ASTM A312 TP348 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 TP348 Stainless Steel Pipe

ASTM A312 TP348 / UNS S34800 stainless steel pipe in SML, WLD and HCW, with C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 10×C with a 1.00% ceiling (footnote G) and Ta ≤0.10%, a 75/30 ksi Table 4 floor and ER347 filler guidance, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP348 / UNS S34800
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP348 Stainless Steel Pipe

ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP348 / UNS S34800, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.

TP348 is the niobium-stabilized sister of TP347 with one extra control: a tantalum ceiling of 0.10%. It shares the footnote G rule of Nb at least 10×C with a 1.00% ceiling, carbon at 0.08% maximum, chromium at 17.0–19.0% and nickel at 9.0–13.0%, with no molybdenum or nitrogen requirement. Tantalum normally travels with niobium in the raw material, and the explicit limit exists because some nuclear and specialty specifications want that residual controlled on the heat. Table 4 releases TP348 at 75 ksi [515 MPa] / 30 ksi [205 MPa], and because it is not an H grade the default 1900 °F [1040 °C] anneal applies.

SHH STEEL can supply ASTM A312 TP348 stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP348.

Market names include 348 stainless pipe, S34800 and “Ta-controlled 347”. The last label is the useful one, because it tells you what to check: everything TP347 needs plus a tantalum result at or below 0.10%. Some edition extracts show the Nb cell for TP348 as an ellipsis with Ta listed separately; we read Nb through footnote G together with the Ta ceiling, and the ordered edition should be checked if your inspector reads it differently.

Within the ASTM A312 series, buyers comparing TP348 usually look next at A312 TP347, A312 TP348H, A312 TP347LN and A312 TP321. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 recognises three manufacturing routes for TP348 pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 10×C with a 1.00% ceiling (footnote G) and Ta ≤0.10%, and every length must be heat treated before release. For TP348 the Table 4 row is the same for every route, but the strip or billet heat must report tantalum as well as niobium, so ask which heat feeds which route.

  • Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
  • Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.

Chemical Composition of ASTM A312 TP348

Two chemistry layers matter for ASTM A312 TP348. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.

Element TP348 / UNS S34800 melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) No requirement (…)
Niobium (Nb) ≥ 10 × C and ≤ 1.00% (footnote G)
Tantalum (Ta) ≤ 0.10
Nitrogen (N) No requirement (…)

Read the table as maxima unless a range is shown. The stabilizer rule for TP348 (Nb ≥10×C, ≤1.00% with Ta ≤0.10%) is not a fixed number; it moves with the actual chemistry of each heat. At C = 0.05%, niobium must be at least 0.50% and no more than 1.00%, and tantalum must separately stay at or below 0.10%. That is why the MTC has to report carbon, niobium and tantalum on the same heat, so both the Nb ≥10×C rule and the Ta ≤0.10% ceiling can be checked.

When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP348 without having to rebuild the arithmetic themselves.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.10 under / 0.15 over 8.90 – 13.15
Niobium (Nb) ≥ 10 × C, ≤ 1.00 0.05 under / over on applicable limit Per heat calculation
Tantalum (Ta) ≤ 0.10 0.05 over ≤ 0.15

Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.

Mechanical Properties of ASTM A312 TP348

Room-temperature tensile requirements for ASTM A312 TP348 come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S34800, not from this product page or from a sister grade’s strength line.

Property TP348
Tensile, min 75 ksi [515 MPa]
Yield, min 30 ksi [205 MPa]
Elongation 35% L / 25% T

TP348 uses a single row regardless of route and wall, so welded and seamless pipe are accepted against the same floor. These are minimum release values, not typical mill results, and they should not be raised or lowered by habit from a sister grade.

Dimensions, Tolerances and Stock Sizes

Dimensional supply for ASTM A312 TP348 pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.

  • Lengths — single random, double random or cut-to-length as ordered
  • Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
  • Jointers — not permitted unless the purchase order allows them

Stock / Available sizes. SHH STEEL quotes TP348 against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP348 is mostly mill-order against a low-tantalum heat; the table shows the enquiry range, not floor stock. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.

Representative size (ASME B36.19) Example OD × wall Typical schedules / notes
NPS 1/2 21.3 mm × 2.77 mm (Sch 40S) Sch 10S / 40S / 80S; instrument and small-bore take-offs
NPS 2 60.3 mm × 3.91 mm (Sch 40S) Sch 10S / 40S / 80S; common process branch size
NPS 4 114.3 mm × 6.02 mm (Sch 40S) Sch 10S / 40S / 80S; frequent stock and mill enquiry size
NPS 6 168.3 mm × 7.11 mm (Sch 40S) Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry
NPS 8 – 12 219.1 mm × 8.18 mm (NPS 8 Sch 40S) Sch 10S / 40S; route and wall decide stock vs mill-order
NPS 14 – 24 Per B36.19 for the ordered schedule Sch 10S / 40S; usually mill-order, often welded
Special OD × wall By agreement State OD, wall (nominal or minimum) and length practice

Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.

Equivalent Grades

Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP348, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.

Designation Notes
ASTM A312 TP348 / UNS S34800 Governing product specification on this page
ASME SA-312 TP348 / S34800 Separate Code Book standard; dual-mark only when the PO names both
TP347 / UNS S34700 Same chemistry without the Ta ≤0.10% ceiling
TP348H / UNS S34809 H grade: C 0.04–0.10%, Nb ≥8×C, Ta ≤0.10%, grain size No. 7 or coarser

We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.

Heat Treatment and Delivery Condition

All A312 pipe is furnished heat treated. TP348 is not an H grade, so it receives the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, since TP348 has no individual Table 2 row. There is no Table 5 grain-size mandate and no clause 6.2 reheat rule, and HCW cold reduction is completed before the final anneal so delivery remains the annealed condition. Supplementary requirement S6 adds a stabilization treatment at an agreed temperature below the solution anneal only when the purchase order invokes it.

Delivery is normally solution annealed and pickled unless the order asks for bright annealing or another finish. The MTC should record the anneal temperature and cooling method actually used, and fabricators who hot form or heavily cold work TP348 bends should re-anneal to the same practice where the governing code requires it, rather than applying a neighbouring grade’s anneal by habit.

Corrosion Resistance

ASTM A312 has no corrosion table, so this is engineering commentary. In general corrosion and intergranular resistance, TP348 behaves like TP347: niobium ties up carbon so welded joints and sensitizing-range service do not leave chromium-depleted grain boundaries. The tantalum ceiling is not a corrosion feature; it is a composition control requested by specifications where tantalum residuals matter, which is why TP348 appears mainly in nuclear and specialty projects.

If the project does not name TP348 or a tantalum limit, A312 TP347 usually does the same corrosion job with far better availability. As with every stabilized 18-10 grade, molybdenum is absent, so chloride pitting cases point elsewhere, and intergranular tests apply only when the order lists them.

Applications of ASTM A312 TP348 Pipe

Applications for ASTM A312 TP348 follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S34800 at the design temperature before final wall selection.

Application area Typical use of TP348 pipe Selection note
Welded process lines Lines exposed to the sensitizing range during welding or service Prove the stabilizer rule on the MTC
Exhaust, expansion-joint and heater piping Intermittent elevated-temperature duty without H-grade creep design Use TP348H when the design is creep-governed
Chemical and refining utility Oxidizing or mildly corrosive service specified with stabilized 18–10 chemistry Prefer Mo grades if chlorides dominate
Code piping packages Dual A312/SA-312 projects with heat traceability Name edition, route, and UNS on the enquiry

TP348 is a specification-driven grade: buyers order it because a project document calls for the Ta ceiling, not because it outperforms TP347 in general service. Plants that run TP348H or TP347 alongside it should keep heats segregated, since the stencils look similar and only the certificate shows the tantalum result.

Weldability

For filler selection, Table 6 maps TP348 to ER347. Qualify the WPS and PQR on actual TP348 base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.

TP348 welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. Stabilization lowers HAZ sensitization risk compared with unstabilized 18-8, but low heat input and controlled interpass remain good practice. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.

Surface Finishes

Surface condition for ASTM A312 TP348 pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.

  • Annealed and pickled — the usual delivery for process piping after solution treatment
  • Bright annealed — by agreement for selected sizes and routes
  • Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
  • Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed

Inspection and Testing

The base acceptance package for ASTM A312 TP348 pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show carbon, niobium and tantalum on the same heat, so both the Nb ≥10×C rule and the Ta ≤0.10% ceiling can be checked.

Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S6 stabilization Stabilizing heat treatment at an agreed temperature
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall read as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.

Packaging and Shipping

Export and domestic shipments of ASTM A312 TP348 pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP348 / UNS S34800, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.

  • Ends capped or bevel-protected as ordered
  • Bundles strapped with protected contact points to limit iron pickup
  • Waterproof wrapping for ocean freight when specified
  • Packing list with heat numbers, sizes and certificate references

We keep TP348 physically segregated from TP347-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP348 we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.

  • Grade control — carbon, niobium and tantalum on the same heat, so both the Nb ≥10×C rule and the Ta ≤0.10% ceiling can be checked stated on the MTC
  • Honest sister-grade advice when TP347 or TP348H would fit the service better
  • Filler guidance for WPS planning: ER347
  • SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
  • Dual A312/SA-312 marking only when the purchase order asks for both
  • Cut lengths, bevelling and project marking coordinated on confirmed orders

If you are still choosing between TP348 and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.

Supply Capability

SHH STEEL can supply ASTM A312 TP348 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.

Item SHH STEEL capability for TP348
Standard ASTM A312 / A312M TP348 / UNS S34800
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL or cut-to-length
Finish Annealed and pickled; bright annealed or polished by agreement
Filler guidance ER347
Testing Tension (75/30 ksi), flattening/bend, hydro or NDE per length; supplementary tests on order
Documents EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes. Representative stock and mill-enquiry sizes for TP348 are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.

Enquiries should state the A312 edition, TP348 (UNS S34800), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.

FAQ

Is ASTM A312 TP348 the same as ASME SA-312 TP348?
They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP348 chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
What is the chemical composition of ASTM A312 TP348 pipe?
Table 1 sets C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 10×C with a 1.00% ceiling (footnote G) and Ta ≤0.10%. These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
What are the mechanical properties of ASTM A312 TP348?
Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum with 35% longitudinal / 25% transverse elongation. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S34800. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
What is the difference between ASTM A312 TP348 and TP347?
Chemistry is the same apart from tantalum. Both have C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–13.0% and Nb at least 10×C up to 1.00%, with the same 75/30 ksi floor, 1900 °F anneal and ER347 filler. TP348 adds a Ta ≤0.10% ceiling, which nuclear and specialty specifications use to control tantalum residuals. A TP347 heat qualifies as TP348 only if tantalum is reported and within limit.
Why does TP348 limit tantalum to 0.10%?
Tantalum is chemically similar to niobium and is often present in niobium additions. Some nuclear specifications want that residual controlled, so A312 provides TP348 with an explicit Ta ≤0.10% ceiling. For ordinary process plants the limit has no practical effect, which is why TP347 is far more common. When the project calls for TP348, the MTC must show the measured Ta value.
What heat treatment does ASTM A312 TP348 require?
TP348 is supplied solution annealed at the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, since TP348 has no individual Table 2 row. It is not an H grade, so there is no Table 5 grain-size requirement, and the MTC should record the temperature and cooling method actually used.
Which filler metal is used to weld ASTM A312 TP348 pipe?
Table 6 maps TP348 to ER347. Qualify the procedure on actual TP348 base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
What sizes of ASTM A312 TP348 pipe can SHH STEEL supply?
We quote TP348 in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
Is TP348 pipe readily available from stock?
Less so than TP347. Because demand is concentrated in nuclear and specialty work, most TP348 orders are mill-order with a heat chosen for low tantalum, and lead times reflect that. Selected common sizes may occasionally be available from qualified heats. Send the full size list, the edition and any project inspection requirements early so we can confirm what is practical.
Can TP348 be dual-certified with TP347?
In principle a heat that meets TP347 and also reports Ta ≤0.10% satisfies both Table 1 rows, since the other limits, tensile floor and anneal are the same. Dual certification should be requested on the purchase order so the MTC and stencil carry both grades. It is a convenient way to cover mixed datasheets, provided the tantalum result is actually on the certificate.
What certificates come with ASTM A312 TP348 pipe from SHH STEEL?
Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP348 it should show carbon, niobium and tantalum on the same heat, so both the Nb ≥10×C rule and the Ta ≤0.10% ceiling can be checked. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.

Conclusion

ASTM A312 TP348 / UNS S34800 is defined by C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 10×C with a 1.00% ceiling (footnote G) and Ta ≤0.10%, a Table 4 floor of 75/30 ksi, and the default 1900 °F [1040 °C] minimum solution anneal followed by rapid cooling, since TP348 has no individual Table 2 row. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X