ASTM A312 TP317 Stainless Steel Pipe
What is ASTM A312 TP317 Stainless Steel Pipe
ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP317 / UNS S31700, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.
TP317 is the higher-molybdenum companion to TP316 in the A312 grade list. Where TP316 carries 2.00–3.00% Mo, TP317 moves the band up to 3.0–4.0% and raises chromium to 18.0–20.0% and nickel to 11.0–15.0%, with carbon capped at 0.08%. That extra point of molybdenum is the whole reason the grade exists: it gives more margin in chloride-bearing and reducing-acid process streams where 316 sits near the edge of its useful range. Table 4 releases TP317 at the same 75 ksi [515 MPa] tensile / 30 ksi [205 MPa] yield floor as TP316, and it is not an H grade, so the default 1900 °F [1040 °C] anneal applies.
SHH STEEL can supply ASTM A312 TP317 stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP317.
Buyers meet this chemistry as 317 stainless pipe, S31700 or simply “317”. The shorthand is where substitutions start: a heat sold as “317” has to show molybdenum inside 3.0–4.0% on the certificate, otherwise it is a 316 heat with a stretched Mo result. Many mills actually roll the low-carbon version and dual-certify TP317/TP317L when carbon also meets 0.035%; that is a legitimate and convenient route, but the dual acceptance should be written on the purchase order rather than assumed.
Within the ASTM A312 series, buyers comparing TP317 usually look next at A312 TP317L, A312 TP316, A312 TP316L and A312 TP316H. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.
Manufacturing Types (SML / WLD / HCW)
ASTM A312 recognises three manufacturing routes for TP317 pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%, and every length must be heat treated before release. For TP317, welded pipe is common in the lighter schedules used for chemical and FGD duty, provided the strip heat itself carries the full 3.0–4.0% molybdenum band.
- Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
- Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
- Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.
Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.
Chemical Composition of ASTM A312 TP317
Two chemistry layers matter for ASTM A312 TP317. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.
| Element | TP317 / UNS S31700 melting analysis |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 18.0 – 20.0 |
| Nickel (Ni) | 11.0 – 15.0 |
| Molybdenum (Mo) | 3.0 – 4.0 |
Read the table as maxima unless a range is shown. For TP317 the element that defines the grade is molybdenum: it must land inside 3.0–4.0% on the heat analysis, and the certificate should quote UNS S31700 rather than a 316-series identity. Against TP317L every band is the same except carbon, which is why dual heats are common and why the carbon result deserves a second look.
When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP317 without having to rebuild the arithmetic themselves.
| Element | Melting (Table 1) | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | ≤ 0.08 | 0.01 over | ≤ 0.09 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 18.0 – 20.0 | 0.20 under / over | 17.80 – 20.20 |
| Nickel (Ni) | 11.0 – 15.0 | 0.15 under / over | 10.85 – 15.15 |
| Molybdenum (Mo) | 3.0 – 4.0 | 0.10 under / over | 2.90 – 4.10 |
Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.
Mechanical Properties of ASTM A312 TP317
Room-temperature tensile requirements for ASTM A312 TP317 come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S31700, not from this product page or from a sister grade’s strength line.
| Property | TP317 |
|---|---|
| Tensile, min | 75 ksi [515 MPa] |
| Yield, min | 30 ksi [205 MPa] |
| Elongation | 35% L / 25% T |
TP317 uses a single row regardless of route and wall, so welded and seamless pipe are accepted against the same floor. These are minimum release values, not typical mill results, and they should not be raised or lowered by habit from a sister grade.
Dimensions, Tolerances and Stock Sizes
Dimensional supply for ASTM A312 TP317 pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.
| NPS designator | Wall over | Wall under |
|---|---|---|
| 1/8 to 2-1/2 incl., all t/D | 20.0% | 12.5% |
| 3 to 18 incl., t/D up to 5% | 22.5% | 12.5% |
| 3 to 18 incl., t/D over 5% | 15.0% | 12.5% |
| 20 and larger, welded, all t/D | 17.5% | 12.5% |
| 20 and larger, seamless, t/D up to 5% | 22.5% | 12.5% |
| 20 and larger, seamless, t/D over 5% | 15.0% | 12.5% |
Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.
- Lengths — single random, double random or cut-to-length as ordered
- Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
- Jointers — not permitted unless the purchase order allows them
Stock / Available sizes. SHH STEEL quotes TP317 against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP317 is held less often than TP317L, so heavier walls and larger NPS are frequently mill-order. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.
| Representative size (ASME B36.19) | Example OD × wall | Typical schedules / notes |
|---|---|---|
| NPS 1/2 | 21.3 mm × 2.77 mm (Sch 40S) | Sch 10S / 40S / 80S; instrument and small-bore take-offs |
| NPS 2 | 60.3 mm × 3.91 mm (Sch 40S) | Sch 10S / 40S / 80S; common process branch size |
| NPS 4 | 114.3 mm × 6.02 mm (Sch 40S) | Sch 10S / 40S / 80S; frequent stock and mill enquiry size |
| NPS 6 | 168.3 mm × 7.11 mm (Sch 40S) | Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry |
| NPS 8 – 12 | 219.1 mm × 8.18 mm (NPS 8 Sch 40S) | Sch 10S / 40S; route and wall decide stock vs mill-order |
| NPS 14 – 24 | Per B36.19 for the ordered schedule | Sch 10S / 40S; usually mill-order, often welded |
| Special OD × wall | By agreement | State OD, wall (nominal or minimum) and length practice |
Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.
Equivalent Grades
Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP317, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.
| Designation | Notes |
|---|---|
| ASTM A312 TP317 / UNS S31700 | Governing product specification on this page |
| ASME SA-312 TP317 / S31700 | Separate Code Book standard; dual-mark only when the PO names both |
| TP317L / UNS S31703 | Low-carbon sister, C ≤0.035%; same Cr, Ni and Mo bands |
| TP316 / UNS S31600 | Lower Mo 2.00–3.00%; not a substitute where 317 was specified |
We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.
Heat Treatment and Delivery Condition
All A312 pipe is furnished heat treated. TP317 is not an H grade, so it receives the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, because UNS S31700 is not listed individually in Table 2. There is no Table 5 grain-size mandate and no clause 6.2 reheat rule, and HCW cold reduction is completed before the final anneal so delivery remains the annealed condition.
Delivery is normally solution annealed and pickled unless the order asks for bright annealing or another finish. The MTC should record the anneal temperature and cooling method actually used, and fabricators who hot form or heavily cold work TP317 bends should re-anneal to the same practice where the governing code requires it, rather than applying a neighbouring grade’s anneal by habit.
Corrosion Resistance
ASTM A312 has no corrosion table, so what follows is engineering commentary rather than a specification requirement. TP317 is chosen because molybdenum, chromium and nickel are all higher than in TP316, which generally improves resistance to pitting and crevice attack in chloride-bearing water and to many reducing acids. It is the usual step up when a plant has seen 316 struggle but does not want to jump to a 6Mo austenitic or a nickel alloy.
Carbon up to 0.08% is the trade-off. A heavily welded TP317 line can sensitize in the heat-affected zone if heat input is careless, so welded aqueous service is usually better served by A312 TP317L, which keeps the same Mo band with carbon at 0.035% maximum. Fitness for a particular medium, temperature and velocity still has to be confirmed from the project corrosion basis or test data; the grade name alone does not guarantee it.
Applications of ASTM A312 TP317 Pipe
Applications for ASTM A312 TP317 follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S31700 at the design temperature before final wall selection.
| Application | Why TP317 | Buyer note |
|---|---|---|
| Chemical process lines where TP316 is marginal | Mo 3.0–4.0% | Consider TP317L if welded aqueous |
| Pulp, paper and flue-gas service | Higher Mo, Cr and Ni than 316 | Validate against actual medium |
| Projects specifying 317 by datasheet | UNS S31700 identity | Confirm Mo on every heat |
TP317 is the standard “more molybdenum than 316” grade in ASTM A312 and is specified when the corrosion basis needs that extra margin without moving to super-austenitic material. It is less widely held than TP316 or TP317L, so lead times can be longer for heavier walls; if the datasheet allows it, saying that dual TP317/TP317L certification is acceptable usually widens the mill and stock options considerably.
Weldability
For filler selection, Table 6 lists TP317, but the filler-class pairing is not clearly populated in the edition extract we work from, so the consumable is agreed on the WPS; ER317-type wire is common industry practice and is recorded here as a project decision, not as a Table 6 mandate. Qualify the WPS and PQR on actual TP317 base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.
TP317 welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. Keep heat input and interpass temperature controlled, because carbon up to 0.08% leaves less margin against heat-affected-zone sensitization than an L grade. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.
Surface Finishes
Surface condition for ASTM A312 TP317 pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.
- Annealed and pickled — the usual delivery for process piping after solution treatment
- Bright annealed — by agreement for selected sizes and routes
- Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
- Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed
Inspection and Testing
The base acceptance package for ASTM A312 TP317 pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show molybdenum inside 3.0–4.0% on every heat, together with the 18.0–20.0% Cr and 11.0–15.0% Ni bands.
Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.
| Option | Purpose |
|---|---|
| S1 product analysis | Confirms chemistry on finished pipe |
| S5 radiography | Weld integrity on WLD pipe |
| S7 intergranular corrosion | A262 Practice E after sensitizing treatment |
| S8 minimum wall | Wall read as minimum rather than nominal |
| S9 weld decay | Compares weld and base-metal loss rates |
EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.
Packaging and Shipping
Export and domestic shipments of ASTM A312 TP317 pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP317 / UNS S31700, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.
- Ends capped or bevel-protected as ordered
- Bundles strapped with protected contact points to limit iron pickup
- Waterproof wrapping for ocean freight when specified
- Packing list with heat numbers, sizes and certificate references
We keep TP317 physically segregated from TP316-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.
Why Choose SHH STEEL
SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP317 we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.
- Grade control — molybdenum inside 3.0–4.0% on every heat, together with the 18.0–20.0% Cr and 11.0–15.0% Ni bands stated on the MTC
- Honest sister-grade advice when TP317L or TP316 would fit the service better
- Filler guidance for WPS planning: by agreement on the WPS (ER317-type practice is common; Table 6 pairing not asserted)
- SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
- Dual A312/SA-312 marking only when the purchase order asks for both
- Cut lengths, bevelling and project marking coordinated on confirmed orders
If you are still choosing between TP317 and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.
Supply Capability
SHH STEEL can supply ASTM A312 TP317 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.
| Item | SHH STEEL capability for TP317 |
|---|---|
| Standard | ASTM A312 / A312M TP317 / UNS S31700 |
| Manufacturing types | SML, WLD, HCW |
| Size | NPS 1/8 and up per ASME B36.19; special OD/wall by agreement |
| Schedules | 5S, 10S, 40S, 80S and non-standard walls |
| Length | SRL, DRL or cut-to-length |
| Finish | Annealed and pickled; bright annealed or polished by agreement |
| Filler guidance | by agreement on the WPS (ER317-type practice is common; Table 6 pairing not asserted) |
| Testing | Tension (75/30 ksi), flattening/bend, hydro or NDE per length; supplementary tests on order |
| Documents | EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes. Representative stock and mill-enquiry sizes for TP317 are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.
Enquiries should state the A312 edition, TP317 (UNS S31700), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.
FAQ
-
Is ASTM A312 TP317 the same as ASME SA-312 TP317?
- They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP317 chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
-
What is the chemical composition of ASTM A312 TP317 pipe?
- Table 1 sets C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%. These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
-
What are the mechanical properties of ASTM A312 TP317?
- Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum with 35% longitudinal / 25% transverse elongation. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S31700. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
-
What is the difference between ASTM A312 TP317 and TP317L?
- The only Table 1 difference is carbon. TP317 allows up to 0.08% C, while TP317L caps carbon at 0.035%; chromium 18.0–20.0%, nickel 11.0–15.0% and molybdenum 3.0–4.0% are identical, and both grades share the 75/30 ksi Table 4 floor. Choose TP317L when the line is heavily welded and used in aqueous service, and accept dual TP317/TP317L heats when carbon meets 0.035%.
-
How does A312 TP317 compare with TP316 pipe?
- TP317 raises molybdenum from the 2.00–3.00% of TP316 to 3.0–4.0%, and also lifts chromium to 18.0–20.0% and nickel to 11.0–15.0%. The tensile floor stays at 75/30 ksi, so the reason to buy TP317 is corrosion margin rather than strength. It is typically specified where TP316 has proved marginal in chloride or reducing-acid service, and the extra alloy shows up in price and availability.
-
What heat treatment does ASTM A312 TP317 require?
- TP317 is supplied solution annealed at the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, because UNS S31700 is not listed individually in Table 2. It is not an H grade, so there is no Table 5 grain-size requirement, and the MTC should record the temperature and cooling method actually used.
-
Which filler metal is used to weld ASTM A312 TP317 pipe?
- Table 6 lists TP317, but the filler-class pairing is not clearly populated in the edition extract we work from, so the consumable is agreed on the WPS; ER317-type wire is common industry practice and is recorded here as a project decision, not as a Table 6 mandate. Qualify the procedure on actual TP317 base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
-
What sizes of ASTM A312 TP317 pipe can SHH STEEL supply?
- We quote TP317 in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
-
Is ASTM A312 TP317 an H grade for high-temperature service?
- No. TP317 is not one of the A312 H grades, so there is no Table 5 grain-size requirement and no special Table 2 row; the default 1900 °F [1040 °C] minimum anneal with rapid cooling applies. Carbon up to 0.08% gives some elevated-temperature strength, but creep-governed designs normally use a true H grade such as TP316H with code allowables confirmed for that UNS number.
-
Why is TP317 pipe harder to find than TP316?
- Demand for 317 chemistry is much smaller than for 316, so fewer mills hold the higher-molybdenum heats and many roll only TP317L. That means heavier walls and larger NPS are often mill-order rather than stock. Allowing dual TP317/TP317L certification on the purchase order, and giving the need date early, are the two most practical ways to shorten lead time without compromising the Mo band.
-
What certificates come with ASTM A312 TP317 pipe from SHH STEEL?
- Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP317 it should show molybdenum inside 3.0–4.0% on every heat, together with the 18.0–20.0% Cr and 11.0–15.0% Ni bands. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.
Conclusion
ASTM A312 TP317 / UNS S31700 is defined by C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0% and Mo 3.0–4.0%, a Table 4 floor of 75/30 ksi, and the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, because UNS S31700 is not listed individually in Table 2. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.