ASTM A312 TP348H Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 TP348H Stainless Steel Pipe

ASTM A312 TP348H / UNS S34809 stainless steel pipe in SML, WLD and HCW, with C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 8×C with a 1.0% ceiling (footnote H) and Ta ≤0.10%, a 75/30 ksi Table 4 floor, Table 5 grain size No. 7 or coarser and ER347 filler guidance, supplied by SHH STEEL with EN 10204 3.1 MTCs.
Grade
TP348H / UNS S34809
Standard
ASTM A312 / A312M
Product form
Seamless (SML), welded (WLD), and heavily cold-worked (HCW) stainless steel pipe
Outside diameter
ASME B36.19 schedules (commonly Sch 5S / 10S / 40S / 80S) and special OD/wall by agreement; typical NPS from 1/8 upward (confirm on enquiry)
Share:
Overview
Manufacturing Types
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A312 TP348H Stainless Steel Pipe

ASTM A312/A312M is the ASTM product specification for seamless, welded and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as a standard; ASME SA-312 is a separate Code Book specification with related text, and the two should not be treated as interchangeable titles on a purchase order. This page is written against A312/A312M for grade TP348H / UNS S34809, with every chemistry, tensile and tolerance figure taken from the referenced A312/A312M tables rather than from catalogue sheets.

TP348H is the elevated-temperature sister of TP348. It keeps the explicit Ta ≤0.10% ceiling and adds the H package: a 0.04–0.10% carbon band, niobium at least 8×C with a 1.0% ceiling under footnote H, Table 5 grain size No. 7 or coarser, and Table 2 anneals of 2000 °F [1100 °C] cold-finished and 1925 °F [1050 °C] hot-finished, with the clause 6.2 reheat and lot-marking rules. Chromium is 17.0–19.0% and nickel 9.0–13.0%, with no molybdenum requirement. Clause 1.2 groups TP348H with the other A312 H grades intended for temperatures where creep and stress-rupture properties matter, and Table 4 releases it at 75/30 ksi.

SHH STEEL can supply ASTM A312 TP348H stainless steel pipe as seamless (SML), welded (WLD) or heavily cold-worked (HCW) product, in ASME B36.19 schedules and in special OD and wall combinations by agreement. EN 10204 3.1 mill test certificates are standard, and third-party 3.2 inspection is arranged when the enquiry names an agency. Dual A312/SA-312 marking is offered only when the purchase order names both standards and the heat qualifies under each; for the separately published ASME page on this grade, see SA312 TP348H.

Commercial names include 348H stainless pipe, S34809 and “Ta-controlled 347H”. The certificate has to carry more evidence than most grades: carbon in band, niobium against 8×C, a measured tantalum value, the grain-size number and the Table 2 anneal temperature. Whether every edition lists Ta in a separate column next to Nb is not fully confirmed in our extract, so check the ordered edition’s Table 1 layout with your inspector.

Within the ASTM A312 series, buyers comparing TP348H usually look next at A312 TP348, A312 TP347H, A312 TP321H and A312 TP347LN. The full grade list sits on the A312/A312M hub, which is the quickest place to check neighbouring chemistries when a datasheet leaves more than one option open.

Manufacturing Types (SML / WLD / HCW)

ASTM A312 recognises three manufacturing routes for TP348H pipe, and the choice is a purchase-order decision driven by the design code, size, wall thickness and how the owner wants the pipe inspected. The route never changes the chemistry: every heat must still meet C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 8×C with a 1.0% ceiling (footnote H) and Ta ≤0.10%, and every length must be heat treated before release. For TP348H the Table 4 row is the same for every route, but the strip or billet heat must report tantalum as well as niobium, so ask which heat feeds which route. Because this is an H grade, the H anneal and grain-size evidence must belong to the finished pipe, whichever route produced it.

  • Seamless (SML) — no welding at any stage; preferred for high pressure, thick walls and owners who exclude welded pipe from the piping class.
  • Welded (WLD) — automatic welding without filler metal, finished so the pipe meets dimensional and mechanical requirements after final heat treatment; ask for the coil or plate heat number on the certificate.
  • Heavily cold-worked (HCW) — welded pipe cold worked at least 35% in wall and weld before the final anneal, again without filler; ordered when the project wants that specific marking and process control.

Every finished length is hydrostatically tested or nondestructively electrically tested, and the mill may choose the method unless the purchase order fixes one. When comparing seamless and welded offers, check the route and the hydro or NDE method on the certificate, not only the grade stamp, so that the test plan matches what the piping class actually requires.

Chemical Composition of ASTM A312 TP348H

Two chemistry layers matter for ASTM A312 TP348H. The melting (heat or ladle) analysis in Table 1 is mandatory for every heat, while product analysis on finished pipe applies only when Supplementary Requirement S1 or the purchase order asks for it, using the ASTM A480/A480M Table A1.1 tolerances referenced through A999/A999M. The table below gives the Table 1 melting limits that the mill must report on the certificate.

Element TP348H / UNS S34809 melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) No requirement (…)
Niobium (Nb) ≥ 8 × C and ≤ 1.0% (footnote H)
Tantalum (Ta) ≤ 0.10
Nitrogen (N) No requirement (…)

Read the table as maxima unless a range is shown. The stabilizer rule for TP348H (Nb ≥8×C, ≤1.0% with Ta ≤0.10%) is not a fixed number; it moves with the actual chemistry of each heat. At C = 0.08%, niobium must be at least 0.64%, at C = 0.10% at least 0.80%, and tantalum must stay at or below 0.10% throughout. That is why the MTC has to report the 0.04–0.10% carbon band, niobium against 8×C, tantalum at or below 0.10% and the measured Table 5 grain size.

When product analysis is ordered, finished-pipe chemistry is judged against Table 1 widened by the A480 tolerances. The next table pairs each Table 1 limit with its tolerance and the resulting product-analysis bound, so receiving inspectors can clear a check analysis on TP348H without having to rebuild the arithmetic themselves.

Element Melting (Table 1) Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.10 under / 0.15 over 8.90 – 13.15
Niobium (Nb) ≥ 8 × C, ≤ 1.0 0.05 under / over on applicable limit Per heat calculation
Tantalum (Ta) ≤ 0.10 0.05 over ≤ 0.15

Product analysis is not automatic under ASTM A312: if your client inspector expects check analyses on finished lengths, order S1 explicitly. A product result inside the widened bound but outside Table 1 is acceptable as a check analysis; it does not mean the heat analysis itself may drift, and SHH STEEL reports actual ladle values rather than unpublished tighter windows.

Mechanical Properties of ASTM A312 TP348H

Room-temperature tensile requirements for ASTM A312 TP348H come from Table 4 and are summarised below. They are the minimum release values for the lot; actual certificate values are usually higher, but design allowables still come from the applicable code for UNS S34809, not from this product page or from a sister grade’s strength line.

Property TP348H
Tensile, min 75 ksi [515 MPa]
Yield, min 30 ksi [205 MPa]
Elongation 35% L / 25% T
Grain size (Table 5) No. 7 or coarser

TP348H uses a single row regardless of route and wall, so welded and seamless pipe are accepted against the same floor. These are minimum release values, not typical mill results, and they should not be raised or lowered by habit from a sister grade. The Table 5 grain size of ASTM No. 7 or coarser travels with the tensile results; ask for the measured number on the MTC rather than a bare “complies”.

Dimensions, Tolerances and Stock Sizes

Dimensional supply for ASTM A312 TP348H pipe follows ASME B36.19 schedules for the common NPS and schedule combinations, with special OD and wall available by agreement when a project needs a section the schedules do not cover. Outside-diameter variations follow ASTM A999/A999M, and wall-thickness variations follow A312 Table 3, summarised below with t/D meaning specified wall divided by ordered OD.

NPS designator Wall over Wall under
1/8 to 2-1/2 incl., all t/D 20.0% 12.5%
3 to 18 incl., t/D up to 5% 22.5% 12.5%
3 to 18 incl., t/D over 5% 15.0% 12.5%
20 and larger, welded, all t/D 17.5% 12.5%
20 and larger, seamless, t/D up to 5% 22.5% 12.5%
20 and larger, seamless, t/D over 5% 15.0% 12.5%

Reading the table, the 12.5% under-tolerance is constant while the over-tolerance depends on NPS, t/D and, above NPS 20, on whether the pipe is welded or seamless. State on the purchase order whether wall is nominal or minimum (Supplementary S8), because the two readings produce different pipe from the same size line, and recheck pressure design after under-tolerance on light Sch 10S walls.

  • Lengths — single random, double random or cut-to-length as ordered
  • Ends — plain or bevelled; confirm bevel angle and root face when the WPS is already frozen
  • Jointers — not permitted unless the purchase order allows them

Stock / Available sizes. SHH STEEL quotes TP348H against a practical stock-and-mill enquiry range rather than a frozen SKU list. The representative sizes below, with example OD × wall figures from ASME B36.19, are the combinations we most often discuss for this grade. TP348H is almost always mill-order; the table shows the range we quote, not sizes on the floor. Availability by route and exact wall is confirmed on enquiry, and we do not publish tonnages against individual lines.

Representative size (ASME B36.19) Example OD × wall Typical schedules / notes
NPS 1/2 21.3 mm × 2.77 mm (Sch 40S) Sch 10S / 40S / 80S; instrument and small-bore take-offs
NPS 2 60.3 mm × 3.91 mm (Sch 40S) Sch 10S / 40S / 80S; common process branch size
NPS 4 114.3 mm × 6.02 mm (Sch 40S) Sch 10S / 40S / 80S; frequent stock and mill enquiry size
NPS 6 168.3 mm × 7.11 mm (Sch 40S) Sch 10S / 40S / 80S; confirm SML vs WLD on enquiry
NPS 8 – 12 219.1 mm × 8.18 mm (NPS 8 Sch 40S) Sch 10S / 40S; route and wall decide stock vs mill-order
NPS 14 – 24 Per B36.19 for the ordered schedule Sch 10S / 40S; usually mill-order, often welded
Special OD × wall By agreement State OD, wall (nominal or minimum) and length practice

Read the table as a guide to where enquiries usually land, not a promise that every size is on the floor; special OD × wall, non-standard lengths and mixed SML/WLD packages are routine on enquiry.

Equivalent Grades

Equivalent designations help sourcing, but they do not replace the ASTM A312 grade line on the purchase order. The table below lists the primary ASTM identity for TP348H, the separately published ASME specification, and the sister grades buyers most often confuse with it on enquiries.

Designation Notes
ASTM A312 TP348H / UNS S34809 Governing product specification on this page
ASME SA-312 TP348H / S34809 Separate Code Book standard; dual-mark only when the PO names both
TP348 / UNS S34800 Standard-carbon sister; C ≤0.08%, Nb ≥10×C, Ta ≤0.10%
TP347H / UNS S34709 Same H package without the Ta ceiling

We deliberately do not list an EN or JIS number for this grade here, because ASTM A312 does not define one and near-equivalents rarely match every Table 1 limit; treat any cross-standard equivalence as an engineering decision against both specifications. Within A312 itself, sister grades each have their own Table 1 and Table 4 rows, so a shared market label is never a reason to swap one for another without the datasheet owner agreeing.

Heat Treatment and Delivery Condition

All A312 pipe is furnished heat treated. For TP348H, Table 2 sets 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. Those temperatures are above the 1900 °F default used for the standard-carbon sister because the anneal also has to develop the coarse grain that Table 5 requires, and the clause 6.2 reheat rules and lot marking apply whenever pipe is reheated after the qualifying anneal.

Supplementary requirement S6, a stabilization heat treatment at an agreed temperature below the solution anneal, applies only when the purchase order specifies it; if it is ordered, agree the temperature at enquiry and confirm it on the MTC. Delivery is normally solution annealed and pickled, and the certificate should record the anneal temperature, the cooling method and whether the pipe was cold- or hot-finished, since that decides which Table 2 minimum applies.

Corrosion Resistance

ASTM A312 has no corrosion table, so this is engineering commentary. TP348H behaves like TP347H in service: niobium stabilization resists sensitization after welding, and the H package supports creep strength in hot steam and process lines. The tantalum ceiling is a composition control demanded mainly by nuclear and specialty specifications, not a feature that improves corrosion or strength.

If the project does not call for a Ta limit, A312 TP347H does the same elevated-temperature job with much wider availability. Do not substitute TP348 into a TP348H line, because the lower carbon and lack of grain-size control change the creep basis. S6 stabilization is available by agreement but is never assumed.

Applications of ASTM A312 TP348H Pipe

Applications for ASTM A312 TP348H follow directly from its chemistry and heat-treatment package. The table below summarises where buyers typically place the grade and what to check before freezing the order; always confirm code allowables for UNS S34809 at the design temperature before final wall selection.

Application area Typical use of TP348H pipe Selection note
Superheater and reheater piping Elevated-temperature steam lines where creep strength is in the design basis Confirm grain size and Table 2 anneal on the MTC
Refinery heater and hydroprocessing lines Hot hydrocarbon service with welded joints Check allowable stresses for UNS S34809 at design temperature
Petrochemical furnace outlets Transfer and header piping in the creep range Agree S6 at enquiry if the licensor requires it
Code piping packages Dual A312/SA-312 projects with heat traceability Name edition, route, and UNS on the enquiry

TP348H is a specification-driven grade: it is ordered because a project calls for the Ta ceiling together with H-grade creep properties. Keep TP348H, TP347H and TP348 heats segregated through fabrication, since only the certificate distinguishes them, and confirm allowable stresses for UNS S34809 at design temperature before final wall selection.

Weldability

For filler selection, Table 6 maps TP348H to ER347. Qualify the WPS and PQR on actual TP348H base metal and freeze the consumable before production welds. Mill longitudinal welds on WLD and HCW pipe are made without filler metal, so Table 6 guidance applies to fabrication joints, not to the mill seam.

TP348H welds readily by GTAW for roots and thin walls, GMAW for productive fill passes and SMAW for field girth welds, with orbital GTAW common on repetitive high-integrity joints. For H-grade service, match the consumable’s carbon to the creep design and avoid low-carbon wire that would weaken the joint at temperature. Girth-weld NDE and cleanliness follow the fabrication code, such as ASME B31 and Section IX, which A312 does not rewrite.

Surface Finishes

Surface condition for ASTM A312 TP348H pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, embedded free iron, residual scale and chloride contamination from handling can matter as much as the nominal finish name, especially on aqueous and clean-process lines.

  • Annealed and pickled — the usual delivery for process piping after solution treatment
  • Bright annealed — by agreement for selected sizes and routes
  • Mechanically polished OD/ID — grit or Ra target by agreement; polishing does not replace annealing
  • Bead-finished welded OD — weld bead rolled or ground flush on WLD/HCW pipe as agreed

Inspection and Testing

The base acceptance package for ASTM A312 TP348H pipe combines heat analysis against Table 1, Table 4 tension tests, flattening or bend tests per route and size, heat-treatment evidence, and a hydrostatic or nondestructive electric test on every length. For this grade the certificate should show the 0.04–0.10% carbon band, niobium against 8×C, tantalum at or below 0.10% and the measured Table 5 grain size, on the same line items as the tensile results.

Supplementary requirements are optional until written on the order. The options buyers request most often for this grade are summarised below, and each one should be priced and scheduled at enquiry rather than added after the pipe is rolled.

Option Purpose
S1 product analysis Confirms chemistry on finished pipe
S5 radiography Weld integrity on WLD pipe
S6 stabilization Stabilizing heat treatment at an agreed temperature
S7 intergranular corrosion A262 Practice E after sensitizing treatment
S8 minimum wall Wall read as minimum rather than nominal
S9 weld decay Compares weld and base-metal loss rates

EN 10204 3.1 certification is our standard document set, and 3.2 third-party witness by an agency such as SGS, Bureau Veritas or TÜV is arranged when the enquiry names it and its hold points. Hydrostatic versus NDE selection also belongs on the PO.

Packaging and Shipping

Export and domestic shipments of ASTM A312 TP348H pipe are packed for handling and for ocean or land transport. Each length is marked with ASTM A312 (and SA-312 only when dual-certified), TP348H / UNS S34809, the route, size and heat number, and bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.

  • Ends capped or bevel-protected as ordered
  • Bundles strapped with protected contact points to limit iron pickup
  • Waterproof wrapping for ocean freight when specified
  • Packing list with heat numbers, sizes and certificate references

We keep TP348H physically segregated from TP347-family heats in the yard and on the packing list, because stencils look alike and mix-ups are expensive once pipe is cut.

Why Choose SHH STEEL

SHH STEEL supplies specification-driven stainless pipe and plate, and for ASTM A312 TP348H we quote against the edition you name rather than a generic catalogue sheet. We report full Table 1 chemistry, Table 4 results and heat-treatment evidence, keep heat identity unbroken from melt to finished length, and match route and size to the enquiry instead of pushing a one-size stock answer.

  • Grade control — the 0.04–0.10% carbon band, niobium against 8×C, tantalum at or below 0.10% and the measured Table 5 grain size stated on the MTC
  • Honest sister-grade advice when TP348 or TP347H would fit the service better
  • Filler guidance for WPS planning: ER347
  • SML, WLD and HCW routes with EN 10204 3.1 MTCs; 3.2 inspection on request
  • Dual A312/SA-312 marking only when the purchase order asks for both
  • Cut lengths, bevelling and project marking coordinated on confirmed orders

If you are still choosing between TP348H and its sister grades, send the design temperature, the medium, the welded or seamless preference and any project chemistry limits. We would rather tell you that a more available grade does the job than sell you a harder-to-source heat you do not need, and that conversation is cheapest before the purchase order is frozen.

Supply Capability

SHH STEEL can supply ASTM A312 TP348H stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarises the routes, sizes, finishes, tests and documents we regularly quote for this grade,.

Item SHH STEEL capability for TP348H
Standard ASTM A312 / A312M TP348H / UNS S34809
Manufacturing types SML, WLD, HCW
Size NPS 1/8 and up per ASME B36.19; special OD/wall by agreement
Schedules 5S, 10S, 40S, 80S and non-standard walls
Length SRL, DRL or cut-to-length
Finish Annealed and pickled; bright annealed or polished by agreement
Filler guidance ER347
Testing Tension (75/30 ksi), Table 5 grain size No. 7 or coarser, flattening/bend, hydro or NDE per length; supplementary tests on order
Documents EN 10204 3.1 with full Table 1 chemistry; 3.2 / third-party inspection on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes. Representative stock and mill-enquiry sizes for TP348H are listed in the Dimensions section, typically NPS 1/2–24 in Sch 10S/40S/80S with example OD × wall figures per ASME B36.19. Selected common combinations may ship from stock, while heavy-wall seamless, unusual schedules and special cut lengths are normally mill-order. We do not invent warehouse SKUs or tonnages, so ask for a live check against your size list.

Enquiries should state the A312 edition, TP348H (UNS S34809), SML/WLD/HCW, NPS or OD × wall with nominal or minimum wall, length practice, finish, and any product-analysis, corrosion-test or 3.2 requirements, so mill slots line up with your need date. Dual SA-312 marking, cut lengths, bevelling and packing-list marking are available on confirmed orders.

FAQ

Is ASTM A312 TP348H the same as ASME SA-312 TP348H?
They are two independent standards. ASTM A312/A312M is the ASTM product specification, while ASME SA-312 is the Code Book specification used for ASME-stamped work. For a referenced edition the TP348H chemistry and tensile rows are technically aligned, but a purchase order should name the standard it needs, and dual A312/SA-312 marking is available only when both are written on the order and the heat qualifies under each.
What is the chemical composition of ASTM A312 TP348H pipe?
Table 1 sets C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 8×C with a 1.0% ceiling (footnote H) and Ta ≤0.10%. These are heat-analysis limits that the mill must report for every heat. If product analysis is ordered under S1, finished pipe is judged against Table 1 widened by the ASTM A480 Table A1.1 tolerances shown in the chemistry section of this page.
What are the mechanical properties of ASTM A312 TP348H?
Table 4 requires 75 ksi [515 MPa] tensile and 30 ksi [205 MPa] yield minimum with 35% longitudinal / 25% transverse elongation, plus grain size ASTM No. 7 or coarser. These are minimum release values; mill results are usually higher, but design allowables come from the governing code for UNS S34809. Hardness is not separately mandated by Table 4, so state a limit on the order if fabrication needs one.
What is the difference between ASTM A312 TP348H and TP347H?
They share the 0.04–0.10% carbon band, Nb ≥8×C with a 1.0% cap, Cr 17.0–19.0%, Ni 9.0–13.0%, Table 5 grain size, Table 2 anneals and the 75/30 ksi floor. TP348H adds a Ta ≤0.10% ceiling, which nuclear and specialty specifications use to control tantalum residuals. Without that requirement in the project documents, TP347H is normally the more available and economical choice.
What is the difference between ASTM A312 TP348H and TP348?
TP348 caps carbon at 0.08% and needs Nb at least 10×C, with the default 1900 °F anneal and no grain-size rule. TP348H uses a 0.04–0.10% carbon band, an 8×C niobium rule, Table 5 grain size No. 7 or coarser and anneals of 2000 °F cold-finished or 1925 °F hot-finished. Both keep Ta ≤0.10%, ER347 filler and the 75/30 ksi floor.
What heat treatment does ASTM A312 TP348H require?
TP348H is supplied solution annealed at 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. As an H grade it must also meet Table 5 grain size No. 7 or coarser and the clause 6.2 reheat and lot-marking rules, and S6 stabilization is added only when ordered.
Which filler metal is used to weld ASTM A312 TP348H pipe?
Table 6 maps TP348H to ER347. Qualify the procedure on actual TP348H base metal and freeze the classification on the WPS and PQR before production. The mill seam on WLD and HCW pipe is made without filler, so this guidance applies to fabrication joints only.
What sizes of ASTM A312 TP348H pipe can SHH STEEL supply?
We quote TP348H in ASME B36.19 sizes from NPS 1/8 upward, most often NPS 1/2–24 in Sch 10S, 40S and 80S, for example 114.3 mm × 6.02 mm for NPS 4 Sch 40S, plus special OD × wall by agreement. Selected common sizes may ship from stock, and heavy walls or unusual schedules are usually mill-order, confirmed on enquiry.
How much niobium does a TP348H heat need?
Niobium must be at least eight times the carbon and no more than 1.0%. At C = 0.08% that means at least 0.64% Nb, and at the top of the band, C = 0.10%, at least 0.80%. Tantalum must separately stay at or below 0.10%. All three values belong on the MTC, because without them neither footnote H nor the tantalum ceiling can be verified.
Is TP348H pipe a stock item?
Rarely. TP348H combines H-grade heat treatment with a tantalum ceiling, and demand comes mostly from nuclear and specialty projects, so most orders are mill-order against a qualified heat. Selected sizes may sometimes be available from existing qualified material. Give us the full size list, route, edition and inspection plan early, and we will confirm realistic lead times.
What certificates come with ASTM A312 TP348H pipe from SHH STEEL?
Every shipment carries an EN 10204 3.1 mill test certificate with full Table 1 heat chemistry, Table 4 tensile results, heat-treatment details and the hydro or NDE method. For TP348H it should show the 0.04–0.10% carbon band, niobium against 8×C, tantalum at or below 0.10% and the measured Table 5 grain size. Third-party 3.2 inspection and supplementary tests such as S1 or S7 are added when named on the order.

Conclusion

ASTM A312 TP348H / UNS S34809 is defined by C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb at least 8×C with a 1.0% ceiling (footnote H) and Ta ≤0.10%, a Table 4 floor of 75/30 ksi with grain size No. 7 or coarser, and 2000 °F [1100 °C] minimum for cold-finished pipe and 1925 °F [1050 °C] minimum for hot-finished pipe per Table 2, followed by rapid cooling. Order it by grade and UNS number rather than market shorthand, state the route, size, wall basis, finish and any supplementary tests, and keep the sister grades on their own datasheets. Treat ASME SA-312 as a separate standard that is added only when dual marking is genuinely required. For grade selection, stock checks or a quotation against your size list, browse the A312/A312M range or email SHH STEEL at admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X