUS304N1 are commonly cited approximate equivalents that were not verified line-by-line against the EN or JIS texts for this page; they do not replace an engineered approval when a project specification names A312. Within ASTM A312, sister grades such as A312 TP304ASTM A312 TP304, A312 TP304LNASTM A312 TP304LN, A312 TP304LASTM A312 TP304L, A312 TP304HASTM A312 TP304H share family traits but differ in carbon, nitrogen, molybdenum, or tensile floor, and none is a silent substitute for TP304N.

Heat Treatment and Delivery Condition

All pipe furnished to ASTM A312 has to be heat treated. TP304N is not individually listed in Table 2, so it takes the default solution anneal at a minimum of 1900 °F [1040 °C], followed by water quenching or another rapid cool sufficient to prevent precipitation. The anneal dissolves carbides and nitrides and restores the fully austenitic structure on which both strength and corrosion behaviour rely, and the anneal statement belongs on the mill test certificate for every lot.

Seamless pipe may be quenched directly after hot forming when the ordered edition allows it and the finishing temperature is not below the minimum anneal temperature; TP304N is not an H grade, so the H-grade reheat rules do not apply. HCW cold reduction is performed before the final anneal, so delivery is always the annealed condition. Any re-anneal in fabrication should follow the same minimum temperature and rapid cool, and long holds in the sensitization or nitride-precipitation range should be avoided.

Corrosion Resistance

ASTM A312 has no corrosion-rate table, so the notes below are engineering commentary. TP304N behaves like other 304-family grades in general corrosion; the required nitrogen band raises strength but does not create a molybdenum-bearing pitting grade. Buyers sometimes assume the N suffix means better corrosion resistance, and in chloride service it does not replace Mo.

  • Welded joints — carbon may be up to 0.08%, so sensitization risk is higher than A312 TP304LASTM A312 TP304L or A312 TP304LNASTM A312 TP304LN; order S7 when as-welded integrity must be shown
  • Chlorides / seawater — no Mo; prefer A312 TP316ASTM A312 TP316 or A312 TP316LASTM A312 TP316L
  • Cryogenic service — nitrogen-stabilized austenite is often attractive; confirm impact and code listing

Keep surfaces free of carbon-steel contamination and heat tint, and do not treat residual nitrogen in ordinary TP304 as a substitute for the 0.10–0.16% band required here.

Applications of ASTM A312 TP304N Pipe

Applications for ASTM A312 TP304N pipe follow from its Table 1 chemistry and Table 4 floor. The table below is a buyer’s map of typical service and the point to check on each enquiry, not a substitute for corrosion engineering or code design.

Application Why TP304N Note
Pressure piping in plants standardized on 304 Higher allowables allow lighter walls with familiar chemistry Check code listing at design temperature
Cryogenic and LNG auxiliaries Nitrogen stabilizes austenite and keeps toughness Impact tests per governing code
Nuclear and power auxiliaries Nitrogen-strengthened 304 variants used where strength and stability needed Owner specifications often add requirements
Food, beverage, pharma utilities 304 hygiene with more strength Specify finish and passivation
Heat exchangers and pressure vessels Shell and connection pipe Tube and plate under separate specs
High-pressure gas lines Strength in a weldable 18-8 Weld procedure qualified on S30451

For chloride-heavy or seawater service, confirm whether TP304N is adequate or whether a higher-Mo or duplex grade is the better answer.

Weldability

TP304N is welded by the GTAW, GMAW, SMAW, and orbital processes common on 300-series pipe. ASTM A312 Table 6 lists ER308 (UNS S30880 / W30840) as the filler for this grade; record it on the WPS and PQR so the deposit matches the intent of the ordered pipe. Mill longitudinal welds on WLD and HCW pipe are made without filler, so Table 6 applies to repairs and shop or field girth welds.

In practice, qualify the procedure on TP304N with any owner ferrite or NDE extras included, control heat input and interpass temperature on thin Sch 5S/10S walls, back-purge roots on high-integrity lines, and keep joints free of oil, paint, and carbon-steel contamination. Girth-weld NDE is separate from the mill hydro or electric test and should be agreed before fabrication.

Surface Finishes

The standard delivery finish for ASTM A312 TP304N pipe is solution annealed and pickled, so the surface is free of heat-treat scale. Bright-annealed, polished, or special cleanliness finishes are available when the purchase order states them, and any roughness limit or end bevel should be written as a number. Owners with marking-ink or chloride cleanliness rules should state them on the order so the mill can plan the route.

Inspection and Testing

Every length of ASTM A312 TP304N pipe receives the mandatory tests of the specification: heat analysis, tensile testing at the required frequency, flattening or bend testing as applicable, and either a hydrostatic test or a permitted nondestructive electric test. Supplementary requirements stay optional until the purchase order invokes them; the common ones are summarized below.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Receiving review should confirm the stencil reads TP304N, the ladle chemistry meets Table 1 including ≤0.08% carbon and N 0.10–0.16%, tensile results meet 80/35 ksi, the anneal statement is present, and ordered S-numbers appear on the MTC. Look-alike sisters such as A312 TP304ASTM A312 TP304, A312 TP304LNASTM A312 TP304LN should be bundled and tagged separately.

Packaging and Shipping

Packaging for ASTM A312 TP304N pipe is planned around surface protection and identity. Bundles are strapped with protected banding, ends are capped, and packing lists carry heat numbers that match the certificates, so receiving can tie every length back to its MTC without guesswork. Export loads go in seaworthy bundles or cases, and mixed-grade loads are tagged piece by piece.

Why Choose SHH STEEL

SHH STEEL supplies ASTM A312 TP304N / UNS S30451 as an ASTM-ordered product first. We quote the edition you name, report the full Table 1 chemistry on the EN 10204 3.1 certificate, and verify the 80/35 ksi floor before shipment. Dual SA-312 marking is added only when the order asks for Code Book identity, and we never blur the two standards into one title.

We check supplier certificates against Table 1 and Table 4 before shipment, so a missing nitrogen value or a sister-grade tensile floor is caught at the mill, not at your fabricator.

  • Specification control — Table 1 and Table 4 checked for TP304N; 1900 °F [1040 °C] anneal stated
  • Routes — SML, WLD, and HCW quoted to the route you name
  • Documents — EN 10204 3.1 standard; 3.2 when arranged with the inspector
  • No silent substitution — sister grades are never shipped in place of TP304N

Supply Capability

SHH STEEL quotes ASTM A312 TP304N against the size list, manufacturing type, and edition year on your enquiry. The table below is our commercial envelope, not a live inventory.

Item SHH STEEL capability for TP304N
Standard ASTM A312 / A312M (dual SA-312 marking when the PO asks)
Grade TP304N / UNS S30451
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; bright annealed or polished on enquiry
Certification EN 10204 3.1 MTC; 3.2 when arranged
Supplementary tests S1, S5, S7, S8, S9 and owner extras on order

Stock / available sizes

For stock enquiries we work from the representative range below, which follows common B36.19 stainless schedules and frequently requested OD × wall combinations. Ask for a confirmed list against your matrix, because availability changes with heat cycles.

Item Representative supply / stock enquiry range
NPS (typical) 1/2, 3/4, 1, 1-1/2, 2, 3, 4, 6, 8, 10, 12, 14, 16, 18, 20, 24 (confirm on enquiry)
Schedules (B36.19) Sch 5S, 10S, 40S, 80S; heavier or lighter walls by agreement
Common OD × wall examples 21.3 × 2.11 mm (NPS 1/2 Sch 40S); 33.4 × 3.38 mm (NPS 1 Sch 40S); 60.3 × 3.91 mm (NPS 2 Sch 40S); 88.9 × 5.49 mm (NPS 3 Sch 40S); 114.3 × 6.02 mm (NPS 4 Sch 40S); 168.3 × 7.11 mm (NPS 6 Sch 40S)
Special sizes Non-B36.19 OD/wall, cut-to-length, and HCW finishes — quoted on enquiry, not a fixed warehouse SKU list
Length SRL, DRL, or cut-to-length per PO

TP304LN and TP304N are specialist nitrogen grades held less deeply than commodity TP304/TP304L, so most packages are mill runs grouped by heat. Send the size matrix, edition year, route, finish, and S-number extras for a priced availability reply. Hub: A312/A312MASTM A312 / A312M product hub.

FAQ

Is ASTM A312 the same as ASME SA-312 for TP304N?
No. ASTM A312 / A312M is the ASTM product standard, while ASME SA-312 / SA-312M is a separate Code Book adoption used when a boiler or pressure-vessel code requires an ASME-listed material. The grade tables usually align and one heat can be dual-marked when the order asks, but the names are not synonyms. Order ASTM A312 TP304N when your project cites ASTM, and add SA-312 marking only for Code work.
What is the UNS number and chemistry of TP304N?
ASTM A312 Table 1 lists TP304N as UNS S30451 with C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16%. Those limits define the grade on the mill certificate. Put both TP304N and UNS S30451 on the purchase order so the heat cannot be confused with a sister grade that looks identical but differs in carbon, nitrogen, or molybdenum.
Seamless vs welded TP304N pipe — which should I order?
SML, WLD, and HCW are all legitimate ASTM A312 routes for TP304N, and chemistry does not change between them. Seamless suits heavy walls and specifications that exclude welds. Welded and HCW are economical in thinner walls and larger diameters, and HCW gives a wrought weld zone. Choose by design code, size, and inspection preference, and check the route letters on the certificate.
Does ASTM A312 set a hardness limit for TP304N?
No. Table 4 sets tensile strength, yield strength, and elongation minima for TP304N but lists no hardness maximum for this grade. If fabrication or an owner specification needs a hardness ceiling, write it on the purchase order as an extra requirement. Do not treat a catalog HB or HRB figure as an A312 number when reviewing certificates.
What filler metal and heat treatment apply to TP304N?
ASTM A312 Table 6 lists ER308 (UNS S30880 / W30840) for TP304N, and because the grade is not individually listed in Table 2 it takes the default 1900 °F [1040 °C] minimum solution anneal with rapid cooling. Record the filler on the WPS and PQR, and confirm the anneal statement appears on every mill certificate before the pipe is released to fabrication.
What wall-thickness tolerance applies to ASTM A312 TP304N pipe?
Wall tolerance follows the Table 3 pattern: for example, NPS 1/8 to 2-1/2 at all t/D carries +20.0% / −12.5% on nominal wall, with different over-tolerance bands for larger sizes and t/D ratios. When Supplementary Requirement S8 is invoked, wall is treated as a minimum rather than nominal, so state S8 on the order when your design is based on minimum wall.
How does TP304N differ from TP304?
Both allow carbon up to 0.08% with the same chromium range, but TP304N requires nitrogen 0.10–0.16% and lifts the Table 4 floor to 80/35 ksi from 75/30 ksi. Ordinary residual nitrogen in TP304 does not meet that band, so the certificate must report nitrogen inside the range before the pipe can be accepted as TP304N.
What is the difference between TP304N and TP304LN?
Both require nitrogen 0.10–0.16%. TP304N allows carbon up to 0.08% with an 80/35 ksi floor; TP304LN limits carbon to 0.035% with a 75/30 ksi floor and a nickel range of 8.0–12.0%. Pick TP304N for maximum 304-family strength and TP304LN when low-carbon weld behaviour is mandatory for the service.
Is TP304N more corrosion resistant than TP304?
Not in a way that replaces molybdenum. Nitrogen strengthens the austenite, but ASTM A312 does not make TP304N a pitting-resistant grade, and its corrosion behaviour in most services is close to TP304. For chloride, brackish, or seawater duty, look at TP316 or TP316L instead of relying on the N suffix alone.
Can higher-strength TP304N allow a thinner wall?
Only when the governing code allowable-stress tables for UNS S30451 at the design temperature support it. The 80/35 ksi room-temperature floor is necessary but not sufficient for a schedule change. Have the piping designer check the code allowables and any project minimum-thickness rules before ordering a lighter schedule than the TP304 design used.

Conclusion

ASTM A312 TP304N / UNS S30451 is ordered under ASTM A312 / A312M as a stand-alone product standard, with C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 8.0–11.0%, and N 0.10–0.16% in Table 1, a 80/35 ksi Table 4 floor with 35% L / 25% T elongation, the default 1900 °F [1040 °C] solution anneal, and ER308 (UNS S30880 / W30840) filler from Table 6. ASME SA-312 remains a separate Code Book document, so request dual marking only when the order needs it. Specify route, size and wall, finish, chemistry reporting, and supplementary tests explicitly, and compare sister grades such as ASTM A312 TP304, ASTM A312 TP304LN, ASTM A312 TP304L before substituting. For availability against your size matrix, contact SHH STEEL at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X