Product Showcase
GB/T 714 Carbon Steel Plates
SHH STEEL offers GB/T 714-compliant Q345qD/Q460qD structural steel plates. GB/T 714 specifies high-strength low-alloy steels for welded structures in bridges and heavy engineering. Tough, weldable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 714 Q500qNHF Weathering Bridge Steel Supplier
GB/T 714 Q500qNHF (Q500qFNH) is weathering bridge steel plate with 500 MPa minimum yield, 54 J Charpy at −60°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q500qNHE Weathering Bridge Steel Supplier
GB/T 714 Q500qNHE (Q500qENH) is weathering bridge steel plate with 500 MPa minimum yield, 120 J Charpy at −40°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q500qNHD Weathering Bridge Steel Supplier
GB/T 714 Q500qNHD (Q500qDNH) is weathering bridge steel plate with 500 MPa minimum yield, 120 J Charpy at −20°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q460qNHF Weathering Bridge Steel Supplier
GB/T 714 Q460qNHF (Q460qFNH) is weathering bridge steel plate with 460 MPa minimum yield, 47 J Charpy at −60°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q460qNHE Weathering Bridge Steel Supplier
GB/T 714 Q460qNHE (Q460qENH) is weathering bridge steel plate with 460 MPa minimum yield, 120 J Charpy at −40°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q460qNHD Weathering Bridge Steel Supplier
GB/T 714 Q460qNHD (Q460qDNH) is weathering bridge steel plate with 460 MPa minimum yield, 120 J Charpy at −20°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q420qNHF Weathering Bridge Steel Supplier
GB/T 714 Q420qNHF (Q420qFNH) is weathering bridge steel plate with 420 MPa minimum yield, 47 J Charpy at −60°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q420qNHE Weathering Bridge Steel Supplier
GB/T 714 Q420qNHE (Q420qENH) is weathering bridge steel plate with 420 MPa minimum yield, 120 J Charpy at −40°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q420qNHD Weathering Bridge Steel Supplier
GB/T 714 Q420qNHD (Q420qDNH) is weathering bridge steel plate with 420 MPa minimum yield, 120 J Charpy at −20°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q390qNH Weathering Bridge Steel Supplier
GB/T 714 Q390qNH (Q390qNH) is weathering bridge steel plate with 390 MPa minimum yield, Charpy in C, D or E grade, Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More -
GB/T 714 Q370qNHF Weathering Bridge Steel Supplier
Q370qNHF (standard notation Q370qFNH) is a GB/T 714-2015 weathering bridge steel with 370 MPa yield and −60°C Charpy. GB/T 714-2025 lists this level in C, D and E only, so SHH STEEL supplies it to the 2015 edition or as Q370qENH with an agreed −60°C test, mill-direct.View More -
GB/T 714 Q370qNHE Weathering Bridge Steel Supplier
GB/T 714 Q370qNHE (Q370qENH) is weathering bridge steel plate with 370 MPa minimum yield, 120 J Charpy at −40°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.View More
GB/T 714 Carbon Steel Plates
High-Strength Low Alloy Plates
SHH STEEL, a leading High-Strength Low Alloy Plates exporter, produces and exports HSLA steel plates for construction, bridges, and automotive applications. Our plates, like ASTM A572 Grade 50, offer superior strength-to-weight ratios and excellent weldability, meeting global standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Trust SHH STEEL for durable high-strength low alloy plates and custom solutions for structural projects.
High-Strength Low Alloy Plates
X