ASTM A312 TP317L Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 TP317L Stainless Steel Pipe

ASTM A312 TP317L / UNS S31703 stainless steel pipe in SML, WLD and HCW, with C ≤0.035%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%, a 75/30 ksi Table 4 floor and low-carbon consumable by agreement on the WPS (Table 6 pairing not asserted) filler guidance, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP317L / UNS S31703
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP317L Stainless Steel Pipe

ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP317L / UNS S31703, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.

TP317L is the low-carbon version of TP317. Table 1 caps carbon at 0.035% and keeps chromium at 18.0–20.0%, nickel at 11.0–15.0% and molybdenum at 3.0–4.0%, so buyers get the higher-molybdenum advantage over TP316L together with better resistance to intergranular attack in weld heat-affected zones. One detail often surprises people coming from 316L work: Table 4 keeps TP317L on the full 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield row, not the reduced 70/25 ksi line used for TP316L. It is not an H grade, so the default 1900 °F [1040 °C] anneal applies.

SHH STEEL can supply ASTM A312 TP317L stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP317L.

Market names include 317L stainless pipe, S31703 and “317L”. Most mills stock this grade rather than straight TP317 and frequently certify the same heat as TP317/TP317L when carbon meets 0.035%, which is convenient for buyers who need both on one project. If the edition you order carries a small-diameter carbon footnote for L grades, check whether it applies to your sizes before relying on the 0.035% figure for every line.

Within the ASTM A312 series, buyers comparing TP317L usually look next at A312 TP317, A312 TP316L, A312 TP316 and A312 TP316LN. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 recognises three manufacturing routes for TP317L pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C ≤0.035%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%, and every length must be heat treated before release. For TP317L, welded pipe is common in the lighter schedules used for chemical and FGD duty, provided the strip heat itself carries the full 3.0–4.0% molybdenum band.

  • Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
  • Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.

Chemical Composition of ASTM A312 TP317L

Two chemistry layers matter for ASTM A312 TP317L. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.

Element TP317L / UNS S31703 melting analysis
Carbon (C) ≤ 0.035
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 11.0 – 15.0
Molybdenum (Mo) 3.0 – 4.0

Read the table as maxima unless a range is shown. For TP317L the element that defines the grade is molybdenum: it must land inside 3.0–4.0% on the heat analysis, and the certificate should quote UNS S31703 rather than a 316-series identity. Carbon at or below 0.035% is the second defining number, and a heat meeting both can usually be dual-certified TP317/TP317L.

When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP317L without having to rebuild the arithmetic themselves.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.035 0.01 over ≤ 0.045
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 11.0 – 15.0 0.15 under / over 10.85 – 15.15
Molybdenum (Mo) 3.0 – 4.0 0.10 under / over 2.90 – 4.10

Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.

Mechanical Properties of ASTM A312 TP317L

Room-temperature tensile requirements for ASTM A312 TP317L come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S31703, not from this product page or from a sister grade’s strength line.

Property TP317L
Tensile, min 75 ksi [515 MPa]
Yield, min 30 ksi [205 MPa]
Elongation 35% L / 25% T

TP317L uses a single row regardless of route and wall, so welded and seamless pipe are accepted against the same floor. The 75/30 ksi row is higher than the 70/25 ksi used for TP316L, so do not carry 316L acceptance habits across.

Dimensions, Tolerances and Stock Sizes

Dimensional supply for ASTM A312 TP317L pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.

  • Lengths — single random, double random or cut-to-length as ordered
  • Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
  • Jointers — not permitted unless the purchase order allows them

Stock / Available sizes. SHH STEEL quotes TP317L against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP317L is the more commonly held 317-family grade, often in dual TP317/TP317L heats. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.

Representative size (ASME B36.19) Example OD × wall Typical schedules / notes
NPS 1/2 21.3 mm × 2.77 mm (Sch 40S) Sch 10S / 40S / 80S; instrument and small-bore take-offs
NPS 2 60.3 mm × 3.91 mm (Sch 40S) Sch 10S / 40S / 80S; common process branch size
NPS 4 114.3 mm × 6.02 mm (Sch 40S) Sch 10S / 40S / 80S; frequent stock and mill enquiry size
NPS 6 168.3 mm × 7.11 mm (Sch 40S) Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry
NPS 8 – 12 219.1 mm × 8.18 mm (NPS 8 Sch 40S) Sch 10S / 40S; route and wall decide stock vs mill-order
NPS 14 – 24 Per B36.19 for the ordered schedule Sch 10S / 40S; usually mill-order, often welded
Special OD × wall By agreement State OD, wall (nominal or minimum) and length practice

Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.

Equivalent Grades

Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP317L, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.

Designation Notes
ASTM A312 TP317L / UNS S31703 Governing product specification on this page
ASME SA-312 TP317L / S31703 Separate Code Book standard; dual-mark only when the PO names both
TP317 / UNS S31700 Standard-carbon sister, C ≤0.08%; dual heats common
TP316L / UNS S31603 Lower Mo 2.00–3.00% and 70/25 ksi row

We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.

Heat Treatment and Delivery Condition

All A312 pipe is furnished heat treated. TP317L is not an H grade, so it receives the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, because UNS S31703 is not listed individually in Table 2. There is no Table 5 grain-size mandate and no clause 6.2 reheat rule, and HCW cold reduction is completed before the final anneal so delivery remains the annealed condition.

Delivery is normally solution annealed and pickled unless the order asks for bright annealing or another finish. The MTC should record the anneal temperature and cooling method actually used, and fabricators who hot form or heavily cold work TP317L bends should re-anneal to the same practice where the governing code requires it, rather than applying a neighbouring grade’s anneal by habit.

Corrosion Resistance

ASTM A312 does not publish corrosion rates, so this is engineering commentary. TP317L combines the 3.0–4.0% molybdenum of the 317 family with low carbon, which is why it is so often specified for heavily welded process piping in chloride-bearing or acidic media where TP316L is marginal. Low carbon limits chromium-carbide precipitation in the heat-affected zone, so the weld area keeps corrosion resistance close to that of the parent pipe.

Low carbon does not raise pitting resistance by itself; that comes from molybdenum and chromium, which are identical to TP317. If chlorides are severe enough to need more than 4% Mo, the conversation moves to the high-Mo UNS grades in A312 rather than to a heavier TP317L wall. For lines that will be welded but not exposed to strong chlorides, A312 TP316L usually remains the more economical choice.

Applications of ASTM A312 TP317L Pipe

Applications for ASTM A312 TP317L follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S31703 at the design temperature before final wall selection.

Application Why TP317L Buyer note
Welded chemical process piping beyond 316L Low C with Mo 3.0–4.0% Qualify WPS on TP317L
FGD, pulp and paper lines Higher Mo, Cr and Ni than 316L Validate against actual medium
Stock programmes needing 317 and 317L Dual TP317/TP317L when C ≤0.035% State dual acceptance on PO

TP317L is the welded-service counterpart to TP317 and the form most mills actually hold, often dual-certified with TP317. It is specified when the corrosion basis needs more molybdenum than TP316L and the piping will be heavily welded. Enquiries should state UNS S31703, the 75/30 ksi row and any small-diameter carbon footnote considerations for the ordered sizes.

Weldability

For filler selection, Table 6 lists TP317L, but the filler-class pairing is not clearly populated in the edition extract we work from, so a low-carbon consumable is agreed on the WPS; low-carbon 317-type wire is common practice and is recorded here as a project decision rather than a Table 6 mandate. Qualify the WPS and PQR on actual TP317L base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.

TP317L welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. Low carbon helps, but heat input and interpass control still matter on multipass joints. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.

Surface Finishes

Surface condition for ASTM A312 TP317L pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.

  • Annealed and pickled — the usual delivery for process piping after solution treatment
  • Bright annealed — by agreement for selected sizes and routes
  • Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
  • Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed

Inspection and Testing

The base acceptance package for ASTM A312 TP317L pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show carbon at or below 0.035% and molybdenum inside 3.0–4.0% on the same heat.

Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall read as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.

Packaging and Shipping

Export and domestic shipments of ASTM A312 TP317L pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP317L / UNS S31703, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.

  • Ends capped or bevel-protected as ordered
  • Bundles strapped with protected contact points to limit iron pickup
  • Waterproof wrapping for ocean freight when specified
  • Packing list with heat numbers, sizes and certificate references

We keep TP317L physically segregated from TP316-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP317L we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.

  • Grade control — carbon at or below 0.035% and molybdenum inside 3.0–4.0% on the same heat stated on the MTC
  • Honest sister-grade advice when TP317 or TP316L would fit the service better
  • Filler guidance for WPS planning: low-carbon consumable by agreement on the WPS (Table 6 pairing not asserted)
  • SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
  • Dual A312/SA-312 marking only when the purchase order asks for both
  • Cut lengths, bevelling and project marking coordinated on confirmed orders

If you are still choosing between TP317L and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.

Supply Capability

SHH STEEL can supply ASTM A312 TP317L stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.

Item SHH STEEL capability for TP317L
Standard ASTM A312 / A312M TP317L / UNS S31703
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL or cut-to-length
Finish Annealed and pickled; bright annealed or polished by agreement
Filler guidance low-carbon consumable by agreement on the WPS (Table 6 pairing not asserted)
Testing Tension (75/30 ksi), flattening/bend, hydro or NDE per length; supplementary tests on order
Documents EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes. Representative stock and mill-enquiry sizes for TP317L are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.

Enquiries should state the A312 edition, TP317L (UNS S31703), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.

FAQ

Is ASTM A312 TP317L the same as ASME SA-312 TP317L?
They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP317L chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
What is the chemical composition of ASTM A312 TP317L pipe?
Table 1 sets C ≤0.035%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%. These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
What are the mechanical properties of ASTM A312 TP317L?
Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum with 35% longitudinal / 25% transverse elongation. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S31703. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
What is the difference between ASTM A312 TP317L and TP316L?
TP317L carries molybdenum at 3.0–4.0% against 2.00–3.00% for TP316L, with chromium raised to 18.0–20.0% and nickel to 11.0–15.0%. Both are low-carbon grades for welded service. TP317L also keeps the full 75/30 ksi Table 4 floor, whereas TP316L uses 70/25 ksi. Choose TP317L when chloride or acid conditions have outgrown 316L, and keep 316L where it is already proven.
Can ASTM A312 TP317L be dual certified as TP317?
Yes, and it is common practice. Because the two grades differ only in carbon, a heat with carbon at or below 0.035% and molybdenum inside 3.0–4.0% can meet both Table 1 rows, and the tensile floor is the same 75/30 ksi. The dual marking should be requested on the purchase order so the certificate and stencil carry both designations rather than one grade by default.
What heat treatment does ASTM A312 TP317L require?
TP317L is supplied solution annealed at the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, because UNS S31703 is not listed individually in Table 2. It is not an H grade, so there is no Table 5 grain-size requirement, and the MTC should record the temperature and cooling method actually used.
Which filler metal is used to weld ASTM A312 TP317L pipe?
Table 6 lists TP317L, but the filler-class pairing is not clearly populated in the edition extract we work from, so a low-carbon consumable is agreed on the WPS; low-carbon 317-type wire is common practice and is recorded here as a project decision rather than a Table 6 mandate. Qualify the procedure on actual TP317L base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
What sizes of ASTM A312 TP317L pipe can SHH STEEL supply?
We quote TP317L in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
Why does TP317L have a higher tensile floor than TP316L?
Table 4 simply assigns TP317L to the 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield row, while TP316L sits on the 70/25 ksi line. The higher alloy content of the 317 family supports that floor even with low carbon. In practice it means acceptance should not be done on 316L habits; inspectors must check the TP317L row, and designers should use code allowables for UNS S31703.
Is TP317L pipe suitable for flue-gas desulfurization and pulp mill service?
Those are classic markets for the grade, because the higher molybdenum, chromium and nickel than 316L help in acidic, chloride-bearing condensates and bleach-plant liquors. Suitability still depends on the actual chloride level, pH and temperature, so validate it against plant experience or corrosion data. A312 does not certify fitness for a medium; it certifies chemistry, strength, heat treatment and testing.
What certificates come with ASTM A312 TP317L pipe from SHH STEEL?
Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP317L it should show carbon at or below 0.035% and molybdenum inside 3.0–4.0% on the same heat. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.

Conclusion

ASTM A312 TP317L / UNS S31703 is defined by C ≤0.035%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%, a Table 4 floor of 75/30 ksi, and the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, because UNS S31703 is not listed individually in Table 2. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X