ASTM A312 TP321H Stainless Steel Pipe
What is ASTM A312 TP321H Stainless Steel Pipe
ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP321H / UNS S32109, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.
TP321H is the elevated-temperature version of TP321. The controlled 0.04–0.10% carbon band and the coarse-grain requirement support creep strength, while titanium still ties up carbon so grain-boundary sensitization after welding is reduced. Table 1 sets C 0.04–0.10%, N ≤0.10% and Ti at least 4×(C+N) with a 0.70% ceiling, with chromium at 17.0–19.0% and nickel at 9.0–12.0%. As an H grade it carries the full A312 H package: Table 2 anneals of 2000 °F [1100 °C] cold-finished and 1925 °F [1050 °C] hot-finished, Table 5 grain size No. 7 or coarser, and the clause 6.2 reheat and lot-marking rules.
SHH STEEL can supply ASTM A312 TP321H stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP321H.
Commercial names include 321H stainless pipe, S32109 and “high-carbon 321”. Those labels only hold when the MTC shows carbon inside 0.04–0.10%, titanium against the 4×(C+N) rule, a measured grain size and the Table 2 anneal temperature actually used. A plain TP321 heat with 0.05% carbon is not TP321H just because the carbon happens to fall in the H band; without the grain size and H anneal evidence, it remains TP321.
Within the ASTM A312 series, buyers comparing TP321H usually look next at A312 TP321, A312 TP347H, A312 TP304H and A312 TP316H. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.
Manufacturing Types (SML / WLD / HCW)
ASTM A312 recognises three manufacturing routes for TP321H pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–12.0%, N ≤0.10% and Ti at least 4×(C+N) with a 0.70% ceiling, and every length must be heat treated before release. For TP321H the route also selects the Table 4 row: seamless walls over 0.375 in. use the lower 70/25 ksi line, while welded pipe stays at 75/30 ksi for every wall. Because this is an H grade, the H anneal and grain-size evidence must belong to the finished pipe, whichever route produced it.
- Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
- Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
- Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.
Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.
Chemical Composition of ASTM A312 TP321H
Two chemistry layers matter for ASTM A312 TP321H. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.
| Element | TP321H / UNS S32109 melting analysis |
|---|---|
| Carbon (C) | 0.04 – 0.10 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 17.0 – 19.0 |
| Nickel (Ni) | 9.0 – 12.0 |
| Molybdenum (Mo) | No requirement (…) |
| Titanium (Ti) | 4 × (C+N) min, 0.70 max |
| Nitrogen (N) | ≤ 0.10 |
Read the table as maxima unless a range is shown. The stabilizer rule for TP321H (Ti ≥4×(C+N), ≤0.70%) is not a fixed number; it moves with the actual chemistry of each heat. At C = 0.06% and N = 0.04%, C+N = 0.10%, so titanium must be at least 0.40%; do not apply TP321’s 5× factor to an H heat. That is why the MTC has to report the 0.04–0.10% carbon band, nitrogen and titanium on the same heat, plus the measured Table 5 grain size.
When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP321H without having to rebuild the arithmetic themselves.
| Element | Melting (Table 1) | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | 0.04 – 0.10 | 0.01 under / over | 0.03 – 0.11 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 17.0 – 19.0 | 0.20 under / over | 16.80 – 19.20 |
| Nickel (Ni) | 9.0 – 12.0 | 0.10 under / 0.15 over | 8.90 – 12.15 |
| Titanium (Ti) | 4 × (C+N) min, 0.70 max | 0.05 over on max | max ≤ 0.75 product |
| Nitrogen (N) | ≤ 0.10 | 0.01 over | ≤ 0.11 |
Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.
Mechanical Properties of ASTM A312 TP321H
Room-temperature tensile requirements for ASTM A312 TP321H come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S32109, not from this product page or from a sister grade’s strength line.
| Condition | Tensile strength, min | Yield strength, min |
|---|---|---|
| Welded pipe, all walls | 75 ksi [515 MPa] | 30 ksi [205 MPa] |
| Seamless, wall ≤ 0.375 in. [9.5 mm] | 75 ksi [515 MPa] | 30 ksi [205 MPa] |
| Seamless, wall > 0.375 in. [9.5 mm] | 70 ksi [480 MPa] | 25 ksi [170 MPa] |
| Grain size (Table 5) | ASTM No. 7 or coarser | |
Pick the row from the actual route and wall. Welded pipe stays on 75/30 ksi for every wall, but seamless pipe with walls over 0.375 in. [9.5 mm] drops to the 70/25 ksi line, and receiving inspection should check that the MTC quotes the row that matches the shipped product. In the H-grade row the heavy-wall seamless tensile is printed as 70 ksi [480 MPa], not the 485 MPa shown for TP321, so check the metric figure on A312M orders. The Table 5 grain size of ASTM No. 7 or coarser travels with the tensile results; ask for the measured number on the MTC rather than a bare “complies”.
Dimensions, Tolerances and Stock Sizes
Dimensional supply for ASTM A312 TP321H pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.
| NPS designator | Wall over | Wall under |
|---|---|---|
| 1/8 to 2-1/2 incl., all t/D | 20.0% | 12.5% |
| 3 to 18 incl., t/D up to 5% | 22.5% | 12.5% |
| 3 to 18 incl., t/D over 5% | 15.0% | 12.5% |
| 20 and larger, welded, all t/D | 17.5% | 12.5% |
| 20 and larger, seamless, t/D up to 5% | 22.5% | 12.5% |
| 20 and larger, seamless, t/D over 5% | 15.0% | 12.5% |
Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.
- Lengths — single random, double random or cut-to-length as ordered
- Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
- Jointers — not permitted unless the purchase order allows them
Stock / Available sizes. SHH STEEL quotes TP321H against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP321H is held in selected sizes; heavy-wall seamless is normally mill-order against a qualified H heat. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.
| Representative size (ASME B36.19) | Example OD × wall | Typical schedules / notes |
|---|---|---|
| NPS 1/2 | 21.3 mm × 2.77 mm (Sch 40S) | Sch 10S / 40S / 80S; instrument and small-bore take-offs |
| NPS 2 | 60.3 mm × 3.91 mm (Sch 40S) | Sch 10S / 40S / 80S; common process branch size |
| NPS 4 | 114.3 mm × 6.02 mm (Sch 40S) | Sch 10S / 40S / 80S; frequent stock and mill enquiry size |
| NPS 6 | 168.3 mm × 7.11 mm (Sch 40S) | Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry |
| NPS 8 – 12 | 219.1 mm × 8.18 mm (NPS 8 Sch 40S) | Sch 10S / 40S; route and wall decide stock vs mill-order |
| NPS 14 – 24 | Per B36.19 for the ordered schedule | Sch 10S / 40S; usually mill-order, often welded |
| Special OD × wall | By agreement | State OD, wall (nominal or minimum) and length practice |
Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.
Equivalent Grades
Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP321H, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.
| Designation | Notes |
|---|---|
| ASTM A312 TP321H / UNS S32109 | Governing product specification on this page |
| ASME SA-312 TP321H / S32109 | Separate Code Book standard; dual-mark only when the PO names both |
| TP321 / UNS S32100 | Standard-carbon sister; C ≤0.08%, Ti 5×(C+N), default 1900 °F anneal |
| TP347H / UNS S34709 | Nb-stabilized H grade; Nb ≥8×C, Ni up to 13.0% |
We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.
Heat Treatment and Delivery Condition
All A312 pipe is furnished heat treated. For TP321H, Table 2 sets 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. Those temperatures are above the 1900 °F default used for the standard-carbon sister because the anneal also has to develop the coarse grain that Table 5 requires, and the clause 6.2 reheat rules and lot marking apply whenever pipe is reheated after the qualifying anneal.
Supplementary requirement S6, a stabilization heat treatment at an agreed temperature below the solution anneal, applies only when the purchase order specifies it; if it is ordered, agree the temperature at enquiry and confirm it on the MTC. Delivery is normally solution annealed and pickled, and the certificate should record the anneal temperature, the cooling method and whether the pipe was cold- or hot-finished, since that decides which Table 2 minimum applies.
Corrosion Resistance
ASTM A312 contains no corrosion table, so this is engineering commentary. TP321H shares the Cr, Ni and Ti stabilization of TP321, so its resistance to intergranular attack after welding and its oxidation behaviour in hot gas are broadly similar. What changes is the purpose: the H package exists for creep and stress-rupture strength in superheater, reheater and hot hydrocarbon lines, not for better aqueous corrosion resistance.
Do not substitute TP321 or a low-carbon grade into a TP321H line on the argument that lower carbon “corrodes better”. That removes the carbon floor and grain-size control the hot design relied on. Where polythionic-acid stress corrosion during shutdowns is a concern, owners sometimes add S6 stabilization; that is a licensor decision and should be written on the order rather than assumed.
Applications of ASTM A312 TP321H Pipe
Applications for ASTM A312 TP321H follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S32109 at the design temperature before final wall selection.
| Application area | Typical use of TP321H pipe | Selection note |
|---|---|---|
| Superheater and reheater piping | Elevated-temperature steam lines where creep strength is in the design basis | Confirm grain size and Table 2 anneal on the MTC |
| Refinery heater and hydroprocessing lines | Hot hydrocarbon service with welded joints | Check allowable stresses for UNS S32109 at design temperature |
| Petrochemical furnace outlets | Transfer and header piping in the creep range | Agree S6 at enquiry if the licensor requires it |
| Code piping packages | Dual A312/SA-312 projects with heat traceability | Name edition, route, and UNS on the enquiry |
Plants that already run TP321 or TP347H sometimes buy TP321H in the same package, which is sensible only when each line’s datasheet allows the grade being shipped to it. For creep-range lines, confirm the allowable stresses for UNS S32109 at design temperature, and agree any S6 requirement at enquiry so the mill can plan the extra furnace step.
Weldability
For filler selection, Table 6 maps TP321H to the ER321 family; whether the ER347 option shown for TP321 carries over to the H grade is not clearly confirmed in our extract, so agree it on the WPS if you want to use it. Qualify the WPS and PQR on actual TP321H base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.
TP321H welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. For H-grade service, match the consumable’s carbon to the creep design and avoid low-carbon wire that would weaken the joint at temperature. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.
Surface Finishes
Surface condition for ASTM A312 TP321H pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.
- Annealed and pickled — the usual delivery for process piping after solution treatment
- Bright annealed — by agreement for selected sizes and routes
- Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
- Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed
Inspection and Testing
The base acceptance package for ASTM A312 TP321H pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show the 0.04–0.10% carbon band, nitrogen and titanium on the same heat, plus the measured Table 5 grain size, on the same line items as the tensile results.
Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.
| Option | Purpose |
|---|---|
| S1 product analysis | Confirms chemistry on finished pipe |
| S5 radiography | Weld integrity on WLD pipe |
| S6 stabilization | Stabilizing heat treatment at an agreed temperature |
| S7 intergranular corrosion | A262 Practice E after sensitizing treatment |
| S8 minimum wall | Wall read as minimum rather than nominal |
| S9 weld decay | Compares weld and base-metal loss rates |
EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.
Packaging and Shipping
Export and domestic shipments of ASTM A312 TP321H pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP321H / UNS S32109, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.
- Ends capped or bevel-protected as ordered
- Bundles strapped with protected contact points to limit iron pickup
- Waterproof wrapping for ocean freight when specified
- Packing list with heat numbers, sizes and certificate references
We keep TP321H physically segregated from TP321-family and TP347-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.
Why Choose SHH STEEL
SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP321H we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.
- Grade control — the 0.04–0.10% carbon band, nitrogen and titanium on the same heat, plus the measured Table 5 grain size stated on the MTC
- Honest sister-grade advice when TP321 or TP347H would fit the service better
- Filler guidance for WPS planning: ER321 family (ER347 option for the H grade by agreement)
- SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
- Dual A312/SA-312 marking only when the purchase order asks for both
- Cut lengths, bevelling and project marking coordinated on confirmed orders
If you are still choosing between TP321H and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.
Supply Capability
SHH STEEL can supply ASTM A312 TP321H stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.
| Item | SHH STEEL capability for TP321H |
|---|---|
| Standard | ASTM A312 / A312M TP321H / UNS S32109 |
| Manufacturing types | SML, WLD, HCW |
| Size | NPS 1/8 and up per ASME B36.19; special OD/wall by agreement |
| Schedules | 5S, 10S, 40S, 80S and non-standard walls |
| Length | SRL, DRL or cut-to-length |
| Finish | Annealed and pickled; bright annealed or polished by agreement |
| Filler guidance | ER321 family (ER347 option for the H grade by agreement) |
| Testing | Tension (75/30 ksi (70/25 ksi for seamless walls over 0.375 in.)), Table 5 grain size No. 7 or coarser, flattening/bend, hydro or NDE per length; supplementary tests on order |
| Documents | EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes. Representative stock and mill-enquiry sizes for TP321H are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.
Enquiries should state the A312 edition, TP321H (UNS S32109), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.
FAQ
-
Is ASTM A312 TP321H the same as ASME SA-312 TP321H?
- They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP321H chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
-
What is the chemical composition of ASTM A312 TP321H pipe?
- Table 1 sets C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–12.0%, N ≤0.10% and Ti at least 4×(C+N) with a 0.70% ceiling. These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
-
What are the mechanical properties of ASTM A312 TP321H?
- Table 4 requires 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield for welded pipe and seamless walls up to 0.375 in. [9.5 mm], and 70 ksi [480 MPa] / 25 ksi [170 MPa] for seamless walls over 0.375 in., with grain size ASTM No. 7 or coarser. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S32109. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
-
What is the difference between ASTM A312 TP321H and TP321?
- TP321H uses a 0.04–0.10% carbon band where TP321 only caps carbon at 0.08%, and its titanium rule is 4×(C+N) minimum instead of 5×(C+N). TP321H must also meet Table 5 grain size No. 7 or coarser and the Table 2 anneals of 2000 °F cold-finished and 1925 °F hot-finished. Both share the route- and wall-dependent 75/30 or 70/25 ksi Table 4 rows.
-
Should I choose ASTM A312 TP321H or TP347H for high-temperature piping?
- Both are stabilized H grades with the same Table 2 anneal and Table 5 grain size. TP321H uses titanium at 4×(C+N) with nickel 9.0–12.0%; TP347H uses niobium at 8×C with nickel up to 13.0% and keeps a single 75/30 ksi tensile row regardless of wall. Many designers prefer TP347H for heavy welding, but code allowables and plant experience should decide.
-
What heat treatment does ASTM A312 TP321H require?
- TP321H is supplied solution annealed at 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. As an H grade it must also meet Table 5 grain size No. 7 or coarser and the clause 6.2 reheat and lot-marking rules, and S6 stabilization is added only when ordered.
-
Which filler metal is used to weld ASTM A312 TP321H pipe?
- Table 6 maps TP321H to the ER321 family; whether the ER347 option shown for TP321 carries over to the H grade is not clearly confirmed in our extract, so agree it on the WPS if you want to use it. Qualify the procedure on actual TP321H base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
-
What sizes of ASTM A312 TP321H pipe can SHH STEEL supply?
- We quote TP321H in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
-
Why is the heavy-wall seamless tensile for TP321H shown as 480 MPa?
- In the Table 4 row for the H grade, seamless walls over 0.375 in. are listed at 70 ksi [480 MPa] tensile and 25 ksi [170 MPa] yield, whereas the TP321 row prints 485 MPa for the same 70 ksi. The ksi values match; the metric conversion differs. Check which figure the MTC uses, especially on metric A312M orders, so acceptance is done against the correct row.
-
Does TP321H require a grain-size test?
- Yes. Table 5 requires an average grain size of ASTM No. 7 or coarser for TP321H, and it is part of what makes the pipe an elevated-temperature material rather than a TP321 heat with higher carbon. Ask for the measured grain-size number on the MTC instead of a bare “complies” note, and make sure it is traceable to the same heat-treatment lot as the tensile results.
-
What certificates come with ASTM A312 TP321H pipe from SHH STEEL?
- Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP321H it should show the 0.04–0.10% carbon band, nitrogen and titanium on the same heat, plus the measured Table 5 grain size. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.
Conclusion
ASTM A312 TP321H / UNS S32109 is defined by C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–12.0%, N ≤0.10% and Ti at least 4×(C+N) with a 0.70% ceiling, a Table 4 floor of 75/30 ksi (70/25 ksi for seamless walls over 0.375 in.) with grain size No. 7 or coarser, and 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.