GB/T 714 Q460qNHF weathering bridge steel stacked at SHH STEEL warehouse

GB/T 714 Q460qNHF Weathering Bridge Steel Supplier

GB/T 714 Q460qNHF (Q460qFNH) is weathering bridge steel plate with 460 MPa minimum yield, 47 J Charpy at −60°C (12–100 mm), Cu-Cr-Ni chemistry and a weathering index I ≥6.0 for unpainted bridges. SHH STEEL supplies it mill-direct with Z15–Z35, UT and full heat and product analysis.
Keywords
Q460qNHF, Q460qNHF weathering steel, GB/T 714 Q460qNHF, Q460qFNH, Q460qFNH steel plate, Q460qNH, Q460qNHF weathering bridge steel, Q460qFNHZ15, Q460qFNHZ25, Q460qFNHZ35, bridge steel plate, Q460qNHF supplier
Equivalent Grades:
ASTM A709 HPS 70W (Annex B lists it against Q460q) / EN 10025-4 S460ML (not weathering) — Material Specification: GB/T 714-2025 (supersedes GB/T 714-2015) — Delivery: TMCP / TMCP+T
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Q460qNH Quality Grades
GB/T 714-2025 vs 2015
Q460qNHF vs ASTM A709 / EN 10025
Weathering Index and Unpainted Use
Welding and Fatigue
Z15 / Z25 / Z35
Equivalent Material Grades
Testing and Inspection
Dimensions
Tolerances
Price and Ordering
Applications
Supply Capability
Why Choose SHH STEEL
FAQ
Conclusion

What is GB/T 714 Q460qNHF Weathering Bridge Steel?

Q460qNHF is weathering bridge structural steel to GB/T 714. In the standard’s own notation it is written Q460qFNH: Q for yield, 460 for the minimum yield in MPa, q for qiao (bridge), the quality letter, and NH for nai hou, weathering. The letter F means Charpy V-notch testing at −60°C.

Q460qNH is high-strength weathering plate for unpainted main girders and truss chords. Q460qNH is the weathering grade closest to ASTM A709 HPS 70W, which Annex B of GB/T 714-2025 also maps to Q460q. Pcm is capped at 0.23% to 50 mm and 0.25% to 100 mm.

Q460qNHF (Q460qFNH) is 460 MPa weathering plate tested at −60°C (47 J over 12 mm). It is a special-order grade for fracture-critical unpainted members in very cold climates.

GB/T 714-2025, in force since 1 May 2026, fully replaces GB/T 714-2015; the changes for weathering grades are listed below.

SHH STEEL (Shanghai Shenghonghe Import & Export Co., Ltd.) is a steel manufacturer and exporter and global steel mill sourcing partner, mill-direct, China origin. We ship Q460qNHF cut to size with an EN 10204 3.1 or 3.2 certificate. Sister grades are listed under GB/T 714; other unpainted options are under weathering steel plates and EN 10025-5.

Material Specification

Specification element Requirement SHH STEEL compliance
Standard GB/T 714-2025 Q460qFNH Confirmed
Product Single-rolled plate ≤150 mm; hot-rolled strip and cut plate ≤25.4 mm Plate
Thickness with tensile values Up to 130 mm for Q460qNH Confirmed
Minimum yield ReL 460 MPa ≤50 mm; 450 MPa >50–100 mm Confirmed
Minimum tensile Rm 570 MPa ≤100 mm (no upper limit in the standard) Confirmed
Elongation A ≥ 18% Confirmed
Charpy V-notch −60°C, 47 J (12–100 mm), longitudinal Confirmed
Weathering index I ≥ 6.0 (Table 5, footnote c) Calculated on MTC
Delivery condition TMCP or TMCP + tempering As ordered
Weldability index Pcm (Table 8) Printed on MTC
Ultrasonic testing Plate >20 mm: GB/T 2970, Class II or better Every plate
Through-thickness Z15, Z25 or Z35 to GB/T 5313, when ordered As ordered
Dimensions GB/T 709 Confirmed
Certificate GB/T 247; EN 10204 3.1 or 3.2 As ordered

Grades often compared with Q460qNHF are ASTM A709 HPS 70W and EN 10025-4 S460ML; the comparison below shows where they differ.

Chemical Composition: Heat Analysis and Product Analysis

Chemistry for Q460qNHF is fixed at the ladle, but it is verified on plate. GB/T 714 sets the ladle (heat) limits; GB/T 222 sets how far a finished-plate analysis may stray from them.

Table 1 below is the heat (ladle) analysis for Q460qNHF from GB/T 714-2025 Tables 1, 5.

Element Q460qNHF heat analysis (%) Note
C, max 0.11
Si 0.15 – 0.50 Counts in I
Mn 1.10 – 1.50 Min 0.50% for coil only
P, max 0.015 Letter F
S, max 0.006 Letter F
Cu 0.25 – 0.50 Main weathering element
Cr 0.40 – 0.70 Weathering element
Ni 0.30 – 0.40 Weathering element
Mo, max 0.20
Nb 0.010 – 0.100 Microalloy (see note)
V 0.010 – 0.100 Microalloy (see note)
Ti 0.006 – 0.030 Microalloy (see note)
Als 0.015 – 0.050 Alt 0.020–0.055% if total Al is used
N, max 0.0080
B, max (residual) 0.0005 ≤0.0014% if C ≤0.06%
H, max (residual) 0.0002
Weathering index I ≥ 6.0 Calculated from heat analysis

Nb, V, Ti and Al may be added singly or together. Added singly, each must meet the range above; added together, at least one must reach its minimum and Nb + V + Ti ≤ 0.22%. Calcium treatment is required to control sulfide shape.

Table 2 is the product analysis: the limits a check analysis on finished plate is judged against. GB/T 714-2025 clause 7.1.3 calls up GB/T 222 for the permitted deviations.

Element Heat limit (%) Deviation, GB/T 222-2025 Table 1 Q460qNHF product analysis (%)
C ≤ 0.11 +0.02 ≤ 0.13
Si 0.15 – 0.50 ±0.05 0.10 – 0.55
Mn 1.10 – 1.50 ±0.06 1.04 – 1.56
P ≤ 0.015 +0.005 ≤ 0.020
S ≤ 0.006 +0.005 ≤ 0.011
V 0.010 – 0.100 +0.02 / −0.01 ≤ 0.120
Ti 0.006 – 0.030 +0.02 / −0.01 ≤ 0.050
Nb 0.010 – 0.100 ±0.005 (listed for 0.015–0.060%) Above 0.060%: agree in contract
Cu 0.25 – 0.50 ±0.05 0.20 – 0.55
Cr 0.40 – 0.70 ±0.05 0.35 – 0.75
Ni 0.30 – 0.40 ±0.05 0.25 – 0.45
Als 0.015 – 0.050 ±0.003 Lower limit −0.003 (Table 1 row is for Al ≥0.015%; confirm)
Mo ≤ 0.20 Not listed in Table 1 Agree in contract
N ≤ 0.0080 Listed only for 0.010–0.020% Agree in contract

How to read Table 2. Weathering bridge steel is normally classed as low-alloy steel, so Table 1 of GB/T 222 applies. Where the heat limit is a range, the deviation applies to both ends; for one heat, an element may deviate in one direction only.

Mechanical Properties

Tensile values follow Table 9 of GB/T 714-2025 for Q460qNH. Tensile specimens are transverse; round specimens are used above 40 mm. Where yield is not distinct, Rp0.2 replaces ReL.

Nominal thickness ReL min (MPa) Rm min (MPa) A min
≤ 50 mm 460 570 18%
> 50 – 100 mm 450 570 18%
> 100 – 130 mm 385 490 18%

Impact values follow Table 10, on longitudinal specimens, average of three:

Letter / test temperature KV2 ≤12 mm KV2 >12 – 100 mm KV2 >100 – 150 mm
F / −60°C By agreement 47 J Not applicable

One single value may fall below the required average, but not below 70% of it. Plate over 8 mm and under 12 mm is tested with 7.5 mm specimens (75% of the value); 6–8 mm plate with 5 mm specimens (50%). Plate under 6 mm is not impact tested.

180° bend test, transverse: mandrel D = 2a up to 16 mm and 3a above 16 mm; may be omitted when the mill guarantees it. Yield ratio is not mandatory. If the contract asks for it, Annex C recommends ReL/Rm ≤ 0.88 up to 12 mm and ≤ 0.86 above 12 mm for TMCP plate.

Q460qNHD / Q460qNHE / Q460qNHF: Which Quality Grade?

Q460qNHF is tested at −60°C. It suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members. F is the coldest letter in GB/T 714: Charpy at −60°C, P ≤0.015% and S ≤0.006%. It exists only for Q420q and above (and their NH versions), and its energy rises with strength.

Grade Test temp. KV2 ≤12 mm KV2 12–100 mm KV2 >100 mm P / S max (%)
Q460qNHD −20°C 80 J 120 J 47 J 0.025 / 0.015
Q460qNHE −40°C 80 J 120 J 31 J 0.020 / 0.010
Q460qNHF −60°C By agreement 47 J — 0.015 / 0.006

Note that F energy at Q460q is 47 J, not 120 J: the colder test uses a lower energy that GB/T 714-2025 raises with strength, from 47 J at Q420q/Q460q to 77 J at Q690q. Plate up to 12 mm needs an agreed value.

Q460qNHF: What Changed from GB/T 714-2015 to GB/T 714-2025

For Q460qNHF buyers the 2025 edition changes more than the year on the certificate. The points below come from the foreword of GB/T 714-2025 and its tables.

  • The weathering requirement changed: Table 5 now requires a corrosion index I ≥ 6.0, and the 2015 Annex C guide for assessing weathering resistance was deleted.
  • A Pcm table for weathering steel (Table 8) was added.
  • Annex A now gives reference bridge-site environments for unpainted use (chloride, SO₂ and time-of-wetness limits).
  • Yield values above 100 mm were added for Q460qNH (385 MPa for >100–130 mm).
  • Tensile strength is now banded by thickness (e.g. lower minimum Rm above 100 mm) instead of one value.
  • Impact energy is set by thickness band (≤12 mm, 12–100 mm, >100 mm) in Table 10.
  • Yield ratio is no longer a clause value; it is agreed in the contract, with recommendations in informative Annex C.

If a drawing cites 2015 and the plate is made to 2025, get the designer’s written acceptance; tensile strength above 100 mm and the yield-ratio basis differ.

Q460qNHF vs ASTM A709 and EN 10025: Which Grade Matches?

Can Q460qNHF replace a US or European bridge grade, or the other way round? Strength can match; toughness rules differ in kind, not only in number.

Property Q460qNHF ASTM A709 HPS 70W EN 10025-4 S460ML
Min. yield (MPa) 460 (≤50 mm) 485 460 (≤16 mm)
Tensile (MPa) 570 min 585 – 760 540 – 720
Charpy 47 J at −60°C (12–100 mm) CVN by temperature zone; fracture-critical (F) levels 27 J at −50°C
Weathering chemistry Yes, I ≥ 6.0 Yes No

ASTM A709 sets Charpy requirements by temperature zone (1, 2, 3) and by member type: non-fracture-critical (T) or fracture-critical (F). GB/T 714 sets one value per letter, so compare the A709 zone with the GB/T 714 test temperature, not grade with grade.

EN 10025-5 weathering grades are general structural steels without a bridge-specific toughness level of 120 J; they suit many bridges but are not a one-to-one match.

At −60°C, the 47 J required for Q460qNHF is a demanding figure; general structural grades rarely prove any toughness that cold. For the C, D and E letters GB/T 714 asks 120 J, several times the 27–40 J typical of GB/T 1591 plate.

Q460qNHF Atmospheric Corrosion Index I and Unpainted Bridges

GB/T 714-2025 Table 5, footnote c, requires every Q460qNHF heat to reach an atmospheric corrosion index I of at least 6.0, calculated from the heat analysis:

I = 26.01(%Cu) + 3.88(%Ni) + 1.20(%Cr) + 1.49(%Si) + 17.28(%P) − 7.29(%Cu)(%Ni) − 9.10(%Ni)(%P) − 33.39(%Cu)²

This is the same predictive formula used with ASTM G101 for ASTM A709 Grade 50W and ASTM A709 HPS 70W, which makes Chinese and US ASTM A709 weathering steel plates easy to compare with Q460qNHF.

Worked example (our calculation) Cu Ni Cr Si P I
All weathering elements at their Table 5 minimum 0.25 0.30 0.40 0.15 0.010 5.88
Illustrative mid-range heat 0.32 0.36 0.55 0.30 0.012 6.74

Note the first row: a heat that only just meets every Table 5 minimum can still fall short of I = 6.0. That is why we ask the mill to print I on every Q460qNHF certificate, not just the chemistry.

Where can the steel be left unpainted? Annex A of GB/T 714-2025 gives reference bridge-site conditions:

  • Rural or urban atmosphere with annual chloride deposition ≤ 3 mg/(m²·d)
  • Annual SO₂ deposition ≤ 24 mg/(m²·d)
  • Time of wetness ≤ 5,256 h per year (temperature above 0°C and relative humidity above 80%)
  • Coastal sites only if they meet the same limits; for marine atmospheres Annex D points to T/CISA 073

Owners choose Q460qNHF to avoid repainting for decades. That only works if the site matches Annex A and the details shed water. Where the site is borderline, paint the girder ends and leave the rest bare.

Welding Q460qNHF and Fatigue in Bridge Girders

GB/T 714-2025 clause 7.1.2 uses CEV for normalized, QT and TMCP steel with C >0.12%, and Pcm for weathering steel and TMCP steel with C ≤0.12%, both from the heat analysis:

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Pcm = C + Si/30 + Mn/20 + Cu/20 + Ni/60 + Cr/20 + Mo/15 + V/10 + 5B

Index ≤50 mm >50–100 mm >100–130 mm
Pcm, Q460qNH (Table 8) ≤ 0.23 ≤ 0.25 By agreement

The index caps in GB/T 714 are maximums. Real Q460qNHF heats often sit well below them, and preheat should be set from the actual value, not the cap. At −60°C, both weld metal and HAZ must prove toughness. Expect lower heat input, more passes and consumables qualified at −60°C.

Typical consumables for Q460qNHF: weathering-matched Ni-Cu consumables (AWS E8018-W2 type for 345–420 MPa), with higher-strength weathering wires for 460–500 MPa.

Fatigue. Welded details govern fatigue life in a bridge, and their fatigue strength is set by detail category, not by yield strength. Higher-strength plate can carry higher stress ranges only if detailing improves too.

Fatigue design follows JTG D64 (highway) and TB 10091 (railway) in China, EN 1993-1-9 in Europe and AASHTO LRFD in the US; fabrication commonly follows TB 10212, JTG/T 3650 or AWS D1.5.

Q460qFNHZ15, Z25 and Z35: Through-Thickness Plate for Bridges

Lamellar tearing appears in thick plate loaded across its thickness, typically at cruciform joints and anchor plates. A Z grade adds a short-transverse tensile test and a lower sulfur cap.

GB/T 714 adds the Z level to the end of the designation, for example Q460qFNHZ25. The test and acceptance follow GB/T 5313 and apply to plate 15 mm and thicker.

Z grade Heat sulfur, max (%) Reduction of area, avg / single (%)
Z15 0.010 15 / 10
Z25 0.007 25 / 15
Z35 0.005 35 / 25

F chemistry limits S to 0.006%, which already meets the Z25 sulfur cap (0.007%). Only Z35 (S ≤0.005%) needs a further step.

A Z level on Q460qNHF does not change strength or impact rules. It adds a sulfur cap and a short-transverse tensile test. Z options apply across the GB/T 714 bridge steel range.

Equivalent Material Grades

Annex B of GB/T 714-2025 lists foreign grades against each strength level. It is informative: it tells you which families are close, not that the plates are interchangeable.

Standard Grade(s) Fit for Q460qNHF
ASTM A709 ASTM A709 HPS 70W Listed against Q460q in Annex B
EN 10025-4 EN 10025-4 S460ML Strength match, not weathering
EN 10025-6 EN 10025-6 S460QL QT, not weathering
GB/T 714 (painted twin) Q460qF Same strength, no weathering elements

For weathering grades also compare the corrosion index basis. Q460qNHF requires I ≥ 6.0 by the formula above; check that the substitute is assessed on the same basis.

Q460qNHF Testing, UT and Certificate

A batch of Q460qNHF is one grade, one heat, one thickness, one rolling schedule and one heat-treatment condition, up to 60 t. Table 12 of GB/T 714-2025 sets the tests:

Test Frequency Method
Heat analysis 1 per heat GB/T 20066; GB/T 4336 / GB/T 223
Weathering index I Calculated per heat Table 5 formula
Tensile 1 per batch GB/T 2975 / GB/T 228.1
Bend 180° 1 per batch (may be waived if guaranteed) GB/T 232
Charpy V at −60°C 3 specimens per batch GB/T 229
Through-thickness (Z) 3 specimens per batch, when ordered GB/T 5313
Ultrasonic Every plate >20 mm, Class II or better GB/T 2970
Surface and dimensions Every plate Visual and gauges

Impact retest: if a set fails, three more specimens are taken from the same batch. The average of all six must meet the requirement; two values may be below it, but only one below 70%. At −60°C, mills may need trial heats before the production run; we agree the test plan before accepting the order.

Dimensions

Size range for Q460qNHF plate:

  • Thickness: 6 mm – 130 mm under GB/T 714 tensile tables; most orders 10 – 80 mm
  • Width: 1500 – 4000 mm, depending on mill and thickness
  • Length: 6000 – 18000 mm; longer by enquiry
  • Edge: mill edge or cut edge
  • Weight: theoretical, 7.85 g/cm³

Deck plate, webs, flanges, diaphragms and stiffeners are cut to drawing. For U-ribs and rolled sections on the same bridge, see steel beam profiles and steel structural profiles.

Tolerances

GB/T 714-2025 clause 7.6 sends dimensions and shape to GB/T 709. Thickness tolerance is Class B by default: −0.30 mm fixed, plus side by thickness and width.

Nominal thickness (mm) Width ≤ 1500 mm Width > 1500 – 2500 mm
> 8 – 15 −0.30 / +0.80 −0.30 / +1.00
> 15 – 25 −0.30 / +1.00 −0.30 / +1.20
> 25 – 40 −0.30 / +1.10 −0.30 / +1.30
> 40 – 60 −0.30 / +1.30 −0.30 / +1.50
> 60 – 100 −0.30 / +1.50 −0.30 / +1.80
> 100 – 150 −0.30 / +2.10 −0.30 / +2.50

Bridge fabricators often ask for Class C (zero minus) on deck and flange plate so section properties are never under the design value. Wider plates follow the heavier GB/T 709 rows; we state them on the offer.

Q460qNHF Price Factors and How to Order

For Q460qNHF, the base price follows the market; grade, letter, size and testing extras decide the rest.

Cost driver Effect on price
Strength level Q460q Higher levels need more alloy and tighter rolling control
Quality letter Highest extra: −60°C testing, S ≤0.006%, limited mills
Weathering alloys Cu, Cr, Ni additions and I-index control add a weathering extra
Delivery route TMCP / TMCP+T
Thickness Over 60 mm and under 10 mm carry size extras
Z15 / Z25 / Z35 Low-sulfur heat, Z test, UT; Z35 costs most
Width and length Over 3000 mm wide or 15 m long needs mill confirmation
Quantity per size Mill minimums per heat and size
Inspection and processing 3.2 witness, profile cutting, blasting, priming quoted per item

To get a firm quote in one round, send:

  • Grade, edition and Z level, e.g. Q460qFNHZ25 to GB/T 714-2025
  • Thickness × width × length and pieces or tonnes
  • Delivery route and UT class if beyond Class II
  • Certificate type and inspector
  • Destination port and Incoterm

We quote plate price, extras and freight line by line. Need another letter? See Q460qNHD, Q460qNHE.

Applications

Sector Typical Q460qNHF components
Unpainted highway bridges Plate girders and box girders in rural and urban atmospheres
Railway bridges Truss members, plate girders, bracing
Remote and mountain sites Bridges where repainting access is difficult or costly
Urban viaducts Exposed girders with architectural rust finish
Pedestrian bridges Unpainted box sections

The letter F suits Arctic and sub-Arctic bridges, high-latitude rail lines and owners who want the largest toughness margin for fracture-critical members.

Q460qNHF is the wrong plate for marine splash zones, tunnels, sites with heavy de-icing salt spray, or members that stay wet. There, use painted Q460qF or look at marine-atmosphere grades under T/CISA 073.

Supply Capability and Global Delivery

SHH STEEL sources Q460qNHF from first-line bridge-plate mills, including drafters of GB/T 714-2025 such as Ansteel, Valin Xiangtan, Jiangyin Xingcheng, Wuyang, Shougang and Xinyu.

  • Certificates: EN 10204 3.1 standard; 3.2 with third-party witness (SGS, BV, TÜV or owner’s inspector)
  • Tests: tensile, −60°C Charpy, bend, Z test, UT, product analysis, weathering index
  • Processing: CNC plasma and flame cutting, bevelling, drilling, shot blasting and priming (or blasting only, for unpainted weathering steel)
  • Terms: FOB Shanghai, CFR, CIF; TT, LC or TT + LC
  • Marking: steel-stamped and paint-marked with grade, heat, size and mill, per GB/T 247

Our Q460qNHF exports follow Chinese bridge design abroad: railway and highway bridges built by EPC contractors in Asia, Africa and Latin America.

Lead time: about 45–60 days from mill rolling; Z35, F letter or 3.2 inspection adds about 1–2 weeks. Sea time from Shanghai is about 7–12 days to Southeast Asia and 28–35 days to North Europe.

Why Choose SHH STEEL

SHH STEEL works mill-direct as a steel manufacturer and exporter and global steel mill sourcing partner, China origin. Every Q460qNHF plate is traced to its heat.

Before shipment we check four lines on every Q460qNHF certificate: yield and tensile for the actual thickness band, Charpy at −60°C, the Pcm and weathering index, and UT results. If one fails, the plate does not ship as Q460qNHF.

Q460qNHF is a mill campaign item; we combine sizes into one heat where possible to keep cost and lead time under control.

We also tell buyers when another grade fits better. Neighbouring levels are Q420qNHF and Q500qNHF. The painted counterpart is Q460qF. Browse more structural steel plates and high strength low alloy plates.

FAQ

What is Q460qNHF steel?
Q460qNHF (Q460qFNH) is weathering bridge steel plate to GB/T 714-2025. It has 460 MPa minimum yield up to 50 mm, 570 MPa minimum tensile, Charpy impact of 47 J at −60°C for 12–100 mm plate, and Cu-Cr-Ni chemistry with a corrosion index I of at least 6.0 for unpainted bridges.
What impact energy does Q460qNHF need at −60°C?
GB/T 714-2025 requires at least 47 J at −60°C on longitudinal specimens for Q460qNHF plate over 12 mm and up to 100 mm. For plate 12 mm and thinner the value is by agreement. F energy rises with strength: 47 J for Q420q and Q460q, 54 J for Q500q, 60 J for Q550q, 69 J for Q620q and 77 J for Q690q.
What is the maximum thickness of Q460qNHF?
GB/T 714-2025 covers bridge plate up to 150 mm, but tensile values for Q460qNH stop at 130 mm. Above that there is no table value, so Q460qNHF cannot be certified thicker than 130 mm without a special agreement.
What is the ASTM or EN equivalent of Q460qNHF?
Close grades for Q460qNHF: ASTM A709 HPS 70W (Annex B lists it against Q460q) / EN 10025-4 S460ML (not weathering). These are close families, not drop-in substitutes; compare yield at thickness, impact temperature and energy, and the weldability index before substituting.
What does the q mean in GB/T 714 bridge steel grades?
The lowercase q stands for qiao, Chinese for bridge. In a grade such as Q420qD, Q means yield, 420 is the minimum yield in MPa, q marks bridge steel to GB/T 714 and D is the quality letter (−20°C Charpy). NH after the letter, as in Q420qDNH, marks weathering steel.
What welding consumables are used for Q460qNHF?
Use low-hydrogen consumables that match both strength and weathering behaviour, typically Ni-Cu bearing electrodes and wires (AWS E8018-W2 type at 345–420 MPa). Exposed weld metal must weather like the plate, or it will corrode faster.

Conclusion

Q460qNHF to GB/T 714 is weathering bridge steel with 460 MPa minimum yield, Cu-Cr-Ni chemistry, a weathering index of at least 6.0 and 47 J Charpy at −60°C for 12–100 mm plate.

It sits between Q420qNHF and Q500qNHF in the weathering range, with Q460qNHD and Q460qNHE as sister letters. We check every Q460qNHF order against GB/T 714-2025 before quoting, so the offer, the test plan and the certificate all match the drawing.

From SHH STEEL, Q460qNHF arrives with traceable heat numbers, a complete EN 10204 3.1 or 3.2 certificate and, if ordered, third-party witness, product analysis and Z testing.

We ship from Shanghai to bridge builders worldwide. Browse the full GB/T 714 range or other weathering steel plates.

Send the edition, quality letter, Z level and size list; we confirm mill, delivery route, lead time and price in one reply. Contact SHH STEEL for a mill-direct quotation on Q460qNHF weathering bridge steel.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X