GB/T 714 Q390q TMCP Bridge Steel Plate Supplier
What is GB/T 714 Q390q Bridge Steel Plate?
Q390q is a bridge structural steel grade in GB/T 714-2025: Q for yield, 390 for the minimum yield in MPa, q for qiao (bridge). It is ordered with a quality letter: Q390qC (0°C), Q390qD (−20°C) or Q390qE (−40°C). This page covers all three.
Q390q is the new TMCP grade added in GB/T 714-2025 to close the gap between Q370q and Q420q. Before 2026, designers had to jump from 370 MPa to 420 MPa, and from C ≤0.14% chemistry to the leaner C ≤0.11% family. Q390q keeps the Q345q/Q370q chemistry box with a CEV cap of 0.41% and gives 390 MPa yield.
Q390q is new: it did not exist before GB/T 714-2025 took effect on 1 May 2026. It is a TMCP grade in letters C, D and E, with the familiar C ≤0.14% chemistry, a CEV cap of 0.41% and 390 MPa yield up to 50 mm. Designers use it to avoid jumping straight from Q370q to Q420q.
GB/T 714-2025 has been in force since 1 May 2026, replacing GB/T 714-2015 in full. If your specification was written earlier, check the edition before ordering: some table values changed, and a few grades were added or dropped.
SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q390q cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714.
Material Specification
| Specification element | Requirement | SHH STEEL compliance |
|---|---|---|
| Standard | GB/T 714-2025 Q390q | Confirmed |
| Product | Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm | Plate |
| Thickness with tensile values | Up to 130 mm for Q390q | Confirmed |
| Minimum yield ReL | 390 MPa ≤50 mm; 380 MPa >50–100 mm | Confirmed |
| Minimum tensile Rm | 520 MPa ≤100 mm (no upper limit in the standard) | Confirmed |
| Elongation A | ≥ 20% | Confirmed |
| Charpy V-notch | C 0°C / D −20°C / E −40°C, 120 J (12–100 mm) | Confirmed |
| Delivery condition | TMCP or TMCP + tempering | As ordered |
| Weldability index | CEV (Table 6) and Pcm (Table 7) | Printed on MTC |
| Ultrasonic testing | Plate >20 mm: GB/T 2970, Class II or better | Every plate |
| Through-thickness | Z15, Z25 or Z35 to GB/T 5313, when ordered | As ordered |
| Dimensions | GB/T 709 | Confirmed |
| Certificate | GB/T 247; EN 10204 3.1 or 3.2 | As ordered |
Grades often compared with Q390q are ASTM A709 Grade 50, EN 10025-4 S355M and EN 10025-4 S420M; the comparison below shows where they differ.
Chemical Composition: Heat Analysis and Product Analysis
Read the Q390q certificate with two tables in mind: heat limits from GB/T 714 and product limits from GB/T 222. A plate can pass one and be argued over in the other if the basis is not written into the contract.
Table 1 below is the heat (ladle) analysis for Q390q from GB/T 714-2025 Tables 1, 3.
| Element | Q390q C / D / E, TMCP (%) |
|---|---|
| C, max | 0.14 |
| Si, max | 0.55 |
| Mn | 0.80 – 1.60 |
| P, max | 0.030 / 0.025 / 0.020 |
| S, max | 0.025 / 0.015 / 0.010 |
| Nb | 0.010 – 0.090 |
| V | 0.010 – 0.080 |
| Ti | 0.006 – 0.030 |
| Als | 0.010 – 0.045 |
| Cr, max | 0.30 |
| Ni, max | 0.30 |
| Cu, max | 0.30 |
| Mo, max | — |
| N, max | 0.0080 |
| B, max | 0.0005 residual (≤0.0014 if C ≤0.10%) |
| H, max | 0.0002 |
Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%.
Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.
| Element | Heat limit (%) | Deviation, GB/T 222-2025 Table 1 | Q390q product analysis (%) |
|---|---|---|---|
| C | ≤ 0.14 | +0.02 | ≤ 0.16 |
| Si | ≤ 0.55 | +0.05 | ≤ 0.60 |
| Mn | 0.80 – 1.60 | ±0.06 | 0.74 – 1.66 |
| P | ≤ 0.030 (C letter) | +0.005 | ≤ 0.035 |
| S | ≤ 0.025 (C letter) | +0.005 | ≤ 0.030 |
| V | 0.010 – 0.080 | +0.02 / −0.01 | ≤ 0.100 |
| Ti | 0.006 – 0.030 | +0.02 / −0.01 | ≤ 0.050 |
| Nb | 0.010 – 0.090 | ±0.005 (listed for 0.015–0.060%) | Above 0.060%: agree in contract |
| Cr | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Ni | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Cu | ≤ 0.30 | +0.05 | ≤ 0.35 |
| Als | 0.010 – 0.045 | ±0.003 | Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm) |
| Mo | — | Not listed in Table 1 | — |
| N | ≤ 0.0080 | Listed only for 0.010–0.020% | Agree in contract |
How to read Table 2. Q390q TMCP heats are low-alloy steel, so Table 1 of GB/T 222 applies. Si ≤0.55% is above 0.37%, so +0.05% applies; Mn falls in the 0.80–1.70% band, so ±0.06%. For one heat, an element may deviate in one direction only.
Mechanical Properties
Tensile values follow Table 9 of GB/T 714-2025 for Q390q. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.
| Nominal thickness | ReL min (MPa) | Rm min (MPa) | A min |
|---|---|---|---|
| ≤ 50 mm | 390 | 520 | 20% |
| > 50 – 100 mm | 380 | 520 | 20% |
| > 100 – 130 mm | 335 | 450 | 20% |
Impact values follow Table 10, on longitudinal specimens, average of three:
| Letter / test temperature | KV2 ≤12 mm | KV2 >12 – 100 mm | KV2 >100 – 130 mm |
|---|---|---|---|
| C / 0°C | 80 J | 120 J | 55 J |
| D / −20°C | 80 J | 120 J | 47 J |
| E / −40°C | 80 J | 120 J | 31 J |
One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.
180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.85 above 12 mm for TMCP plate.
Q390q C, D or E: Which Quality Grade?
Q390q is ordered with a letter. All three share chemistry box, strength and Pcm/CEV cap; they differ in test temperature and in P and S limits.
| Grade | Test temp. | KV2 ≤12 mm | KV2 12–100 mm | KV2 >100 mm | P / S max (%) |
|---|---|---|---|---|---|
| Q390qC | 0°C | 80 J | 120 J | 55 J | 0.030 / 0.025 |
| Q390qD | −20°C | 80 J | 120 J | 47 J | 0.025 / 0.015 |
| Q390qE | −40°C | 80 J | 120 J | 31 J | 0.020 / 0.010 |
Pick C for sites that stay near or above 0°C, D for winters down to about −20°C, and E for colder sites or thick, restrained members. There is no F letter at the 390 MPa level; for −60°C look at Q420qF.
Q390q: What Changed from GB/T 714-2015 to GB/T 714-2025
For Q390q buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.
- Q390q is a new TMCP grade with its own CEV (0.41%) and Pcm (0.21%) caps; it did not exist in 2015.
- The Mn range for TMCP steel was revised: the minimum is now 0.80%, and the maximum may be raised to 2.00% by agreement.
- CEV and Pcm limits were revised (Tables 6 and 7).
- Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
- Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
- Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.
- Section products were removed; the standard now covers plate and strip only.
- Delivery is TMCP, TMCP + tempering or QT; normalizing is kept only for Q345q/Q370q plate over 100 mm by agreement.
If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.
Q390q vs ASTM A709 and EN 10025: Which Grade Matches?
Can Q390q replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.
| Property | Q390q | ASTM A709 Grade 50 | EN 10025-4 S355M | EN 10025-4 S420M |
|---|---|---|---|---|
| Min. yield (MPa) | 390 (≤50 mm) | 345 | 355 (≤16 mm) | 420 (≤16 mm) |
| Tensile (MPa) | 520 min | 450 min | 470 – 630 | 520 – 680 |
| Charpy | 120 J at 0 / −20 / −40°C (C/D/E) | CVN by temperature zone and member type (T / F) | 40 J at −20°C | 40 J at −20°C |
| Weathering chemistry | No | No | No | No |
ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.
EN 10025-3/-4/-6 grades show yield at the thinnest band; their values fall with thickness. GB/T 714 keeps 390 MPa to 50 mm. EN tensile ranges have upper limits; GB/T 714 gives minimums only.
The 120 J requirement in GB/T 714 for 12–100 mm plate is several times the 27–40 J typical of general structural grades. That margin is the main reason bridge owners specify Q390q rather than GB/T 1591 plate.
Q390q Delivery Condition: TMCP vs Normalized vs Quenched and Tempered
GB/T 714-2025 clause 3.2 defines TMCP as rolling with the final deformation in a controlled temperature range, including accelerated cooling with or without tempering (self-tempering included) but excluding direct quenching and quench-and-temper. The delivery route must be stated on the certificate.
| Route | Available for Q390q | Weldability index | Notes |
|---|---|---|---|
| TMCP | Yes, standard | CEV (C >0.12%) or Pcm | Up to 130 mm |
| TMCP + tempering | Yes | Same as TMCP | Common on thick or E/F plate |
| Normalized | No | — | Dropped in 2025 for this level |
| Quenched and tempered | Not listed | — | Use GB/T 16270 if QT is required |
Q390q is TMCP-only, which is why it appears in the title as ‘Q390q TMCP’. Its chemistry allows C up to 0.14%, so CEV applies above 0.12% C and Pcm at or below.
Ask for the route on the purchase order. It changes the weldability index, the welding procedure and, for heavy plate, the price of Q390q.
Welding Q390q and Fatigue in Bridge Girders
GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:
CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15
Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B
| Index | ≤50 mm | >50–100 mm | >100–130 mm |
|---|---|---|---|
| CEV, TMCP, C >0.12% (Table 6) | ≤ 0.41 | ≤ 0.41 | by agreement |
| Pcm, TMCP (Table 7) | ≤ 0.21 | ≤ 0.21 | ≤ 0.21 |
Welding Q390q to bridge codes means qualified procedures, qualified welders and NDT of every primary weld. The plate’s job is to give stable chemistry from heat to heat.
Typical consumables for Q390q: E55-class low-hydrogen consumables (AWS E8018 type).
Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.
Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.
Q390qDZ15, Z25 and Z35: Through-Thickness Plate for Bridges
Z15, Z25 and Z35 tell the mill how much through-thickness ductility a plate must prove. The higher the number, the lower the sulfur and the higher the cost.
GB/T 714 adds the Z level to the end of the designation, for example Q390qDZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.
| Z grade | Heat sulfur, max (%) | Reduction of area, avg / single (%) |
|---|---|---|
| Z15 | 0.010 | 15 / 10 |
| Z25 | 0.007 | 25 / 15 |
| Z35 | 0.005 | 35 / 25 |
Q390q C-letter plate allows S up to 0.025%, D 0.015% and E 0.010%; only E meets the Z15 sulfur cap without a dedicated heat.
A Z level on Q390q does not change strength or impact rules. It adds a sulfur cap and a short-transverse tensile test. Z options apply across the GB/T 714 bridge steel range.
Equivalent Material Grades
Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.
| Standard | Grade(s) | Fit for Q390q |
|---|---|---|
| EN 10025-4 | EN 10025-4 S420M | Closest; higher yield |
| ASTM A709 | ASTM A709 Grade 50 | Closest; lower yield |
| GB/T 1591 | GB/T 1591 Q390MD | Same yield, general structural |
| JIS G3106 | JIS G3106 SM520C | Closest by strength |
| GB/T 714 (weathering twin) | Q390qNH | Same strength, weathering chemistry |
Before substituting, compare three things line by line: minimum yield at the actual thickness, the impact test temperature and energy, and the weldability index. For Q390q, the 120 J impact level and the Pcm/CEV caps are usually the hardest to match.
Q390q Testing, UT and Certificate
A batch of Q390q is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:
| Test | Frequency | Method |
|---|---|---|
| Heat analysis | 1 per heat | GB/T 20066; GB/T 4336 / GB/T 223 |
| Tensile | 1 per batch | GB/T 2975 / GB/T 228.1 |
| Bend 180° | 1 per batch (may be waived if guaranteed) | GB/T 232 |
| Charpy V at the ordered letter’s temperature | 3 specimens per batch | GB/T 229 |
| Through-thickness (Z) | 3 specimens per batch, when ordered | GB/T 5313 |
| Ultrasonic | Every plate >20 mm, Class II or better | GB/T 2970 |
| Surface and dimensions | Every plate | Visual and gauges |
Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%.
Surface defects may be ground out within the minus tolerance (clause 7.4.3); deeper repairs need the buyer’s consent.
Dimensions
Common Q390q sizes:
- Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 8 – 60 mm
- Width: 1500 – 4000 mm, depending on mill and thickness
- Length: 6000 – 18000 mm; longer by enquiry
- Edge: mill edge or cut edge
- Weight: theoretical, 7.85 g/cm³
Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.
Tolerances
GB/T 714 does not set its own size tolerances; Q390q follows GB/T 709. Other tolerance standards can be agreed in the contract (clause 7.6.2).
| Nominal thickness (mm) | Width ≤ 1500 mm | Width > 1500 – 2500 mm |
|---|---|---|
| > 8 – 15 | −0.30 / +0.80 | −0.30 / +1.00 |
| > 15 – 25 | −0.30 / +1.00 | −0.30 / +1.20 |
| > 25 – 40 | −0.30 / +1.10 | −0.30 / +1.30 |
| > 40 – 60 | −0.30 / +1.30 | −0.30 / +1.50 |
| > 60 – 100 | −0.30 / +1.50 | −0.30 / +1.80 |
| > 100 – 150 | −0.30 / +2.10 | −0.30 / +2.50 |
Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.
Q390q Price Factors and How to Order
Price questions on Q390q usually come down to the extras in the table below.
| Cost driver | Effect on price |
|---|---|
| Strength level Q390q | Higher levels need more alloy and tighter rolling control |
| Quality letter | C < D < E; letter chosen on order |
| Delivery route | TMCP / TMCP+T |
| Thickness | Over 60 mm and under 10 mm carry size extras |
| Z15 / Z25 / Z35 | Low-sulfur heat, Z test, UT; Z35 costs most |
| Width and length | Over 3000 mm wide or 15 m long needs mill confirmation |
| Quantity per size | Mill minimums per heat and size |
| Inspection and processing | 3.2 witness, profile cutting, blasting, priming quoted per item |
To get a firm quote in one round, send:
- Grade, edition and Z level, e.g. Q390qDZ25 to GB/T 714-2025
- Thickness × width × length and pieces or tonnes
- Delivery route and UT class if beyond Class II
- Certificate type and inspector
- Destination port and Incoterm
We quote plate price, extras and freight line by line, so offers can be compared like for like.
Applications
| Sector | Typical Q390q components |
|---|---|
| Highway box girders | Webs and flanges where Q370q is just short of strength |
| Railway bridges | Truss chords and plate girders |
| Steel-concrete composite girders | Bottom flanges and webs |
| Arch and cable-stayed bridges | Secondary girders, cross beams |
| Retrofit | Strengthening plates matched to 390 MPa design values |
The C/D/E choice suits bridges from warm to cold climates, chosen by letter.
It is the wrong plate for pressure equipment (pressure vessel steel plates), unpainted exposure (weathering steel plates) or ship hulls (shipbuilding steel plates).
Supply Capability and Global Delivery
SHH STEEL sources Q390q from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.
- Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
- Tests: tensile, C/D/E Charpy, bend, Z test, UT, product analysis
- Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming
- Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
- Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247
Most of our Q390q goes to overseas bridge projects with Chinese designers or contractors; we also supply local fabricators abroad.
Lead time: about 30–45 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.
Why Choose SHH STEEL
Mill-direct, China origin: SHH STEEL is a steel manufacturer and exporter and global steel mill sourcing partner, and Q390q is one of the bridge grades we handle regularly.
Before shipment we check four lines on every Q390q certificate: yield and tensile for the actual thickness band, Charpy at the ordered letter, the CEV or Pcm for the delivery route, and UT results. If one fails, the plate does not ship as Q390q.
Because Q390q is new, check that your fabricator’s welding procedures and the owner’s specification already cover it. We can supply mill data on trial heats to support procedure qualification.
We also tell buyers when another grade fits better. Neighbouring levels are Q370qD and Q420qE. The weathering counterpart is Q390qNH. Browse more structural steel plates and high strength low alloy plates.
FAQ
-
What is Q390q steel?
- Q390q is a TMCP bridge steel grade added in GB/T 714-2025. It has 390 MPa minimum yield up to 50 mm, 520 MPa minimum tensile, 20% elongation, CEV ≤0.41% and 120 J Charpy impact for 12–100 mm plate in grade C (0°C), D (−20°C) or E (−40°C).
-
What is the difference between Q390qC, Q390qD and Q390qE?
- Only the impact test temperature and the P and S limits. C is tested at 0°C, D at −20°C and E at −40°C, all requiring 120 J for 12–100 mm plate. P/S caps are 0.030/0.025% for C, 0.025/0.015% for D and 0.020/0.010% for E.
-
Is Q390q the same as Q390D?
- No. Q390D is general structural steel (GB/T 1591), while Q390q is bridge steel to GB/T 714 with lower P and S, controlled weldability index, mandatory UT above 20 mm and 120 J impact for 12–100 mm plate. Bridge plate can replace general plate, not the reverse.
-
What is the ASTM or EN equivalent of Q390q?
- Close grades for Q390q: No equivalent listed in Annex B / closest: EN 10025-4 S420M (higher), ASTM A709 Grade 50. These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
-
Can GB/T 714 bridge plate be normalized?
- Only in one case. GB/T 714-2025 clause 6.2 requires TMCP, TMCP + tempering or quenched and tempered delivery, but Q345q and Q370q plate over 100 mm and up to 150 mm may be normalized by agreement.
-
Does steel grade affect fatigue life of a Q390q bridge girder?
- Very little. Fatigue life of welded bridge details is governed by the detail category and stress range, not by yield strength. Higher-strength plate raises working stress, so detailing and weld quality must improve to keep the same fatigue life.
Conclusion
Q390q to GB/T 714-2025 is the new TMCP bridge grade with 390 MPa yield, CEV ≤0.41% and 120 J Charpy in C, D or E grade.
It sits between Q370q (C, D, E) and Q420q (D, E, F) in the bridge range, filling the 390 MPa step that GB/T 714-2015 did not have. We check every Q390q order against GB/T 714-2025 before quoting, so the offer, the test plan and the certificate all match the drawing.
Our Q390q certificates carry heat chemistry, weldability index, tensile and Charpy data to EN 10204 3.1 or 3.2. SHH STEEL can add product analysis, Z15–Z35 and witness inspection.
We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other high strength low alloy plates.
Contact SHH STEEL with your Q390q requirements. We confirm the mill, delivery route, testing and price before you commit.