ASTM A312 TP347 / UNS S34700 stainless steel pipe in SML, WLD and HCW, with C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 10×C with a 1.00% ceiling (footnote G), a 75/30 ksi Table 4 floor and ER347 filler guidance, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP347 / UNS S34700
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP347 Stainless Steel Pipe

ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP347 / UNS S34700, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.

TP347 is the niobium-stabilized member of the 18Cr–10Ni family. Niobium forms very stable carbides, which keeps chromium in solution next to welds and has made the grade a long-standing choice for welded service in the sensitizing temperature range. Table 1 sets C ≤0.08% and Nb at least 10×C with a 1.00% ceiling under footnote G, with chromium at 17.0–19.0% and nickel at 9.0–13.0%; molybdenum is not required, and footnote M confirms that niobium and columbium are the same element. Table 4 uses a single 75 ksi [515 MPa] / 30 ksi [205 MPa] row, and because TP347 is not an H grade the default 1900 °F [1040 °C] anneal applies.

SHH STEEL can supply ASTM A312 TP347 stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP347.

Buyers meet this grade as 347 stainless pipe, S34700 or “Cb-stabilized 18-10”; an MTC reporting “Cb” instead of “Nb” is describing the same element. The important check is arithmetic: the niobium minimum moves with each heat’s carbon. TP347, TP347H and TP347LN share the “347” label but are three different Table 1 rows, so order the exact grade and UNS rather than the family name.

Within the ASTM A312 series, buyers comparing TP347 usually look next at A312 TP347H, A312 TP347LN, A312 TP348 and A312 TP321. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 recognises three manufacturing routes for TP347 pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 10×C with a 1.00% ceiling (footnote G), and every length must be heat treated before release. For TP347 the Table 4 row is the same for every route and wall, so the route decision rests on code acceptance, size and inspection preference rather than strength.

  • Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
  • Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.

Chemical Composition of ASTM A312 TP347

Two chemistry layers matter for ASTM A312 TP347. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.

Element TP347 / UNS S34700 melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) No requirement (…)
Niobium (Nb) / Columbium (Cb) ≥ 10 × C and ≤ 1.00% (footnote G)

Read the table as maxima unless a range is shown. The stabilizer rule for TP347 (Nb ≥10×C, ≤1.00%) is not a fixed number; it moves with the actual chemistry of each heat. At C = 0.05%, niobium must be at least 0.50% and no more than 1.00%; footnote M confirms Nb and Cb are the same element. That is why the MTC has to report carbon and niobium on the same heat, so the Nb ≥10×C, ≤1.00% rule can be proven.

When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP347 without having to rebuild the arithmetic themselves.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.10 under / 0.15 over 8.90 – 13.15
Niobium (Nb) ≥ 10 × C, ≤ 1.00% 0.05 over on max max ≤ 1.05 product; min tied to C

Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.

Mechanical Properties of ASTM A312 TP347

Room-temperature tensile requirements for ASTM A312 TP347 come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S34700, not from this product page or from a sister grade’s strength line.

Property TP347 requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm (or 4D) 35% longitudinal / 25% transverse, min

TP347 uses a single row regardless of route and wall, so welded and seamless pipe are accepted against the same floor. These are minimum release values, not typical mill results, and they should not be raised or lowered by habit from a sister grade.

Dimensions, Tolerances and Stock Sizes

Dimensional supply for ASTM A312 TP347 pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.

  • Lengths — single random, double random or cut-to-length as ordered
  • Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
  • Jointers — not permitted unless the purchase order allows them

Stock / Available sizes. SHH STEEL quotes TP347 against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP347 is commonly available in the main Sch 10S/40S sizes, with heavier walls often mill-order. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.

Representative size (ASME B36.19) Example OD × wall Typical schedules / notes
NPS 1/2 21.3 mm × 2.77 mm (Sch 40S) Sch 10S / 40S / 80S; instrument and small-bore take-offs
NPS 2 60.3 mm × 3.91 mm (Sch 40S) Sch 10S / 40S / 80S; common process branch size
NPS 4 114.3 mm × 6.02 mm (Sch 40S) Sch 10S / 40S / 80S; frequent stock and mill enquiry size
NPS 6 168.3 mm × 7.11 mm (Sch 40S) Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry
NPS 8 – 12 219.1 mm × 8.18 mm (NPS 8 Sch 40S) Sch 10S / 40S; route and wall decide stock vs mill-order
NPS 14 – 24 Per B36.19 for the ordered schedule Sch 10S / 40S; usually mill-order, often welded
Special OD × wall By agreement State OD, wall (nominal or minimum) and length practice

Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.

Equivalent Grades

Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP347, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.

Designation Notes
ASTM A312 TP347 / UNS S34700 Governing product specification on this page
ASME SA-312 TP347 / S34700 Separate Code Book standard; dual-mark only when the PO names both
TP347H / UNS S34709 H grade: C 0.04–0.10%, Nb ≥8×C, grain size No. 7 or coarser
TP347LN / UNS S34751 Low-carbon nitrogen-bearing Nb grade, Nb 0.20–0.50%
TP321 / UNS S32100 Ti-stabilized sister; Ni up to 12.0%

We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.

Heat Treatment and Delivery Condition

All A312 pipe is furnished heat treated. TP347 is not an H grade, so it receives the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, since TP347 has no individual Table 2 row. There is no Table 5 grain-size mandate and no clause 6.2 reheat rule, and HCW cold reduction is completed before the final anneal so delivery remains the annealed condition. Supplementary requirement S6 adds a stabilization treatment at an agreed temperature below the solution anneal only when the purchase order invokes it.

Delivery is normally solution annealed and pickled unless the order asks for bright annealing or another finish. The MTC should record the anneal temperature and cooling method actually used, and fabricators who hot form or heavily cold work TP347 bends should re-anneal to the same practice where the governing code requires it, rather than applying a neighbouring grade’s anneal by habit.

Corrosion Resistance

ASTM A312 has no corrosion table, so this is engineering commentary. TP347 is chosen where welded joints or service in the sensitizing range would put unstabilized 18-8 at risk of intergranular attack. Niobium carbides are very stable and niobium is less prone than titanium to loss across the arc, which is why 347 chemistry is so common in heavily welded hot process lines and why ER347 is the matching filler for several stabilized grades.

Stabilization does not add pitting resistance, so chloride-driven corrosion cases still point towards molybdenum-bearing grades. Where very low carbon with nitrogen is wanted for welded aqueous service, A312 TP347LN is the specialised option, and where creep strength governs, A312 TP347H brings the H package. Intergranular corrosion tests apply only when written on the order.

Applications of ASTM A312 TP347 Pipe

Applications for ASTM A312 TP347 follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S34700 at the design temperature before final wall selection.

Application area Typical use of TP347 pipe Selection note
Welded process lines Lines exposed to the sensitizing range during welding or service Prove the stabilizer rule on the MTC
Exhaust, expansion-joint and heater piping Intermittent elevated-temperature duty without H-grade creep design Use TP347H when the design is creep-governed
Chemical and refining utility Oxidizing or mildly corrosive service specified with stabilized 18–10 chemistry Prefer Mo grades if chlorides dominate
Code piping packages Dual A312/SA-312 projects with heat traceability Name edition, route, and UNS on the enquiry

Plants that already run TP347H or TP321 sometimes buy TP347 in the same package, which is sensible only when each line’s datasheet allows the grade being shipped to it. TP347 is also a frequent choice for expansion-joint and exhaust piping that sees intermittent heat without a creep-governed design; once creep enters the calculation, move to TP347H rather than relying on TP347 carbon.

Weldability

For filler selection, Table 6 maps TP347 to ER347. Qualify the WPS and PQR on actual TP347 base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.

TP347 welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. Stabilization lowers HAZ sensitization risk compared with unstabilized 18-8, but low heat input and controlled interpass remain good practice. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.

Surface Finishes

Surface condition for ASTM A312 TP347 pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.

  • Annealed and pickled — the usual delivery for process piping after solution treatment
  • Bright annealed — by agreement for selected sizes and routes
  • Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
  • Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed

Inspection and Testing

The base acceptance package for ASTM A312 TP347 pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show carbon and niobium on the same heat, so the Nb ≥10×C, ≤1.00% rule can be proven.

Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S6 stabilization Stabilizing heat treatment at an agreed temperature
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall read as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.

Packaging and Shipping

Export and domestic shipments of ASTM A312 TP347 pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP347 / UNS S34700, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.

  • Ends capped or bevel-protected as ordered
  • Bundles strapped with protected contact points to limit iron pickup
  • Waterproof wrapping for ocean freight when specified
  • Packing list with heat numbers, sizes and certificate references

We keep TP347 physically segregated from other 347-family and TP321-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP347 we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.

  • Grade control — carbon and niobium on the same heat, so the Nb ≥10×C, ≤1.00% rule can be proven stated on the MTC
  • Honest sister-grade advice when TP347H or TP347LN would fit the service better
  • Filler guidance for WPS planning: ER347
  • SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
  • Dual A312/SA-312 marking only when the purchase order asks for both
  • Cut lengths, bevelling and project marking coordinated on confirmed orders

If you are still choosing between TP347 and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.

Supply Capability

SHH STEEL can supply ASTM A312 TP347 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.

Item SHH STEEL capability for TP347
Standard ASTM A312 / A312M TP347 / UNS S34700
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL or cut-to-length
Finish Annealed and pickled; bright annealed or polished by agreement
Filler guidance ER347
Testing Tension (75/30 ksi), flattening/bend, hydro or NDE per length; supplementary tests on order
Documents EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes. Representative stock and mill-enquiry sizes for TP347 are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.

Enquiries should state the A312 edition, TP347 (UNS S34700), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.

FAQ

Is ASTM A312 TP347 the same as ASME SA-312 TP347?
They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP347 chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
What is the chemical composition of ASTM A312 TP347 pipe?
Table 1 sets C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 10×C with a 1.00% ceiling (footnote G). These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
What are the mechanical properties of ASTM A312 TP347?
Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum with 35% longitudinal / 25% transverse elongation, on a single row regardless of route and wall. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S34700. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
What is the difference between ASTM A312 TP347 and TP347H?
TP347 caps carbon at 0.08% and needs niobium at least 10×C, with the default 1900 °F anneal and no grain-size rule. TP347H uses a 0.04–0.10% carbon band, a lower 8×C niobium multiplier with a 1.0% cap, Table 5 grain size No. 7 or coarser and Table 2 anneals of 2000 °F cold-finished or 1925 °F hot-finished. Both keep the 75/30 ksi floor.
Is ASTM A312 TP347 better than TP321 for welded pipe?
Both resist sensitization, but they stabilize differently. TP347 relies on niobium at 10×C minimum and allows nickel up to 13.0%; TP321 relies on titanium at 5×(C+N) and caps nickel at 12.0%. Niobium is less likely to be lost across the arc, so TP347 is often preferred for heavy multipass welding, and TP347 keeps one 75/30 ksi row for every wall, unlike TP321.
What heat treatment does ASTM A312 TP347 require?
TP347 is supplied solution annealed at the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, since TP347 has no individual Table 2 row. It is not an H grade, so there is no Table 5 grain-size requirement, and the MTC should record the temperature and cooling method actually used.
Which filler metal is used to weld ASTM A312 TP347 pipe?
Table 6 maps TP347 to ER347. Qualify the procedure on actual TP347 base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
What sizes of ASTM A312 TP347 pipe can SHH STEEL supply?
We quote TP347 in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
How do I check the niobium requirement on a TP347 certificate?
Multiply the reported carbon by ten. At C = 0.05% the heat needs at least 0.50% Nb, and no heat may exceed 1.00% Nb. If the certificate reports “Cb”, that is the same element under the older name. Without both carbon and niobium on the MTC, the footnote G rule cannot be checked, so a summary saying “stabilized” is not enough for acceptance.
Does ASTM A312 TP347 need supplementary requirement S6?
Only if the purchase order asks for it. S6 is an optional stabilization heat treatment at an agreed temperature below the solution anneal, often requested by licensors for hot hydrocarbon service. It adds a furnace step and should be priced and scheduled at enquiry. Without S6 on the order, TP347 ships solution annealed at the default 1900 °F [1040 °C] minimum with rapid cooling.
What certificates come with ASTM A312 TP347 pipe from SHH STEEL?
Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP347 it should show carbon and niobium on the same heat, so the Nb ≥10×C, ≤1.00% rule can be proven. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.

Conclusion

ASTM A312 TP347 / UNS S34700 is defined by C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 10×C with a 1.00% ceiling (footnote G), a Table 4 floor of 75/30 ksi, and the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, since TP347 has no individual Table 2 row. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X