ASTM A312 TP347H Stainless Steel Pipe
What is ASTM A312 TP347H Stainless Steel Pipe
ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP347H / UNS S34709, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.
TP347H is the elevated-temperature version of TP347. The 0.04–0.10% carbon band and the coarse-grain requirement support creep strength, while niobium still stabilizes carbon so grain-boundary sensitization after welding is reduced. Table 1 sets C 0.04–0.10% and Nb at least 8×C with a 1.0% ceiling under footnote H, with chromium at 17.0–19.0% and nickel at 9.0–13.0%. As an H grade it carries the full A312 package: Table 2 anneals of 2000 °F [1100 °C] cold-finished and 1925 °F [1050 °C] hot-finished, Table 5 grain size No. 7 or coarser, and the clause 6.2 reheat and lot-marking rules, all on a single 75/30 ksi Table 4 row.
SHH STEEL can supply ASTM A312 TP347H stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP347H.
Commercial names include 347H stainless pipe, S34709 and “H-grade 347”. Those labels only hold when the MTC shows carbon in the 0.04–0.10% band, niobium against the 8×C rule, the measured grain size and the Table 2 anneal actually used. Do not carry TP347’s 10×C factor over to H heats, and do not accept a plain TP347 heat as TP347H simply because its carbon sits in the H band.
Within the ASTM A312 series, buyers comparing TP347H usually look next at A312 TP347, A312 TP321H, A312 TP348H and A312 TP304H. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.
Manufacturing Types (SML / WLD / HCW)
ASTM A312 recognises three manufacturing routes for TP347H pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 8×C with a 1.0% ceiling (footnote H), and every length must be heat treated before release. For TP347H the Table 4 row is the same for every route and wall, so the route decision rests on code acceptance, size and inspection preference rather than strength. Because this is an H grade, the H anneal and grain-size evidence must belong to the finished pipe, whichever route produced it.
- Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
- Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
- Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.
Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.
Chemical Composition of ASTM A312 TP347H
Two chemistry layers matter for ASTM A312 TP347H. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.
| Element | TP347H / UNS S34709 melting analysis |
|---|---|
| Carbon (C) | 0.04 – 0.10 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 17.0 – 19.0 |
| Nickel (Ni) | 9.0 – 13.0 |
| Molybdenum (Mo) | No requirement (…) |
| Niobium (Nb) / Columbium (Cb) | ≥ 8 × C and ≤ 1.0% (footnote H) |
Read the table as maxima unless a range is shown. The stabilizer rule for TP347H (Nb ≥8×C, ≤1.0%) is not a fixed number; it moves with the actual chemistry of each heat. At C = 0.08%, niobium must be at least 0.64%, and even at C = 0.10% the 8×C minimum is 0.80%, still under the 1.0% cap. That is why the MTC has to report the 0.04–0.10% carbon band and niobium against the 8×C rule, plus the measured Table 5 grain size.
When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP347H without having to rebuild the arithmetic themselves.
| Element | Melting (Table 1) | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | 0.04 – 0.10 | 0.01 under / over | 0.03 – 0.11 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 17.0 – 19.0 | 0.20 under / over | 16.80 – 19.20 |
| Nickel (Ni) | 9.0 – 13.0 | 0.10 under / 0.15 over | 8.90 – 13.15 |
| Niobium (Nb) | ≥ 8 × C, ≤ 1.0% | 0.05 over on max | max ≤ 1.05 product; min tied to C |
Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.
Mechanical Properties of ASTM A312 TP347H
Room-temperature tensile requirements for ASTM A312 TP347H come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S34709, not from this product page or from a sister grade’s strength line.
| Property | TP347H requirement (Table 4) |
|---|---|
| Tensile strength, min | 75 ksi [515 MPa] |
| Yield strength (0.2% offset), min | 30 ksi [205 MPa] |
| Elongation in 2 in. or 50 mm (or 4D) | 35% longitudinal / 25% transverse, min |
| Grain size (Table 5) | ASTM No. 7 or coarser |
TP347H uses a single row regardless of route and wall, so welded and seamless pipe are accepted against the same floor. These are minimum release values, not typical mill results, and they should not be raised or lowered by habit from a sister grade. The Table 5 grain size of ASTM No. 7 or coarser travels with the tensile results; ask for the measured number on the MTC rather than a bare “complies”.
Dimensions, Tolerances and Stock Sizes
Dimensional supply for ASTM A312 TP347H pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.
| NPS designator | Wall over | Wall under |
|---|---|---|
| 1/8 to 2-1/2 incl., all t/D | 20.0% | 12.5% |
| 3 to 18 incl., t/D up to 5% | 22.5% | 12.5% |
| 3 to 18 incl., t/D over 5% | 15.0% | 12.5% |
| 20 and larger, welded, all t/D | 17.5% | 12.5% |
| 20 and larger, seamless, t/D up to 5% | 22.5% | 12.5% |
| 20 and larger, seamless, t/D over 5% | 15.0% | 12.5% |
Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.
- Lengths — single random, double random or cut-to-length as ordered
- Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
- Jointers — not permitted unless the purchase order allows them
Stock / Available sizes. SHH STEEL quotes TP347H against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP347H is held in selected seamless sizes for heater and boiler work; other walls are mill-order. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.
| Representative size (ASME B36.19) | Example OD × wall | Typical schedules / notes |
|---|---|---|
| NPS 1/2 | 21.3 mm × 2.77 mm (Sch 40S) | Sch 10S / 40S / 80S; instrument and small-bore take-offs |
| NPS 2 | 60.3 mm × 3.91 mm (Sch 40S) | Sch 10S / 40S / 80S; common process branch size |
| NPS 4 | 114.3 mm × 6.02 mm (Sch 40S) | Sch 10S / 40S / 80S; frequent stock and mill enquiry size |
| NPS 6 | 168.3 mm × 7.11 mm (Sch 40S) | Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry |
| NPS 8 – 12 | 219.1 mm × 8.18 mm (NPS 8 Sch 40S) | Sch 10S / 40S; route and wall decide stock vs mill-order |
| NPS 14 – 24 | Per B36.19 for the ordered schedule | Sch 10S / 40S; usually mill-order, often welded |
| Special OD × wall | By agreement | State OD, wall (nominal or minimum) and length practice |
Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.
Equivalent Grades
Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP347H, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.
| Designation | Notes |
|---|---|
| ASTM A312 TP347H / UNS S34709 | Governing product specification on this page |
| ASME SA-312 TP347H / S34709 | Separate Code Book standard; dual-mark only when the PO names both |
| TP347 / UNS S34700 | Standard-carbon sister; C ≤0.08%, Nb ≥10×C, default 1900 °F anneal |
| TP321H / UNS S32109 | Ti-stabilized H grade |
| TP348H / UNS S34809 | Same H package plus Ta ≤0.10% |
We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.
Heat Treatment and Delivery Condition
All A312 pipe is furnished heat treated. For TP347H, Table 2 sets 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. Those temperatures are above the 1900 °F default used for the standard-carbon sister because the anneal also has to develop the coarse grain that Table 5 requires, and the clause 6.2 reheat rules and lot marking apply whenever pipe is reheated after the qualifying anneal.
Supplementary requirement S6, a stabilization heat treatment at an agreed temperature below the solution anneal, applies only when the purchase order specifies it; if it is ordered, agree the temperature at enquiry and confirm it on the MTC. Delivery is normally solution annealed and pickled, and the certificate should record the anneal temperature, the cooling method and whether the pipe was cold- or hot-finished, since that decides which Table 2 minimum applies.
Corrosion Resistance
ASTM A312 does not contain corrosion requirements, so this is engineering commentary. TP347H shares niobium stabilization with TP347, so it resists intergranular attack after welding and handles oxidizing hot gas well; its real job, however, is creep and stress-rupture strength in superheater, reheater, heater and hydroprocessing lines. The H package of carbon band, grain size and higher anneal is what the design allowables assume.
Do not substitute TP347 or TP347LN into a TP347H line because they are “the same 347”. Lower carbon and finer grain reduce elevated-temperature strength, and the design calculation would no longer hold. Where owners worry about polythionic-acid stress corrosion during shutdowns, S6 stabilization can be added by agreement; it is never automatic under A312.
Applications of ASTM A312 TP347H Pipe
Applications for ASTM A312 TP347H follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S34709 at the design temperature before final wall selection.
| Application area | Typical use of TP347H pipe | Selection note |
|---|---|---|
| Superheater and reheater piping | Elevated-temperature steam lines where creep strength is in the design basis | Confirm grain size and Table 2 anneal on the MTC |
| Refinery heater and hydroprocessing lines | Hot hydrocarbon service with welded joints | Check allowable stresses for UNS S34709 at design temperature |
| Petrochemical furnace outlets | Transfer and header piping in the creep range | Agree S6 at enquiry if the licensor requires it |
| Code piping packages | Dual A312/SA-312 projects with heat traceability | Name edition, route, and UNS on the enquiry |
Plants that already run TP347 or TP321H sometimes buy TP347H in the same package, which works only when each line’s datasheet allows the grade being shipped to it. For creep-range lines, check allowable stresses for UNS S34709 at the design temperature and agree any S6 requirement at enquiry so the extra furnace step is in the schedule.
Weldability
For filler selection, Table 6 maps TP347H to ER347. Qualify the WPS and PQR on actual TP347H base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.
TP347H welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. For H-grade service, match the consumable’s carbon to the creep design and avoid low-carbon wire that would weaken the joint at temperature. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.
Surface Finishes
Surface condition for ASTM A312 TP347H pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.
- Annealed and pickled — the usual delivery for process piping after solution treatment
- Bright annealed — by agreement for selected sizes and routes
- Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
- Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed
Inspection and Testing
The base acceptance package for ASTM A312 TP347H pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show the 0.04–0.10% carbon band and niobium against the 8×C rule, plus the measured Table 5 grain size, on the same line items as the tensile results.
Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.
| Option | Purpose |
|---|---|
| S1 product analysis | Confirms chemistry on finished pipe |
| S5 radiography | Weld integrity on WLD pipe |
| S6 stabilization | Stabilizing heat treatment at an agreed temperature |
| S7 intergranular corrosion | A262 Practice E after sensitizing treatment |
| S8 minimum wall | Wall read as minimum rather than nominal |
| S9 weld decay | Compares weld and base-metal loss rates |
EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.
Packaging and Shipping
Export and domestic shipments of ASTM A312 TP347H pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP347H / UNS S34709, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.
- Ends capped or bevel-protected as ordered
- Bundles strapped with protected contact points to limit iron pickup
- Waterproof wrapping for ocean freight when specified
- Packing list with heat numbers, sizes and certificate references
We keep TP347H physically segregated from other 347-family and TP321-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.
Why Choose SHH STEEL
SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP347H we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.
- Grade control — the 0.04–0.10% carbon band and niobium against the 8×C rule, plus the measured Table 5 grain size stated on the MTC
- Honest sister-grade advice when TP347 or TP321H would fit the service better
- Filler guidance for WPS planning: ER347
- SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
- Dual A312/SA-312 marking only when the purchase order asks for both
- Cut lengths, bevelling and project marking coordinated on confirmed orders
If you are still choosing between TP347H and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.
Supply Capability
SHH STEEL can supply ASTM A312 TP347H stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.
| Item | SHH STEEL capability for TP347H |
|---|---|
| Standard | ASTM A312 / A312M TP347H / UNS S34709 |
| Manufacturing types | SML, WLD, HCW |
| Size | NPS 1/8 and up per ASME B36.19; special OD/wall by agreement |
| Schedules | 5S, 10S, 40S, 80S and non-standard walls |
| Length | SRL, DRL or cut-to-length |
| Finish | Annealed and pickled; bright annealed or polished by agreement |
| Filler guidance | ER347 |
| Testing | Tension (75/30 ksi), Table 5 grain size No. 7 or coarser, flattening/bend, hydro or NDE per length; supplementary tests on order |
| Documents | EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes. Representative stock and mill-enquiry sizes for TP347H are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.
Enquiries should state the A312 edition, TP347H (UNS S34709), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.
FAQ
-
Is ASTM A312 TP347H the same as ASME SA-312 TP347H?
- They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP347H chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
-
What is the chemical composition of ASTM A312 TP347H pipe?
- Table 1 sets C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 8×C with a 1.0% ceiling (footnote H). These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
-
What are the mechanical properties of ASTM A312 TP347H?
- Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum with 35% longitudinal / 25% transverse elongation, plus grain size ASTM No. 7 or coarser. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S34709. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
-
What is the difference between ASTM A312 TP347H and TP347?
- TP347H carries a 0.04–0.10% carbon band where TP347 only caps carbon at 0.08%, and its niobium rule is at least 8×C with a 1.0% cap instead of 10×C. TP347H also needs Table 5 grain size No. 7 or coarser and Table 2 anneals of 2000 °F cold-finished or 1925 °F hot-finished. Both share the 75/30 ksi Table 4 row and ER347 filler.
-
Is A312 TP347H or TP321H better for superheater piping?
- Both are stabilized H grades with the same anneal temperatures and grain-size rule. TP347H uses niobium at 8×C and one 75/30 ksi tensile row for every wall, while TP321H uses titanium at 4×(C+N) and drops to 70/25 ksi on heavy seamless walls. Many boiler and refinery owners favour TP347H for heavy welding, but the code allowables for each UNS number should make the final call.
-
What heat treatment does ASTM A312 TP347H require?
- TP347H is supplied solution annealed at 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. As an H grade it must also meet Table 5 grain size No. 7 or coarser and the clause 6.2 reheat and lot-marking rules, and S6 stabilization is added only when ordered.
-
Which filler metal is used to weld ASTM A312 TP347H pipe?
- Table 6 maps TP347H to ER347. Qualify the procedure on actual TP347H base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
-
What sizes of ASTM A312 TP347H pipe can SHH STEEL supply?
- We quote TP347H in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
-
How much niobium does a TP347H heat need?
- Multiply the carbon by eight. At C = 0.08% the minimum is 0.64% Nb, and even at the top of the carbon band, C = 0.10%, the minimum is 0.80%, still under the 1.0% ceiling of footnote H. The MTC must report both carbon and niobium, otherwise the rule cannot be checked; a certificate applying the TP347 10×C factor is using the wrong row.
-
Can TP347H pipe be supplied welded instead of seamless?
- Yes. ASTM A312 allows SML, WLD and HCW routes for TP347H, and the welded seam is made without filler before the H-grade anneal. Seamless is often preferred for thick walls and creep-critical headers, but welded pipe is valid where the design code and owner specification accept it. State the route on the enquiry so grain-size and anneal evidence follow the right product.
-
What certificates come with ASTM A312 TP347H pipe from SHH STEEL?
- Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP347H it should show the 0.04–0.10% carbon band and niobium against the 8×C rule, plus the measured Table 5 grain size. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.
Conclusion
ASTM A312 TP347H / UNS S34709 is defined by C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 8×C with a 1.0% ceiling (footnote H), a Table 4 floor of 75/30 ksi with grain size No. 7 or coarser, and 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.