ASTM A312 UNS S20400 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S20400 Stainless Steel Pipe

ASTM A312 UNS S20400 high-manganese nitrogen-strengthened stainless steel pipe in SML, WLD and HCW, with C ≤0.030%, Mn 7.0–9.0%, Ni 1.50–3.00%, N 0.15–0.30%, a 95/48 ksi Table 4 floor and ER209 filler, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
UNS S20400
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 UNS S20400 Stainless Steel Pipe

A312/A312M is the ASTM product specification for seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as an ASTM standard, and this page is written against it. UNS S20400 is one of the less common rows in its Table 1, and that is exactly why buyers ask us to spell out what the specification actually fixes for this alloy and what is left to agreement between purchaser and mill.

UNS S20400 is one of the A312 rows that carries no TP designation at all; Table 1 lists it by UNS number only. It is a low-carbon chromium-manganese-nitrogen alloy with 15.0–17.0% chromium, 7.0–9.0% manganese, only 1.50–3.00% nickel, and 0.15–0.30% nitrogen, and the nitrogen gives it a Table 4 floor of 95 ksi tensile and 48 ksi yield. It appeals to buyers who want higher strength than TP304L with a low carbon ceiling of 0.030% and very low nickel.

SHH STEEL can supply ASTM A312 UNS S20400 pipe as seamless (SML), welded (WLD), or heavily cold-worked (HCW) product, in ASME B36.19 stainless schedules or special OD and wall by agreement, with EN 10204 3.1 mill test certificates that report the full Table 1 heat analysis, the Table 4 tension results, and the heat-treatment record. Where a purchase order also asks for ASME SA-312 marking, dual marking can be offered on heats that qualify under both documents, but the ASTM grade remains the one this page describes.

Because there is no TP name, the order should simply read ASTM A312 UNS S20400, and the certificate should do the same. Enquiries sometimes arrive with a 200-series trade name or a plate grade from another specification, and those have to be translated back to this Table 1 row, because several 200-series alloys differ from S20400 in nickel, manganese, or nitrogen.

If UNS S20400 turns out not to be the right fit, the closest sister pages in the same ASTM series are A312 TPXM-11, A312 TPXM-29, A312 TPXM-10, A312 TP201LN, and A312 TP304L. All A312 grades are collected on the A312/A312M hub, so a short list can be compared against one standard before the enquiry goes out.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 allows three manufacturing routes for UNS S20400 pipe, and the route is a purchase-order decision rather than a property of the grade. Whichever route is chosen, the heat must still meet the same Table 1 limits (C ≤0.030%, Mn 7.0–9.0%, Cr 15.0–17.0%, Ni 1.50–3.00%, and N 0.15–0.30%), the same Table 4 tension floor, and the same 1900 °F [1040 °C] minimum solution anneal (Table 2 default) with rapid cooling heat-treatment requirement before any length is released.

  • Seamless (SML) pierced and hot or cold finished, chosen for heavy wall, high pressure, or owner specifications that exclude a weld seam
  • Welded (WLD) formed from flat-rolled product and welded without filler or with filler where the edition allows, economical in thinner walls and larger diameters
  • Heavily cold-worked (HCW) welded pipe given at least 35% cold reduction of the weld and base metal before the final anneal, which refines the weld structure toward seamless behaviour

S20400 is mostly produced as welded pipe from strip in thinner walls, with seamless available by campaign, so the accepted route has a large effect on lead time for this grade. Tell us which route your design code or client specification accepts, because a quotation that leaves the route open forces the mill to choose and can create disputes at receiving inspection.

Chemical Composition of ASTM A312 UNS S20400

The melting analysis in Table 1 is what the heat must meet when it is cast, and it is the first table a reviewer should compare against the mill certificate. For UNS S20400 the defining limits are C ≤0.030%, Mn 7.0–9.0%, Cr 15.0–17.0%, Ni 1.50–3.00%, and N 0.15–0.30%. The table below reproduces the Table 1 row as published, with elements carrying no requirement shown as such rather than filled with invented values.

Element UNS S20400 melting analysis
Carbon (C) ≤ 0.030
Manganese (Mn) 7.0 – 9.0
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 15.0 – 17.0
Nickel (Ni) 1.50 – 3.00
Nitrogen (N) 0.15 – 0.30
Molybdenum (Mo) … (no requirement)
Copper (Cu) … (no requirement)

Nickel at 1.50–3.00% is the line that sets S20400 apart from every 300-series grade, and manganese at 7.0–9.0% with nitrogen at 0.15–0.30% replaces it as the austenite stabilizer. The carbon ceiling of 0.030% is lower than TP304L, which is good news for welded service. Molybdenum and copper carry no requirement.

Product analysis is a separate check made on the finished pipe, and ASTM A312 refers it to the permitted variations in ASTM A480 Table A1.1. The second table adds those tolerances to the melt limits so you can see the band that a check analysis on the pipe is allowed to fall within when Supplementary Requirement S1 or an owner check is ordered.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.030 0.005 over ≤ 0.035
Manganese (Mn) 7.0 – 9.0 0.06 under / over 6.94 – 9.06
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 15.0 – 17.0 0.20 under / over 14.80 – 17.20
Nickel (Ni) 1.50 – 3.00 0.07 under / over 1.43 – 3.07
Nitrogen (N) 0.15 – 0.30 0.01 under / 0.03 over 0.14 – 0.33

Read the product limits as acceptance bounds for a check analysis only. A heat that sits outside the Table 1 melt range is non-conforming even if a later product analysis lands inside the widened band, so the certificate should always show the ladle analysis first.

Mechanical Properties of ASTM A312 UNS S20400

Table 4 sets the room-temperature tension requirements for UNS S20400: 95 ksi [635 MPa] tensile strength and 48 ksi [330 MPa] yield strength minimum, with elongation of 35% longitudinal / 25% transverse minimum. The table below shows those values in the form used on the specification, and the mill certificate should report actual results against each line.

Property UNS S20400 requirement (Table 4)
Tensile strength, min 95 ksi [635 MPa]
Yield strength (0.2% offset), min 48 ksi [330 MPa]
Elongation in 2 in. or 50 mm (or 4D) 35% longitudinal / 25% transverse, min

Table 4 prints 635 MPa as the metric tensile value for this UNS, and that published figure is used here rather than a converted 655 MPa. The 48 ksi yield is more than twice the 25 ksi of TP304L, which is what allows a lighter wall where the governing code lists S20400, and it means filler matching cannot be an afterthought.

No hardness maximum is set for this grade in Table 4, so a hardness figure on a certificate is information rather than an acceptance criterion unless your order adds one. If a project specification imposes hardness or impact testing, write it on the purchase order so the mill can plan the test pieces before the pipe is cut.

Dimensions, Tolerances and Stock Sizes

Dimensions for ASTM A312 UNS S20400 pipe are normally ordered by NPS and schedule from ASME B36.19, or by outside diameter and wall where the design calls for a non-standard size. Outside-diameter tolerance and wall tolerance come from the specification itself, and wall is read as nominal unless Supplementary Requirement S8 asks for minimum wall. The permitted variations in wall thickness from Table 3 are shown below by NPS band and wall-to-diameter ratio.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

In practice the under-tolerance of 12.5% is the figure that matters for pressure design, because the designer has already sized the nominal wall with that allowance in mind. The over-tolerance varies with NPS and the wall-to-diameter ratio, which matters more for fit-up and weld preparation than for strength. For UNS S20400, whose higher strength or special chemistry often justifies a lighter or more closely engineered wall, confirm whether your calculation assumed nominal or minimum wall before the order is placed.

Stock / Available sizes. The table below shows the representative size band we quote for ASTM A312 UNS S20400, with example OD × wall combinations taken from B36.19 schedules. It is a supply and stock-enquiry range rather than a promise that every size sits on the floor today: for S20400 welded light-wall sizes in Sch 10S and 40S are the most likely to be available from existing material, while seamless and heavy wall are mill orders. Special OD, special wall, and cut lengths are always handled on enquiry.

Representative size Example OD × wall Typical schedules / notes
NPS 1/2 – 2 21.34 × 2.77 mm (NPS 1/2 Sch 40S); 60.33 × 3.91 mm (NPS 2 Sch 40S) Sch 10S / 40S / 80S; small-bore process and instrument take-offs
NPS 2-1/2 – 6 88.90 × 5.49 mm (NPS 3 Sch 40S); 168.28 × 3.40 mm (NPS 6 Sch 10S) Sch 10S / 40S / 80S; the most frequent enquiry band
NPS 8 – 12 219.08 × 8.18 mm (NPS 8 Sch 40S); 323.85 × 4.57 mm (NPS 12 Sch 10S) Sch 10S / 40S; confirm SML or WLD route on enquiry
NPS 14 – 24 406.40 × 4.78 mm (NPS 16 Sch 10S); 609.60 × 9.53 mm (NPS 24 Sch 40S) Sch 10S / 40S; usually mill-order, mostly welded
Special OD × wall Any OD and wall the mill can qualify On enquiry: state OD, nominal or minimum wall, and length practice

Read the example sizes as orientation for writing the enquiry, not as a price list. When you send a size list we check live availability line by line, separate what can ship from existing material from what needs a mill slot, and give the lead time for each group so the purchase order can be split if the schedule demands it.

Equivalent Grades

Buyers often arrive with a trade name, a plate designation, or a European number rather than the A312 row. The table below maps the names we see on enquiries for UNS S20400, but only the ASTM A312 grade and UNS number are contractual on this page; everything else is a cross-reference that needs checking against its own standard.

Designation Notes
ASTM A312 UNS S20400 Governing grade on this page (no TP name)
ASME SA-312 UNS S20400 Separate Code standard; dual mark only when the order names both
200-series trade names Confirm the full Table 1 row; other 200-series alloys differ
AWS A5.9 ER209 Filler listed for S20400 in Table 6
EN / JIS No one-to-one equivalent asserted

The ASME SA-312 row is listed because some Code projects require it, not because it is a synonym. ASME SA-312 is a separate standard adopted into the Boiler and Pressure Vessel Code, and the SA312 UNS S20400 page covers that document on its own terms. When both marks are wanted, the order should name both specifications and their editions so the certificate can state compliance with each.

Heat Treatment and Delivery Condition

S20400 has no individual row in Table 2, so it falls under the default for all grades not individually listed: solution anneal at 1900 °F [1040 °C] minimum, followed by water quenching or another rapid cool fast enough to prevent harmful carbide reprecipitation. Seamless pipe may be quenched directly after hot forming if the finishing temperature is not below that minimum. HCW product is cold reduced before the final anneal, so cold work is never the delivered condition.

Delivery condition for UNS S20400 is solution annealed, then descaled by pickling or by blasting and pickling, straightened, and cut to the ordered length practice. HCW pipe receives its cold reduction before the final anneal, so cold work is never the delivered condition. Ask for the actual annealing temperature and cooling method to be recorded on the certificate, because a reviewer cannot otherwise confirm the Table 2 requirement from the document alone.

Corrosion Resistance

ASTM A312 contains no corrosion table, so the following is engineering commentary rather than a specification requirement. With 15–17% chromium, S20400 has lower chromium than the 304 family, so its general corrosion resistance is somewhat below TP304L in aggressive waters, even though nitrogen helps pitting resistance. It is best suited to atmospheric, fresh-water, food-contact, and mildly corrosive service rather than chloride-bearing process water.

The 0.030% carbon ceiling is a genuine advantage after welding, because chromium-carbide sensitization in the heat-affected zone is unlikely, and S7 testing can document that when needed. Chloride stress corrosion cracking at elevated temperature remains a risk, and warm chloride-bearing water should be reviewed before the grade is chosen.

Applications of ASTM A312 UNS S20400 Pipe

Applications for ASTM A312 UNS S20400 pipe focus on strength and low nickel in moderately corrosive service. The table below gives the typical uses we see, each subject to code confirmation for this UNS number.

Application area Typical use of S20400 pipe Selection note
Utility and process piping Water, air, mild chemical transfer lines ordered to A312 Confirm fluid compatibility with S20400 chemistry
Structural / architectural Handrail, support, and decorative pipe ordered as A312 product 48 ksi min yield can help section design vs TP304
Transportation / OEM Frames and piping kits converting to A312 documentation Dual SA312/A312 marking often requested; mark UNS S20400 clearly
General corrosive service Mild to moderate environments without heavy chlorides Prefer TP316/TP316L if chlorides dominate
High-strength lean-nickel service Where 95/48 ksi Table 4 floors are specified with S20400 chemistry Do not substitute TP201 or TP201LN without engineering review
Cost-sensitive austenitic piping Where lean Ni bill of material is accepted by the end-user Fitness for service first; nickel savings second

Treat the table as a starting point for discussion with the process licensor or corrosion engineer, not as an approval. Code allowable stresses, temperature limits, and any owner material lists decide whether UNS S20400 is acceptable on a given line, and those checks should be made before the pipe is ordered rather than after it arrives.

Weldability

S20400 welds by GTAW, GMAW, SMAW, and orbital processes with normal austenitic practice: clean joints, controlled heat input and interpass temperature, and back-purged roots, with procedures qualified on the actual high-manganese, lean-nickel chemistry. Table 6 lists ER209 (UNS S20980 / W32240) as the filler for S20400 where mill seam repairs use filler, and ER209 is also the usual matching consumable for field girth welds. ER308 is not the Table 6 filler and may undermatch strength.

Qualify the procedure on UNS S20400 itself rather than on a convenient 304 coupon, because the qualification has to demonstrate the strength and soundness of this chemistry. Clean joint preparation, controlled heat input and interpass temperature, and a back-purged root are the normal baseline; the certificate for any WLD pipe should also state whether filler metal was used in the longitudinal seam.

Surface Finishes

Surface condition for ASTM A312 UNS S20400 pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, residual scale, embedded free iron, and chloride contamination from handling can matter as much as the nominal finish name, and they are far easier to prevent at the mill than to correct on site.

  • Annealed and pickled the standard delivery after solution treatment for process piping
  • Blasted and pickled when heavier scale needs mechanical help before chemical descaling
  • Bright annealed by agreement, generally on smaller sizes where the furnace atmosphere can be controlled
  • Passivated or polished by agreement, with the method and acceptance criteria written on the order

For UNS S20400, the high manganese content gives a slightly darker pickled finish than 304L; this is cosmetic, but a thorough final pickle is important because the lower chromium leaves less margin against surface contamination. If the line will be inspected for surface iron, specify the test method at the enquiry stage so that the packing and handling plan supports it.

Inspection and Testing

The base acceptance package for ASTM A312 UNS S20400 pipe combines heat analysis, tension testing, the flattening or bend test that applies to the manufacturing type, and a hydrostatic or non-destructive electric test on every length. Visual and dimensional inspection confirm the size and surface before marking. For S20400 the lines to check first are nickel, manganese, nitrogen, and the 48 ksi yield, because those values are what distinguish it from other 200-series alloys that can look similar on a quick review.

Supplementary requirements are optional until they are written on the order. The options buyers request most often for this grade are summarized below, and each one adds test time that should be allowed for in the delivery schedule.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Third-party inspection, witness points, and EN 10204 3.2 certification are available when the order names the inspection agency. Agree the hold points before production starts, because witnessing a hydrotest or a tension test after the fact is not possible.

Packaging and Shipping

ASTM A312 UNS S20400 pipe is packed for handling and for ocean or land transport. Each length is marked with ASTM A312, the grade UNS S20400, the manufacturing type, size, heat number, and the test method used, with SA-312 added only when the order asks for dual marking. Bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.

  • End caps or bevel protectors fitted as ordered
  • Bundles strapped with protected contact points to limit iron pick-up
  • Wooden cases or seaworthy bundles for export, with moisture protection for sea freight
  • Small-bore or polished pipe cased separately where damage risk is higher

Stainless pipe should not be stored or lifted in contact with carbon steel, and for a specialty grade such as UNS S20400 it is worth keeping the material segregated by heat on arrival, since mixing it with common 304 stock is the most frequent cause of misuse on site.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe, and for a specialty grade such as ASTM A312 UNS S20400 we quote against the edition you name rather than a generic catalogue sheet. We report the full Table 1 heat analysis, the Table 4 tension results, and the heat-treatment record, and we tell you early when a size or route is a mill order instead of letting the lead time surprise you.

  • Clear handling of UNS-only A312 rows, so the order, stencil, and certificate all carry the same designation
  • Clear advice on sister grades under ASTM A312, so UNS S20400 is not confused with a commoner alloy that looks similar on paper
  • Honest separation of specification requirements from producer or market guidance in every document we send
  • EN 10204 3.1 certificates as standard, with third-party inspection and 3.2 certification on request

The aim is a delivery that clears receiving inspection on the first review. That means the certificate, the stencil, and the purchase order all say the same thing about grade, UNS number, manufacturing type, size, and heat treatment, and that any agreed variation is written down before the pipe is made.

Supply Capability

SHH STEEL can supply ASTM A312 UNS S20400 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade, and each line can be narrowed to your project specification.

Item SHH STEEL capability for UNS S20400
Standard ASTM A312 / A312M, UNS S20400
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD and wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length Single random, double random, or cut to length
Heat treatment 1900 °F [1040 °C] minimum solution anneal (Table 2 default) with rapid cooling
Filler guidance ER209 (S20980 / W32240) per Table 6
Testing Tension (95/48 ksi), flattening or bend, hydrostatic or electric test per length; S1, S5, S7, S8, S9 on order
Documents EN 10204 3.1 with full Table 1 analysis; 3.2 and third-party inspection on request
Trade terms FOB, CFR, CIF, EXW and other agreed Incoterms

Stock / Available sizes. The representative band for UNS S20400 is NPS 1/2 to 24 in Sch 10S, 40S, and 80S as listed under Dimensions. Selected common OD × wall combinations may be available from existing material, while heavy-wall seamless, unusual schedules, and special cut lengths are normally mill orders. We do not publish stock part numbers or tonnage claims for this grade; ask for a live check against your size list instead.

Enquiries move fastest when they state the A312 edition, UNS S20400, the manufacturing type, NPS or OD × wall (and whether the wall is nominal or minimum), length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirements. Dual SA-312 marking, bevelled ends, and cut lengths are available on confirmed orders when the order says so.

FAQ

Is ASTM A312 UNS S20400 the same as ASME SA-312 UNS S20400?
They are two independent standards. ASTM A312/A312M is the ASTM product specification, and ASME SA-312 is the separate document adopted into the Boiler and Pressure Vessel Code. The technical rows for UNS S20400 are closely aligned in current editions, but a pipe is only certified to the document named on the order, so when both are needed the purchase order should list both specifications and editions and the certificate should state compliance with each.
What is the UNS number for ASTM A312 UNS S20400?
This grade has no TP designation in Table 1; it is listed and ordered simply as UNS S20400. The UNS number should appear on the mill certificate and on the stencil next to the ASTM A312 mark, because a trade name alone makes it hard for receiving inspection to tie the chemistry on the certificate to the pipe in the rack.
What are the tensile and yield requirements for ASTM A312 UNS S20400 pipe?
Table 4 requires 95 ksi [635 MPa] tensile strength and 48 ksi [330 MPa] yield strength minimum, with elongation of 35% longitudinal / 25% transverse minimum. These are room-temperature minimums for acceptance only; design allowables at temperature come from the applicable piping code, and they should be checked there before a wall thickness is fixed.
What heat treatment does ASTM A312 UNS S20400 pipe receive?
S20400 is not individually listed in Table 2, so the default applies: solution anneal at 1900 °F [1040 °C] minimum, then water quench or rapid cool. The delivered condition is solution annealed and descaled, and the certificate should record the actual annealing temperature and the cooling method so a reviewer can confirm the requirement without asking the mill.
Which filler metal is used to weld ASTM A312 UNS S20400?
Table 6 lists AWS A5.9 ER209 (UNS S20980 / W32240) for S20400, which matches the strength and nitrogen of the base metal; ER308 is not the listed filler and can leave the weld undermatched. Whatever is chosen should be recorded on the WPS and PQR, and the procedure should be qualified on UNS S20400 base metal so that the joint strength and soundness are demonstrated on the real chemistry.
Is ASTM A312 UNS S20400 pipe available seamless and welded?
Yes. ASTM A312 allows seamless (SML), welded (WLD), and heavily cold-worked (HCW) pipe for UNS S20400, all meeting the same chemistry, tension, and heat-treatment rules. Seamless is usual for heavy wall and high pressure, while welded is often more economical in thin walls and larger diameters; state the accepted route on the order.
What sizes of ASTM A312 UNS S20400 pipe can SHH STEEL supply?
We quote NPS 1/2 to 24 in Sch 10S, 40S, and 80S as the representative band, plus NPS 1/8 and up and special OD and wall by agreement. Some common sizes may be available from existing material, while heavy-wall seamless and unusual schedules are normally mill orders, so send a size list for a live check.
What documents come with ASTM A312 UNS S20400 pipe?
Each shipment carries an EN 10204 3.1 mill test certificate showing the A312 edition, UNS S20400, manufacturing type, heat number, the full Table 1 heat analysis, Table 4 tension results, heat treatment, and the hydrostatic or electric test. Third-party inspection and 3.2 certification can be added when the order names the agency.
Why does UNS S20400 have no TP grade name in ASTM A312?
Some alloys were added to A312 by UNS number only, and Table 1 shows an ellipsis in the grade column for S20400. That does not make it a lesser grade; it simply means the order, stencil, and certificate should read ASTM A312 UNS S20400 rather than inventing a TP name.
Is UNS S20400 stronger than TP304L?
Yes. Table 4 requires 95 ksi tensile and 48 ksi yield for S20400, against 70 ksi and 25 ksi for TP304L, while both have low carbon ceilings. The strength comes from nitrogen and manganese rather than nickel, so the design benefit only applies where the piping code lists allowable stresses for S20400.
Can UNS S20400 replace TP304 in all services?
No. Its chromium of 15–17% is lower than the 18–20% of TP304, so in aggressive or chloride-bearing water it has less corrosion margin. It is a good choice where strength and low nickel matter in mild service, but substitutions should be reviewed by a corrosion or materials engineer.

Conclusion

ASTM A312 UNS S20400 (UNS S20400) is a UNS-only, low-carbon, lean-nickel Cr-Mn-N grade with a 95/48 ksi floor, ordered when strength and low nickel matter more than maximum corrosion margin. The specification fixes C ≤0.030%, Mn 7.0–9.0%, Cr 15.0–17.0%, Ni 1.50–3.00%, and N 0.15–0.30%, a Table 4 floor of 95 ksi [635 MPa] tensile and 48 ksi [330 MPa] yield, and 1900 °F [1040 °C] minimum solution anneal (Table 2 default) with rapid cooling heat treatment, while filler selection is ER209 per Table 6. Put the manufacturing type, size and wall basis, finish, and any supplementary tests on the purchase order, and review the EN 10204 3.1 certificate against Tables 1, 2, and 4 before release. SHH STEEL can supply ASTM A312 UNS S20400 pipe to the edition you name; compare sister grades on the A312/A312M hub, or send your size list to admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X