GB/T 714 Q460qD bridge steel plate stacked at SHH STEEL warehouse

GB/T 714 Q460qD Bridge Steel Plate Supplier

GB/T 714 Q460qD is bridge structural steel plate with 460 MPa minimum yield, 570 MPa minimum tensile and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. SHH STEEL supplies Q460qD mill-direct, TMCP / TMCP+T, up to 130 mm, with Z15–Z35, UT and heat and product analysis.
Keywords
Q460qD, Q460qD steel plate, GB/T 714 Q460qD, Q460q-D, Q460q D, Q460qD bridge steel, Q460qDZ15, Q460qDZ25, Q460qDZ35, bridge steel plate, Q460qD supplier
Equivalent Grades:
ASTM A709 HPS 70W / EN 10025-4 S460M, S460ML / EN 10025-6 S460Q, S460QL, S460QL1 (Annex B) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q460q Quality Grades
GB/T 714-2025 vs 2015
Q460qD vs ASTM A709 / EN 10025
TMCP vs Normalized vs QT
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q460qD Bridge Steel Plate?

Q460qD is bridge structural steel plate to GB/T 714. Q stands for yield, 460 is the minimum yield in MPa for plate up to 50 mm, q stands for qiao (bridge) and D is the quality grade: Charpy V-notch at −20°C on longitudinal specimens.

Q460q is high-strength TMCP plate for main load paths on long-span bridges, where 460 MPa yield cuts flange thickness and weld volume. Annex B of GB/T 714-2025 lists ASTM A709 HPS 70W against Q460q. In practice, Q460q is chosen where Q420q flanges would exceed about 50–60 mm and welding cost starts to dominate.

Q460qD gives 460 MPa yield with a −20°C Charpy and Pcm ≤0.22% to 50 mm. It is the grade designers turn to when Q420q flanges become too thick to weld economically.

GB/T 714-2015 is no longer current. Its replacement, GB/T 714-2025, was published on 31 October 2025 and became effective on 1 May 2026. Where a contract still names the 2015 edition, we certify to it and flag any difference from 2025.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q460qD cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q460qD Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 130 mm for Q460q Confirmed
Minimum yield ReL 460 MPa ≤50 mm; 450 MPa >50–100 mm Confirmed
Minimum tensile Rm 570 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 18% Confirmed
Charpy V-notch −20°C, 120 J (12–100 mm), longitudinal Confirmed
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 7) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q460qD are ASTM A709 HPS 70W, EN 10025-4 S460M and EN 10025-4 S460ML; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Chemistry for Q460qD is fixed at the ladle, but it is verified on plate. GB/T 714 sets the ladle (heat) limits; GB/T 222 sets how far a finished-plate analysis may stray from them.

Table 1 below is the heat (ladle) analysis for Q460qD from GB/T 714-2025 Tables 1, 3.

Element Q460qD TMCP (%)
C, max 0.11
Si, max 0.55
Mn 0.80 – 1.70
P, max 0.025
S, max 0.015
Nb 0.010 – 0.090
V 0.010 – 0.080
Ti 0.006 – 0.030
Als 0.010 – 0.045
Cr, max 0.50
Ni, max 0.30
Cu, max 0.30
Mo, max 0.25
N, max 0.0080
B, max 0.0005 residual (≤0.0014 if C ≤0.10%)
H, max 0.0002

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q460qD product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si ≤ 0.55 +0.05 ≤ 0.60
Mn 0.80 – 1.70 ±0.06 0.74 – 1.76
P ≤ 0.025 +0.005 ≤ 0.030
S ≤ 0.015 +0.005 ≤ 0.020
V 0.010 – 0.080 +0.02 / −0.01 ≤ 0.100
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.090 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cr ≤ 0.50 +0.05 ≤ 0.55
Ni ≤ 0.30 +0.05 ≤ 0.35
Cu ≤ 0.30 +0.05 ≤ 0.35
Als 0.010 – 0.045 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.25 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Q460q TMCP heats are low-alloy steel, so Table 1 of GB/T 222 applies. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn falls in the 0.80–1.70% band, so ±0.06%. For one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q460q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 460 570 18%
> 50 – 100 mm 450 570 18%
> 100 – 130 mm 385 490 18%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
D / −20°C 80 J 120 J 47 J

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.

Q460qD / Q460qE / Q460qF: Which Quality Grade?

Q460qD is tested at −20°C. It suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C. D is the most specified letter on Chinese bridge drawings. It is tested at −20°C and the melt is tighter than C: P ≤0.025%, S ≤0.015%.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q460qD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q460qE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q460qF −60°C By agreement 47 J — 0.015 / 0.006

Over-specifying the letter costs money; under-specifying it costs safety. Choose from the lowest service or erection temperature, then step up one letter for thick, restrained or fracture-critical members.

Q460qD: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q460qD buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • Yield values above 100 mm were added (385 MPa for >100–130 mm).
  • The Mn range for TMCP steel was revised: the minimum is now 0.80%, and the maximum may be raised to 2.00% by agreement.
  • CEV and Pcm limits were revised (Tables 6 and 7).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
  • Section products were removed; the standard now covers plate and strip only.
  • Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q460qD vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q460qD replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q460qD ASTM A709 HPS 70W EN 10025-4 S460M EN 10025-4 S460ML
Min. yield (MPa) 460 (≤50 mm) 485 460 (≤16 mm) 460 (≤16 mm)
Tensile (MPa) 570 min 585 – 760 540 – 720 540 – 720
Charpy 120 J at −20°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels 40 J at −20°C 27 J at −50°C
Weathering chemistry No Yes No No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 460 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.

The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q460qD rather than GB/T 1591 plate.

Q460qD Delivery Condition: TMCP vs Normalized vs Quenched and Tempered

GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.

Route Available for Q460qD Weldability index Notes
TMCP Yes, standard Pcm (C ≤0.11%) Up to 130 mm
TMCP + tempering Yes Same as TMCP Common on thick or E/F plate
Normalized No — Dropped in 2025 for this level
Quenched and tempered Not listed — Use GB/T 16270 if QT is required

Q460q is TMCP or TMCP + tempering. If a project insists on QT, GB/T 16270 Q460 grades are the alternative, with different toughness rules. D-letter plate is usually plain TMCP; tempering is added mainly for heavy plate or tight yield-ratio limits.

Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q460qD.

Welding Q460qD and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, TMCP (Table 7) ≤ 0.22 ≤ 0.23 ≤ 0.23

Welding Q460qD to bridge codes means qualified procedures, qualified welders and NDT of every primary weld. The plate’s job is to give stable chemistry from heat to heat. At −20°C, most procedures qualified on TMCP plate pass HAZ impact without special measures; keep multi-wire SAW heat input inside the qualified band.

Typical consumables for Q460qD: E55/E62-class consumables (AWS E8018 / E9018 type).

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q460qDZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Bridge node plates, anchor boxes and pylon walls take weld shrinkage through their thickness. If the plate holds sulfide stringers, it can tear in steps under the weld. Z grades prove through-thickness ductility.

GB/T 714 adds the Z level to the end of the designation, for example Q460qDZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

D chemistry allows S up to 0.015%. Z15 needs S ≤0.010% and Z25 needs ≤0.007%, so Z plate is still made from a dedicated low-sulfur heat.

Most bridges need Z on a small share of the tonnage. Mark it item by item on the cutting list rather than on the whole Q460qD order. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q460qD
ASTM A709 ASTM A709 HPS 70W Listed in Annex B
EN 10025-4 EN 10025-4 S460M, EN 10025-4 S460ML Listed in Annex B
EN 10025-6 EN 10025-6 S460Q, EN 10025-6 S460QL, EN 10025-6 S460QL1 Listed in Annex B
GB/T 16270 GB/T 16270 Q460D QT alternative
GB/T 1591 GB/T 1591 Q460MD General structural
GB/T 714 (weathering twin) Q460qNHD Same strength, weathering chemistry

Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q460qD, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.

Q460qD Testing, UT and Certificate

A batch of Q460qD is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −20°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −20°C the 120 J level is comfortable for well-made TMCP plate, but we still check each batch value, not just the average.

Dimensions

Typical Q460qD dimensions on our offers:

  • Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

Q460qD plate is rolled to GB/T 709 tolerances. Class B (−0.30 mm) is standard; Class C (zero minus) can be agreed.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q460qD Price Factors and How to Order

For Q460qD, the base price follows the market; grade, letter, size and testing extras decide the rest.

Cost driver Effect on price
Strength level Q460q Higher levels need more alloy and tighter rolling control
Quality letter Small extra for −20°C testing and cleaner melt
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q460qDZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q460qE, Q460qF.

Applications

Sector Typical Q460qD components
Long-span truss bridges Highly stressed chords and node plates
Cable-stayed bridges Pylon steel anchor boxes, main girder flanges
Suspension bridges Stiffening truss chords
Railway bridges Heavy-haul truss members
Arch bridges Arch rib plate

The letter D suits most highway and railway bridges in central and northern China, Europe and North America, where winter lows reach about −20°C.

It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).

Supply Capability and Global Delivery

SHH STEEL sources Q460qD from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −20°C Charpy, bend, Z test, UT, product analysis
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Most of our Q460qD goes to overseas bridge projects with Chinese designers or contractors; we also supply local fabricators abroad.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. For Q460qD that means bridge plate from bridge-plate mills, not relabelled structural plate.

Before shipment we check four lines on every Q460qD certificate: yield and tensile for the actual thickness band, Charpy at −20°C, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q460qD.

Ask for the actual Pcm on the certificate. At 460 MPa, fabricators set preheat from it, and a low-Pcm heat can save days of preheating on a big girder.

We also tell buyers when another grade fits better. Neighbouring levels are Q420qD and Q500qD. The weathering counterpart is Q460qNHD. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q460qD steel?
Q460qD is bridge structural steel plate to GB/T 714-2025. It has 460 MPa minimum yield up to 50 mm, 570 MPa minimum tensile, 18% elongation and Charpy V-notch impact of 120 J at −20°C for 12–100 mm plate. It is delivered TMCP or TMCP + tempering.
What is the difference between Q460qD and Q460qE?
Strength and chemistry box are the same. Q460qD is Charpy tested at −20°C, Q460qE at −40°C, both needing 120 J for 12–100 mm plate. P/S caps are 0.025/0.015% for D and 0.020/0.010% for E. Choose by the lowest service or erection temperature.
What is the maximum thickness of Q460qD?
GB/T 714-2025 covers bridge plate up to 150 mm, but tensile values for Q460q stop at 130 mm. Above that there is no table value, so Q460qD cannot be certified thicker than 130 mm without a special agreement.
What is the ASTM or EN equivalent of Q460qD?
Close grades for Q460qD: ASTM A709 HPS 70W / EN 10025-4 S460M, S460ML / EN 10025-6 S460Q, S460QL, S460QL1 (Annex B). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
What is the batch size for GB/T 714 bridge plate testing?
Up to 60 t of one grade, heat, thickness, rolling schedule and heat-treatment condition. Each batch gets one tensile test, one bend test and one set of three Charpy specimens; heat analysis is reported per heat.
Is Q460qD weldable?
Yes. GB/T 714-2025 caps the weldability index for Q460qD up to 50 mm at Pcm ≤0.22%. Preheat depends on actual chemistry, thickness and restraint, and is fixed by the qualified welding procedure.

Conclusion

Q460qD to GB/T 714-2025 is bridge plate with 460 MPa minimum yield, 570 MPa minimum tensile and 120 J Charpy at −20°C for 12–100 mm plate.

It sits between Q420qD and Q500qD in the bridge range, with Q460qE and Q460qF as sister letters. For Q460qD, the deciding numbers on the certificate are yield at the actual thickness, Charpy at −20°C and the weldability index for the delivery route.

With SHH STEEL the Q460qD certificate is complete: heat chemistry, weldability index, yield, tensile, elongation and Charpy, to EN 10204 3.1 or 3.2. Add product analysis, a Z level or a stricter UT class as needed.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.

Email the cutting list and the owner’s specification. We return a line-by-line offer with test plan and lead time. Contact SHH STEEL for Q460qD bridge steel plate.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response