ASTM A312 TP304 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 TP304 Stainless Steel Pipe

ASTM A312 TP304 / UNS S30400 stainless steel pipe in SML, WLD and HCW, with Cr 18.0–20.0%, Ni 8.0–11.0% and C ≤0.08%, a 75/30 ksi Table 4 floor and a 1900 °F solution anneal, supplied by SHH STEEL to ASME B36.19 with EN 10204 3.1 MTCs.
Grade
TP304 / UNS S30400
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP304 Stainless Steel Pipe

ASTM A312 / A312M is the ASTM International product specification for seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. Within that specification, Grade TP304 is the workhorse 18-8 chromium-nickel austenitic listed under UNS S30400, with Table 1 melting limits of carbon ≤0.08%, chromium 18.0–20.0%, and nickel 8.0–11.0%. Buyers who write “304 pipe” on a bill of materials still need to name A312 (or the separate ASME SA-312 adoption) on the purchase order so the mill knows which product standard, tests, and marking rules apply.

SHH STEEL can supply ASTM A312 TP304 stainless steel pipe as seamless (SML), welded (WLD), and heavily cold-worked (HCW) product in ASME B36.19 schedules and special OD/wall by agreement, shipped with EN 10204 3.1 mill test certificates that report the full Table 1 ladle chemistry and the Table 4 tensile results. When a project also needs ASME Code Book marking, we dual-mark A312 / SA-312 on the same lengths only if the purchase order says so — ASTM A312 and ASME SA-312 remain two independent standards. Browse the full grade family on the A312/A312M

Commercially, TP304 is still called 304, 18-8, or S30400; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A312 TP304L, A312 TP304H, A312 TP316 / A312 TP316L, and lean-nickel options such as A312 TP201 or A312 TP201LN. For ASME Section-stamp work that cites SA-312, see the separate SA312 TP304 page — written to the ASME standard, not as a synonym title for this ASTM page.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 recognizes three manufacturing types for TP304, and the stencil must state which one you received. Seamless (SML) pipe is pierced or extruded from solid billet without a weld seam and is preferred for higher-pressure, cyclic, or owner-mandated seamless service. Welded (WLD) pipe is formed from strip or plate, fusion-welded, then worked and heat-treated so the weld meets the same tensile and flattening requirements as the base metal.

Heavily cold-worked (HCW) pipe starts as welded product and receives a controlled cold reduction that raises strength and refines the weld zone; A312 treats HCW as its own manufacturing type with distinct marking rules. Name SML, WLD, or HCW on the enquiry rather than writing “304 pipe” alone. SHH STEEL quotes all three routes and states the type on both the stencil and the EN 10204 3.1 certificate.

Chemical Composition of A312 TP304

Two chemistry layers matter for TP304 under ASTM A312. The melting (heat or ladle) analysis is mandatory for every heat under Table 1, while product analysis on finished pipe applies only when Supplementary Requirement S1 or equivalent purchase-order wording is ordered. Product tolerances are not printed inside A312 itself; they flow through ASTM A999/A999M from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise tighter catalogue chemistry windows that the ASTM standard does not publish.

The tables below reproduce the Table 1 heat analysis for TP304 / UNS S30400 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element, so it need not be determined or reported on the certificate.

Melting analysis (heat / ladle analysis) — Table 1

Element TP304 (UNS S30400) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 11.0 0.10 under / 0.15 over 7.90 – 11.15

The 18–20% chromium and 8–11% nickel balance makes TP304 the reference 18-8 austenitic grade: chromium builds the passive film and nickel keeps the structure fully austenitic after the 1900 °F solution anneal. Carbon is capped at 0.08% on the melt; heats that also meet the TP304L carbon ceiling and overlapping nickel band can be dual-certified to A312 TP304L when both tensile floors are satisfied.

When product analysis is ordered, finished pipe may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20% and Ni 7.90–11.15%. Those are the only product limits we quote. Put any tighter project carbon or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of A312 TP304

ASTM A312 Table 4 sets the tensile acceptance floor for TP304 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum longitudinal and 25% minimum transverse in 2 in. or 50 mm (or 4D). Every length — or the representative specimen scheme the edition allows — must meet those numbers after the final solution anneal. Table 4 does not list a hardness maximum for TP304; if a project specification needs a hardness cap, it must be written into the purchase order as an additional requirement rather than assumed from a catalogue HB or HRB figure.

Property TP304 requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm (or 4D) 35% longitudinal / 25% transverse, min

Dimensions and Tolerances

Dimensional supply for ASTM A312 TP304 pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special outside diameter and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3 as summarized below. State on the purchase order whether wall is nominal or minimum (Supplementary Requirement S8), because the two readings produce different pipe from the same size line.

NPS designator Over Under
1/8 – 2-1/2, all t/D 20.0% 12.5%
3 – 18, t/D ≤ 5% 22.5% 12.5%
3 – 18, t/D > 5% 15.0% 12.5%
≥ 20 welded 17.5% 12.5%
≥ 20 seamless, t/D ≤ 5% 22.5% 12.5%
≥ 20 seamless, t/D > 5% 15.0% 12.5%

Source: ASTM A312 Table 3; outside-diameter variations per A999/A999M. The under-tolerance column is 12.5% across the listed bands, while the over-tolerance depends on NPS and the t/D ratio — a detail that matters when you are calculating weight or fitting clearance on thin-wall Sch 5S and 10S pipe. Lengths may be single random, double random, or cut-to-length; put the cut list on the enquiry so mill and stock lengths can be mixed efficiently.

Equivalent Grades

Equivalence language around TP304 is often looser than the purchase order can afford. ASTM A312 Grade TP304 / UNS S30400 is the governing designation for this article; EN 1.4301 and JIS SUS304 are approximate wrought names that point to similar chemistry families but are not automatic substitutes on an A312 mill test certificate. When a datasheet says “equivalent to 304,” confirm which product standard, tensile table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASTM A312 / A312M Grade TP304 Governing ASTM pipe product standard for this article
UNS S30400 Unified number listed in Table 1
ASME SA-312 TP304 Separate ASME Code Book adoption of the A312 grade text — dual-mark only when the PO asks
EN 1.4301 (X5CrNi18-10) Approximate wrought stainless designation; order EN product forms under the relevant EN pipe/tube specs, not by EN number alone on an A312 MTC
JIS SUS304 Approximate Japanese grade name; confirm the Japanese pipe/tube product standard when ordering JIS product

ASME SA-312 TP304 is the separate Code Book adoption of the same grade text; dual A312/SA-312 marking is a purchase-order option, not a claim that the two standards are one document. Compare low-carbon and molybdenum sisters on their own ASTM A312 pages before swapping grades.

Heat Treatment and Delivery Condition

Unless a grade is individually listed with a different temperature in ASTM A312 Table 2, TP304 falls under the default solution-anneal minimum of 1900 °F [1040 °C], followed by water quenching or rapid cooling to hold carbon in solution. Cold-finished and hot-finished pipe both use that same Table 2 default. Skipping the anneal can leave as-welded or as-cold-worked structures that sensitize in service even when ladle chemistry looked acceptable.

Delivery condition for SHH STEEL TP304 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment. When Supplementary Requirement S7 is ordered, the corrosion test report travels with the heat-treatment record.

Corrosion Resistance

TP304’s chromium-rich passive film handles a wide band of oxidizing acids, organic media, and clean aqueous services that do not lean heavily on chlorides. In chloride-bearing waters, coastal atmospheres, and many food brines, pitting and crevice attack become limiting, and buyers usually step up to A312 TP316 or A312 TP316L. Intergranular corrosion after welding is controlled by ordering A312 TP304L or by solution annealing after welding when the sequence allows.

ASTM A312 itself does not publish a corrosion-rate table for TP304; selection remains engineering judgment against fluid, temperature, and inspection philosophy. When a specification calls for ASTM A262 Practice E, invoke Supplementary Requirement S7 so the test is contractual. SHH STEEL will not rank TP304 as equal to 316 in chlorides — that claim is not supported by the product standard.

Applications of A312 TP304 Pipe

Because TP304 is the default austenitic pipe grade in so many owner specifications, it shows up across chemical transfer, food and beverage utilities, pharmaceutical water systems, power-plant auxiliary lines, cryogenic transfer, and architectural stainless work. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid and fabrication route, not only for the familiar “304” name on the BOM.

Application area Typical use of TP304 pipe Selection note
Chemical and process piping Acids, caustics, solvents, and mild corrosive transfer lines ordered to A312 Confirm fluid compatibility; prefer TP316/TP316L if chlorides dominate
Food, beverage, and dairy Hygienic transfer and utility lines where 304 stainless is accepted Follow hygiene finish and welding procedure requirements
Pharmaceutical / biotech Process and utility stainless lines ordered as A312 product State Ra/polish and documentation on the enquiry when required
Power and utility Condensate, feedwater auxiliary, and general plant stainless piping Dual A312/SA-312 marking often requested for Code work
Cryogenic service Liquefied-gas transfer where austenitic toughness is required Confirm low-temperature code acceptance for the grade
Architectural / structural Exposed pipe, supports, and decorative stainless ordered to A312 Finish and marking language matter as much as grade

For as-welded lines consider TP304L or dual TP304/TP304L; for creep-range service open TP304H; for seawater, bleach, and chloride-rich liquors move to the molybdenum grades listed on the same ASTM A312 hub.

Weldability

TP304 welds readily with matching or near-matching austenitic filler. ASTM A312 Table 6 lists ER308 / UNS S30800 and W30840 as the reference filler classification for TP304; project welding procedures may call ER308L when the fabrication prefers low-carbon deposit chemistry even though the base metal is standard TP304. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable piping code — A312 governs the pipe product, not the field weld procedure.

For pipe that will enter service as-welded in a sensitizing environment, many owners change the base metal to A312 TP304L rather than relying on a perfect weld procedure to protect standard-carbon TP304. Specify surface finish and end preparation on the pipe PO for orbital or hygienic welds. SHH STEEL can note the Table 6 filler reference on request documents; filler supply itself is a fabrication purchase unless the contract says otherwise.

Surface Finishes

Standard mill delivery for ASTM A312 TP304 is solution annealed and pickled, leaving a clean matte finish suitable for most process and utility piping. Blasted-and-pickled surfaces are available when a more uniform dull appearance is wanted after scale removal. Bright annealing under protective atmosphere produces a smoother reflective surface used on some architectural and clean-utility lines and must be called out because it changes the heat-treatment route.

Polished finishes (for example a stated grit or Ra) are fabrication or service-center operations on top of A312 product, not automatic with the grade stamp. When a hygienic specification quotes an Ra maximum on the bore, put it on the pipe purchase order with its own acceptance language. SHH STEEL stencils grade and heat treatment as standard requirements; polish remains commercial.

Inspection and Testing

Base ASTM A312 testing for TP304 includes heat analysis, tension tests to the Table 4 floors, flattening or bend tests as applicable to the manufacturing type, and either hydrostatic testing or nondestructive electric testing of each length. The purchaser chooses hydro versus NDE in line with the product standard’s options; both are acceptance routes, not informal upgrades. Marking includes the ASTM designation, grade, manufacturing type, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP304 orders are summarized below. Invoke them by number on the purchase order; mills will not assume S5 radiography or S7 intergranular testing from a verbal “full certs” note.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall interpreted as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

Packaging and Shipping

TP304 pipe leaves SHH STEEL bundled, capped, and tagged for export or domestic delivery according to the length mix on the order. Bundle tags repeat the ASTM A312 grade, manufacturing type, size, heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for polished or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project end-cap colors should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A312 TP304 as a product standard with enforceable chemistry, tensile, heat-treatment, and marking rules — not as a catalogue nickname for “any 304 pipe.” The MTC reports the full Table 1 ladle chemistry and Table 4 tensile pair; the stencil carries the manufacturing type actually ordered; and dual A312/SA-312 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 304-family conversation honest. If the isometric is mostly as-welded and sensitization-sensitive, we steer toward A312 TP304L or dual TP304/TP304L. If chlorides dominate, we open A312 TP316 / A312 TP316L. If nickel cost drives a lean alternative, we compare A312 TP201 / A312 TP201LN with clear UNS numbers. The A312/A312M is organized the same way — grade by grade under ASTM.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, polish, and third-party inspection are defined extras. The pipe that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A312 TP304 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against.

Item SHH STEEL capability for TP304
Standard ASTM A312 / A312M (dual SA-312 marking on request) Grade TP304 / UNS S30400
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL, or cut-to-length
Finish Annealed and pickled; blasted and pickled; bright annealed or polished by agreement
Testing Tension (75/30 ksi), flattening/bend, hydro or NDE per length; full Table 1 chemistry on MTC; S1/S5/S7/S8/S9 on order
Documents EN 10204 3.1 with full Table 1 chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP304 pipe against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the combinations buyers most often request under ASME B36.19; availability of any single NPS × schedule on a given week depends on mill rolling and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP304
NPS 1/2, 3/4, 1, 1-1/4, 1-1/2, 2, 2-1/2, 3, 4, 5, 6, 8, 10, 12, 14, 16, 18, 20, 24 (intermediates and larger on enquiry)
Schedules Sch 5S, 10S, 40S, 80S per ASME B36.19; other walls by agreement
Common OD × wall examples 21.3 × 2.77 mm (NPS 1/2 Sch 40S); 33.4 × 3.38 mm (NPS 1 Sch 40S); 60.3 × 3.91 mm (NPS 2 Sch 40S); 88.9 × 5.49 mm (NPS 3 Sch 40S); 114.3 × 6.02 mm (NPS 4 Sch 40S); 168.3 × 7.11 mm (NPS 6 Sch 40S); 219.1 × 8.18 mm (NPS 8 Sch 40S) — illustrative B36.19 sizes
Length SRL, DRL, or cut-to-length on enquiry
Special Non-standard OD/wall, heavy wall, HCW, and polished finishes — confirm on enquiry before the heat is reserved

When you send an enquiry, list NPS × schedule (or OD × wall), manufacturing type (SML / WLD / HCW), quantity or cut list, required marking (A312 alone or dual A312/SA-312), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, manufacturing type, quantity or cut lengths, required marking (A312 or dual A312/SA-312), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry and tensile against Table 1 and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASTM A312 / A312M product standard that governs this page.

FAQ

Is ASTM A312 the same as ASME SA-312 for TP304?
No. ASTM A312 / A312M is the ASTM International product specification; ASME SA-312 / SA-312M is the separate ASME Code Book adoption of that grade text. Chemistry and tensile floors align closely, but they are two independent standards. Dual-mark A312/SA-312 pipe only when the purchase order asks for both names on the stencil and MTC.
Seamless vs welded TP304 — which should I order under ASTM A312?
Order seamless (SML) when the specification prefers a homogeneous wall without a weld seam. Order welded (WLD) when the code accepts welded austenitic pipe and cost or lead time favors strip-formed product. Heavily cold-worked (HCW) is a third A312 manufacturing type. Name SML, WLD, or HCW on the PO; "304 pipe" alone is not enough.
Hydrostatic test vs NDE — which do I get on TP304 pipe?
ASTM A312 allows either hydrostatic testing or nondestructive electric testing of each length as the standard integrity screen. Neither is an informal upgrade over the other inside the product standard. State the preferred route on the enquiry if your end user mandates hydro or a specific NDE method.
Does A312 Table 4 set a hardness limit for TP304?
No. Table 4 for TP304 lists tensile strength, yield strength, and elongation minima only — no hardness maximum. If a project needs a maximum HB or HRB value, write it into the purchase order as an additional requirement with an agreed test method; catalogue hardness is not an ASTM A312 acceptance criterion.
What is the UNS number and chemistry of ASTM A312 TP304?
TP304 is UNS S30400. Table 1 melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 18.0–20.0%, and nickel 8.0–11.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when S1 is ordered, from A480 Table A1.1 tolerances.
TP304 vs TP304L — which should I order?
Order TP304 when the specification calls for the standard 75/30 ksi tensile floor and carbon ≤0.08% is acceptable. Order TP304L when as-welded intergranular resistance is the driver and the lower 70/25 ksi floor is acceptable. Dual TP304/TP304L certification is possible on qualifying heats — ask for it on the PO rather than assuming it.
TP304 vs TP316 — which is better in chlorides?
TP316 / TP316L adds molybdenum and generally resists chloride pitting and crevice corrosion better than TP304 in seawater, brines, and many process waters. TP304 remains appropriate for many oxidizing and low-chloride services. ASTM A312 does not publish a chloride ranking table; open the TP316 pages on the hub when chlorides dominate.
TP304 vs TP201 — are they interchangeable under ASTM A312?
No. TP201 (UNS S20100) is a lean-nickel manganese-nitrogen austenitic with different Table 1 chemistry and its own tensile row. Some mild utility services can use either grade after engineering review, but stamps, UNS numbers, and MTCs must stay distinct. Compare the TP201 page when nickel cost is the issue, not when a 304 specification must be met literally.
What heat treatment does ASTM A312 require for TP304?
TP304 uses the Table 2 default solution-anneal minimum of 1900 °F [1040 °C] with water quenching or rapid cooling, because the grade is not individually listed at a different temperature. Both cold-finished and hot-finished pipe follow that default. The anneal and quench must be reflected on the mill test certificate.
What filler metal should I use to weld TP304 pipe?
ASTM A312 Table 6 references ER308 / S30800 and W30840 for TP304. Many fabrication specifications prefer ER308L deposits for lower carbon in the weld metal even when the base pipe is standard TP304. The construction-code WPS governs process and inspection; confirm filler brand and lot requirements with the fabricator.
Can you dual-certify ASTM A312 and ASME SA-312 TP304, or TP304/TP304L?
Yes on both axes when the heat and testing support it. Dual A312/SA-312 marking is available when the purchase order requests both independent standards. Dual TP304/TP304L is available when ladle chemistry meets the tighter carbon rules and tensile results clear both Table 4 floors. Spell the required marking on the enquiry so the heat is selected correctly.

Conclusion

ASTM A312 TP304 / UNS S30400 remains the reference 18-8 stainless steel pipe grade for high-temperature and general corrosive service when molybdenum is not required and standard carbon is acceptable. SHH STEEL supplies SML, WLD, and HCW product to ASME B36.19 and special OD/wall, solution annealed, tested to Table 4, and documented on EN 10204 3.1 certificates — with dual SA-312 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the ASTM A312/A312M product hub, then send your size list and marking requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X