ASTM A312 TP309H Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 TP309H Stainless Steel Pipe

ASTM A312 TP309H / UNS S30909 heat-resisting stainless steel pipe in SML, WLD and HCW, with C 0.04–0.10%, Cr 22.0–24.0%, Ni 12.0–15.0%, a 75/30 ksi Table 4 floor and a 1900 °F anneal and grain size No. 6 or coarser, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP309H / UNS S30909
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP309H Stainless Steel Pipe

ASTM A312/A312M is the ASTM product specification for seamless, straight-seam welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as an ASTM document, with its own chemistry table, tensile table, heat-treatment table, and testing clauses, and a purchase order written to it should name the ASTM edition directly. This page covers Grade TP309H / UNS S30909 under that specification and draws every number from the referenced A312/A312M tables rather than from catalogue habit.

TP309H is the controlled-carbon, grain-size-controlled high-temperature member of the 23Cr–13Ni ASTM A312 family. Table 1 sets C 0.04–0.10%, Cr 22.0–24.0%, Ni 12.0–15.0%, with manganese capped at 2.00%, silicon at 1.00%, phosphorus at 0.045% and sulfur at 0.030%. The 309 family sits one step above the 304 family in chromium and nickel, and buyers usually reach for it when a line runs hot enough in air or combustion gas that 18-8 grades start to scale. Table 4 releases the grade at 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield with 35% longitudinal / 25% transverse elongation, and the pipe is delivered solution annealed at 1900 °F [1040 °C] minimum with rapid cooling.

The “H” suffix is not a marketing tag: it means a carbon floor of 0.04%, a carbon ceiling of 0.10%, ASTM grain size No. 6 or coarser, and a reheated solution anneal before quench, all of which exist to protect creep strength at elevated temperature. Read the suffix as part of the grade identity, because a length stenciled only “309” does not tell receiving inspection which Table 1 row the heat was melted to.

SHH STEEL can supply ASTM A312 TP309H stainless steel pipe as seamless (SML), welded (WLD), or heavily cold-worked (HCW) product in ASME B36.19 schedules and in special OD and wall combinations, with EN 10204 3.1 mill test certificates as the standard document package and EN 10204 3.2 or third-party witness when the enquiry asks for it. Where a project also runs under the ASME Boiler and Pressure Vessel Code, dual A312/SA-312 marking can be arranged, but only when the purchase order names both standards and the heat qualifies under each. ASME SA-312 is a separate standard with its own adoption history, and the same grade is described on its own page at SA312 TP309H.

Buyers comparing TP309H within the ASTM A312 series usually look next at A312 TP309S, A312 TP309Cb, A312 TP309HCb, and at the matching 310-family grade A312 TP310H. The full grade list is on the A312/A312M hub, which is the quickest way to check a neighbouring grade when the datasheet leaves more than one heat-resisting option open.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 allows three manufacturing routes for TP309H pipe, and the choice belongs on the purchase order because it changes inspection, marking, and sometimes the design allowance, while it never changes the chemistry. Whichever route is chosen, the heat must still meet C 0.04–0.10%, Cr 22.0–24.0%, Ni 12.0–15.0%, and every length still has to pass through the solution anneal before release.

  • Seamless (SML) — produced without welding at any stage, and preferred for high-pressure service, heavy wall, and owners who exclude welded pipe from the line class. For creep-critical heater loops and thick walls, seamless is often preferred, but welded and HCW product remain valid when the design class and the inspection plan accept them.
  • Welded (WLD) — made by an automatic welding process with no filler metal in the longitudinal seam, then solution annealed. Ask for the strip or plate heat number on the certificate, because that heat is what carries the Table 1 chemistry.
  • Heavily cold-worked (HCW) — welded pipe cold worked by at least 35% reduction in both wall and weld before the final anneal, with the weld radiographed before cold work. Order HCW only when the project specifically calls for that marking and its process controls.

Chemical Composition of ASTM A312 TP309H

Two layers of chemistry matter on an ASTM A312 TP309H order. The heat (ladle) analysis is mandatory for every heat and must meet Table 1, while product analysis on the finished pipe is made only when the purchase order calls for it, using the tolerances that A312 brings in through ASTM A999/A999M and ASTM A480/A480M Table A1.1. SHH STEEL reports actual heat values on the certificate and, when ordered, product values as well; we do not quote tighter in-house windows as if they were part of the standard.

Heat analysis — ASTM A312 Table 1

The table below sets out the Table 1 heat-analysis limits for TP309H / UNS S30909. Values are maxima unless a range is shown, and an ellipsis means the edition places no requirement on that element.

Element TP309H / UNS S30909 heat analysis, %
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 15.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)

Reading the table, the line that separates TP309H from TP309S is carbon: TP309H has a minimum of 0.04% as well as a maximum of 0.10%, whereas TP309S is simply capped at 0.08%. Chromium at 22.0–24.0% and nickel at 12.0–15.0% are unchanged from the S grade, and this H row has no molybdenum requirement in Table 1, so a heat that happens to carry molybdenum is reported but not judged against a limit. A certificate showing carbon below 0.04% cannot be accepted as TP309H, however good the other numbers look.

Product analysis — A480/A480M Table A1.1 tolerances

When product analysis is ordered, the Table A1.1 tolerances are applied to the Table 1 limits as shown below. The tolerance applies to an individual product determination; it does not widen the heat-analysis range that the mill must meet in the first place.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 22.0 – 24.0 0.25 under / over 21.75 – 24.25
Nickel (Ni) 12.0 – 15.0 0.15 under / over 11.85 – 15.15

309 family side by side

Because four 309-family rows sit next to each other in Table 1, it helps to see them together. The comparison below uses the same Table 1 values and shows where TP309H differs from its sisters; chromium is 22.0–24.0% for all four.

Element TP309S TP309H TP309Cb TP309HCb
C ≤ 0.08 0.04 – 0.10 ≤ 0.08 0.04 – 0.10
Ni 12.0 – 15.0 12.0 – 15.0 12.0 – 16.0 12.0 – 16.0
Mo ≤ 0.75 … ≤ 0.75 ≤ 0.75
Nb … … 10×C – 1.10 10×C – 1.10
Table 5 grain size — No. 6 or coarser — No. 6 or coarser

Reading across, the S and Cb grades share the 0.08% carbon cap, the H and HCb grades share the 0.04–0.10% band and the Table 5 grain-size rule, and the niobium line appears only on the two stabilized rows. In the 309 family the stabilized grades also allow nickel up to 16.0%, against 15.0% for TP309S and TP309H. The differences look small on paper but they decide which heats a mill can allocate, so name the exact TP designation and UNS number on the order instead of a family name.

Mechanical Properties of ASTM A312 TP309H

Room-temperature tensile requirements for TP309H come from ASTM A312 Table 4. They are minima for release testing, not typical values, and they are the same 75/30 ksi floor shared by the other 309-family grades. Mill results usually sit above these figures, but design should still use the table unless the purchase order states higher guaranteed values.

Property ASTM A312 TP309H / UNS S30909
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm (or 4D) 35% longitudinal / 25% transverse, min
Grain size (Table 5) ASTM No. 6 or coarser
Hardness No maximum in Table 4

The row that sets TP309H apart is grain size. Table 5 requires ASTM grain size No. 6 or coarser, and that check is what lets the H grade carry its elevated-temperature strength, because a coarser austenite grain resists creep better than a fine one. The tensile floor itself is no higher than TP309S, so a buyer comparing room-temperature certificates will not see the difference; it shows up in the grain-size report and in the carbon band.

Dimensions, Tolerances and Stock Sizes

Dimensional supply for ASTM A312 TP309H follows ASME B36.19 for the standard NPS and schedule combinations, with special outside diameters and walls available by agreement when a furnace, heater, or duct needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarized below.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

In short, the under-tolerance on wall is 12.5% across the whole range, while the permitted over-tolerance depends on the NPS, the wall-to-diameter ratio, and for NPS 20 and larger on whether the pipe is welded or seamless. State on the order whether the wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same line item, and the difference matters most on thin-wall heat-resisting ducts.

  • Lengths — single random, double random, or cut-to-length as ordered
  • Cut lengths — normally no more than 1/4 in. [6 mm] over the ordered length unless the PO sets a tighter band
  • Ends — plain or beveled; confirm bevel angle and root face if the WPS is already fixed
  • Jointers — not permitted unless the purchase order expressly allows them

Stock / Available sizes

SHH STEEL quotes ASTM A312 TP309H against a practical stock-and-mill enquiry range rather than a fixed list of stock-keeping units. The representative sizes below are the combinations most often discussed for this grade; availability for a given manufacturing route and exact wall still has to be confirmed at enquiry, and we do not publish tonnages against individual lines.

Representative size (ASME B36.19) Typical schedules / notes for TP309H
NPS 1/2 – 2 Sch 10S / 40S / 80S; instrument and small process connections
NPS 2-1/2 – 6 Sch 10S / 40S / 80S; common furnace and process line sizes
NPS 8 – 12 Sch 10S / 40S; confirm SML or WLD at enquiry
NPS 14 – 24 Sch 10S / 40S; usually welded and often mill-order depending on wall
Special OD × wall By agreement — state OD, wall (nominal or minimum), and length practice

Example enquiries we handle are framed as OD × wall, for instance NPS 4 Sch 40S or a special OD with a minimum wall for a heater coil, and we answer with what can ship from selected stock and what needs a mill slot. H-grade stock is thinner than S-grade stock because grain size and carbon band have to be confirmed on each heat, so many lines are mill-order. Special sizes, cut lengths, and mixed seamless and welded packages are on enquiry.

Equivalent Grades

Equivalence for TP309H is first an identity question within ASTM A312 and only second a cross-reference to other systems. The governing designation on this page is ASTM A312 Grade TP309H / UNS S30909; trade names, plate counterparts, and foreign designations all need to be mapped back to that row before a mill is asked to substitute or dual-mark.

Designation Notes
ASTM A312 / A312M TP309H / UNS S30909 Governing pipe grade for this page
ASME SA-312 TP309H Separate ASME standard; dual marking only when the PO names both and the heat qualifies
309H (trade names) Confirm UNS S30909 chemistry on the MTC; not a grade name by itself
ASTM A240 UNS S30909 Plate and sheet counterpart — not a pipe specification
EN / JIS No one-to-one equivalent asserted here

Read the notes column literally: an EN or JIS designation is a starting point for engineering comparison, not a substitute grade, and for an H or stabilized grade the carbon band, niobium line, and grain-size rule rarely map across cleanly. Within ASTM A312 the closest relatives are A312 TP309S, A312 TP309Cb, A312 TP309HCb, but each one is a separate row with its own limits, so an order for one is not satisfied by a certificate for another.

Compared with A312 TP304H, the 309 family carries more chromium and nickel and gains roughly one step of oxidation resistance, but it is not a substitute for A312 TP310H where the line really needs 25Cr–20Ni. Where a project spans pipe and plate, carry the same UNS number through both forms but still order the pipe to A312.

Heat Treatment and Delivery Condition

All pipe furnished to ASTM A312 is heat treated. Table 2 lists TP309H in the same group as TP309HCb, TP310H, TP310HCb at a solution-annealing temperature of 1900 °F [1040 °C] minimum, followed by water quenching or another rapid cool. The temperature looks the same as the default used for many non-H grades, but the route to it is different: clause 6.2 requires H-grade pipe to be reheated to the solution temperature for the required time before quenching, so a direct quench straight off the hot-forming operation is not accepted for TP309H.

  • Reheated solution anneal — 1900 °F [1040 °C] minimum, then rapid cool (Table 2)
  • Grain size — ASTM grain size No. 6 or coarser, reported on the certificate
  • Lot identification — heat number and heat-treatment lot marked on each length (clause 17)
  • Surface — free of scale and contaminating iron; pickled or equivalent as ordered

For an H grade the furnace record is part of the product, so ask for the heat-treatment lot on the certificate and keep it matched to the stencil on each length. That is how receiving inspection connects a given pipe to its grain-size result. If the purchase order also requires a post-fabrication treatment, write the temperature and hold time explicitly and make sure it does not undo the grain structure the H grade was bought for.

Corrosion Resistance

The case for TP309H is primarily oxidation and scaling resistance at high temperature. The 22.0–24.0% chromium forms a protective oxide that holds up in hot air and many combustion atmospheres where 18-8 grades scale away, and the 12.0–15.0% nickel keeps the matrix fully austenitic and tough through thermal cycling. The 309 family sits between the 304 family and the 310 family, which makes it a cost-effective step up when 304 is visibly scaling but 310 is more alloy than the line needs.

The controlled carbon band that gives TP309H its creep strength also makes it more prone to sensitization than TP309S when weld zones sit in the carbide-precipitation range. In continuous hot service this is often acceptable, but where shutdown condensate or polythionic acid is a concern the stabilized H grade A312 TP309HCb is the more defensive choice.

Applications of ASTM A312 TP309H Pipe

Buyers typically select TP309H when the design is in the creep range and the code allowables depend on an H grade with controlled carbon and grain size. The table below lists the services where we most often see the grade on an enquiry, together with the reason it is chosen and the point worth checking before ordering.

Application Why TP309H Check before ordering
Fired-heater radiant and convection tubes Creep strength from C band and grain size Confirm code listing for UNS S30909
High-temperature transfer lines H-grade allowables Reheated anneal on the certificate
Furnace headers and manifolds Elevated-temperature strength Seamless often preferred on heavy wall
Thermal processing equipment Oxidation and creep together Check thermal fatigue at supports
Steam and hot-gas service Long-term strength at temperature Consider HCb if welds see condensate

Reading the table, the common thread is heat: TP309H is rarely bought for room-temperature corrosion alone, where cheaper grades do the job. Typical size mixes run from instrument connections at NPS 1/2–2, through process lines at NPS 3–8, up to welded ducts at NPS 12–24, and the availability of fittings and flanges in matching chemistry can limit the line list, so check companion components before the isometrics are frozen. When TP309H replaces another grade in an existing unit, review the weld procedures as well, because a base-metal change alone does not update a WPS.

Weldability

TP309H welds readily by GTAW, GMAW, SMAW, and SAW, and its fully austenitic structure means no preheat is normally required. The mill longitudinal seam on WLD and HCW pipe is made without filler metal, so the filler question only arises for field and shop joints. Table 6 of A312 shows no AWS filler classification for TP309H, which means the filler is selected by agreement on the welding procedure specification rather than dictated by the pipe standard.

In practice the WPS will usually choose a matching 309-type filler, or a richer one where dilution or dissimilar joints are involved, and that choice should be documented and qualified for the service temperature. For H-grade service the filler should be selected so that the weld metal keeps adequate elevated-temperature strength; a low-carbon filler can leave the joint weaker than the pipe at temperature. Keep interpass temperatures controlled, as for other high-alloy austenitics, to limit hot-cracking risk in a fully austenitic weld, and avoid long holds in the carbide-precipitation range during repair welding.

Surface Finishes

A312 requires pipe to be free of scale and contaminating iron particles, and the way that condition is reached becomes the surface finish. For TP309H, which mostly goes into hot service, the finish is usually chosen for cleanliness and inspection rather than appearance, but it still needs to be stated on the order so the mill and the receiving inspector are working to the same expectation.

  • Annealed and pickled — the standard mill finish for most sizes; matte and free of scale
  • Bright annealed — for smaller sizes where a clean, oxide-free bore is wanted; the anneal must still meet the Table 2 minimum
  • Blasted and pickled — common on heavier walls and larger diameters
  • Polished — by agreement where internal or external roughness is specified
  • Passivated — on request where the end-user specification asks for it

Inspection and Testing

Base inspection and testing for ASTM A312 TP309H combine chemistry, mechanical, and integrity checks, and the list below is the usual acceptance package. Supplementary requirements apply only when they are written on the purchase order.

  • Heat analysis — every heat against Table 1 for TP309H, including C 0.04–0.10%, Cr 22.0–24.0%, Ni 12.0–15.0%
  • Product analysis — when ordered, using A480 Table A1.1 tolerances
  • Tension test — Table 4 tensile, yield, and elongation on a lot basis (75/30 ksi minima)
  • Grain size — ASTM grain size No. 6 or coarser
  • Flattening test — or the alternative bend where permitted, typically on 5% of the lot
  • Hydrostatic or electric test — every length; manufacturer’s option unless the order fixes the method
  • Visual and dimensional check — against the ordered size and the tolerance clauses

EN 10204 3.1 is the standard certificate from SHH STEEL supply. For this H grade it reports the carbon value against the 0.04–0.10% band, the Table 5 grain-size result, and the heat-treatment lot, in addition to the Table 4 results. EN 10204 3.2 or third-party witness by SGS, Bureau Veritas, TÜV, or the buyer’s nominated agency is arranged when specified, and the inspector should be booked before final testing rather than after the pipe is packed.

Supplementary options worth considering for TP309H are summarized below; none of them applies unless the order names it.

Option Purpose
S1 product analysis Confirms chemistry on the finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E check of the as-supplied condition
S8 minimum wall Wall ordered as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

On receipt, check the stencil reads TP309H or S30909 and not just “309,” then compare the certificate against the limits above. Confirm the carbon sits inside the H band and the grain-size result is reported. Positive material identification by optical emission on a sample length is a sensible extra when several 309-family grades share the same storage area, because handheld XRF cannot resolve carbon.

Packaging and Shipping

Packaging for ASTM A312 TP309H is chosen to keep the surface free of iron contamination and the ends protected through export transit. Each length carries the A312 marking required by clause 17, normally including the manufacturer, the specification, the grade, the manufacturing type, the size, the heat number and heat-treatment lot, and the test method, and the packing list repeats those identifiers so bundles can be checked without unpacking.

  • End caps on all lengths; bevel protectors on beveled ends
  • Bundles strapped with non-metallic or covered straps to avoid contact with carbon steel
  • Wooden cases or crates for bright-annealed, polished, or thin-wall pipe
  • Moisture protection for sea freight on request
  • Packing lists that match heat numbers to bundle numbers

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe, and for ASTM A312 TP309H we quote against the edition you name rather than a generic catalogue sheet. We report the full Table 1 chemistry, the Table 4 results, and the heat-treatment evidence the grade calls for, and we match the manufacturing route and size to the enquiry instead of pushing whatever is nearest on the shelf.

  • H-grade control — carbon 0.04–0.10%, grain size No. 6 or coarser, and reheated anneal stated on the MTC
  • Straight advice when a sister grade such as TP309S or TP309Cb would actually suit the service better
  • SML, WLD, and HCW routes with EN 10204 3.1 certificates; 3.2 inspection on request
  • Dual A312/SA-312 marking only when the purchase order asks for both standards
  • Cut lengths, beveling, and project packing coordinated on confirmed orders

If you are still choosing between 309-family grades, send the design temperature, the atmosphere, whether the line is welded heavily in fabrication, and whether shutdown condensate is expected. We will answer with the grade that fits that combination rather than the one whose name is closest to the datasheet.

Supply Capability

SHH STEEL can supply ASTM A312 TP309H / UNS S30909 stainless steel pipe to the edition and manufacturing type named on your enquiry. The table summarizes the routes, sizes, finishes, and documents we regularly quote for this grade, and it is a capability statement rather than a promise that every combination is in stock today.

Item SHH STEEL capability for TP309H
Standard ASTM A312 / A312M TP309H / UNS S30909
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension (75/30 ksi), flattening/bend, hydro or NDE per length; Table 5 grain size No. 6 or coarser; S1/S5/S7/S8/S9 on order
Documents EN 10204 3.1; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes. The representative range for TP309H is set out in the Dimensions section: NPS 1/2–24 with Sch 10S, 40S, and 80S as typical, plus special OD × wall on enquiry. Selected common sizes may be available from stock or recent heats, while heavy-wall seamless, unusual schedules, and special cut lengths are normally mill-order. We do not invent stock lists or tonnage claims, so ask for a live check against your size list.

A good enquiry for this grade states the A312 edition, TP309H (UNS S30909), the manufacturing type, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirement. With that information we can line up a mill slot or a stock allocation against your need date, and combining project sizes into one heat helps with chemistry consistency and mill minimums.

FAQ

Is ASTM A312 the same as ASME SA-312 for TP309H?
No. ASTM A312/A312M and ASME SA-312 are two independent standards, even though the referenced editions are closely aligned on Table 1 chemistry, Table 4 tensile values, and most testing language for TP309H. If the piping is built to the ASME Code, name both standards on the purchase order and ask for dual marking; otherwise order to ASTM A312 alone and do not treat the titles as synonyms.
What is the UNS number for ASTM A312 TP309H?
The UNS number is UNS S30909. It identifies the same chemistry across product forms, so plate to ASTM A240 and pipe to ASTM A312 can share it, but the pipe still has to be ordered and certified to A312. Put both the TP designation and the UNS number on the order and check that both appear on the certificate and the stencil.
What chemical composition defines TP309H pipe?
Table 1 of ASTM A312 sets C 0.04–0.10%, Cr 22.0–24.0%, Ni 12.0–15.0%, with Mn ≤2.00%, Si ≤1.00%, P ≤0.045% and S ≤0.030%. Those limits apply to the heat analysis; product analysis, when ordered, uses the A480 Table A1.1 tolerances, which widen individual readings slightly but never replace the heat requirement.
What are the tensile requirements for ASTM A312 TP309H?
Table 4 requires 75 ksi [515 MPa] minimum tensile strength and 30 ksi [205 MPa] minimum yield strength, with elongation of 35% longitudinal and 25% transverse. These are the same floors as the other 309-family grades. There is no hardness maximum in Table 4, so any hardness limit for bending or expanding must be written on the order.
TP309H vs TP309S — what is the difference?
TP309H carries a carbon band of 0.04–0.10%, ASTM grain size No. 6 or coarser, and a clause 6.2 reheated anneal; TP309S simply caps carbon at 0.08% with no grain-size rule. The tensile floor is the same 75/30 ksi, so the difference is in elevated-temperature behaviour, and an S-grade certificate cannot be relabelled as H after the fact.
TP309H vs TP310H — which grade suits higher temperature?
The 310 family, with chromium 24.0–26.0% and nickel 19.0–22.0%, has more oxidation and scaling margin than the 309 family at 22.0–24.0% chromium, so TP310H is the more conservative choice for the hottest sections. The step between families is mainly about oxidation margin, not room-temperature strength, because both share the 75/30 ksi Table 4 floor. Choose by the actual atmosphere and metal temperature, and remember that the richer grade costs more and can be harder to source in special sizes.
What heat treatment applies to ASTM A312 TP309H pipe?
Table 2 lists TP309H at 1900 °F [1040 °C] minimum followed by rapid cooling. Because it is an H grade, clause 6.2 requires the pipe to be reheated to that temperature before quenching, so direct quench after hot forming is not accepted, and the heat-treatment lot must be marked on each length.
Seamless vs welded TP309H pipe — which is better?
Neither is better in general. Seamless suits heavy walls, high pressure, and line classes that exclude welded pipe, while welded pipe is economical on larger diameters and thinner walls and is common in furnace ducting. Both must meet the same Table 1 chemistry and Table 4 tensile values, and the choice should follow the design code and the inspection plan.
What filler metal is used to weld TP309H pipe?
Table 6 of ASTM A312 shows no AWS filler classification for TP309H, so the filler is chosen by agreement and recorded on the welding procedure specification. A matching 309-type filler is typical, with a richer filler for dissimilar joints, and the procedure should be qualified for the service temperature rather than copied from a room-temperature job.
Hydrostatic test vs NDE — which do I get on TP309H pipe?
Every length receives either a hydrostatic test or a nondestructive electric test, and the manufacturer chooses unless the purchase order specifies one. If your inspection plan depends on a particular method, write it on the order. Pipe NPS 10 and larger may ship marked “NH” only when the purchaser accepts a system test instead of the hydrotest.
Does TP309H require grain-size control?
Yes. Table 5 requires ASTM grain size No. 6 or coarser for TP309H, and the result should be reported on the certificate together with the heat-treatment lot. The coarser grain supports creep strength at elevated temperature, which is why H grades carry this requirement and the S and plain Cb grades do not.
What sizes of TP309H pipe can SHH STEEL supply?
SHH STEEL quotes TP309H across ASME B36.19 sizes, typically NPS 1/2–24 in Sch 10S, 40S, and 80S, plus special OD and wall by agreement. Some common sizes may come from stock or recent heats, while heavy-wall seamless and unusual sizes are mill-order. Send your size list for a live availability check.

Conclusion

ASTM A312 TP309H / UNS S30909 is the controlled-carbon, grain-size-controlled high-temperature member of the 23Cr–13Ni family, with C 0.04–0.10%, Cr 22.0–24.0%, Ni 12.0–15.0%, a 75/30 ksi Table 4 floor with 35% L / 25% T elongation, and a solution anneal at 1900 °F [1040 °C] minimum with clause 6.2 reheat and grain size No. 6 or coarser. It is ordered for heat, not for general corrosion, and it is not a drop-in for A312 TP309S. Put the manufacturing type, size and wall basis, finish, and the grade-specific evidence on the purchase order, then review the EN 10204 3.1 certificate before release. SHH STEEL can supply TP309H pipe to the edition you name; browse the sister grades on the A312/A312M hub, or send your size list to admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *