ASTM A312 UNS S30815 Stainless Steel Pipe
What is ASTM A312 UNS S30815 Stainless Steel Pipe
A312/A312M is the ASTM product specification for seamless, welded, and heavily cold-worked austenitic stainless steel pipe intended for high-temperature and general corrosive service. It stands on its own as an ASTM standard, and this page is written against it. UNS S30815 is one of the less common rows in its Table 1, and that is exactly why buyers ask us to spell out what the specification actually fixes for this alloy and what is left to agreement between purchaser and mill.
UNS S30815 is the leading heat-resisting alloy among the UNS-only rows of A312. It builds on a 20.0–22.0% chromium, 10.0–12.0% nickel base with 1.40–2.00% silicon, 0.14–0.20% nitrogen, and 0.03–0.08% cerium, and carbon is held at 0.05–0.10% for creep strength. The result is an alloy designed for higher temperatures than S30415, with a Table 4 floor of 87 ksi tensile and 45 ksi yield, used where 309 and 310 types are the usual alternatives.
SHH STEEL can supply ASTM A312 UNS S30815 pipe as seamless (SML), welded (WLD), or heavily cold-worked (HCW) product, in ASME B36.19 stainless schedules or special OD and wall by agreement, with EN 10204 3.1 mill test certificates that report the full Table 1 heat analysis, the Table 4 tension results, and the heat-treatment record. Where a purchase order also asks for ASME SA-312 marking, dual marking can be offered on heats that qualify under both documents, but the ASTM grade remains the one this page describes.
Order it as ASTM A312 UNS S30815; it is very widely known by a producer trade name, and European enquiries may cite EN 1.4835, but both are cross-references only. The certificate has to show the cerium and nitrogen lines, which a 309 or 310 template will not include.
If UNS S30815 turns out not to be the right fit, the closest sister pages in the same ASTM series are A312 UNS S30415, A312 TP309S, A312 TP310S, A312 UNS S30615, and A312 TP304H. All A312 grades are collected on the A312/A312M hub, so a short list can be compared against one standard before the enquiry goes out.
Manufacturing Types (SML / WLD / HCW)
ASTM A312 allows three manufacturing routes for UNS S30815 pipe, and the route is a purchase-order decision rather than a property of the grade. Whichever route is chosen, the heat must still meet the same Table 1 limits (C 0.05–0.10%, Mn ≤0.80%, Si 1.40–2.00%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, and Ce 0.03–0.08%), the same Table 4 tension floor, and the same 1920 °F [1050 °C] minimum solution anneal (Table 2, listed with S31272) with rapid cooling heat-treatment requirement before any length is released.
- Seamless (SML) pierced and hot or cold finished, chosen for heavy wall, high pressure, or owner specifications that exclude a weld seam
- Welded (WLD) formed from flat-rolled product and welded without filler or with filler where the edition allows, economical in thinner walls and larger diameters
- Heavily cold-worked (HCW) welded pipe given at least 35% cold reduction of the weld and base metal before the final anneal, which refines the weld structure toward seamless behaviour
S30815 is produced by several mills, so seamless and welded pipe are both quoted regularly, but the Table 2 heat treatment and reheat rule mean that the mill’s anneal capability should be confirmed with the quotation. Tell us which route your design code or client specification accepts, because a quotation that leaves the route open forces the mill to choose and can create disputes at receiving inspection.
Chemical Composition of ASTM A312 UNS S30815
The melting analysis in Table 1 is what the heat must meet when it is cast, and it is the first table a reviewer should compare against the mill certificate. For UNS S30815 the defining limits are C 0.05–0.10%, Mn ≤0.80%, Si 1.40–2.00%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, and Ce 0.03–0.08%. The table below reproduces the Table 1 row as published, with elements carrying no requirement shown as such rather than filled with invented values.
| Element | UNS S30815 melting analysis |
|---|---|
| Carbon (C) | 0.05 – 0.10 |
| Manganese (Mn) | ≤ 0.80 |
| Phosphorus (P) | ≤ 0.040 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | 1.40 – 2.00 |
| Chromium (Cr) | 20.0 – 22.0 |
| Nickel (Ni) | 10.0 – 12.0 |
| Nitrogen (N) | 0.14 – 0.20 |
| Cerium (Ce) | 0.03 – 0.08 |
| Molybdenum (Mo) | … (no requirement) |
Chromium at 20.0–22.0% and silicon at 1.40–2.00% carry the oxidation resistance, cerium at 0.03–0.08% improves scale adhesion, and nitrogen at 0.14–0.20% with carbon at 0.05–0.10% gives creep strength. Manganese is held to 0.80% maximum, and all of these should be read off the certificate individually.
Product analysis is a separate check made on the finished pipe, and ASTM A312 refers it to the permitted variations in ASTM A480 Table A1.1. The second table adds those tolerances to the melt limits so you can see the band that a check analysis on the pipe is allowed to fall within when Supplementary Requirement S1 or an owner check is ordered.
| Element | Melting (Table 1) | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | 0.05 – 0.10 | 0.01 under / over | 0.04 – 0.11 |
| Manganese (Mn) | ≤ 0.80 | 0.03 over | ≤ 0.83 |
| Phosphorus (P) | ≤ 0.040 | 0.005 over | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | 1.40 – 2.00 | 0.10 under / over | 1.30 – 2.10 |
| Chromium (Cr) | 20.0 – 22.0 | 0.20 under / 0.25 over | 19.80 – 22.25 |
| Nickel (Ni) | 10.0 – 12.0 | 0.10 under / 0.15 over | 9.90 – 12.15 |
| Nitrogen (N) | 0.14 – 0.20 | 0.01 under / 0.02 over | 0.13 – 0.22 |
| Cerium (Ce) | 0.03 – 0.08 | Not listed in A480 Table A1.1 | Not established—by agreement |
Read the product limits as acceptance bounds for a check analysis only. A heat that sits outside the Table 1 melt range is non-conforming even if a later product analysis lands inside the widened band, so the certificate should always show the ladle analysis first. Cerium has no row in A480 Table A1.1, so a product tolerance for it is not established and any check limit is by agreement.
Since S30815 is the natural step up from S30415, the next table places the two Table 1 rows side by side.
| Element | S30415 | S30815 |
|---|---|---|
| C | 0.04 – 0.06 | 0.05 – 0.10 |
| Mn | ≤ 0.80 | ≤ 0.80 |
| P | ≤ 0.045 | ≤ 0.040 |
| Si | 1.00 – 2.00 | 1.40 – 2.00 |
| Cr | 18.0 – 19.0 | 20.0 – 22.0 |
| Ni | 9.0 – 10.0 | 10.0 – 12.0 |
| N | 0.12 – 0.18 | 0.14 – 0.20 |
| Ce | 0.03 – 0.08 | 0.03 – 0.08 |
Mechanical Properties of ASTM A312 UNS S30815
Table 4 sets the room-temperature tension requirements for UNS S30815: 87 ksi [600 MPa] tensile strength and 45 ksi [310 MPa] yield strength minimum, with elongation of 35% longitudinal / 25% transverse minimum. The table below shows those values in the form used on the specification, and the mill certificate should report actual results against each line.
| Property (Table 4) | UNS S30815 |
|---|---|
| Tensile strength, min | 87 ksi [600 MPa] |
| Yield strength (0.2% offset), min | 45 ksi [310 MPa] |
| Elongation in 2 in. or 50 mm (or 4D), min | 35% longitudinal / 25% transverse |
| Hardness | No maximum listed in Table 4 |
| Grain size | Not listed in Table 5 |
The comparison below puts the S30815 Table 4 floor beside TP304H, TP309S, and S30415.
| Grade | UNS | Tensile min, ksi [MPa] | Yield min, ksi [MPa] |
|---|---|---|---|
| TP304H | S30409 | 75 [515] | 30 [205] |
| TP309S | S30908 | 75 [515] | 30 [205] |
| — | S30415 | 87 [600] | 42 [290] |
| — | S30815 | 87 [600] | 45 [310] |
The 45 ksi yield is half again the 30 ksi of TP309S, and the alloy is designed to keep a creep-strength advantage over 309 and 310 types at temperature. Table 4 is a room-temperature acceptance check only; S30815 is not in Table 5, and elevated-temperature allowables must come from the governing code for this UNS.
No hardness maximum is set for this grade in Table 4, so a hardness figure on a certificate is information rather than an acceptance criterion unless your order adds one. If a project specification imposes hardness or impact testing, write it on the purchase order so the mill can plan the test pieces before the pipe is cut.
Dimensions, Tolerances and Stock Sizes
Dimensions for ASTM A312 UNS S30815 pipe are normally ordered by NPS and schedule from ASME B36.19, or by outside diameter and wall where the design calls for a non-standard size. Outside-diameter tolerance and wall tolerance come from the specification itself, and wall is read as nominal unless Supplementary Requirement S8 asks for minimum wall. The permitted variations in wall thickness from Table 3 are shown below by NPS band and wall-to-diameter ratio.
| NPS designator | Wall over | Wall under |
|---|---|---|
| 1/8 to 2-1/2 incl., all t/D | 20.0% | 12.5% |
| 3 to 18 incl., t/D up to 5% | 22.5% | 12.5% |
| 3 to 18 incl., t/D over 5% | 15.0% | 12.5% |
| 20 and larger, welded, all t/D | 17.5% | 12.5% |
| 20 and larger, seamless, t/D up to 5% | 22.5% | 12.5% |
| 20 and larger, seamless, t/D over 5% | 15.0% | 12.5% |
In practice the under-tolerance of 12.5% is the figure that matters for pressure design, because the designer has already sized the nominal wall with that allowance in mind. The over-tolerance varies with NPS and the wall-to-diameter ratio, which matters more for fit-up and weld preparation than for strength. For UNS S30815, whose higher strength or special chemistry often justifies a lighter or more closely engineered wall, confirm whether your calculation assumed nominal or minimum wall before the order is placed.
Stock / Available sizes. The table below shows the representative size band we quote for ASTM A312 UNS S30815, with example OD × wall combinations taken from B36.19 schedules. It is a supply and stock-enquiry range rather than a promise that every size sits on the floor today: for S30815 a range of seamless sizes in Sch 10S and 40S may be available from existing material, while larger welded sizes and heavy walls are planned as mill orders. Special OD, special wall, and cut lengths are always handled on enquiry.
| Representative size | Example OD × wall | Typical schedules / notes |
|---|---|---|
| NPS 1/2 – 2 | 21.34 × 2.77 mm (NPS 1/2 Sch 40S); 60.33 × 3.91 mm (NPS 2 Sch 40S) | Sch 10S / 40S / 80S; small-bore process and instrument take-offs |
| NPS 2-1/2 – 6 | 88.90 × 5.49 mm (NPS 3 Sch 40S); 168.28 × 3.40 mm (NPS 6 Sch 10S) | Sch 10S / 40S / 80S; the most frequent enquiry band |
| NPS 8 – 12 | 219.08 × 8.18 mm (NPS 8 Sch 40S); 323.85 × 4.57 mm (NPS 12 Sch 10S) | Sch 10S / 40S; confirm SML or WLD route on enquiry |
| NPS 14 – 24 | 406.40 × 4.78 mm (NPS 16 Sch 10S); 609.60 × 9.53 mm (NPS 24 Sch 40S) | Sch 10S / 40S; usually mill-order, mostly welded |
| Special OD × wall | Any OD and wall the mill can qualify | On enquiry: state OD, nominal or minimum wall, and length practice |
Read the example sizes as orientation for writing the enquiry, not as a price list. When you send a size list we check live availability line by line, separate what can ship from existing material from what needs a mill slot, and give the lead time for each group so the purchase order can be split if the schedule demands it.
Equivalent Grades
Buyers often arrive with a trade name, a plate designation, or a European number rather than the A312 row. The table below maps the names we see on enquiries for UNS S30815, but only the ASTM A312 grade and UNS number are contractual on this page; everything else is a cross-reference that needs checking against its own standard.
| Designation | Notes |
|---|---|
| ASTM A312 UNS S30815 | Governing grade on this page (no TP name) |
| ASME SA-312 UNS S30815 | Separate Code standard; dual mark only when the order names both |
| EN 1.4835 | Commonly cited European counterpart; verify against the EN standard |
| ASTM A240 / A213 S30815 | Plate and tube counterparts under separate specifications |
| Producer trade names | Order by UNS S30815, not by trade name |
The ASME SA-312 row is listed because some Code projects require it, not because it is a synonym. ASME SA-312 is a separate standard adopted into the Boiler and Pressure Vessel Code, and the SA312 UNS S30815 page covers that document on its own terms. When both marks are wanted, the order should name both specifications and their editions so the certificate can state compliance with each.
Heat Treatment and Delivery Condition
S30815 has its own Table 2 row, listed with S31272, at 1920 °F [1050 °C] minimum followed by rapid cooling under note D. Clause 6.2 then adds an important rule: S30815 is one of the grades that must be reheated to the solution temperature before quenching, so seamless pipe may not be quenched directly from the hot-forming heat as most grades can be. Clause 17 also requires the heat-treatment lot to be identified in the marking alongside the heat number, so check both on the stencil and certificate.
Delivery condition for UNS S30815 is solution annealed, then descaled by pickling or by blasting and pickling, straightened, and cut to the ordered length practice. HCW pipe receives its cold reduction before the final anneal, so cold work is never the delivered condition. Ask for the actual annealing temperature and cooling method to be recorded on the certificate, because a reviewer cannot otherwise confirm the Table 2 requirement from the document alone.
Corrosion Resistance
ASTM A312 contains no corrosion table, so the following is engineering commentary rather than a specification requirement. S30815 is designed for oxidation and hot-gas service. Silicon and cerium help form a thin, adherent oxide that resists spalling during thermal cycling, and producer literature cites useful oxidation resistance to about 2010 °F [1100 °C]; that is guidance, not an A312 requirement.
In aqueous service it behaves broadly like other 21Cr-11Ni alloys and is not intended for chloride-bearing water or strong acids. Long exposure in the sigma-forming range can reduce ductility, and sulfur-bearing or carburizing atmospheres need a specific review before the oxidation advantage is relied upon.
Applications of ASTM A312 UNS S30815 Pipe
Applications for ASTM A312 UNS S30815 pipe are in high-temperature equipment where oxidation resistance and creep strength both matter. The table below summarizes the typical uses.
| Application | Role of S30815 | Note |
|---|---|---|
| Petrochemical and refinery furnace components | Tube supports, hangers, hot-gas piping | Confirm code listing for pressure parts |
| Industrial furnace radiant tubes and muffles | Oxidation resistance with high strength | Check carburizing potential |
| Recuperators and heat exchangers | High-temperature air and flue gas | Cold-end condensate risk |
| Fluidized bed and incinerator internals | Hot gas and abrasion | Ash chemistry matters |
| Cement and mineral processing | Burner pipes, cyclone parts | Alkali attack possible |
| Power and boiler components | Soot-blower, superheater supports, hot ducts | Thermal cycling resistance |
Treat the table as a starting point for discussion with the process licensor or corrosion engineer, not as an approval. Code allowable stresses, temperature limits, and any owner material lists decide whether UNS S30815 is acceptable on a given line, and those checks should be made before the pipe is ordered rather than after it arrives.
Weldability
S30815 welds well with GTAW, GMAW, SMAW, and SAW using normal austenitic practice and moderate heat input. It is not listed in Table 6, so ASTM A312 names no AWS A5.9 class and filler is by agreement; producers supply matching consumables that keep the oxidation and creep properties of the joint, while a 309-type filler is sometimes used where the joint will see lower temperature. Record the choice on the WPS and qualify on S30815.
Qualify the procedure on UNS S30815 itself rather than on a convenient 304 coupon, because the qualification has to demonstrate the strength and soundness of this chemistry. Clean joint preparation, controlled heat input and interpass temperature, and a back-purged root are the normal baseline; the certificate for any WLD pipe should also state whether filler metal was used in the longitudinal seam.
Surface Finishes
Surface condition for ASTM A312 UNS S30815 pipe should be stated on the purchase order rather than left to mill default. On stainless pipe, residual scale, embedded free iron, and chloride contamination from handling can matter as much as the nominal finish name, and they are far easier to prevent at the mill than to correct on site.
- Annealed and pickled the standard delivery after solution treatment for process piping
- Blasted and pickled when heavier scale needs mechanical help before chemical descaling
- Bright annealed by agreement, generally on smaller sizes where the furnace atmosphere can be controlled
- Passivated or polished by agreement, with the method and acceptance criteria written on the order
For UNS S30815, heavy hot-finishing scale should be removed by pickling or blasting so the protective oxide can form evenly in service; bright finishes are rarely relevant. If the line will be inspected for surface iron, specify the test method at the enquiry stage so that the packing and handling plan supports it.
Inspection and Testing
The base acceptance package for ASTM A312 UNS S30815 pipe combines heat analysis, tension testing, the flattening or bend test that applies to the manufacturing type, and a hydrostatic or non-destructive electric test on every length. Visual and dimensional inspection confirm the size and surface before marking. For S30815 the certificate should show cerium, nitrogen, silicon, and carbon, the 1920 °F anneal with confirmation of the clause 6.2 reheat, and the heat-treatment lot marking required by clause 17.
Supplementary requirements are optional until they are written on the order. The options buyers request most often for this grade are summarized below, and each one adds test time that should be allowed for in the delivery schedule.
| Option | Purpose |
|---|---|
| S1 product analysis | Confirms chemistry on finished pipe |
| S5 radiography | Weld integrity on WLD pipe |
| S7 intergranular corrosion | A262 Practice E after sensitizing treatment |
| S8 minimum wall | Wall interpreted as minimum rather than nominal |
| S9 weld decay | Compares weld and base-metal loss rates |
Third-party inspection, witness points, and EN 10204 3.2 certification are available when the order names the inspection agency. Agree the hold points before production starts, because witnessing a hydrotest or a tension test after the fact is not possible.
Packaging and Shipping
ASTM A312 UNS S30815 pipe is packed for handling and for ocean or land transport. Each length is marked with ASTM A312, the grade UNS S30815, the manufacturing type, size, heat number, and the test method used, with SA-312 added only when the order asks for dual marking. Bundle lists repeat the heat numbers so receiving can match pipe to certificates without opening every wrap.
- End caps or bevel protectors fitted as ordered
- Bundles strapped with protected contact points to limit iron pick-up
- Wooden cases or seaworthy bundles for export, with moisture protection for sea freight
- Small-bore or polished pipe cased separately where damage risk is higher
Stainless pipe should not be stored or lifted in contact with carbon steel, and for a specialty grade such as UNS S30815 it is worth keeping the material segregated by heat on arrival, since mixing it with common 304 stock is the most frequent cause of misuse on site.
Why Choose SHH STEEL
SHH STEEL supplies specification-driven stainless pipe, and for a specialty grade such as ASTM A312 UNS S30815 we quote against the edition you name rather than a generic catalogue sheet. We report the full Table 1 heat analysis, the Table 4 tension results, and the heat-treatment record, and we tell you early when a size or route is a mill order instead of letting the lead time surprise you.
- Clear handling of the S30815 Table 2 anneal, the clause 6.2 reheat rule, and lot marking
- Clear advice on sister grades under ASTM A312, so UNS S30815 is not confused with a commoner alloy that looks similar on paper
- Honest separation of specification requirements from producer or market guidance in every document we send
- EN 10204 3.1 certificates as standard, with third-party inspection and 3.2 certification on request
The aim is a delivery that clears receiving inspection on the first review. That means the certificate, the stencil, and the purchase order all say the same thing about grade, UNS number, manufacturing type, size, and heat treatment, and that any agreed variation is written down before the pipe is made.
Supply Capability
SHH STEEL can supply ASTM A312 UNS S30815 stainless steel pipe against the edition and manufacturing type named on your enquiry. The capability table below summarizes the routes, sizes, finishes, and documents we regularly quote for this grade, and each line can be narrowed to your project specification.
| Item | SHH STEEL capability for UNS S30815 |
|---|---|
| Standard | ASTM A312 / A312M, UNS S30815 |
| Manufacturing types | SML, WLD, HCW |
| Size | NPS 1/8 and up per ASME B36.19; special OD and wall by agreement |
| Schedules | 5S, 10S, 40S, 80S and non-standard walls |
| Length | Single random, double random, or cut to length |
| Heat treatment | 1920 °F [1050 °C] minimum solution anneal (Table 2, listed with S31272) with rapid cooling |
| Filler guidance | Not listed in Table 6; filler by agreement (matching or 309-type, recorded on the WPS) |
| Testing | Tension (87/45 ksi), flattening or bend, hydrostatic or electric test per length; S1, S5, S7, S8, S9 on order |
| Documents | EN 10204 3.1 with full Table 1 analysis; 3.2 and third-party inspection on request |
| Trade terms | FOB, CFR, CIF, EXW and other agreed Incoterms |
Stock / Available sizes. The representative band for UNS S30815 is NPS 1/2 to 24 in Sch 10S, 40S, and 80S as listed under Dimensions. Selected common OD × wall combinations may be available from existing material, while heavy-wall seamless, unusual schedules, and special cut lengths are normally mill orders. We do not publish stock part numbers or tonnage claims for this grade; ask for a live check against your size list instead.
Enquiries move fastest when they state the A312 edition, UNS S30815, the manufacturing type, NPS or OD × wall (and whether the wall is nominal or minimum), length practice, finish, and any product-analysis, corrosion-test, or 3.2 requirements. Dual SA-312 marking, bevelled ends, and cut lengths are available on confirmed orders when the order says so.
FAQ
-
Is ASTM A312 UNS S30815 the same as ASME SA-312 UNS S30815?
- They are two independent standards. ASTM A312/A312M is the ASTM product specification, and ASME SA-312 is the separate document adopted into the Boiler and Pressure Vessel Code. The technical rows for UNS S30815 are closely aligned in current editions, but a pipe is only certified to the document named on the order, so when both are needed the purchase order should list both specifications and editions and the certificate should state compliance with each.
-
What is the UNS number for ASTM A312 UNS S30815?
- This alloy has no TP name in A312 Table 1; it is ordered as UNS S30815 and is widely known by a producer trade name. The UNS number should appear on the mill certificate and on the stencil next to the ASTM A312 mark, because a trade name alone makes it hard for receiving inspection to tie the chemistry on the certificate to the pipe in the rack.
-
What are the tensile and yield requirements for ASTM A312 UNS S30815 pipe?
- Table 4 requires 87 ksi [600 MPa] tensile strength and 45 ksi [310 MPa] yield strength minimum, with elongation of 35% longitudinal / 25% transverse minimum. These are room-temperature minimums for acceptance only; design allowables at temperature come from the applicable piping code, and they should be checked there before a wall thickness is fixed.
-
What heat treatment does ASTM A312 UNS S30815 pipe receive?
- Table 2 lists S30815 at 1920 °F [1050 °C] minimum with rapid cooling, and clause 6.2 requires it to be reheated to that temperature before quenching rather than quenched directly after hot forming. The delivered condition is solution annealed and descaled, and the certificate should record the actual annealing temperature and the cooling method so a reviewer can confirm the requirement without asking the mill.
-
Which filler metal is used to weld ASTM A312 UNS S30815?
- S30815 is not listed in Table 6, so ASTM A312 names no AWS A5.9 class; matching consumables from producers keep the joint’s high-temperature properties, and the agreed filler must be recorded. Whatever is chosen should be recorded on the WPS and PQR, and the procedure should be qualified on UNS S30815 base metal so that the joint strength and soundness are demonstrated on the real chemistry.
-
Is ASTM A312 UNS S30815 pipe available seamless and welded?
- Yes. ASTM A312 allows seamless (SML), welded (WLD), and heavily cold-worked (HCW) pipe for UNS S30815, all meeting the same chemistry, tension, and heat-treatment rules. Seamless is usual for heavy wall and high pressure, while welded is often more economical in thin walls and larger diameters; state the accepted route on the order.
-
What sizes of ASTM A312 UNS S30815 pipe can SHH STEEL supply?
- We quote NPS 1/2 to 24 in Sch 10S, 40S, and 80S as the representative band, plus NPS 1/8 and up and special OD and wall by agreement. Some common sizes may be available from existing material, while heavy-wall seamless and unusual schedules are normally mill orders, so send a size list for a live check.
-
What documents come with ASTM A312 UNS S30815 pipe?
- Each shipment carries an EN 10204 3.1 mill test certificate showing the A312 edition, UNS S30815, manufacturing type, heat number, the full Table 1 heat analysis, Table 4 tension results, heat treatment, and the hydrostatic or electric test. Third-party inspection and 3.2 certification can be added when the order names the agency.
-
How does UNS S30815 compare with TP310S?
- TP310S relies on 24–26% chromium and 19–22% nickel, while S30815 uses 20–22% chromium and 10–12% nickel with silicon, nitrogen, and cerium. S30815 has a higher 87/45 ksi Table 4 floor and is designed for better creep strength, while TP310S has more alloy margin in some aggressive atmospheres.
-
Why must S30815 be reheated before quenching?
- Clause 6.2 names S30815, along with the H grades and a few other alloys, as material that must be reheated to the solution-treatment temperature before quenching. Direct quenching from the hot-forming heat could leave the carbon and nitrogen distribution uncontrolled, so the separate anneal ensures a consistent structure.
-
What is the difference between UNS S30815 and UNS S30415?
- Both use silicon, nitrogen, and cerium, but S30815 has more chromium (20–22% against 18–19%) and nickel (10–12% against 9–10%), a 1920 °F Table 2 anneal with mandatory reheat, and a 45 ksi yield floor. It is aimed at higher temperatures than S30415.
Conclusion
ASTM A312 UNS S30815 (UNS S30815) is the 21Cr-11Ni heat-resisting alloy of the series with silicon, nitrogen, and cerium, an 87/45 ksi floor, and a 1920 °F Table 2 anneal with mandatory reheat before quench. The specification fixes C 0.05–0.10%, Mn ≤0.80%, Si 1.40–2.00%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, and Ce 0.03–0.08%, a Table 4 floor of 87 ksi [600 MPa] tensile and 45 ksi [310 MPa] yield, and 1920 °F [1050 °C] minimum solution anneal (Table 2, listed with S31272) with rapid cooling heat treatment, while filler selection is by agreement because S30815 is not listed in Table 6. Put the manufacturing type, size and wall basis, finish, and any supplementary tests on the purchase order, and review the EN 10204 3.1 certificate against Tables 1, 2, and 4 before release. SHH STEEL can supply ASTM A312 UNS S30815 pipe to the edition you name; compare sister grades on the A312/A312M hub, or send your size list to admin@steelspecs.com.